Nicolas Guillaume
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Nicolas Guillaume has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Ahmad Bsiesy
CNRS, CEA/LETI-Minatec, Grenoble INP, LTM, Université Grenoble Alpes 1 , Grenoble 38054
2 shared publications - Christelle Charpin-Nicolle
LETI, Univ. Grenoble Alpes, CEA, Leti 2 , F-38000 Grenoble, France
2 shared publications Etienne Nowak
LETI, Univ. Grenoble Alpes, CEA, Leti 2 , F-38000 Grenoble, France
2 shared publications- Evgeniy V. Skopin
CNRS, CEA/LETI-Minatec, Grenoble INP, LTM, Université Grenoble Alpes 1 , Grenoble 38054
2 shared publications - Gauthier Lefevre
Univ. Grenoble Alpes, CEA, Liten 3 , Grenoble F-38000
2 shared publications - Liliane Alrifai
CEA, LETI, Universit Grenoble Alpes, Grenoble, France
2 shared publications
Latest Publications
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Vers la réalisation de composants nanoélectroniques par anodisation localisée par AFM
Ce travail de thèse se compose de deux parties : tout d’abord nous avons caractérisé sur le plan morphologique des motifs de TiOx réalisés par anodisation localisée par AFM (LAO) dans des couches pleines plaques de 5 nm de titane. Nous avons étudié l’influence de la tension d’oxydation, de la vitesse de balayage de la pointe AFM, de l’humidité relative de l’environnement, du mode AFM (contact ou intermittent) et du type de pointe. Les motifs les plus fins atteignent une largeur à mi-hauteur de 21 nm pour 2.2 nm de hauteur, ils sont obtenus avec une pointe PtSi utilisée en mode intermittent sous une tension de polarisation de -7V, une vitesse de balayage de 0.4 µm.s-1 et dans un environnement comportant une humidité de 43%. La deuxième partie de notre travail a été consacrée à l’élaboration et à la caractérisation de jonctions planaires MIM Ti/TiOx/Ti. Ces jonctions sont des motifs TLM de titane comportant une ligne transverse de TiOx réalisée par LAO. Lorsque les jonctions sont stressées électriquement sous air, une transformation morphologique irréversible se produit pour une densité de courant et un champ électrique atteignant de l’ordre de 7.1010 A.m-2 et 3.107 V.m-1 respectivement. Des analyses chimiques et structurales basées sur la microscopie électronique à transmission ont montré que la ligne initiale de TiOx amorphe s’était considérablement élargie et est constituée d’une zone de TiOx cristallin. Cette transformation peut être évitée en appliquant le stress électrique sous vide. Enfin des mesures électriques en température ont permis d’élucider les mécanismes de conduction : émission Schottky sous vide et conduction ionique sous air.
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Vers la réalisation de composants nanoélectroniques par anodisation localisée par AFM
Ce travail de thèse se compose de deux parties : tout d’abord nous avons caractérisé sur le plan morphologique des motifs de TiOx réalisés par anodisation localisée par AFM (LAO) dans des couches pleines plaques de 5 nm de titane. Nous avons étudié l’influence de la tension d’oxydation, de la vitesse de balayage de la pointe AFM, de l’humidité relative de l’environnement, du mode AFM (contact ou intermittent) et du type de pointe. Les motifs les plus fins atteignent une largeur à mi-hauteur de 21 nm pour 2.2 nm de hauteur, ils sont obtenus avec une pointe PtSi utilisée en mode intermittent sous une tension de polarisation de -7V, une vitesse de balayage de 0.4 µm.s-1 et dans un environnement comportant une humidité de 43%. La deuxième partie de notre travail a été consacrée à l’élaboration et à la caractérisation de jonctions planaires MIM Ti/TiOx/Ti. Ces jonctions sont des motifs TLM de titane comportant une ligne transverse de TiOx réalisée par LAO. Lorsque les jonctions sont stressées électriquement sous air, une transformation morphologique irréversible se produit pour une densité de courant et un champ électrique atteignant de l’ordre de 7.1010 A.m-2 et 3.107 V.m-1 respectivement. Des analyses chimiques et structurales basées sur la microscopie électronique à transmission ont montré que la ligne initiale de TiOx amorphe s’était considérablement élargie et est constituée d’une zone de TiOx cristallin. Cette transformation peut être évitée en appliquant le stress électrique sous vide. Enfin des mesures électriques en température ont permis d’élucider les mécanismes de conduction : émission Schottky sous vide et conduction ionique sous air.
