- Debdeep Jena
Department of Materials Science and Engineering, Cornell University 2 , Ithaca, New York 14853
7 shared publications - Huili Grace Xing
Cornell University
7 shared publications - Chandrashekhar Savant
Department of Materials Science and Engineering, Cornell University 3 , Ithaca, New York 14853
5 shared publications - Thai-Son Nguyen
Department of Materials Science and Engineering, Cornell University 3 , Ithaca, New York 14853
4 shared publications - Anand Ithepalli
Department of Materials Science and Engineering, Cornell University 1 , Ithaca, New York 14850
3 shared publications - Craig L. Perkins
National Laboratory of the Rockies Golden Colorado USA
2 shared publications
Latest Publications
- 28 July 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 140 (4)
Annealing reduces leakage current in MBE grown AlScN and AlYN films
Ternary aluminum scandium nitride (AlScN) and aluminum yttrium nitride (AlYN) are emerging wide-bandgap piezoelectric and ferroelectric materials with significant potential for next-generation electronic devices. This work investigates the impact of post-growth annealing on the structural, electrical, and piezoelectric properties of AlScN and AlYN thin films grown by plasma-assisted by molecular beam epitaxy on tungsten electrodes. Annealing is performed in vacuum, air, and nitrogen atmospheres at temperatures ranging from 750 to 1100 °C. It is observed that annealing in air and nitrogen lowers the leakage current in AlScN and AlYN films. Piezoelectric coefficient (d33) enhancements as high as 137 pm/V for AlScN and 8.05 pm/V for AlYN are observed for less leaky, nitrogen-annealed samples at 750 °C. Preservation of ferroelectric switching properties post-annealing is confirmed by piezo-response force microscopy and PUND measurements. These findings highlight the role of thermal treatments on the performance of AlScN and AlYN for piezoelectric, ferroelectric, and high-K dielectric device applications.
- 28 July 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 140 (4)
Annealing reduces leakage current in MBE grown AlScN and AlYN films
Ternary aluminum scandium nitride (AlScN) and aluminum yttrium nitride (AlYN) are emerging wide-bandgap piezoelectric and ferroelectric materials with significant potential for next-generation electronic devices. This work investigates the impact of post-growth annealing on the structural, electrical, and piezoelectric properties of AlScN and AlYN thin films grown by plasma-assisted by molecular beam epitaxy on tungsten electrodes. Annealing is performed in vacuum, air, and nitrogen atmospheres at temperatures ranging from 750 to 1100 °C. It is observed that annealing in air and nitrogen lowers the leakage current in AlScN and AlYN films. Piezoelectric coefficient (d33) enhancements as high as 137 pm/V for AlScN and 8.05 pm/V for AlYN are observed for less leaky, nitrogen-annealed samples at 750 °C. Preservation of ferroelectric switching properties post-annealing is confirmed by piezo-response force microscopy and PUND measurements. These findings highlight the role of thermal treatments on the performance of AlScN and AlYN for piezoelectric, ferroelectric, and high-K dielectric device applications.
- Open Access
- 1 June 2026
- Published by AIP Publishing in AIP Advances
- Vol. 16 (6)
Step-flow homoepitaxial growth of m -sapphire and integration with superconducting TiN
We report step-flow homoepitaxial growth of Al2O3 on m-plane sapphire at a relatively low substrate temperature of 650 °C using molecular beam epitaxy (MBE). The films exhibit atomically smooth terraces with step heights of 0.58 nm, corresponding to two-thirds of the m-plane lattice spacing. A decrease in growth rate of sapphire with increasing aluminum flux beyond a certain value is observed, a growth regime not previously reported for sapphire homoepitaxy. Oxygen plasma surface pre-treatment is found to produce highly uniform step heights and terrace widths upon MBE, enabling reproducible step-flow growth. The m-plane orientation stabilizes the growth of (110)-oriented TiN, eliminating the twin domains observed in TiN grown on c-plane sapphire. TiN films grown on homoepitaxial m-plane Al2O3 show superconductivity below Tc = 5.4 K, room-temperature resistivity of 31.9 μΩ cm, and residual resistivity ratio (RRR) of 2.7, compared to 18.2 μΩ cm and RRR = 3.3 grown directly on as-received substrates. The findings indicate that for qubit applications, m-plane sapphire homoepitaxial layers/epitaxial TiN superconductor interfaces without air exposure are feasible.
