Deborah Stona
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Deborah Stona has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Ana Maria Spohr
Pontifícia Universidade Católica do Rio Grande do Sul, Brazil
1 shared publication - Laerte Ohse
Pontifícia Universidade Católica do Rio Grande do Sul, Brazil
1 shared publication - Luiz Henrique Burnett Júnior
Department of Restorative Dentistry, School of Dentistry, Pontifical Catholic University of Rio Grande do Sul, Porto Alegre, Brazil
1 shared publication - Marilia Mattos Sly
Department of Restorative Dentistry & Prosthodontics, UTHealth Houston School of Dentistry, Houston, USA
1 shared publication
Latest Publications
- Open Access
- 1 September 2021
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 32 (5) , 105-113
Fracture strength of teeth restored with milled ultrathin occlusal veneers made of polymer-infiltrated ceramic
The purpose was to evaluate, in vitro, the fracture strength of teeth restored with 0.3- or 0.6-mm-thick occlusal veneers made of Vita Enamic® bonded to enamel or dentin. Fifty third molars were allocated into five groups (n=10): Group C - control (sound teeth); Group 0.3E - 0.3-mm-thick occlusal veneers bonded to enamel; Group 0.6E - 0.6-mm-thick occlusal veneers bonded to enamel; Group 0.3D - 0.3-mm-thick occlusal veneers bonded to dentin; Group 0.6D - 0.6-mm-thick occlusal veneers bonded to dentin. After luting with Single Bond Universal and Filtek Z-100, the samples were subjected to fracture strength test in a universal testing machine. The fractures were classified as irreparable and reparable. Data were analyzed with 2-way and 1-way ANOVA (α=.05) followed by Tukey’s test. The teeth restored with 0.3-mm-thick occlusal veneers (2658 N) achieved significantly higher fracture strength compared to the teeth restored with 0.6-mm-thick occlusal veneers (2070 N) (p=0.017). The teeth restored with occlusal veneers bonded to enamel (2648 N) had significantly higher fracture strength compared to the teeth restored with occlusal veneers bonded to dentin (2049 N) (p=0.015). Group C (3355 N) and Group 0.3E (2965 N) did not differ significantly from each other, being the fracture strength significantly higher than the other groups (p<0.05). The fractures were predominantly reparable. The teeth restored with 0.3-mm-thick occlusal veneers achieved higher fracture strength compared to the teeth restored with 0.6-mm-thick occlusal veneers. The supporting substrate influenced the fracture strength, which was higher for the teeth restored with occlusal veneers bonded to enamel.
- 1 September 2021
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 32 (5) , 105-113
Open AccessFracture strength of teeth restored with milled ultrathin occlusal veneers made of polymer-infiltrated ceramic
The purpose was to evaluate, in vitro, the fracture strength of teeth restored with 0.3- or 0.6-mm-thick occlusal veneers made of Vita Enamic® bonded to enamel or dentin. Fifty third molars were allocated into five groups (n=10): Group C - control (sound teeth); Group 0.3E - 0.3-mm-thick occlusal veneers bonded to enamel; Group 0.6E - 0.6-mm-thick occlusal veneers bonded to enamel; Group 0.3D - 0.3-mm-thick occlusal veneers bonded to dentin; Group 0.6D - 0.6-mm-thick occlusal veneers bonded to dentin. After luting with Single Bond Universal and Filtek Z-100, the samples were subjected to fracture strength test in a universal testing machine. The fractures were classified as irreparable and reparable. Data were analyzed with 2-way and 1-way ANOVA (α=.05) followed by Tukey’s test. The teeth restored with 0.3-mm-thick occlusal veneers (2658 N) achieved significantly higher fracture strength compared to the teeth restored with 0.6-mm-thick occlusal veneers (2070 N) (p=0.017). The teeth restored with occlusal veneers bonded to enamel (2648 N) had significantly higher fracture strength compared to the teeth restored with occlusal veneers bonded to dentin (2049 N) (p=0.015). Group C (3355 N) and Group 0.3E (2965 N) did not differ significantly from each other, being the fracture strength significantly higher than the other groups (p<0.05). The fractures were predominantly reparable. The teeth restored with 0.3-mm-thick occlusal veneers achieved higher fracture strength compared to the teeth restored with 0.6-mm-thick occlusal veneers. The supporting substrate influenced the fracture strength, which was higher for the teeth restored with occlusal veneers bonded to enamel.