Anne Berger
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Anne Berger has a total of 54 co-authors. Here are the top co-authors by number of shared publications:
- Hubert Andreas Gasteiger
Technical University of Munich
11 shared publications Felix N. Buechi
Paul Scherrer Institut
3 shared publicationsMichele Bozzetti
3 shared publicationsYen-Chun Chen
Paul Scherrer Institut
3 shared publicationsJacqueline Gatzemeier
Technical University of Munich
2 shared publicationsRobin Girod
Institute of Materials, Ecole Polytechnique Fédérale de Lausanne, 1015 Lausanne, Switzerland
2 shared publications
Latest Publications
- Open Access
- 1 June 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (6) , 060536
Temperature Dependence of the Chemical vs the Electrochemical Electrolyte Oxidation in Lithium-Ion Batteries with Ni-Rich CAMs: Gas Evolution, Salt Decomposition, and Metal Dissolution
Operating lithium-ion batteries (LIBs) to high charging cut-off potentials allows us to accommodate a further push in energy density. However, it requires a thorough understanding of the interplay and temperature dependence of parasitic reactions that aggravate the aging of the electrolyte and the cathode/anode electrodes. In the present study we investigated the interplay of the chemical and the electrochemical electrolyte oxidation, how they are related to the dissolution of transition metal (TM) ions from the cathode active material (CAM), and how they shift or accelerate with temperature. Through an optimized electrochemical protocol an excellent potential dependence of the gas evolution of a LiNi0.80Co0.15Al0.05O2 (NCA) charged against a free-standing graphite on a lithium metal electrode in a LP47 electrolyte was achieved. We identified O2 and PF5 gas as suitable proxies for the chemical and electrochemical electrolyte oxidation, respectively. Both processes are separated by at least 300 mV over a temperature range from 10 to 45 °C. Through temperature-dependent operando hard X-ray absorption spectroscopy measurements and their comparison with the gassing results, it will be shown, that the electrochemical oxidation of the electrolyte is directly linked to the dissolution of TMs, while the chemical electrolyte oxidation mainly leaves the transition metal dissolution unaffected.
- 1 June 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (6) , 060536
Open AccessTemperature Dependence of the Chemical vs the Electrochemical Electrolyte Oxidation in Lithium-Ion Batteries with Ni-Rich CAMs: Gas Evolution, Salt Decomposition, and Metal Dissolution
Operating lithium-ion batteries (LIBs) to high charging cut-off potentials allows us to accommodate a further push in energy density. However, it requires a thorough understanding of the interplay and temperature dependence of parasitic reactions that aggravate the aging of the electrolyte and the cathode/anode electrodes. In the present study we investigated the interplay of the chemical and the electrochemical electrolyte oxidation, how they are related to the dissolution of transition metal (TM) ions from the cathode active material (CAM), and how they shift or accelerate with temperature. Through an optimized electrochemical protocol an excellent potential dependence of the gas evolution of a LiNi0.80Co0.15Al0.05O2 (NCA) charged against a free-standing graphite on a lithium metal electrode in a LP47 electrolyte was achieved. We identified O2 and PF5 gas as suitable proxies for the chemical and electrochemical electrolyte oxidation, respectively. Both processes are separated by at least 300 mV over a temperature range from 10 to 45 °C. Through temperature-dependent operando hard X-ray absorption spectroscopy measurements and their comparison with the gassing results, it will be shown, that the electrochemical oxidation of the electrolyte is directly linked to the dissolution of TMs, while the chemical electrolyte oxidation mainly leaves the transition metal dissolution unaffected.
- Open Access
- 1 March 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (3) , 036505
On Tortuosity and Water Management in Hydrophobic and Hydrophilic Microporous Layers with Different Carbon Structures
To improve mass transport limitations in proton exchange membrane fuel cells (PEMFCs), a detailed analysis of the gas diffusion layer structure can aid to understand the transport processes of oxygen to the catalyst layer and the liquid water removal mechanism. Herein, the effect of tortuosity was studied using two different microporous layer (MPL) structures and their hydrophobic and hydrophilic clones. Focused ion beam—scanning electron microscopy tomography showed that all structures had similar porosity but different characteristic pore diameters. Volumetric analysis using the Laplace solver TauFactor and the PuMA random walk method yielded a tortuosity of 1.2–1.3 for both MPLs, and these values were confirmed by experiments based on limiting current measurements in a single-cell PEMFC. The inclusion of Knudsen diffusion in the MPL proved to be essential for both methods. Subsequent analysis using experimental operating conditions that induce liquid water formation suggested that different water filling mechanisms occur in MPLs with different surface wettability. A mechanistic understanding of the water filling processes was investigated by simulations, considering the effect of liquid water saturation in different pore size domains. It was found that the tortuosity increases more drastically when narrow pores are blocked by liquid water, consistent with the experiments.