- Open Access
- 16 July 2025
- Published by Wiley in Advanced Functional Materials
- Vol. 36 (1)
Wafer‐Scale Integration of α‐quartz Thin Films toward Super High Frequency Piezoelectric bioNEMS for Chikungunya Virus Detection
Micro and nanoelectromechanical systems (MEMS/NEMS), especially piezoelectric resonators, offer a promising strategy for the manufacturing of point‐of‐care devices providing rapid, sensitive, and field‐deployable tests with minimal user training for the diagnostics of viral infections. High‐frequency (HF) MEMS/NEMS have the potential for ultrasensitive mass‐loading devices. Yet, their use for biomedical applications requires challenging manufacturing qualities. Here, a large‐scale chemical integration of epitaxial α‐quartz (100) thin films is developed on silicon wafers up to 4‐inches. This methodology allows the microfabrication of wafer‐scale piezoelectric α‐quartz/silicon bioMEMS using a recognition layer capable of selectively detecting Chikungunya virus. Using contact‐free vibrometry, a mass sensitivity of the bioMEMS device of 22.4 pg Hz −1 is showen in liquid conditions and a Chikungunya virus limit of detection of 9 ng ml −1 . To reach piezoelectric transduction for compact quartz sensor devices, NEMS resonators are developed at super HF, i.e., 17.8 GHz with a quality factor of 280, which represents a QxF product of 4.98·10 12 . These α‐quartz NEMS can reach thicknesses between 100 and 800 nm and lateral dimensions up to 9 mm 2 . This work opens the door for cost‐efficient single‐chip epitaxial piezoelectric α‐quartz/Si ultrasensitive NEMS sensors manufactured exclusively by soft‐chemistry for biomedical applications and many other fields.
- 16 July 2025
- Published by Wiley in Advanced Functional Materials
- Vol. 36 (1)
Open AccessWafer‐Scale Integration of α‐quartz Thin Films toward Super High Frequency Piezoelectric bioNEMS for Chikungunya Virus Detection
Micro and nanoelectromechanical systems (MEMS/NEMS), especially piezoelectric resonators, offer a promising strategy for the manufacturing of point‐of‐care devices providing rapid, sensitive, and field‐deployable tests with minimal user training for the diagnostics of viral infections. High‐frequency (HF) MEMS/NEMS have the potential for ultrasensitive mass‐loading devices. Yet, their use for biomedical applications requires challenging manufacturing qualities. Here, a large‐scale chemical integration of epitaxial α‐quartz (100) thin films is developed on silicon wafers up to 4‐inches. This methodology allows the microfabrication of wafer‐scale piezoelectric α‐quartz/silicon bioMEMS using a recognition layer capable of selectively detecting Chikungunya virus. Using contact‐free vibrometry, a mass sensitivity of the bioMEMS device of 22.4 pg Hz −1 is showen in liquid conditions and a Chikungunya virus limit of detection of 9 ng ml −1 . To reach piezoelectric transduction for compact quartz sensor devices, NEMS resonators are developed at super HF, i.e., 17.8 GHz with a quality factor of 280, which represents a QxF product of 4.98·10 12 . These α‐quartz NEMS can reach thicknesses between 100 and 800 nm and lateral dimensions up to 9 mm 2 . This work opens the door for cost‐efficient single‐chip epitaxial piezoelectric α‐quartz/Si ultrasensitive NEMS sensors manufactured exclusively by soft‐chemistry for biomedical applications and many other fields.
- Open Access
- 17 July 2023
- Published by AIP Publishing in Applied Physics Letters
- Vol. 123 (3)
Doped and undoped ferroelectric HfO2: Role of Gd-doping in stabilizing the ferroelectric phase
Doped hafnium oxide was shown to exhibit a strong ferroelectric behavior. It was implied that doping allows the stabilization of a HfO2 non-centrosymmetric orthorhombic phase, a prerequisite for ferroelectric behavior. However, a number of reports showed comparable ferroelectric properties in undoped HfO2, although with different behaviors of the remanent polarization upon layer thickness. In this work, the ferroelectric properties and crystalline structure of doped and undoped HfO2 layers as a function of the layer thickness were studied. The results show similar properties for ultrathin layers. Indeed, both show a linear increase in the orthorhombic/tetragonal crystalline phase amount and of remanent polarization as a function of thickness up to 7 nm. For higher thicknesses, a strong increase in the monoclinic phase is observed in undoped layers alongside a strong decrease in the remanent polarization whereas, for doped layers, the remanent polarization continues to increase with thickness. The experimental results suggest that the stabilization of the undoped HfO2 orthorhombic ferroelectric phase is due to mechanical stress, which is particularly high in ultrathin layers but relaxes for thicker layers.
