Loïc Coulomb
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Loïc Coulomb has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- Mickaël Beaudhuin
ICGM, Univ. Montpellier, CNRS, ENSCM
4 shared publications - Romain Viennois
ICGM, Univ. Montpellier, CNRS, ENSCM
3 shared publications - Benjamin Villeroy
Université Paris Est Créteil, CNRS, ICMPE, UMR 7182, 2 rue Henri Dunant, 94320 Thiais, France
2 shared publications - Claude Estournès
CIRIMAT, Université de Toulouse, Toulouse INP, CNRS, 118 Route de Narbonne, CEDEX 9, 31062 Toulouse, France
2 shared publications - Adrien Moll
Université Paris-Saclay, UMR8182 CNRS, Institut de Chimie Moléculaire et des Matériaux d’Orsay
1 shared publication - Adrien Moll
ICMMO (UMR CNRS 8182), University of Paris-Saclay, Gif sur Yvette, France
1 shared publication
Latest Publications
- Open Access
Lattice Dynamics, Transport and Thermoelectric Properties of Bi-Sb Alloys Obtained by Mechanical Alloying and Spark Plasma Sintering
We report on the successful synthesis of Bi1−xSbx alloys via mechanical alloying followed by sintering via spark plasma sintering, and the study of their lattice dynamics by Raman spectroscopy as well as their transport and thermoelectric properties. We observed an upshift of the frequency of the Raman-active Eg vibrational mode with increasing Sb content but no significant change for the frequency of the Raman-active A1g vibrational mode. Conversely, the linewidth of the Eg vibrational mode did not change significantly with increasing Sb content, whereas a twofold increase was observed for the A1g vibrational mode. Moreover, we confirm the emergence of several new vibrational modes with Sb alloying that could be associated with Bi-Sb and Sb-Sb vibrations. Rather large magnetoresistance was observed for all samples at room temperature. From the Seebeck coefficients, we determined the energy bandgaps in our samples, which are larger than those in bulk compounds, presumably due to the electronic confinement effect. We report a rather large thermoelectric power factor of 2–3 mW/m.K2 and thermoelectric figure of merit ZT of 0.15–0.23 at room temperature. However, ZT values were not improved at room temperature compared to prior works because of the rather large thermal conductivity of 3.75–4.5 W/m.K at room temperature. We find a larger resistivity, Seebeck coefficient, and power factor for the samples sintered at 200 °C for 5 min than for the samples sintered at 220 °C for 15 min, but similar thermal conductivity, resulting in larger ZT for the samples obtained in the first conditions. The samples with low Sb content x = 0.05 have a lower power factor and larger thermal conductivity than the samples with x = 0.12 and x = 0.15 for the same sintering conditions, which results in lower ZT for x = 0.05.
Open AccessLattice Dynamics, Transport and Thermoelectric Properties of Bi-Sb Alloys Obtained by Mechanical Alloying and Spark Plasma Sintering
We report on the successful synthesis of Bi1−xSbx alloys via mechanical alloying followed by sintering via spark plasma sintering, and the study of their lattice dynamics by Raman spectroscopy as well as their transport and thermoelectric properties. We observed an upshift of the frequency of the Raman-active Eg vibrational mode with increasing Sb content but no significant change for the frequency of the Raman-active A1g vibrational mode. Conversely, the linewidth of the Eg vibrational mode did not change significantly with increasing Sb content, whereas a twofold increase was observed for the A1g vibrational mode. Moreover, we confirm the emergence of several new vibrational modes with Sb alloying that could be associated with Bi-Sb and Sb-Sb vibrations. Rather large magnetoresistance was observed for all samples at room temperature. From the Seebeck coefficients, we determined the energy bandgaps in our samples, which are larger than those in bulk compounds, presumably due to the electronic confinement effect. We report a rather large thermoelectric power factor of 2–3 mW/m.K2 and thermoelectric figure of merit ZT of 0.15–0.23 at room temperature. However, ZT values were not improved at room temperature compared to prior works because of the rather large thermal conductivity of 3.75–4.5 W/m.K at room temperature. We find a larger resistivity, Seebeck coefficient, and power factor for the samples sintered at 200 °C for 5 min than for the samples sintered at 220 °C for 15 min, but similar thermal conductivity, resulting in larger ZT for the samples obtained in the first conditions. The samples with low Sb content x = 0.05 have a lower power factor and larger thermal conductivity than the samples with x = 0.12 and x = 0.15 for the same sintering conditions, which results in lower ZT for x = 0.05.