- 1 March 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (3) , 036505
Open AccessOn Tortuosity and Water Management in Hydrophobic and Hydrophilic Microporous Layers with Different Carbon Structures
To improve mass transport limitations in proton exchange membrane fuel cells (PEMFCs), a detailed analysis of the gas diffusion layer structure can aid to understand the transport processes of oxygen to the catalyst layer and the liquid water removal mechanism. Herein, the effect of tortuosity was studied using two different microporous layer (MPL) structures and their hydrophobic and hydrophilic clones. Focused ion beam—scanning electron microscopy tomography showed that all structures had similar porosity but different characteristic pore diameters. Volumetric analysis using the Laplace solver TauFactor and the PuMA random walk method yielded a tortuosity of 1.2–1.3 for both MPLs, and these values were confirmed by experiments based on limiting current measurements in a single-cell PEMFC. The inclusion of Knudsen diffusion in the MPL proved to be essential for both methods. Subsequent analysis using experimental operating conditions that induce liquid water formation suggested that different water filling mechanisms occur in MPLs with different surface wettability. A mechanistic understanding of the water filling processes was investigated by simulations, considering the effect of liquid water saturation in different pore size domains. It was found that the tortuosity increases more drastically when narrow pores are blocked by liquid water, consistent with the experiments.
- Open Access
- 1 January 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (1) , 014508
Determination of the τ/ε-Ratio for Gas Diffusion Substrates and Microporous Layers in a Proton Exchange Membrane Fuel Cell
An understanding of the GDL properties is crucial for high-current-density operation of proton exchange membrane fuel cells (PEMFCs). The parameters porosity ( ε ) and tortuosity ( τ ) directly link the theoretical diffusivity in free space and the effective diffusivity in the structure. The τ / ε -ratio is therefore an important descriptor for the gas diffusion in a porous network. This study characterizes the τ / ε -ratio for gas diffusion layer substrate (GDL-S) materials from two suppliers (Toray, Freudenberg) and for one microporous layer (MPL) using limiting current measurements in an operating fuel cell. However, only the application of a new analysis method that considers the contribution from Knudsen diffusion allows for the τ / ε -determination of GDL-S materials which have carbon black added to the structure (e.g., Freudenberg GDL-S); this method can then also be used for the determination of the τ / ε -ratio of porous networks containing small pores like MPLs. Here, we assess the contribution of pressure-independent Knudsen diffusion to the overall diffusion and introduce a mixed diffusion coefficient, which includes both Knudsen and molecular diffusion. This analysis serves as a guideline to estimate the contribution of the respective diffusive processes for gas diffusion materials utilized in PEMFCs, where pore sizes resulting in different diffusion regimes are present.
- 1 January 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (1) , 014508
Open AccessDetermination of the τ/ε-Ratio for Gas Diffusion Substrates and Microporous Layers in a Proton Exchange Membrane Fuel Cell
An understanding of the GDL properties is crucial for high-current-density operation of proton exchange membrane fuel cells (PEMFCs). The parameters porosity ( ε ) and tortuosity ( τ ) directly link the theoretical diffusivity in free space and the effective diffusivity in the structure. The τ / ε -ratio is therefore an important descriptor for the gas diffusion in a porous network. This study characterizes the τ / ε -ratio for gas diffusion layer substrate (GDL-S) materials from two suppliers (Toray, Freudenberg) and for one microporous layer (MPL) using limiting current measurements in an operating fuel cell. However, only the application of a new analysis method that considers the contribution from Knudsen diffusion allows for the τ / ε -determination of GDL-S materials which have carbon black added to the structure (e.g., Freudenberg GDL-S); this method can then also be used for the determination of the τ / ε -ratio of porous networks containing small pores like MPLs. Here, we assess the contribution of pressure-independent Knudsen diffusion to the overall diffusion and introduce a mixed diffusion coefficient, which includes both Knudsen and molecular diffusion. This analysis serves as a guideline to estimate the contribution of the respective diffusive processes for gas diffusion materials utilized in PEMFCs, where pore sizes resulting in different diffusion regimes are present.