- 17 July 2023
- Published by AIP Publishing in Applied Physics Letters
- Vol. 123 (3)
Open AccessDoped and undoped ferroelectric HfO2: Role of Gd-doping in stabilizing the ferroelectric phase
Doped hafnium oxide was shown to exhibit a strong ferroelectric behavior. It was implied that doping allows the stabilization of a HfO2 non-centrosymmetric orthorhombic phase, a prerequisite for ferroelectric behavior. However, a number of reports showed comparable ferroelectric properties in undoped HfO2, although with different behaviors of the remanent polarization upon layer thickness. In this work, the ferroelectric properties and crystalline structure of doped and undoped HfO2 layers as a function of the layer thickness were studied. The results show similar properties for ultrathin layers. Indeed, both show a linear increase in the orthorhombic/tetragonal crystalline phase amount and of remanent polarization as a function of thickness up to 7 nm. For higher thicknesses, a strong increase in the monoclinic phase is observed in undoped layers alongside a strong decrease in the remanent polarization whereas, for doped layers, the remanent polarization continues to increase with thickness. The experimental results suggest that the stabilization of the undoped HfO2 orthorhombic ferroelectric phase is due to mechanical stress, which is particularly high in ultrathin layers but relaxes for thicker layers.
- Open Access
- 25 April 2022
- Published by AIP Publishing in Applied Physics Letters
- Vol. 120 (17) , 172901
Sub-10-nm ferroelectric Gd-doped HfO2 layers
Sub-10 nm thick gadolinium-doped hafnia (Gd:HfO2) layers were grown in metal–insulator–metal (TiN/Gd:HfO2/TiN) stacks using a plasma-enhanced atomic layer deposition process. Thermally annealed Gd:HfO2 layers with a thickness of 8.8, 6.6, and 4.4 nm exhibited orthorhombic crystalline structure and showed ferroelectric properties. Indeed, polarization vs electric field hysteresis loops were recorded with 2Pr polarization ranging from 2 to 20 μC/cm2. The studied layers showed the same coercive electric field (∼2 MV/cm). Consequently, polarization switching voltage between +Pr and −Pr decreased down to 0.9 V for the thinnest layer. Remanent polarization cycling showed a strong wake-up effect, with no fatigue, up to 109, followed by a stabilization up to 1010 cycles, where 2Pr reached 33 μC/cm2 for 8.8 nm Gd:HfO2. This endurance result and the absence of noticeable remanent polarization fatigue can be attributed to the optimal chemical composition of the TiN/Gd:HfO2 interface, which is supposed to be at the origin of defect generation, mostly oxygen vacancies, that leads to ferroelectric polarization fatigue.
- 25 April 2022
- Published by AIP Publishing in Applied Physics Letters
- Vol. 120 (17) , 172901
Open AccessSub-10-nm ferroelectric Gd-doped HfO2 layers
Sub-10 nm thick gadolinium-doped hafnia (Gd:HfO2) layers were grown in metal–insulator–metal (TiN/Gd:HfO2/TiN) stacks using a plasma-enhanced atomic layer deposition process. Thermally annealed Gd:HfO2 layers with a thickness of 8.8, 6.6, and 4.4 nm exhibited orthorhombic crystalline structure and showed ferroelectric properties. Indeed, polarization vs electric field hysteresis loops were recorded with 2Pr polarization ranging from 2 to 20 μC/cm2. The studied layers showed the same coercive electric field (∼2 MV/cm). Consequently, polarization switching voltage between +Pr and −Pr decreased down to 0.9 V for the thinnest layer. Remanent polarization cycling showed a strong wake-up effect, with no fatigue, up to 109, followed by a stabilization up to 1010 cycles, where 2Pr reached 33 μC/cm2 for 8.8 nm Gd:HfO2. This endurance result and the absence of noticeable remanent polarization fatigue can be attributed to the optimal chemical composition of the TiN/Gd:HfO2 interface, which is supposed to be at the origin of defect generation, mostly oxygen vacancies, that leads to ferroelectric polarization fatigue.