- 1 June 2026
- Published by AIP Publishing in AIP Advances
- Vol. 16 (6)
Open AccessStep-flow homoepitaxial growth of m -sapphire and integration with superconducting TiN
We report step-flow homoepitaxial growth of Al2O3 on m-plane sapphire at a relatively low substrate temperature of 650 °C using molecular beam epitaxy (MBE). The films exhibit atomically smooth terraces with step heights of 0.58 nm, corresponding to two-thirds of the m-plane lattice spacing. A decrease in growth rate of sapphire with increasing aluminum flux beyond a certain value is observed, a growth regime not previously reported for sapphire homoepitaxy. Oxygen plasma surface pre-treatment is found to produce highly uniform step heights and terrace widths upon MBE, enabling reproducible step-flow growth. The m-plane orientation stabilizes the growth of (110)-oriented TiN, eliminating the twin domains observed in TiN grown on c-plane sapphire. TiN films grown on homoepitaxial m-plane Al2O3 show superconductivity below Tc = 5.4 K, room-temperature resistivity of 31.9 μΩ cm, and residual resistivity ratio (RRR) of 2.7, compared to 18.2 μΩ cm and RRR = 3.3 grown directly on as-received substrates. The findings indicate that for qubit applications, m-plane sapphire homoepitaxial layers/epitaxial TiN superconductor interfaces without air exposure are feasible.
- Open Access
- 23 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (12)
Molecular beam epitaxy and characterization of wurtzite InScN
We report the molecular beam epitaxial growth and characterization of wurtzite InScN thin films. We find that wurtzite InScN can be grown on GaN substrates under metal-rich conditions, resulting in smooth surfaces with <1 nm roughness and a two-dimensional growth mode. We further find that InScN can be stabilized in the wurtzite crystalline phase for Sc content up to at least 10.4%. We measure and report the lattice parameters of wurtzite InScN as a function of Sc content and find that between ∼5% and 8% Sc mole fraction InScN has a similar a lattice constant to InN. The c/a ratio deviates from the ideal tetrahedral value of 1.633 as Sc content increases. The optical absorption edge of wurtzite InScN monotonically increases over a Sc content range of 0%–10.4% from 0.8 to 1.05 eV, accompanied by a shift in the peak index of refraction and extinction coefficient. The E2high Raman peak of InScN shows negligible shift with increasing Sc content compared to a gradual increase in the A1 (LO) peak position. These fundamental observations can facilitate the future design of InN-based devices.
- 23 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (12)
Open AccessMolecular beam epitaxy and characterization of wurtzite InScN
We report the molecular beam epitaxial growth and characterization of wurtzite InScN thin films. We find that wurtzite InScN can be grown on GaN substrates under metal-rich conditions, resulting in smooth surfaces with <1 nm roughness and a two-dimensional growth mode. We further find that InScN can be stabilized in the wurtzite crystalline phase for Sc content up to at least 10.4%. We measure and report the lattice parameters of wurtzite InScN as a function of Sc content and find that between ∼5% and 8% Sc mole fraction InScN has a similar a lattice constant to InN. The c/a ratio deviates from the ideal tetrahedral value of 1.633 as Sc content increases. The optical absorption edge of wurtzite InScN monotonically increases over a Sc content range of 0%–10.4% from 0.8 to 1.05 eV, accompanied by a shift in the peak index of refraction and extinction coefficient. The E2high Raman peak of InScN shows negligible shift with increasing Sc content compared to a gradual increase in the A1 (LO) peak position. These fundamental observations can facilitate the future design of InN-based devices.