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1790
Effects of Operating Conditions on Membrane Electrode Assembly Saturation and Hydration Revealed By Operando Small- & Wide-Angle X-Ray Scattering
Operando scanning small- and wide-angle X-ray scattering (SAXS&WAXS) at the cSAXS beamline of the Swiss Light Source was employed in this study to examine the water saturation of polymer electrolyte fuel cell (PEFC) component, particularly in the nanoscale pore space of catalyst layers (CL) and the membrane hydration state. A small beam size (≈7x30 microns) and ≈0.6 microns through-plane step size enabled to resolve of the bulk CLs (Pt/C Ketjen Black based, 0.1 mgPt/cm2; ≈7 microns thick) separated by a 15-micron membrane. Additionally, it allows for precise registration in case of membrane swelling during operation, which is a prerequisite for the analysis of the operando scattering data. Due to the difference in electron density variation between solid-void and solid-liquid interfaces, any change in CL saturation results in different scattering intensity profiles, which can be quantified by Invariant calculations (see Fig. 1a & b). The presentation will give insights into CL saturation evolution concerning relative humidity, operating pressure and current density. Differences in the CL saturation, and membrane hydration indicated by a change in d-spacing of the ionomer peak (1), were observed between wet nitrogen flushing and cell operation (see Fig. 1c & d). However, the cathode microporous layer (MPL) saturation seems to be unaffected for a Li100-based MPL on a Freudenberg H14 gas diffusion layer (GDL) substrate. The length scale-specific scattering data will provide a better understanding of mass transport in PEFC’s materials and allow us to push material design development forward. We acknowledge the Paul Scherrer Institut, Villigen, Switzerland for provision of synchrotron radiation beamtime at beamline cSAXS of the Swiss Light Source. References: S. W. Shi, A. Z. Weber and A. Kusoglu, J Membrane Sci, 516, 123 (2016). Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1790
Effects of Operating Conditions on Membrane Electrode Assembly Saturation and Hydration Revealed By Operando Small- & Wide-Angle X-Ray Scattering
Operando scanning small- and wide-angle X-ray scattering (SAXS&WAXS) at the cSAXS beamline of the Swiss Light Source was employed in this study to examine the water saturation of polymer electrolyte fuel cell (PEFC) component, particularly in the nanoscale pore space of catalyst layers (CL) and the membrane hydration state. A small beam size (≈7x30 microns) and ≈0.6 microns through-plane step size enabled to resolve of the bulk CLs (Pt/C Ketjen Black based, 0.1 mgPt/cm2; ≈7 microns thick) separated by a 15-micron membrane. Additionally, it allows for precise registration in case of membrane swelling during operation, which is a prerequisite for the analysis of the operando scattering data. Due to the difference in electron density variation between solid-void and solid-liquid interfaces, any change in CL saturation results in different scattering intensity profiles, which can be quantified by Invariant calculations (see Fig. 1a & b). The presentation will give insights into CL saturation evolution concerning relative humidity, operating pressure and current density. Differences in the CL saturation, and membrane hydration indicated by a change in d-spacing of the ionomer peak (1), were observed between wet nitrogen flushing and cell operation (see Fig. 1c & d). However, the cathode microporous layer (MPL) saturation seems to be unaffected for a Li100-based MPL on a Freudenberg H14 gas diffusion layer (GDL) substrate. The length scale-specific scattering data will provide a better understanding of mass transport in PEFC’s materials and allow us to push material design development forward. We acknowledge the Paul Scherrer Institut, Villigen, Switzerland for provision of synchrotron radiation beamtime at beamline cSAXS of the Swiss Light Source. References: S. W. Shi, A. Z. Weber and A. Kusoglu, J Membrane Sci, 516, 123 (2016). Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1766
Importance of Directed Water Removal: Intruding Microporous Layer Material into the Gas Diffusion Layer Substrate
Proton exchange membrane fuel cells (PEMFC) are an essential component of net zero emission scenarios by the International Energy Agency (IEA), most prominent in the heavy-duty transportation sector.[1-2] During operation, the PEMFC is subject to different operating conditions, particularly wet conditions where liquid water removal is crucial. It was observed that a microporous layer (MPL), commonly consisting of a carbon component (e.g. carbon black, carbon fibers) and a hydrophobic binder (e.g. PTFE), placed at the interface of the catalyst layer (CL) and the gas diffusion layer substrate (GDL-S), has a large impact on the water removal properties. Among other advantages, the addition of an MPL can guide the localization of water clusters in the GDL.