- 25 August 2023
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 968
Impact of the nanostructuring on the thermal and thermoelectric properties of α-SrSi2
- 25 August 2023
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 968
Impact of the nanostructuring on the thermal and thermoelectric properties of α-SrSi2
- Open Access
Reactive Spark Plasma Sintering and Thermoelectric Properties of Zintl Semiconducting Ca14Si19 Compound
We present a new reactive spark plasma sintering (RSPS) technique for synthesizing the rhombohedral CaSi phase. The RSPS approach reduces the synthesis time from several weeks to a few minutes. The RSPS was found to be sufficient for obtaining a high level of purity of the CaSi under a pressure of 100 MPa for a dwell period of 5 min at a temperature of 900 C. From electrical resistivity measurements, we were able to determine the energy band gap of CaSi to eV. The Seebeck coefficient shows CaSi as a p-type semiconductor at room temperature. It becomes n-type with increasing temperature pointing to significant bipolar and conduction band contributions due to the narrow bandgap of the compound.Open AccessReactive Spark Plasma Sintering and Thermoelectric Properties of Zintl Semiconducting Ca14Si19 Compound
We present a new reactive spark plasma sintering (RSPS) technique for synthesizing the rhombohedral CaSi phase. The RSPS approach reduces the synthesis time from several weeks to a few minutes. The RSPS was found to be sufficient for obtaining a high level of purity of the CaSi under a pressure of 100 MPa for a dwell period of 5 min at a temperature of 900 C. From electrical resistivity measurements, we were able to determine the energy band gap of CaSi to eV. The Seebeck coefficient shows CaSi as a p-type semiconductor at room temperature. It becomes n-type with increasing temperature pointing to significant bipolar and conduction band contributions due to the narrow bandgap of the compound. - Open Access
- 26 October 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (11) , 2852
Effect of Nanostructuring on the Thermoelectric Properties of β-FeSi2
Nanostructured β-FeSi2 and β-Fe0.95Co0.05Si2 specimens with a relative density of up to 95% were synthesized by combining a top-down approach and spark plasma sintering. The thermoelectric properties of a 50 nm crystallite size β-FeSi2 sample were compared to those of an annealed one, and for the former a strong decrease in lattice thermal conductivity and an upshift of the maximum Seebeck’s coefficient were shown, resulting in an improvement of the figure of merit by a factor of 1.7 at 670 K. For β-Fe0.95Co0.05Si2, one observes that the figure of merit is increased by a factor of 1.2 at 723 K between long time annealed and nanostructured samples mainly due to an increase in the phonon scattering and an increase in the point defects. This results in both a decrease in the thermal conductivity to 3.95 W/mK at 330 K and an increase in the power factor to 0.63 mW/mK2 at 723 K.
- 26 October 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (11) , 2852
Open AccessEffect of Nanostructuring on the Thermoelectric Properties of β-FeSi2
Nanostructured β-FeSi2 and β-Fe0.95Co0.05Si2 specimens with a relative density of up to 95% were synthesized by combining a top-down approach and spark plasma sintering. The thermoelectric properties of a 50 nm crystallite size β-FeSi2 sample were compared to those of an annealed one, and for the former a strong decrease in lattice thermal conductivity and an upshift of the maximum Seebeck’s coefficient were shown, resulting in an improvement of the figure of merit by a factor of 1.7 at 670 K. For β-Fe0.95Co0.05Si2, one observes that the figure of merit is increased by a factor of 1.2 at 723 K between long time annealed and nanostructured samples mainly due to an increase in the phonon scattering and an increase in the point defects. This results in both a decrease in the thermal conductivity to 3.95 W/mK at 330 K and an increase in the power factor to 0.63 mW/mK2 at 723 K.