Chayanan Boonrawd
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Chayanan Boonrawd has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Darapond Triampo
Department of Chemistry, Faculty of Science, Mahidol University, Nakhon Pathom 73170, Thailand
2 shared publications - Supan Yodyingyong
Institute for Innovative Learning, Mahidol University, Nakhon Pathom 73170, Thailand
2 shared publications - Lazhar Benyahia
IMMM, UMR 6283 CNRS - Le Mans Université, Avenue Olivier Messiaen, 72085 Le Mans Cedex 9, France
1 shared publication - Wanwilai Vittayakorn
Electroceramics Research Laboratory (ECRL), College of Materials Innovation and Technology, King Mongkut’s Institute of Technology Ladkrabang, Bangkok 10520, Thailand
1 shared publication
Latest Publications
- Open Access
Effect of Pre-Vulcanization Time on Structure and Thermal Insulation of Natural Rubber Latex/Silica Aerogel Composites
Polymer/Silica aerogel (SA) composites improve mechanical properties strategically, but the mixing process disrupts the aerogel’s structure, reducing its efficiency due to polymer chains filling the pores. Pre-vulcanized natural rubber latex (PVNRL) with a higher crosslink density can strain the moving chains, thereby preserving the SA-porous structure in the bulk composite for thermal insulation materials. This study aimed to investigate the effects of PVNRL pre-vulcanization time and SA-immersion time in PVNRL. For PVNRL/SA composite preparation, various PVNRL, from 0 days to 8 days of pre-vulcanization time, were mixed with a fixed SA content of 20 parts per hundred of rubber (phr) using a latex compounding method. Subsequently, the PVNRL/SA slurries were cast on glass plates with 0, 3, and 6 days to obtain the PVNRL/SA composite. Considering the effect of pre-vulcanization time, the crosslink density of the composite increased and revealed a peak at PVNRL/SA with 8-day PVNRL by 7.277 ± 0.881 μmol , corresponding to the closest percentage of pore area in the SA’s structure to the pristine SA, and eventually a 42.41% lower thermal conductivity than the PVNRL/SA with 0-day PVNRL exhibited. In addition, the thermal conductivity increased more slowly over immersion time with the presence of 8-day PVNRL. The proposed correlation states that increasing the pre-vulcanization improves the thermal insulation performance of PVNRL/SA composites, emphasizing the reduction of filled SA’s pore with unvulcanized NR chains. Furthermore, the PVNRL/SA composite with 8-day PVNRL maintains thermal stability at 387.3 °C, and can be flexed at room temperature. These fascinating discoveries may be advantageous for further applications related to thin-film and flexible thermal insulation materials.Open AccessEffect of Pre-Vulcanization Time on Structure and Thermal Insulation of Natural Rubber Latex/Silica Aerogel Composites
Polymer/Silica aerogel (SA) composites improve mechanical properties strategically, but the mixing process disrupts the aerogel’s structure, reducing its efficiency due to polymer chains filling the pores. Pre-vulcanized natural rubber latex (PVNRL) with a higher crosslink density can strain the moving chains, thereby preserving the SA-porous structure in the bulk composite for thermal insulation materials. This study aimed to investigate the effects of PVNRL pre-vulcanization time and SA-immersion time in PVNRL. For PVNRL/SA composite preparation, various PVNRL, from 0 days to 8 days of pre-vulcanization time, were mixed with a fixed SA content of 20 parts per hundred of rubber (phr) using a latex compounding method. Subsequently, the PVNRL/SA slurries were cast on glass plates with 0, 3, and 6 days to obtain the PVNRL/SA composite. Considering the effect of pre-vulcanization time, the crosslink density of the composite increased and revealed a peak at PVNRL/SA with 8-day PVNRL by 7.277 ± 0.881 μmol , corresponding to the closest percentage of pore area in the SA’s structure to the pristine SA, and eventually a 42.41% lower thermal conductivity than the PVNRL/SA with 0-day PVNRL exhibited. In addition, the thermal conductivity increased more slowly over immersion time with the presence of 8-day PVNRL. The proposed correlation states that increasing the pre-vulcanization improves the thermal insulation performance of PVNRL/SA composites, emphasizing the reduction of filled SA’s pore with unvulcanized NR chains. Furthermore, the PVNRL/SA composite with 8-day PVNRL maintains thermal stability at 387.3 °C, and can be flexed at room temperature. These fascinating discoveries may be advantageous for further applications related to thin-film and flexible thermal insulation materials. - Open Access
Novel Solvent–Latex Mixing: Thermal Insulation Performance of Silica Aerogel/Natural Rubber Composite
In this work, the novel natural rubber latex (NRL) mixing was approached. The mixing process was carried out by using n-hexane as the dispersed phase of silica aerogel which acted as thermal insulation filler prior to NRL mixing. The silica aerogel/NR composites were prepared with different silica aerogel contents of 20, 40, 60, 80, and 100 parts per hundred rubber (phr). The morphology of the 40 phr composite showed the NR macropore formation with silica aerogel intercalated layers. The optimal content of silica aerogels and n-hexane were the key to obtaining the NR macropore. The thermal insulation performance of silica aerogel/NR composites was investigated because of their porous structures. The thermal conductivity of the composites were lower than that of the neat NR sheet and decreased from 0.081 to 0.055 W m−1·K−1 with increasing silica aerogel content. The lower densities of the composites than that of the NR sheet were revealed noticeably. In addition, the silica aerogel/NR composites exhibited a higher heat retardant ability than that of the NR sheet, and the comparable glass transition temperatures (Tg) of the composites and the neat NR indicated the maintained flexibility at ambient temperature or higher, which can benefit various temperature applications. The overall results demonstrated that the silica aerogel/NR composites from the novel NRL mixing preparation could be a promising technique to develop the porous materials and be utilised as thermal insulation products and building constructions.
Open AccessNovel Solvent–Latex Mixing: Thermal Insulation Performance of Silica Aerogel/Natural Rubber Composite
In this work, the novel natural rubber latex (NRL) mixing was approached. The mixing process was carried out by using n-hexane as the dispersed phase of silica aerogel which acted as thermal insulation filler prior to NRL mixing. The silica aerogel/NR composites were prepared with different silica aerogel contents of 20, 40, 60, 80, and 100 parts per hundred rubber (phr). The morphology of the 40 phr composite showed the NR macropore formation with silica aerogel intercalated layers. The optimal content of silica aerogels and n-hexane were the key to obtaining the NR macropore. The thermal insulation performance of silica aerogel/NR composites was investigated because of their porous structures. The thermal conductivity of the composites were lower than that of the neat NR sheet and decreased from 0.081 to 0.055 W m−1·K−1 with increasing silica aerogel content. The lower densities of the composites than that of the NR sheet were revealed noticeably. In addition, the silica aerogel/NR composites exhibited a higher heat retardant ability than that of the NR sheet, and the comparable glass transition temperatures (Tg) of the composites and the neat NR indicated the maintained flexibility at ambient temperature or higher, which can benefit various temperature applications. The overall results demonstrated that the silica aerogel/NR composites from the novel NRL mixing preparation could be a promising technique to develop the porous materials and be utilised as thermal insulation products and building constructions.