[3] However, if interfaces exhibit large interfacial gaps, as was demonstrated for the CL/MPL interface,[4] liquid water can accumulate in the large openings, thereby creating a mass transport barrier. Seeking to understand the importance of interfaces, which can either guide water formation or create obstacles, this study further investigates the MPL/GDL-S interface. We created an intruding MPL by pressing the MPL slurry into the GDL-S using mechanical force (further on referred to as “intruded-GDL”) and compared it to a GDL, where the MPL sits quasi on top (further on referred to as “sheet-GDL”). Figure 1a shows a cross-sectional scanning electron microscopy (SEM image) of the sheet-GDL, while Figure 1b shows an intruded-GDL. The boundaries between the MPL material and the GDL-S are marked in red. The MPL/GDL-S interface of the sheet-GDL is relatively flat, following only the surface contour of the GDL-S, while the MPL/GDL-S interface of the intruded-GDL is pressed into the GDL-S and locally penetrates deeper into the GDL-S. It is also visible that the penetration into the GDL-S is inhomogeneous. We characterized the altered morphology using SEM (see Figure 1), mercury intrusion porosimetry (MIP), and x-ray tomographic microscopy (XTM). We found that the MPL of the intruded-MPL intrudes significantly into the GDL-S and preferably fills the larger pores of the GDL-S. Both types of GDLs were subject to single-cell fuel cell testing under various operating conditions. We found that the intruding MPL poses an additional oxygen transport resistance at dry conditions compared to the sheet-GDL. Under conditions where liquid water formation can be expected, the intruded-GDL starts to have an advantage compared to the sheet-GDL. From the data obtained in this study, a delicate interplay between the additional dry transport resistance, the missing macropores that were filled with MPL material, and the guided water removal properties can be deduced. We can derive an improved water removal mechanism for the intruded-GDL as a cause of the structural changes, which can serve as a guideline to improve GDL design parameters. References [1] IEA, Net Zero by 2050 2021,https://www.iea.org/reports/net-zero-by-2050. [2] D. A. Cullen, K. C. Neyerlin, R. K. Ahluwalia, R. Mukundan, K. L. More, R. L. Borup, A. Z. Weber, D. J. Myers, A. Kusoglu, Nat. Energy 2021, 6, 462-474. [3] J. T. Gostick, M. A. Ioannidis, M. W. Fowler, M. D. Pritzker, Electrochem. commun. 2009, 11, 576-579. [4] I. V. Zenyuk, E. C. Kumbur, S. Litster, J. Power Sources 2013, 241, 379-387. Acknowledgements We gratefully acknowledge funding from the Swiss National Science Foundation under the Sinergia grant number 180335. Figure 1 . SEM cross-sectional images different GDL configurations: a) a sheet-GDL; b) an intruded-GDL. The contours of the MPL material is marked with red lines. The MPL of the sheet-GDL is situated on top of the GDL-S, following the GDL-S surface contour, while the MPL of the intruded-GDL intrudes into larger pores of the GDL-S in an inhomogeneous manner. Figure 1
- 22 December 2023
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2023-02 (37) , 1766
Importance of Directed Water Removal: Intruding Microporous Layer Material into the Gas Diffusion Layer Substrate
Proton exchange membrane fuel cells (PEMFC) are an essential component of net zero emission scenarios by the International Energy Agency (IEA), most prominent in the heavy-duty transportation sector.[1-2] During operation, the PEMFC is subject to different operating conditions, particularly wet conditions where liquid water removal is crucial. It was observed that a microporous layer (MPL), commonly consisting of a carbon component (e.g. carbon black, carbon fibers) and a hydrophobic binder (e.g. PTFE), placed at the interface of the catalyst layer (CL) and the gas diffusion layer substrate (GDL-S), has a large impact on the water removal properties. Among other advantages, the addition of an MPL can guide the localization of water clusters in the GDL.[3] However, if interfaces exhibit large interfacial gaps, as was demonstrated for the CL/MPL interface,[4] liquid water can accumulate in the large openings, thereby creating a mass transport barrier. Seeking to understand the importance of interfaces, which can either guide water formation or create obstacles, this study further investigates the MPL/GDL-S interface. We created an intruding MPL by pressing the MPL slurry into the GDL-S using mechanical force (further on referred to as “intruded-GDL”) and compared it to a GDL, where the MPL sits quasi on top (further on referred to as “sheet-GDL”). Figure 1a shows a cross-sectional scanning electron microscopy (SEM image) of the sheet-GDL, while Figure 1b shows an intruded-GDL. The boundaries between the MPL material and the GDL-S are marked in red. The MPL/GDL-S interface of the sheet-GDL is relatively flat, following only the surface contour of the GDL-S, while the MPL/GDL-S interface of the intruded-GDL is pressed into the GDL-S and locally penetrates deeper into the GDL-S. It is also visible that the penetration into the GDL-S is inhomogeneous. We characterized the altered morphology using SEM (see Figure 1), mercury intrusion porosimetry (MIP), and x-ray tomographic microscopy (XTM). We found that the MPL of the intruded-MPL intrudes significantly into the GDL-S and preferably fills the larger pores of the GDL-S. Both types of GDLs were subject to single-cell fuel cell testing under various operating conditions. We found that the intruding MPL poses an additional oxygen transport resistance at dry conditions compared to the sheet-GDL. Under conditions where liquid water formation can be expected, the intruded-GDL starts to have an advantage compared to the sheet-GDL. From the data obtained in this study, a delicate interplay between the additional dry transport resistance, the missing macropores that were filled with MPL material, and the guided water removal properties can be deduced. We can derive an improved water removal mechanism for the intruded-GDL as a cause of the structural changes, which can serve as a guideline to improve GDL design parameters. References [1] IEA, Net Zero by 2050 2021,https://www.iea.org/reports/net-zero-by-2050. [2] D. A. Cullen, K. C. Neyerlin, R. K. Ahluwalia, R. Mukundan, K. L. More, R. L. Borup, A. Z. Weber, D. J. Myers, A. Kusoglu, Nat. Energy 2021, 6, 462-474. [3] J. T. Gostick, M. A. Ioannidis, M. W. Fowler, M. D. Pritzker, Electrochem. commun. 