Riccardo Ferraresi
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Riccardo Ferraresi has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Giovanna Cornacchia
Department of Mechanical and Industrial Engineering, University of Brescia, Via Branze 38, 25123 Brescia, BS, Italy
2 shared publications Andrea Avanzini
Department of Mechanical and Industrial Engineering University of Brescia via Branze 38 25123 Brescia Italy
1 shared publicationCandida Petrogalli
Department of Mechanical and Industrial Engineering University of Brescia via Branze 38 25123 Brescia Italy
1 shared publication- Omar Bologna
Department of Mechanical and Industrial Engineering, University of Brescia, Via Branze 38, 25123 Brescia, BS, Italy
1 shared publication Silvia Cecchel
Research and Development Streparava S.p.A. Via Zocco 13 25030 Adro (BS) Italy
1 shared publication- Silvia Cecchel
Streparava SpA, Via Zocco 13, 25030 Adro, BS, Italy
1 shared publication
Latest Publications
- Open Access
From Microstructure to Mechanical Performance: Characterization of Similar and Dissimilar Welds in Cast, Wrought, and LPBF Aluminum Alloys
Hybrid lightweight structures increasingly combine cast, wrought, and additively manufactured aluminum alloys, but the mechanical response of their welded joints remains strongly material-dependent. In this study, cast EN AC-42100-T6, wrought EN AW-6082-T6, and laser powder bed fusion (LPBF) AlSi10Mg stress-relieved plates were welded in 4 and 8 mm configurations using cold metal transfer and pulsed multi-control processes over two campaigns. Weld defects, microstructure, hardness profiles, and tensile properties were analyzed using a framework combining a hardness derived local yield-stress descriptor (σy,loc), a cumulative hardness deficit (IDHV), and a porosity increment metric (ΔP). The second campaign eliminated fusion and penetration related defects, but did not mitigate fusion zone porosity in LPBF-related joints, which reached 13.7% in the 8 mm LPBF–Cast joint. Hardness analysis showed the widest hardness-affected region in the wrought alloy, an intermediate response in the cast alloy, and localized alteration in LPBF. Tensile results identified three degradation modes: strength loss associated with heat-affected zone (HAZ) softening in wrought-containing joints, ductility limitation associated with the initial cast condition, and porosity-associated ductility loss in LPBF-related joints. The lower yield strength reduction in LPBF-related joints does not imply improved performance, as fracture remains strongly influenced by fusion zone porosity. The results support material specific mitigation and design strategies for hybrid welded aluminum structures.
Open AccessFrom Microstructure to Mechanical Performance: Characterization of Similar and Dissimilar Welds in Cast, Wrought, and LPBF Aluminum Alloys
Hybrid lightweight structures increasingly combine cast, wrought, and additively manufactured aluminum alloys, but the mechanical response of their welded joints remains strongly material-dependent. In this study, cast EN AC-42100-T6, wrought EN AW-6082-T6, and laser powder bed fusion (LPBF) AlSi10Mg stress-relieved plates were welded in 4 and 8 mm configurations using cold metal transfer and pulsed multi-control processes over two campaigns. Weld defects, microstructure, hardness profiles, and tensile properties were analyzed using a framework combining a hardness derived local yield-stress descriptor (σy,loc), a cumulative hardness deficit (IDHV), and a porosity increment metric (ΔP). The second campaign eliminated fusion and penetration related defects, but did not mitigate fusion zone porosity in LPBF-related joints, which reached 13.7% in the 8 mm LPBF–Cast joint. Hardness analysis showed the widest hardness-affected region in the wrought alloy, an intermediate response in the cast alloy, and localized alteration in LPBF. Tensile results identified three degradation modes: strength loss associated with heat-affected zone (HAZ) softening in wrought-containing joints, ductility limitation associated with the initial cast condition, and porosity-associated ductility loss in LPBF-related joints. The lower yield strength reduction in LPBF-related joints does not imply improved performance, as fracture remains strongly influenced by fusion zone porosity. The results support material specific mitigation and design strategies for hybrid welded aluminum structures.
- Open Access
- 19 November 2021
- Published by Wiley in Advanced Engineering Materials
- Vol. 24 (4)
Microstructural, Mechanical, and Tribological Evolution under Different Heat Treatment Conditions of Inconel 625 Alloy Fabricated by Selective Laser Melting
Additive manufacturing (AM) can be particularly advantageous to manufacture components designed to meet challenging structural requirements. Selective laser melting (SLM) microstructure is different than that obtained by traditional manufacturing process; in particular, mechanical and microstructural features achieved herein are influenced by the entire thermal history, including the manufacturing process and the heat treatment (HT) with relevant role of the slow cooling rate adopted. In fact, both the process and the HTs can significantly modify the microstructure and related mechanical and tribological properties. To better understand how mechanical response can be tuned to meet different requirements, in this article the effects of four different vacuum HTs on microstructures, mechanical properties, and wear behavior of Inconel 625 produced with SLM are deeply investigated. In general, the results confirm that HT can significantly change the microstructure and mechanical or tribological properties of Inconel 625. Among the examined HT, solution + aging and direct aging improve the strength of the alloy, whereas annealing leads to recrystallization, reducing strength in favor of ductility. Stress relieving does not significantly change the microstructure and mechanical properties. Considering tribological behavior, only direct aging HT leads to a remarkable improvement, with a reduction in friction coefficient and wear rate.
- 19 November 2021
- Published by Wiley in Advanced Engineering Materials
- Vol. 24 (4)
Open AccessMicrostructural, Mechanical, and Tribological Evolution under Different Heat Treatment Conditions of Inconel 625 Alloy Fabricated by Selective Laser Melting
Additive manufacturing (AM) can be particularly advantageous to manufacture components designed to meet challenging structural requirements. Selective laser melting (SLM) microstructure is different than that obtained by traditional manufacturing process; in particular, mechanical and microstructural features achieved herein are influenced by the entire thermal history, including the manufacturing process and the heat treatment (HT) with relevant role of the slow cooling rate adopted. In fact, both the process and the HTs can significantly modify the microstructure and related mechanical and tribological properties. To better understand how mechanical response can be tuned to meet different requirements, in this article the effects of four different vacuum HTs on microstructures, mechanical properties, and wear behavior of Inconel 625 produced with SLM are deeply investigated. In general, the results confirm that HT can significantly change the microstructure and mechanical or tribological properties of Inconel 625. Among the examined HT, solution + aging and direct aging improve the strength of the alloy, whereas annealing leads to recrystallization, reducing strength in favor of ductility. Stress relieving does not significantly change the microstructure and mechanical properties. Considering tribological behavior, only direct aging HT leads to a remarkable improvement, with a reduction in friction coefficient and wear rate.