Hailiang Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Hailiang Wang has a total of 60 co-authors. Here are the top co-authors by number of shared publications:
- Hailong Wang
School of Materials Science and Engineering Zhengzhou University Zhengzhou China
4 shared publications Hailong Wang
3 shared publicationsJingli Shi
3 shared publicationsMingliang Li
3 shared publicationsYongqiang Chen
3 shared publicationsBingbing Fan
2 shared publications
Latest Publications
- 6 September 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (25) , 47526-47541
Multidimensional structural design realizes synergistic enhancement of mechanical properties and electromagnetic wave absorption of B4C-Graphite-SiCw composites
- 6 September 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (25) , 47526-47541
Multidimensional structural design realizes synergistic enhancement of mechanical properties and electromagnetic wave absorption of B4C-Graphite-SiCw composites
- 28 September 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (1)
Toward a low‐temperature sintering of carbon fiber toughened high entropy boride composite with Co addition
Dense C f /(ZrHfNbTaCr)B 2 –SiC (CBS‐Co) composite is successfully prepared at a low temperature of 1500°C by adding 5 vol.% Co. Liquid Co accelerates the particle rearrangement and significantly enhances the relative density of CBS‐Co (95.2%). In situ formed Co 2 B phase by diffusion reaction bonds tightly with high entropy diboride (HEB) and SiC grains in CBS‐Co. Due to the promotion of relative density and interfacial bonding strength, CBS‐Co exhibits a high flexural strength (283 ± 23 MPa). Structural damages of carbon fibers are effectively prevented by compact fiber coating. The well‐preserved fibers play dominant roles to increase the fracture toughness of CBS‐Co (4.77 ± .5 MPa·m 1/2 ). Moreover, SiO 2 ‐rich oxide layer can effectively heal flaws and inhibit oxygen diffusion, achieving relatively high flexural strength after oxidation at 1300°C of CBS‐Co composite. This work provides a stepping stone for developing high‐performance carbon fiber toughened HEB composites based on low temperature liquid‐phase sintering technology.
- 28 September 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (1)
Toward a low‐temperature sintering of carbon fiber toughened high entropy boride composite with Co addition
Dense C f /(ZrHfNbTaCr)B 2 –SiC (CBS‐Co) composite is successfully prepared at a low temperature of 1500°C by adding 5 vol.% Co. Liquid Co accelerates the particle rearrangement and significantly enhances the relative density of CBS‐Co (95.2%). In situ formed Co 2 B phase by diffusion reaction bonds tightly with high entropy diboride (HEB) and SiC grains in CBS‐Co. Due to the promotion of relative density and interfacial bonding strength, CBS‐Co exhibits a high flexural strength (283 ± 23 MPa). Structural damages of carbon fibers are effectively prevented by compact fiber coating. The well‐preserved fibers play dominant roles to increase the fracture toughness of CBS‐Co (4.77 ± .5 MPa·m 1/2 ). Moreover, SiO 2 ‐rich oxide layer can effectively heal flaws and inhibit oxygen diffusion, achieving relatively high flexural strength after oxidation at 1300°C of CBS‐Co composite. This work provides a stepping stone for developing high‐performance carbon fiber toughened HEB composites based on low temperature liquid‐phase sintering technology.
- 27 November 2023
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 589
Fabrication and conductivity of zirconium doped Li2TiO3 tritium breeder
- 27 November 2023
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 589
Fabrication and conductivity of zirconium doped Li2TiO3 tritium breeder
- Open Access
- 27 June 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (4)
Insight into the effect of coexistence of CO2 and H2 on stoichiometric and defective PuO2 surfaces hydriding from first-principles study
Studying the effect of coexistence of CO2 and H2 on plutonium hydriding is of great significance for nuclear safety storage and disposal. In this work, we studied the microscopic adsorption morphology of CO2 and H2 molecules with low and high coverage on stoichiometric PuO2 (111) and (110) surfaces. The adsorption energy results showed that both CO2 and H2 have relatively strong reactivity with the (110) surface. The CO2 molecule may be dominant in competitive adsorption with H2. The influences of the coexistence of CO2 and H2 on the adsorption and dissociation behavior for H2 on stoichiometric and defective surfaces were further researched. The CO2 adsorption configuration on the defect surface reveals that the O atom attempts to “heal” the oxygen vacancy. The results show that the presence of CO2 can weaken the interface interaction between H2 and the surface, and increase the H2 dissociation energy barrier on the surface from about 0.518 eV to about 0.791 eV. The electronic properties and work function show that the adsorbed CO2 hinders the electron interaction between H2 and surface resulting in the blocking of hydrogen adsorption and dissociation, which may be the reason for inhibiting the hydrogenation of plutonium. Our study could provide new insights into the CO2 effect on the hydriding process of active metals.