2009, 11, 576-579. [4] I. V. Zenyuk, E. C. Kumbur, S. Litster, J. Power Sources 2013, 241, 379-387. Acknowledgements We gratefully acknowledge funding from the Swiss National Science Foundation under the Sinergia grant number 180335. Figure 1 . SEM cross-sectional images different GDL configurations: a) a sheet-GDL; b) an intruded-GDL. The contours of the MPL material is marked with red lines. The MPL of the sheet-GDL is situated on top of the GDL-S, following the GDL-S surface contour, while the MPL of the intruded-GDL intrudes into larger pores of the GDL-S in an inhomogeneous manner. Figure 1
- Open Access
- 1 September 2023
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 170 (9) , 094509
Analysis of the MPL/GDL Interface: Impact of MPL Intrusion into the GDL Substrate
Interfaces are crucial for the water management in polymer electrolyte membrane fuel cells (PEMFCs). The introduction of a microporous layer (MPL) had a revolutionary effect on the water distribution by improving the interface between the catalyst layer and the gas diffusion layer substrate (GDL-S). Hence, it is vital to maximize the improvement by further characterizing and advancing the properties of the interfaces, in this case the MPL/GDL-S interface. This study aims at fabricating a GDL with an MPL that intrudes into the GDL-S, analyzing the impact on the GDL-S structure and on PEMFC performance. Mercury intrusion porosimetry (MIP) and ex situ X-ray tomography (XTM) show that the intrusion of the MPL into the hydrophobic GDL-S proceeds via the preferential filling of the GDL-S macropores, thereby reducing their size and volume fraction in the GDL-S. While an intruding MPL leads to a small performance increase under wet PEMFC operating conditions, this improvement could only be achieved by a careful management between the extent of MPL intrusion and the partial macropore blocking in the GDL-S. Furthermore, the impact of MPL intrusion on the liquid water saturation of the GDL was quantified by operando XTM. The results provide design guidelines for improved GDLs.
- 1 September 2023
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 170 (9) , 094509
Open AccessAnalysis of the MPL/GDL Interface: Impact of MPL Intrusion into the GDL Substrate
Interfaces are crucial for the water management in polymer electrolyte membrane fuel cells (PEMFCs). The introduction of a microporous layer (MPL) had a revolutionary effect on the water distribution by improving the interface between the catalyst layer and the gas diffusion layer substrate (GDL-S). Hence, it is vital to maximize the improvement by further characterizing and advancing the properties of the interfaces, in this case the MPL/GDL-S interface. This study aims at fabricating a GDL with an MPL that intrudes into the GDL-S, analyzing the impact on the GDL-S structure and on PEMFC performance. Mercury intrusion porosimetry (MIP) and ex situ X-ray tomography (XTM) show that the intrusion of the MPL into the hydrophobic GDL-S proceeds via the preferential filling of the GDL-S macropores, thereby reducing their size and volume fraction in the GDL-S. While an intruding MPL leads to a small performance increase under wet PEMFC operating conditions, this improvement could only be achieved by a careful management between the extent of MPL intrusion and the partial macropore blocking in the GDL-S. Furthermore, the impact of MPL intrusion on the liquid water saturation of the GDL was quantified by operando XTM. The results provide design guidelines for improved GDLs.
- Open Access
- 1 July 2023
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 170 (7) , 074502
Catalyst Aggregate Size Effect on the Mass Transport Properties of Non-Noble Metal Catalyst Layers for PEMFC Cathodes
Non-noble metal catalysts (NNMCs) are regarded as a promising alternative to the costly Pt-based materials required to catalyze the oxygen reduction reaction (ORR) in proton exchange membrane fuel cell (PEMFC) cathodes. However, the large diversity of NNMC synthesis approaches reported in the literature results in materials featuring a wide variety of particle sizes and morphologies, and the effect of these properties on these catalysts’ PEMFC performance remains poorly understood. To shed light on this matter, in this work we studied the physical and electrochemical properties of NNMC layers prepared from materials featuring broadly different aggregate sizes, whereby this property was tuned by ball milling the precursors used in the NNMCs’ synthesis in the absence vs presence of a solvent. This led to two NNMCs featuring similar Fe-speciations and ORR-activities, but with vastly different aggregate sizes of >5 μm vs ≈100 nm, respectively. Following the extensive characterization of catalyst layers (CLs) prepared with these materials via electron microscopy and X-ray tomography, PEMFC tests at different loadings unveiled that the smaller aggregate size and ≈20% higher porosity of the CL prepared from the wet-milled sample resulted in an improvement of its mass transport properties (as well as a ≈2-fold enhancement of its peak power density under H2/air operation) over the dry-milled material.
