IPInsung Park

Insung Park

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Insung Park has a total of 25 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Aging Effects in REBCO Tapes Solder Joint Made With Indium-Tin

    by Gaël Berthet, Hyunsoo Park, Insung Park, Wonseok Jang, Wonju Jung, Jeonghwan Park, Minkyu Sun, Haigun Lee, Seungyong Hahn, Sangjin Lee

    With the promises of nuclear fusion, an increasing number of fusion magnet projects are employing $\mathrm{(RE)Ba}_{2}\text{Cu}_{3}\mathrm{O}_{7-\updelta}$ (REBCO) tapes. These magnets often include multiple demountable joints, which typically incorporate low-temperature solder either in the joint itself or in the cable. Such solders usually contain elements that diffuse readily in copper, raising concerns about the aging effects. This study investigates the impact of the InterMetallic-Compound (IMC) growth on the joints properties through room-temperature aging and annealing. Eutectic indium-tin solder joints stored for nine months in a desiccator did not exhibit any significant change in their properties. Given the strong temperature dependence of the IMC growth, annealing at 100°C was performed to simulate long-term effects. After 6 to 8 days of annealing, critical current degradation was measured in all samples containing solder, indicating that the IMC had grown to the REBCO layer deteriorating it. Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) analyses revealed that even after 20 days, solder elements reached the REBCO layer only in regions where the solder was abundant.


  • Real-Time Thickness Monitoring for Enhanced Geometric Uniformity of REBCO CCs

    by Insung Park, Gwantae Kim, Jeongtae Kim, Hongsoo Ha

    Geometric uniformity is crucial for high-temperature superconducting (HTS) REBCO coated conductors (CCs), particularly in superconducting-magnet applications that demand precise winding geometries. A non-contact, continuous reel-to-reel (R2R) thickness measurement system was implemented in this study to systematically examine thickness profiles at key manufacturing stages, including raw metal substrates, electro polishing (EP), buffer layer deposition, superconducting layer and silver (Ag) deposition, tape slitting, and copper (Cu) electroplating. Static and continuous R2R scanning analyses revealed significant geometric deformations, such as edge tapering caused by asymmetric EP and pronounced edge thickening (so called “dog-bone” shape) due to non-uniform electroplating fields. To mitigate these geometric non-uniformities, advanced strategies adaptive deposition based on real-time thickness mapping, precise field distribution shielding during electroplating, and automated roller gap feedback controls are proposed. Implementing these measures is expected to enhance geometric consistency, improve manufacturing yield, and enable robust quality control for high-performance REBCO CCs.

  • Development of Continuous Thickness Measurement System for Long-Length HTS CCs

    by Insung Park, Gwantae Kim, Hosup Kim, Jeongtae Kim, Hongsoo Ha

    In this article, we present a newly developed continuous thickness measurement system for long-length high-temperature superconducting (HTS) coated conductors (CCs). Uniform thickness in HTS CCs is critical for maintaining consistent magnetic field performance and mechanical integrity, particularly in applications such as superconducting coil windings. Our system employs a reel-to-reel (R2R) mechanism integrated with confocal laser sensors to enable real-time, non-contact thickness measurements. Comprehensive trials were carried out to evaluate the system's accuracy and precision, including static scans at various speeds and comparisons with cross-sectional analysis using optical microscopy. Additionally, the system demonstrated high precision, with repeatability confirmed through 10 repeated measurements along the length and width of a 12 m-long Cu-plated HTS CC. This development is expected to significantly improve the manufacturing process, enhance quality control, and support factory automation for consistent production of high-performance HTS magnets.


  • Proposal of Continuous Thickness Measurement Technology for the Superconducting Wire

    by Insung Park, Gwantae Kim, Hosup Kim, Jeongtae Kim, Hongsoo Ha

    Accurate measurement of thickness holds significant importance during the fabrication of high-temperature superconducting (HTS) magnets using HTS wires. Despite its growing significance, a continuous measurement device for tracking HTS wire thickness remains elusive. When employing superconducting wire in applications like HTS magnets for generating high magnetic fields, it becomes crucial to precisely gauge the wire's thickness beforehand. This preemptive measurement minimizes deviations between the magnet's intended design specifications and the actual manufacturing process. Furthermore, HTS wires often exhibit non-uniform thickness not only along their length but also across their width, highlighting the need for a comprehensive solution. Hence, the imperative arises to devise a continuous measurement tool capable of accurately determining both thickness and shape for long-lengths of HTS wires. In this study, we propose a novel approach: a technology for measuring HTS wire thickness. This proposal utilizes a reel-to-reel transfer device in tandem with a confocal laser sensor to achieve continuous, precise measurement and transfer of lengthy HTS wires.


