AAA. V. Antonova

A. V. Antonova

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


A. V. Antonova has a total of 16 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Study of Conditions for Obtaining Precursors from Heat-Resistant NiAl-Based Alloy Intended for 3D Technologies

    by A. A. Drozdov, K. B. Povarova, A. V. Samokhin, O. A. Skachkov, A. A. Fadeev, A. A. Dorofeev, V. P. Sirotinkin, A. A. Ashmarin, A. V. Antonova, M. A. Bulakhtina, et al.

    —This article is the second in a series of articles devoted to studying the possibilities of preparing high-quality powder materials from heat-resistant light alloys based on refractory monoaluminides of nickel (β-NiAl), ruthenium (β-RuAl) and the FeCrAl system (fechrals) for the production of compact samples/products of complex shapes using additive technologies with minimal final machining. Additive technologies are based on the use of spherical precursor micropowders with a regulated granulometric composition, good fluidity, and an oxide-free surface. In the first article, the possibilities of obtaining precursors from RuAl-based alloys by plasma spheroidization of powders obtained by crushing mixtures from scrap samples of RuAl-based alloys with various additives were considered. This article examines the possibility of obtaining precursors from NiAl-based alloys by plasma spheroidization of powders obtained by crushing mixtures from scrap samples of NiAl-based alloys with various additives. It has been shown that grinding and subsequent grinding of scrap powders in an attritor makes it possible to obtain precursors using the “attrition + plasma spheroidization” scheme with characteristics that make them suitable for additive manufacturing (perfectly round shape, surface almost free of oxides, phase composition—solid solution grains on based on NiAl with thin layers of Ni3Al of nanosized thickness). The nonuniform distribution of alloying elements in NiAl grains is caused by the short duration (5 h) of grinding the initial powders of scrap ingots of various compositions obtained using foundry technology. This can be corrected by increasing the grinding duration to 15 h, which will require the use of the “attrition + granulation + plasma spheroidization” scheme, since the proportion of dispersed powders that must be included in circulation will increase. It has been shown that preliminary reaction alloying in the liquid phase (vacuum arc melting), including the use of recycled materials (scrap alloy samples) as starting materials, allows one to vary the alloy compositions over a wide range, using small volumes of material, and does not require specialized equipment.

  • Intermetallic Alloys Based on γ'Ni3Al: Part I. Features of the Structure, Formation of (γ' + γ) Structures, and Alloying

    by A. A. Drozdov, K. B. Povarova, O. A. Bazyleva, A. V. Antonova, M. A. Bulakhtina, N. A. Alad’EV, A. E. Morozov, I. S. Pavlov

    γ'Ni3Al-based casting alloys have a lower density, higher melting point and resistance to oxidation, and a higher ceiling of operating temperatures than modern heat-resistant nickel alloys. The article discusses the features of the electronic structure and crystallization of domestic (such as VKNA/VIN) and the most advanced foreign (γ' + γ) low-alloyed γ'Ni3Al-based alloys (IC type), and experimental data on the nature of the structures formed during directional crystallization of alloys with different types of alloying and on the nature of the distribution of components in the γ'Ni3Al and γNi phases and structural components in the cellular-dendritic structure of single crystals with 〈111〉 and 〈001〉 crystallographic orientation are presented. The influence of heat treatment on the microstructure, distribution of alloying elements, and mechanical properties of the VKNA type alloys is investigated in a wide range of temperature–time parameters. A comparative analysis of the effect of temperature and duration of heat treatment and cooling rate after heat treatment on the heat resistance of alloys showed that, unlike other Ni3Al-based alloys, for single crystals from the VKNA type economically alloyed alloys and parts made from them (uncooled working blades of aviation gas turbine engines, nozzle apparatuses, jet nozzle spacers, and other parts of the hot path of gas turbine engines), a short-term heat treatment (1150°C/1 h) is necessary and sufficient to relieve casting stresses. The alloys demonstrate high heat resistance at 1100–1200°C and the ability to withstand short-term casting temperatures up to 1250–1300°C.


  • Heat-Resistant RuAl-Based Alloys: III. Powder Alloys—Mechanical Alloying

    by K. B. Povarova, A. E. Morozov, A. A. Drozdov, A. V. Antonova, M. A. Bulakhtina

    Refractory (melting point Tm = 2100°C), heat-resistant ruthenium monoaluminide RuAl, lighter (ρ = 7.97 g/cm3) than Ni superalloys, is considered as a promising material for operation at a high temperature and under relatively low loads in high-velocity gas oxidizing flows. This alloy can be used not only at a temperature higher than operating temperature tw inherent in both nickel superalloys and nickel and titanium aluminides, but also at a temperature higher than the melting point of the latter. RuAl is also an ideal candidate for potential use in protective coatings. In the first part of the paper, RuAl-based cast alloys have been considered. In the second part of the paper, the potentialities of obtaining alloys based on RuAl directly from the initial powders of ruthenium and aluminum by combining the temperature–time modes of reactive alloying (RA), as well as the sequence and intensity of pressure application in the course of RA, are considered. The third part of the paper is devoted to studying the potentialities of powders doped with RuAl (NiAl, TiAl) with a preset composition obtained by means of mechanical alloying used as a starting material.


  • Heat-Resistant RuAl-Based Alloys: Part II. Powder Alloys—Preparation via Reaction Sintering

    by K. B. Povarova, A. E. Morozov, A. A. Drozdov, A. V. Antonova, M. A. Bulakhtina

    Refractory (Tm = 2100°C), heat-resistant ruthenium monoaluminide RuAl, is lighter (ρ = 7.97 g/cm3) than Ni superalloys, is considered a promising candidate material for operation in a high-temperature range and at relatively low loads within high-speed oxidizing gas flows at a temperature higher not only than operating temperature Top but also higher than the melting point Tm inherent both in nickel superalloys and in nickel and titanium aluminides. Ruthenium aluminide RuAl is an ideal candidate for potential use in protective coatings too. In the second part of the paper, we have considered the possibilities for obtaining alloys based on RuAl directly from the initial ruthenium and aluminum powders via combining the temperature–time modes of the reaction sintering (RS), as well as the sequence and intensity of pressure application under RS. In this case, no specialized equipment is required for obtaining initial powders with a given composition, and no restrictions are imposed on the particle size distribution in the initial powders.