AEAhmed Abdelrahman Elshami

Ahmed Abdelrahman Elshami

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Ahmed Abdelrahman Elshami has a total of 26 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effect of Magnetized Water-Based Alkaline Activator on Geopolymer Concrete Mechanical Performance and Durability

    by Sarah A. Khattab, Mohamed M. Yousry Elshikh, Walid E. Elemam, Ahmed A. Elshami, Osama Youssf

    One of the most important challenges in developing the concrete industry is to use sustainable materials that are able to improve concrete properties. Magnetized water (MW) is a type of water that can replace tap water (TW) in conventional concrete and enhance its mechanical properties. However, the performance of MW in geopolymer concrete has not been well investigated up to now. The goal of this study is to measure the effect of using an alkaline activator (AA) made of MW on the mechanical properties and durability of fly ash (FA)-based geopolymer concrete. The AA was a mixture of sodium hydroxide (SH) solution and sodium silicate (SS) solution. Eighteen geopolymer concrete mixes were tested for several fresh, hardened, and durability properties. Of these mixes, nine were prepared with AA made of MW and the other nine were the same but prepared with AA made of TW. The preparation of MW was simply carried out by passing TW across permanent magnets of 1.6 Tesla, and then 1.4 Tesla intensities for 150 cycles. The MW-based AA properties were analyzed and compared to those of the conventional TW-based AA. Several mechanical and durability properties were measured. Scanning electronic microscopy (SEM) analysis was also conducted on selected mixes. The outcomes of the hardened concrete tests demonstrated that while using MW to prepare AA solution contained SH with a molarity of 16 M, an SS/SH ratio of 2, an AA/C ratio of 0.4, a W/C ratio of 10%, and a curing temperature of 115 °C could display the best outcomes in this study when used in geopolymer concrete. Using MW in a geopolymer concrete AA could increase its slump by up to 100% compared to that made of TW. Using MW in the AA enhanced the compressive strength by up to 193%, 192%, and 124% after 7, 28, and 56 days, respectively. The SEM analysis showed that using MW clearly enhanced the surface morphology of geopolymer concrete. The proposed geopolymer concrete made using the MW-based AA in this study sheds the light on a new class of eco-friendly concrete that could possibly be used in many structural applications.


  • Open Access

    Effect of Water Magnetization Technique on the Properties of Metakaolin-Based Sustainable Concrete

    by Ahmed M. Elkerany, Mohamed M. Yousry Elshikh, Ahmed A. Elshami, Osama Youssf

    Using metakaolin (MK) in concrete with magnetized water (MW) has a high possibility to enhance concrete suitability. In this study, the effect of using MK and MW on concrete characteristics was studied through testing twelve concrete mixes. Seven ratios of MK were used in this study, namely 0%, 5%, 10%, and 20%, as an alternative to cement and +5%, +10%, and +20% as a cement additive. In addition, five water magnetization methods were applied on MK concrete. In the first stage of this study, the impact of different MK ratios on the workability of concrete, compressive strength, flexural strength, and tensile strength was studied using traditional tap water (TW) as the concrete mixing water. In the second stage, the best mix (best MK ratio) from the first stage was chosen to study the effect of the water magnetization method on concrete properties and to determine the best method for water magnetization. Scanning electronic microscope (SEM) analysis was also carried out on selected mixes to closely investigate the effect of MK and MW on concrete microstructure. The results showed that the best ratio of MK in concrete was +10% (MK as a 10% cement addition), and the best water magnetization method was to pass the water through 1.6 tesla then through 1.4 tesla magnetic fields. The SEM analysis confirmed the absence of pores after using MW instead of regular TW by increasing the calcium silicate hydrate (CSH) gel and reducing calcium hydroxide (CH). Using MK and MW enhanced the compressive strength by up to 33%, 32%, and 27% at 7, 28, and 365 days, respectively, and MW enhanced the workability by up to 3% compared to that of the control mix.