- 1 July 2023
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 170 (7) , 074502
Open AccessCatalyst Aggregate Size Effect on the Mass Transport Properties of Non-Noble Metal Catalyst Layers for PEMFC Cathodes
Non-noble metal catalysts (NNMCs) are regarded as a promising alternative to the costly Pt-based materials required to catalyze the oxygen reduction reaction (ORR) in proton exchange membrane fuel cell (PEMFC) cathodes. However, the large diversity of NNMC synthesis approaches reported in the literature results in materials featuring a wide variety of particle sizes and morphologies, and the effect of these properties on these catalysts’ PEMFC performance remains poorly understood. To shed light on this matter, in this work we studied the physical and electrochemical properties of NNMC layers prepared from materials featuring broadly different aggregate sizes, whereby this property was tuned by ball milling the precursors used in the NNMCs’ synthesis in the absence vs presence of a solvent. This led to two NNMCs featuring similar Fe-speciations and ORR-activities, but with vastly different aggregate sizes of >5 μm vs ≈100 nm, respectively. Following the extensive characterization of catalyst layers (CLs) prepared with these materials via electron microscopy and X-ray tomography, PEMFC tests at different loadings unveiled that the smaller aggregate size and ≈20% higher porosity of the CL prepared from the wet-milled sample resulted in an improvement of its mass transport properties (as well as a ≈2-fold enhancement of its peak power density under H2/air operation) over the dry-milled material.
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (39) , 1376
Characterizing the Pore Network of Diffusion Media at the Pore Size Scale
Water management by gas diffusion media and electrodes is a fundamental aspect of the performance of electrochemical cells including proton exchange membrane (PEM) fuel cells. In these devices, product liquid water blocks part of the available space for reactants flow, leading to mass transport losses and lowering of the performance1. Pores saturation has been observed with different experimental techniques for GDL substrates, however a detailed saturation process at the pore size scale of the microporous layer (MPL) is necessary. Previously, it was suggested that large pore network domains are responsible for an enhanced water evacuation2, however, possible existence of narrow size constrictions could still limit water evacuation. In this work, we detail the benefits of three-dimensional imaging of the pore network at the typical MPL pore size scale, i.e. the sub-micrometre scale, which is achieved by focused ion beam scanning electron microscope (FIB-SEM) nanotomography. Two different MPL designs were analysed: an acetylene black based MPL, named Li100, and a vapor grown carbon fiber (VGCF) based MPL, the latter showing better performance under high relative humidity conditions2, 3. FIB-SEM tomography volumes in Fig. 1a-b were used to observe the relative distribution of larger pore domains and narrower pore constrictions. By removing narrower sized pores from the network and analysing the connections of large pore domains, we show the existence of a characteristic size for pore constrictions below which the pore network is well connected. This characteristic size is depicted by the red line in Fig. 1c-d, which plots the fraction of connected pores as a function of their minimum size. Constrictions size values for the two MPL designs were further validated with mercury intrusion experiments, since constrictions affect all the intrusions by capillary pressure, such as water flow in hydrophobic MPLs. The calculated parameters, which are representative of the connections between large pore domains, open up new perspectives on the prediction of gas diffusion under realistic conditions. The approach allows evaluation of the effects of alternatively removing larger and narrower pore domains, to understand the saturation-driven tortuosity in different MPL structures. J. Shen, L. Xu, H. Chang, Z. Tu, and S. H. Chan, Energy Conversion and Management, 207, 112537 (2020). C. Simon, D. Kartouzian, D. Müller, F. Wilhelm, and H. A. Gasteiger, Journal of The Electrochemical Society, 164, F1697–F1711 (2017). C. Simon, J. Endres, B. Nefzger-Loders, F. Wilhelm, and H. A. Gasteiger, Journal of The Electrochemical Society, 166, F1022–F1035 (2019). Figure 1
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (39) , 1376
Characterizing the Pore Network of Diffusion Media at the Pore Size Scale