- Open Access
- 16 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (11)
Molecular beam epitaxy of AlScN on Si(111)
Wurtzite aluminum scandium nitride thin films are a leading candidate material for the development of next-generation semiconductor electronic, photonic, and acoustic devices. The integration of high-quality AlScN thin films on a silicon platform is of scientific and commercial interest. Here, we report the successful epitaxial growth of crack-free metal-polar AlScN thin films on (111) silicon substrates by plasma-assisted molecular beam epitaxy. We identify critical nucleation conditions for smooth morphology and growth parameters for high crystal quality and stress mitigation. Using an AlN nucleation layer grown under nitrogen-rich conditions and compositionally graded AlScN buffer layers, we obtain single-phase films with narrow 002 rocking curve FWHM as low as 0.51°, crack-free films up to 150 nm thick with ScN fraction as high as 31%, and surface RMS roughness as low as 0.54 nm over 400μm2, which follow the morphology of the underlying silicon substrates with a mixed 2D–3D growth mode. The lattice parameters, d33 piezoelectric coefficients, and optical bandgap are measured as a function of Sc composition. With increasing Sc composition, the piezoelectric coefficient is enhanced to as high as 34.7 pm/V.
- 16 March 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (11)
Open AccessMolecular beam epitaxy of AlScN on Si(111)
Wurtzite aluminum scandium nitride thin films are a leading candidate material for the development of next-generation semiconductor electronic, photonic, and acoustic devices. The integration of high-quality AlScN thin films on a silicon platform is of scientific and commercial interest. Here, we report the successful epitaxial growth of crack-free metal-polar AlScN thin films on (111) silicon substrates by plasma-assisted molecular beam epitaxy. We identify critical nucleation conditions for smooth morphology and growth parameters for high crystal quality and stress mitigation. Using an AlN nucleation layer grown under nitrogen-rich conditions and compositionally graded AlScN buffer layers, we obtain single-phase films with narrow 002 rocking curve FWHM as low as 0.51°, crack-free films up to 150 nm thick with ScN fraction as high as 31%, and surface RMS roughness as low as 0.54 nm over 400μm2, which follow the morphology of the underlying silicon substrates with a mixed 2D–3D growth mode. The lattice parameters, d33 piezoelectric coefficients, and optical bandgap are measured as a function of Sc composition. With increasing Sc composition, the piezoelectric coefficient is enhanced to as high as 34.7 pm/V.
- Open Access
- 20 February 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (7)
Self-activated growth of cubic AlScN films from molecular nitrogen without plasma
Self-activated growth of ScN was recently reported owing to the ability of scandium to self-catalyze N2 bond breaking, facilitating nitride film growth from molecular N2 without plasma. In this report, we expand this novel synthesis method to explore the possibility of self-activated growth of aluminum–scandium–nitride, an emerging ternary nitride system with enhanced functionalities. We find that the rock salt AlScN film growth of low Al composition from 0% to 48% is possible by self-activated growth. The cubic rock salt AlScN films are phase pure up to 21% Al, whereas mixed rock salt AlScN and intermetallic cubic AlxSc phases appear in films with 28% to 48% Al. Self-activated nitride crystal growth was not observed for films grown with high Al content of 93.7% and 100% Al, which showed cubic AlxSc and FCC α-Al phases, respectively, without any sign of nitrogen incorporation. Lattice parameters of crystalline rock salt AlScN films decrease with increasing Al composition. The self-activated AlScN films, as well as cubic AlxSc and FCC α-Al phase, exhibit twinning and are epitaxial to the 6H-SiC substrate. The findings open up new avenues for the ultralow-energy synthesis of ternary nitrides and beyond.