  • Design of Scalable Superconducting Quantum Circuits Using Flip-Chip Assembly

    by Seong Hyeon Park, Dowon Baek, Insung Park, Seungyong Hahn

    We present design results of scalable superconducting quantum circuits using the flip-chip assembly. In order to achieve the longest relaxation time ( $T_{1}$ ) of a qubit possible, gap between two chips in flip-chip assembly is determined to be 12 μm where low surface dielectric loss from two-level system (TLS) defects can be achieved while maintaining large readout coupling strength between two chips in the flip-chip assembly. Superconducting transmon qubit design is then optimized to have a target anharmonicity of 200 MHz and to have the longer $T_{1}$ in consideration of surface energy participation ratios of TLS defects within the compact footprint. To achieve strong coupling strength but low qubit to qubit crosstalk (ZZ) for fast and high fidelity multi-qubit gates, direct coupler and compact multi-path coupler designs for coupling qubits are compared by numerically solving Hamiltonian of the coupled two qubits. Monte-Carlo simulation results on the yield rate of the extended circuits indicate that low manufacturing errors are required.


  • Improvement of Pinning Properties by Refining Gd2O3 Particles Trapped in GdBa2Cu3O7-δ Coated Conductors Fabricated by the RCE-DR Process

    by Insung Park, Won-Jae Oh, Jae-Hun Lee, Seung-Hyun Moon, Sang-Im Yoo

    In order to improve in-field J c values of GdBCO CCs fabricated by the reactive co-evaporation by deposition and reaction (RCE-DR) process with the nominal composition of Gd:Ba:Cu = 1:1:2.5, the Gd 2 O 3 particles trapped in the GdBCO superconducting matrix were refined by controlling the nucleation and growth temperature of Gd 2 O 3 in the liquid phase before the growth of GdBCO film at the same growth conditions of 860 °C in 150 mTorr oxygen pressure. With decreasing the growth temperature of Gd 2 O 3 from 860 to 820 °C in the oxygen pressure of 30 mTorr, the average particle size of Gd 2 O 3 was monotonously decreased from 125 ± 41 to 73 ± 31 nm. With refining the average particle size of Gd 2 O 3, while J c in a self-field was monotonously decreased, minimum in-field J c values were first increased and then decreased again. With lowering the growth temperature of Gd 2 O 3 , the gradual decrease of self-field J c may be mainly attributed to the gradual degradation of both in-plane and out-of-plane textures, the variation of the minimum in-field J c values might originate mainly from the variation of the stacking fault density, which, however, requires further analysis.


  • Stability phase diagram of GdBaO for the nominal composition of Gd:Ba:Cu=1:1:2.5 in low oxygen pressures

    by Insung Park, Won-Jae Oh, Jae Hun Lee, Seung-Hyun Moon, Sang-Im Yoo

    The phase stability of the GdBa$_{2}$Cu$_{3}$O$_{7}{\delta}$ (GdBCO) compound was carefully investigated for the nominal composition of Gd:Ba:Cu = 1:1:2.5 in low oxygen pressures (PO$_{2}$) of 1-150 mTorr. Since this composition has been employed for the fabrication of GdBCO coated conductors via the reactive co-evaporation deposition and reaction (RCE-DR) process, it is invaluable to accurately determine the phase stability of GdBCO for an optimal processing of RCE-DR. For this study, Gd-Ba-Cu-O amorphous precursor films were deposited on LaAlO$_{3}$ (001) substrates at 200°C by pulsed laser deposition (PLD). Using a reel-to-reel tube furnace, as-deposited amorphous films were annealed at various high temperatures in low PO$_{2}$. Experimental results reveal that the stability boundary of GdBCO for this composition is remarkably shifted to the lower temperature regions compared with that for the nominal composition of Gd:Ba:Cu = 1:2:3.