Water management by gas diffusion media and electrodes is a fundamental aspect of the performance of electrochemical cells including proton exchange membrane (PEM) fuel cells. In these devices, product liquid water blocks part of the available space for reactants flow, leading to mass transport losses and lowering of the performance1. Pores saturation has been observed with different experimental techniques for GDL substrates, however a detailed saturation process at the pore size scale of the microporous layer (MPL) is necessary. Previously, it was suggested that large pore network domains are responsible for an enhanced water evacuation2, however, possible existence of narrow size constrictions could still limit water evacuation. In this work, we detail the benefits of three-dimensional imaging of the pore network at the typical MPL pore size scale, i.e. the sub-micrometre scale, which is achieved by focused ion beam scanning electron microscope (FIB-SEM) nanotomography. Two different MPL designs were analysed: an acetylene black based MPL, named Li100, and a vapor grown carbon fiber (VGCF) based MPL, the latter showing better performance under high relative humidity conditions2, 3. FIB-SEM tomography volumes in Fig. 1a-b were used to observe the relative distribution of larger pore domains and narrower pore constrictions. By removing narrower sized pores from the network and analysing the connections of large pore domains, we show the existence of a characteristic size for pore constrictions below which the pore network is well connected. This characteristic size is depicted by the red line in Fig. 1c-d, which plots the fraction of connected pores as a function of their minimum size. Constrictions size values for the two MPL designs were further validated with mercury intrusion experiments, since constrictions affect all the intrusions by capillary pressure, such as water flow in hydrophobic MPLs. The calculated parameters, which are representative of the connections between large pore domains, open up new perspectives on the prediction of gas diffusion under realistic conditions. The approach allows evaluation of the effects of alternatively removing larger and narrower pore domains, to understand the saturation-driven tortuosity in different MPL structures. J. Shen, L. Xu, H. Chang, Z. Tu, and S. H. Chan, Energy Conversion and Management, 207, 112537 (2020). C. Simon, D. Kartouzian, D. Müller, F. Wilhelm, and H. A. Gasteiger, Journal of The Electrochemical Society, 164, F1697–F1711 (2017). C. Simon, J. Endres, B. Nefzger-Loders, F. Wilhelm, and H. A. Gasteiger, Journal of The Electrochemical Society, 166, F1022–F1035 (2019). Figure 1
- 7 July 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-01 (2) , 172
Spatially Resolved Operando X-Ray Absorption Spectroscopy in NCA/Graphite to Quantify the Potential-Dependent Transition Metal Dissolution and Its Effect on Capacity Fading
Layered transition metal oxides like NCAs (LiNixCoyAlzO2, with x+y+z=1) and NCMs (LiNixCoyMnzO2, with x+y+z=1) are used as cathode active materials (CAMs) for high energy Li-ion batteries due to their high capacity. However, at high upper cut-off potentials, those CAMs suffer from structural instabilities, resulting in severe capacity fading and thus limiting the accessible capacity that can be obtained. Possible causes for the capacity fade at high cut-off potentials and high state-of-charge (SOC) include the (electro)chemical oxidation of the electrolyte oxidation and transition metal (TM) dissolution from the CAM surface.1 Furthermore, layered TM-oxides are known to release lattice oxygen from the near-surface region at high SOC (i.e., at ≈80% SOC when referenced to the total amount of lithium), resulting in reactive oxygen species that induce electrolyte oxidation and HF formation.2 This release of lattice oxygen results in a surface reconstruction from the pristine layered structure to a more resistive spinel- or rocksalt-like structure, thereby inducing an impedance build-up on the cathode. Diffusion of dissolved transition metals to the anode and their subsequent deposition on the anode active material particles can also have a severe effect on cell aging, as the accumulation of metal species on the graphite anode has shown to catalyze the degradation of the protective anode solid/electrolyte interphase (SEI), eventually resulting in the loss of active lithium and in an anode impedance growth. Since the dissolution of manganese is considered to have the most detrimental effect on the anode SEI compared to cobalt and nickel,3 manganese-free NCAs (e.g., LiNi0.8Co0.15Al0.05O2) might have an advantage over manganese-containing NCMs. In this study, we will examine the potential-dependent dissolution of Ni and Co in NCA/graphite cells using operando XAS, and compare it to the potential-dependent dissolution of Ni, Co, and Mn from LiNi0.6Co0.2Mn0.2O2 (NMC622) that we had determined previously by operando XAS.4 Owing to the specially designed geometry of the operando XAS cell,5 we can spectroscopically access and independently investigate the concentration and oxidation state of transition metals, both dissolved in the electrolyte and deposited within the graphite anode. This is illustrated for an NCA/graphite cell in Figure 1. We will also examine the effect of lattice oxygen release from NCA on the NCA/graphite full-cell performance by applying different techniques: We employ a three-electrode Swagelok® type T-cell with a gold wire micro reference electrode (µ-GWRE)6 to quantify the anode and the cathode impedance over the course of 100 cycles as a function of the upper cutoff voltage. In addition, on-line electrochemical mass spectrometry (OEMS)7 is applied to detect the onset SOC for the release of lattice oxygen. From these comparisons, we aim to get a detailed understanding about the influence of transition metal dissolution from NCA on capacity fade and cycle life. References: J. A. Gilbert, I. A. Shkrob, and