- 20 February 2026
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 139 (7)
Open AccessSelf-activated growth of cubic AlScN films from molecular nitrogen without plasma
Self-activated growth of ScN was recently reported owing to the ability of scandium to self-catalyze N2 bond breaking, facilitating nitride film growth from molecular N2 without plasma. In this report, we expand this novel synthesis method to explore the possibility of self-activated growth of aluminum–scandium–nitride, an emerging ternary nitride system with enhanced functionalities. We find that the rock salt AlScN film growth of low Al composition from 0% to 48% is possible by self-activated growth. The cubic rock salt AlScN films are phase pure up to 21% Al, whereas mixed rock salt AlScN and intermetallic cubic AlxSc phases appear in films with 28% to 48% Al. Self-activated nitride crystal growth was not observed for films grown with high Al content of 93.7% and 100% Al, which showed cubic AlxSc and FCC α-Al phases, respectively, without any sign of nitrogen incorporation. Lattice parameters of crystalline rock salt AlScN films decrease with increasing Al composition. The self-activated AlScN films, as well as cubic AlxSc and FCC α-Al phase, exhibit twinning and are epitaxial to the 6H-SiC substrate. The findings open up new avenues for the ultralow-energy synthesis of ternary nitrides and beyond.
- 2 June 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 126 (22)
Structural, electronic, and superconducting properties of MBE-grown tantalum nitride films on c-plane sapphire
Two single crystal phases of tantalum nitride were stabilized on c-plane sapphire using molecular beam epitaxy. The phases were identified to be δ-TaN with a rock salt cubic structure and γ-Ta2N with a hexagonal structure. Atomic force microscopy scans revealed smooth surfaces for both the films with root mean square roughnesses less than 0.3 nm. Phase purity of these films was determined by x-ray diffraction. The Raman spectrum of the phase-pure δ-TaN and γ-Ta2N obtained will serve as a future reference to determine phase purity of tantalum nitride films. Furthermore, the room temperature and low-temperature electronic transport measurements indicated that both of these phases are metallic at room temperature with resistivities of 586.2 μΩ · cm for the 30 nm δ-TaN film and 75.5 μΩ · cm for the 38 nm γ-Ta2N film and become superconducting below 3.6 and 0.48 K, respectively. The superconducting transition temperature reduces with applied magnetic field as expected. Ginzburg–Landau fitting revealed a 0 K critical magnetic field and coherence length of 18 T and 4.2 nm for the 30 nm δ-TaN film and 96 mT and 59 nm for the 38 nm γ-Ta2N film. These tantalum nitride films are of high interest for superconducting resonators and qubits.
- 2 June 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 126 (22)
Structural, electronic, and superconducting properties of MBE-grown tantalum nitride films on c-plane sapphire
Two single crystal phases of tantalum nitride were stabilized on c-plane sapphire using molecular beam epitaxy. The phases were identified to be δ-TaN with a rock salt cubic structure and γ-Ta2N with a hexagonal structure. Atomic force microscopy scans revealed smooth surfaces for both the films with root mean square roughnesses less than 0.3 nm. Phase purity of these films was determined by x-ray diffraction. The Raman spectrum of the phase-pure δ-TaN and γ-Ta2N obtained will serve as a future reference to determine phase purity of tantalum nitride films. Furthermore, the room temperature and low-temperature electronic transport measurements indicated that both of these phases are metallic at room temperature with resistivities of 586.2 μΩ · cm for the 30 nm δ-TaN film and 75.5 μΩ · cm for the 38 nm γ-Ta2N film and become superconducting below 3.6 and 0.48 K, respectively. The superconducting transition temperature reduces with applied magnetic field as expected. Ginzburg–Landau fitting revealed a 0 K critical magnetic field and coherence length of 18 T and 4.2 nm for the 30 nm δ-TaN film and 96 mT and 59 nm for the 38 nm γ-Ta2N film. These tantalum nitride films are of high interest for superconducting resonators and qubits.