- 27 June 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (4)
Open AccessInsight into the effect of coexistence of CO2 and H2 on stoichiometric and defective PuO2 surfaces hydriding from first-principles study
Studying the effect of coexistence of CO2 and H2 on plutonium hydriding is of great significance for nuclear safety storage and disposal. In this work, we studied the microscopic adsorption morphology of CO2 and H2 molecules with low and high coverage on stoichiometric PuO2 (111) and (110) surfaces. The adsorption energy results showed that both CO2 and H2 have relatively strong reactivity with the (110) surface. The CO2 molecule may be dominant in competitive adsorption with H2. The influences of the coexistence of CO2 and H2 on the adsorption and dissociation behavior for H2 on stoichiometric and defective surfaces were further researched. The CO2 adsorption configuration on the defect surface reveals that the O atom attempts to “heal” the oxygen vacancy. The results show that the presence of CO2 can weaken the interface interaction between H2 and the surface, and increase the H2 dissociation energy barrier on the surface from about 0.518 eV to about 0.791 eV. The electronic properties and work function show that the adsorbed CO2 hinders the electron interaction between H2 and surface resulting in the blocking of hydrogen adsorption and dissociation, which may be the reason for inhibiting the hydrogenation of plutonium. Our study could provide new insights into the CO2 effect on the hydriding process of active metals.
- 31 March 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (14) , 6361-6374
New insights for strengthening and toughening mechanisms of dislocation in B4C–ZrB2–SiC composites using vacuum hot pressing assisted by reaction sintering (VHP-RS)
- 31 March 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (14) , 6361-6374
New insights for strengthening and toughening mechanisms of dislocation in B4C–ZrB2–SiC composites using vacuum hot pressing assisted by reaction sintering (VHP-RS)
- Open Access
The Fabrication and Mechanical Properties of Laminated ZrB2-Mo5SiB2 Ceramics with an Mo-Mo5SiB2 Interlayer
The excellent physical and chemical properties of ultra-high temperature ceramics make them suitable for many high-temperature structural components, while their poor toughness and high sintering temperature become key limitations to their application. Laminated toughening has long been considered an effective toughening method to improve the mechanical properties of ceramics. In this study, laminated ZrB2-Mo5SiB2 ceramics with an Mo-Mo5SiB2 interlayer were fabricated by tape casting and hot press sintering at 1900 °C for 2 h. Different layer thickness ratios between the matrix layer and the interlayer were designed to illustrate the toughening mechanism. Both the fracture toughness and flexural strength of the laminated ceramics showed a trend of first increasing and then decreasing with the increase of the layer thickness ratio. High fracture toughness (9.89 ± 0.26 MPa·m1/2) and flexural strength (431.6 ± 15.1 MPa) were obtained when the layer thickness ratio was 13. The improvement in fracture toughness of the laminated ceramics could be attributed to the generation of the residual stress, the deflection and the bifurcation of the cracks. Residual stress that developed in the laminated ceramics was also evaluated.
Open AccessThe Fabrication and Mechanical Properties of Laminated ZrB2-Mo5SiB2 Ceramics with an Mo-Mo5SiB2 Interlayer
The excellent physical and chemical properties of ultra-high temperature ceramics make them suitable for many high-temperature structural components, while their poor toughness and high sintering temperature become key limitations to their application. Laminated toughening has long been considered an effective toughening method to improve the mechanical properties of ceramics. In this study, laminated ZrB2-Mo5SiB2 ceramics with an Mo-Mo5SiB2 interlayer were fabricated by tape casting and hot press sintering at 1900 °C for 2 h. Different layer thickness ratios between the matrix layer and the interlayer were designed to illustrate the toughening mechanism. Both the fracture toughness and flexural strength of the laminated ceramics showed a trend of first increasing and then decreasing with the increase of the layer thickness ratio. High fracture toughness (9.89 ± 0.26 MPa·m1/2) and flexural strength (431.6 ± 15.1 MPa) were obtained when the layer thickness ratio was 13. The improvement in fracture toughness of the laminated ceramics could be attributed to the generation of the residual stress, the deflection and the bifurcation of the cracks. Residual stress that developed in the laminated ceramics was also evaluated.