D. P. Abraham, Journal of The Electrochemical Society, 164 (2), A389-A399 (2017). R. Jung, M. Metzger, F. Maglia, C. Stinner, and H. A. Gasteiger, Journal of The Electrochemical Society, 164 (7), A1361-A1377 (2017). S. Solchenbach, G. Hong, A. T. S. Freiberg, R. Jung, and H. A. Gasteiger, Journal of The Electrochemical Society, 165 (14), A3304-A3312 (2018). R. Jung, F. Linsenmann, R. Thomas, J. Wandt, S. Solchenbach, F. Maglia, C. Stinner, M. Tromp, and H. A. Gasteiger, Journal of The Electrochemical Society, 166 (2), A378-A389 (2019). J. Wandt, A. Freiberg, R. Thomas, Y. Gorlin, A. Siebel, R. Jung, H. A. Gasteiger, and M. Tromp, Journal of Materials Chemistry A, 4 (47), 18300-18305 (2016). S. Solchenbach, D. Pritzl, E. J. Y. Kong, J. Landesfeind, and H. A. Gasteiger, Journal of The Electrochemical Society, 163 (10), A2265-A2272 (2016). N. Tsiouvaras, S. Meini, I. Buchberger, and H. A. Gasteiger, Journal of The Electrochemical Society, 160 (3), A471-A477 (2013). Figure 1
- 7 July 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-01 (2) , 172
Spatially Resolved Operando X-Ray Absorption Spectroscopy in NCA/Graphite to Quantify the Potential-Dependent Transition Metal Dissolution and Its Effect on Capacity Fading
Layered transition metal oxides like NCAs (LiNixCoyAlzO2, with x+y+z=1) and NCMs (LiNixCoyMnzO2, with x+y+z=1) are used as cathode active materials (CAMs) for high energy Li-ion batteries due to their high capacity. However, at high upper cut-off potentials, those CAMs suffer from structural instabilities, resulting in severe capacity fading and thus limiting the accessible capacity that can be obtained. Possible causes for the capacity fade at high cut-off potentials and high state-of-charge (SOC) include the (electro)chemical oxidation of the electrolyte oxidation and transition metal (TM) dissolution from the CAM surface.1 Furthermore, layered TM-oxides are known to release lattice oxygen from the near-surface region at high SOC (i.e., at ≈80% SOC when referenced to the total amount of lithium), resulting in reactive oxygen species that induce electrolyte oxidation and HF formation.2 This release of lattice oxygen results in a surface reconstruction from the pristine layered structure to a more resistive spinel- or rocksalt-like structure, thereby inducing an impedance build-up on the cathode. Diffusion of dissolved transition metals to the anode and their subsequent deposition on the anode active material particles can also have a severe effect on cell aging, as the accumulation of metal species on the graphite anode has shown to catalyze the degradation of the protective anode solid/electrolyte interphase (SEI), eventually resulting in the loss of active lithium and in an anode impedance growth. Since the dissolution of manganese is considered to have the most detrimental effect on the anode SEI compared to cobalt and nickel,3 manganese-free NCAs (e.g., LiNi0.8Co0.15Al0.05O2) might have an advantage over manganese-containing NCMs. In this study, we will examine the potential-dependent dissolution of Ni and Co in NCA/graphite cells using operando XAS, and compare it to the potential-dependent dissolution of Ni, Co, and Mn from LiNi0.6Co0.2Mn0.2O2 (NMC622) that we had determined previously by operando XAS.4 Owing to the specially designed geometry of the operando XAS cell,5 we can spectroscopically access and independently investigate the concentration and oxidation state of transition metals, both dissolved in the electrolyte and deposited within the graphite anode. This is illustrated for an NCA/graphite cell in Figure 1. We will also examine the effect of lattice oxygen release from NCA on the NCA/graphite full-cell performance by applying different techniques: We employ a three-electrode Swagelok® type T-cell with a gold wire micro reference electrode (µ-GWRE)6 to quantify the anode and the cathode impedance over the course of 100 cycles as a function of the upper cutoff voltage. In addition, on-line electrochemical mass spectrometry (OEMS)7 is applied to detect the onset SOC for the release of lattice oxygen. From these comparisons, we aim to get a detailed understanding about the influence of transition metal dissolution from NCA on capacity fade and cycle life. References: J. A. Gilbert, I. A. Shkrob, and D. P. Abraham, Journal of The Electrochemical Society, 164 (2), A389-A399 (2017). R. Jung, M. Metzger, F. Maglia, C. Stinner, and H. A. Gasteiger, Journal of The Electrochemical Society, 164 (7), A1361-A1377 (2017). S. Solchenbach, G. Hong, A. T. S. Freiberg, R. Jung, and H. A. Gasteiger, Journal of The Electrochemical Society, 165 (14), A3304-A3312 (2018). R. Jung, F. Linsenmann, R. Thomas, J. Wandt, S. Solchenbach, F. Maglia, C. Stinner, M. Tromp, and H. A. Gasteiger, Journal of The Electrochemical Society, 166 (2), A378-A389 (2019). J. Wandt, A. Freiberg, R. Thomas, Y. Gorlin, A. Siebel, R. Jung, H. A. Gasteiger, and M. Tromp, Journal of Materials Chemistry A, 4 (47), 18300-18305 (2016). S. Solchenbach, D. Pritzl, E. J. Y. Kong, J. Landesfeind, and H. A. Gasteiger, Journal of The Electrochemical Society, 163 (10), A2265-A2272 (2016). N. Tsiouvaras, S. Meini, I. Buchberger, and H. A. Gasteiger, Journal of The Electrochemical Society, 160 (3), A471-A477 (2013). Figure 1