- 4 July 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 71 (8) , 4968-4976
Performance Limiting Factors of 15-GHz Ku-Band FBARs
We study the loss mechanisms limiting the performance of RF filters with epitaxial aluminum nitride (AlN) thin-film bulk acoustic wave resonators (FBARs) operating at the primary mode of 15 GHz. By measuring the dependence of the resonance frequency and quality factor over the temperature range of 79–400 K, we find that electrical loss in the metal electrodes is the primary limiting factor, followed by acoustic loss in the system as well as dielectric loss in the AlN. We model and discuss the measured intrinsic acoustic attenuation mechanisms in the epitaxial AlN layers. From the quantitative analysis of the temperature-dependent small-signal measurements of the filter RF metrics, we extract several temperature-dependent physical quantities, such as the longitudinal stiffness constant $\textit{c}_{\text{33}}$ of epitaxial AlN, and its longitudinal acoustic phase velocity. A 1% change in the stiffness constant is found to introduce a 100-MHz shift in the resonance frequency. This study identifies roadblocks and provides guidelines for taking the performance of primary mode FBARs to 20 GHz and beyond.
- 4 July 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 71 (8) , 4968-4976
Performance Limiting Factors of 15-GHz Ku-Band FBARs
We study the loss mechanisms limiting the performance of RF filters with epitaxial aluminum nitride (AlN) thin-film bulk acoustic wave resonators (FBARs) operating at the primary mode of 15 GHz. By measuring the dependence of the resonance frequency and quality factor over the temperature range of 79–400 K, we find that electrical loss in the metal electrodes is the primary limiting factor, followed by acoustic loss in the system as well as dielectric loss in the AlN. We model and discuss the measured intrinsic acoustic attenuation mechanisms in the epitaxial AlN layers. From the quantitative analysis of the temperature-dependent small-signal measurements of the filter RF metrics, we extract several temperature-dependent physical quantities, such as the longitudinal stiffness constant $\textit{c}_{\text{33}}$ of epitaxial AlN, and its longitudinal acoustic phase velocity. A 1% change in the stiffness constant is found to introduce a 100-MHz shift in the resonance frequency. This study identifies roadblocks and provides guidelines for taking the performance of primary mode FBARs to 20 GHz and beyond.
- 1 January 2001
- Published by Elsevier in Surface Science
- Vol. 470 (3) , 215-225
Surface properties of Hafnium diboride(0001) as determined by X-ray photoelectron spectroscopy and scanning tunneling microscopy
- 1 January 2001
- Published by Elsevier in Surface Science
- Vol. 470 (3) , 215-225
Surface properties of Hafnium diboride(0001) as determined by X-ray photoelectron spectroscopy and scanning tunneling microscopy
- 1 October 2000
- Published by American Vacuum Society in Surface Science Spectra
- Vol. 7 (4) , 316-321
Characterization of Hafnium Diboride, HfB2 (0001), by XPS
X-ray photoelectron spectra of a clean, well-ordered HfB2 (0001) single crystal surface are reported. A survey spectrum covering a binding energy range of 0 to 1000 eV is shown, which reveals the presence of minor amounts of oxygen and zirconium. Spectra over narrower binding energy ranges are also shown for the Hf 4f, B 1s, and Hf 4s/O 1s regions. A comparison of the Hf 4s/O 1s region before and after oxygen exposure provides for unambiguous assignment of the overlapping O 1s and Hf 4s peaks at binding energies of 531 and 534 eV, respectively.
- 1 October 2000
- Published by American Vacuum Society in Surface Science Spectra
- Vol. 7 (4) , 316-321
Characterization of Hafnium Diboride, HfB2 (0001), by XPS
X-ray photoelectron spectra of a clean, well-ordered HfB2 (0001) single crystal surface are reported. A survey spectrum covering a binding energy range of 0 to 1000 eV is shown, which reveals the presence of minor amounts of oxygen and zirconium. Spectra over narrower binding energy ranges are also shown for the Hf 4f, B 1s, and Hf 4s/O 1s regions. A comparison of the Hf 4s/O 1s region before and after oxygen exposure provides for unambiguous assignment of the overlapping O 1s and Hf 4s peaks at binding energies of 531 and 534 eV, respectively.