- 27 December 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (24) , 244501
Nano-analytical investigation of the forming process in an HfO2-based resistive switching memory
Metal oxide-based resistive random access memory devices are highly attractive candidates for next-generation nonvolatile memories, but the resistive switching phenomena remain poorly understood. This article focuses on the microscopic understanding of the initial forming step, which is decisive for the switching process. The integrated resistive switching memory effect in / / metal insulator metal structures is studied. After forming, transmission electron microscopy investigations pointed out the presence of a funnel-shaped region, in the ON state of the cell, where slightly oxidized ( ) was present within dielectric. Modeling of the measured ON state conductance of the cell with the semi-classical approximation is consistent with a conductive nanometric filament (or a sum of sub-nanometric filaments) present in the funnel-shaped region. The conductive area is likely formed by diffusion after the dielectric breakdown.- 27 December 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (24) , 244501
Nano-analytical investigation of the forming process in an HfO2-based resistive switching memory
Metal oxide-based resistive random access memory devices are highly attractive candidates for next-generation nonvolatile memories, but the resistive switching phenomena remain poorly understood. This article focuses on the microscopic understanding of the initial forming step, which is decisive for the switching process. The integrated resistive switching memory effect in / / metal insulator metal structures is studied. After forming, transmission electron microscopy investigations pointed out the presence of a funnel-shaped region, in the ON state of the cell, where slightly oxidized ( ) was present within dielectric. Modeling of the measured ON state conductance of the cell with the semi-classical approximation is consistent with a conductive nanometric filament (or a sum of sub-nanometric filaments) present in the funnel-shaped region. The conductive area is likely formed by diffusion after the dielectric breakdown.- Open Access
- 7 June 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nuclear Science
- Vol. 68 (8) , 1542-1547
Defect-Induced Phase Transition in Hafnium Oxide Thin Films: Comparing Heavy Ion Irradiation and Oxygen-Engineering Effects
Hafnium oxide acts as a functional dielectric in a variety of traditional and emerging nonvolatile memory technologies. To investigate the effect of heavy ion irradiation on its crystalline structure, highly textured hafnium oxide films were irradiated with 1.635 GeV Au ions of fluences ranging from 1×10 9 to 7×10 12 ions/cm 2 . For monoclinic hafnium oxide films, a fluence-dependent defect-induced phase transition to a defect-stabilized tetragonal phase is identified. In low-temperature tetragonal hafnium oxide films, the X-ray diffraction (XRD) patterns show an out-of-plane lattice constant decrease with increasing irradiation fluence. Observed crystalline changes are strikingly similar to trends found for oxygen-engineered hafnium oxide films, directly grown at varying oxidation conditions. The correlation of structural changes with in vacuo electron spectroscopy data of oxygen-engineered films suggests that the irradiation of hafnium oxide leads to an oxygen loss that increases with fluence. Therefore, the underlying mechanism of the monoclinic to tetragonal phase transition is obviously directly related to oxygen defects. This new information allows predictions of device stability under swift heavy ion irradiation of hafnium oxide-based devices.
- 7 June 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nuclear Science
- Vol. 68 (8) , 1542-1547
Open AccessDefect-Induced Phase Transition in Hafnium Oxide Thin Films: Comparing Heavy Ion Irradiation and Oxygen-Engineering Effects
Hafnium oxide acts as a functional dielectric in a variety of traditional and emerging nonvolatile memory technologies. To investigate the effect of heavy ion irradiation on its crystalline structure, highly textured hafnium oxide films were irradiated with 1.635 GeV Au ions of fluences ranging from 1×10 9 to 7×10 12 ions/cm 2 . For monoclinic hafnium oxide films, a fluence-dependent defect-induced phase transition to a defect-stabilized tetragonal phase is identified. In low-temperature tetragonal hafnium oxide films, the X-ray diffraction (XRD) patterns show an out-of-plane lattice constant decrease with increasing irradiation fluence. Observed crystalline changes are strikingly similar to trends found for oxygen-engineered hafnium oxide films, directly grown at varying oxidation conditions. The correlation of structural changes with in vacuo electron spectroscopy data of oxygen-engineered films suggests that the irradiation of hafnium oxide leads to an oxygen loss that increases with fluence. Therefore, the underlying mechanism of the monoclinic to tetragonal phase transition is obviously directly related to oxygen defects. This new information allows predictions of device stability under swift heavy ion irradiation of hafnium oxide-based devices.