  • Open Access

    Investigating the Effects of Recycled Aggregate and Mineral Admixtures on the Mechanical Properties and Performance of Concrete

    by Amal Fawzy, Ahmed Elshami, Seleem Ahmad

    In this work, the effects of recycled concrete aggregate, modified with mineral admixtures and nanosilica, on the mechanical properties and performance of concrete after curing in tap water for 28 and 90 days were investigated. The compressive (ƒc), indirect tensile (ƒt), and flexural (ƒb) strengths for the cured concrete specimens were measured, and the concrete strength ratios were analyzed. The water and rapid chloride permeabilities were measured. SEM analysis of the microstructure was also performed. The coarse aggregates used were dolomite (control) and recycled concrete aggregate, incorporating different mineral admixtures, including ground, granulated blast slag, granite, and nanosilica. It was found that the slump values of the dolomite concrete decreased compared with recycled aggregate concrete. Compared to the control mix produced with the recycled aggregate, the slump value of the concrete mixes created with the recycled aggregate increased by approximately 11.1% with the addition of binary cementing materials of 1% NS. The results also indicate that the concrete mix containing the recycled aggregate had the highest compressive strength, tensile strength, and flexural strength compared to that of the dolomite aggregate. Regarding the compressive strength, the addition of 1% NS and 15% slag improved the physico-mechanical properties of the recycled aggregate concretes compared to the other mixes after curing in tap water. Compared to the other mixes, the concrete mix containing 1% NS and 15% slag had a comparatively dense and compact microstructure.


  • Open Access

    Investigate the Effect of Recycled Aggregate and Mineral Admixtures on the Mechanical Properties and Performance of Concrete

    by Amal Fawzy, Ahmed El-Shami, Seleem Ahmad

    In this work the effect of recycled concrete aggregate modified with mineral admixtures and Nano-silica on the mechanical properties and performance of the concrete was investigated after curing in tap water for 28 and 90 days. The compressive, ƒc, indirect tensile, ƒt, and flexural, ƒb, strengths for cured concrete specimens were measured and concrete strength ratios were analyzed. The water and rapid chloride permeability were measured. SEM analysis of microstructure was, also, investigated. The coarse aggregates used were dolomite (control) and recycled concrete aggregate with the incorporation of different mineral admixtures including ground granulated blast slag and granite as well as Nano-silica. It was found that, the slump values of the dolomite concrete decreases compared with recycle aggregate concrete. The results indicate that, the concrete mix containing recycle aggregate have the highest compressive strength, tensile strength and flexural strength compered to concrete mix containing dolomite aggregate. As far as the compressive strength is concerned, the addition 1 % NS and 15 % of slag improved the physico-mechanical properties of the recycled aggregate concretes compared to the other mixes after curing in tap water.


  • Open Access

    Characteristics of Sustainable Concrete Containing Metakaolin and Magnetized Water

    by Ahmed M. Elkerany, Mostafa M. Keshta, Mohamed M. Yousry Elshikh, Ahmed A. Elshami, Osama Youssf

    In this study, fourteen sustainable concrete mixes containing metakaolin (MK) as supplementary cement material (SCM) and magnetized water (MW) as concrete mixing water were designed, prepared, tested, analyzed, and compared. The MK was used as a partial replacement of cement weight by 5%, 10%, and 20%, and as an additive to cement by 5%, 10%, and 20% of cement weight. The MW was used to fully replace tap water (TW) in concrete mixes and was prepared using two different magnetic fields of 1.4 tesla (T) and 1.6 T. This experimental research aimed to assess the characteristics of concrete manufactured with MK and MW. The mechanical and durability characteristics of fresh and hardened concrete were measured for the assessment. Microstructural and chemical analyses were carried out on selected materials and concrete mixes. The workability and compressive strength of the materials at 7, 28, and 365 days were measured, in addition to the splitting tensile strength at 28 days and the flexural strength at 28 days. The compressive strength at 365 days was conducted at 18 °C and 100 °C to study the effect of the applied variables on the concrete durability at different elevated temperatures. The microstructural and chemical analyses were conducted using a scanning electron microscope (SEM), energy dispersive X-ray (EDX), and Fourier transform infrared (FTIR) spectroscopy. The results showed that using 10% MK as a cement additive was the best ratio in this study, which enhanced all the measured mechanical characteristics when the TW or MW was used. Using MW instead of TW in MK concrete increased all the mechanical properties measured at 28 days by about 32–35%. The results of the microstructural and chemical analyses supported the compressive strength increase by showing indications of more C-S-H gel production and less CH when using MW in MK concrete. In addition, fewer micro-cracks and pores, and relatively denser concrete, were detected when using MW with 10% MK as a cement additive.


  • Open Access

    Effects of Five Sources of Mixing Water on Durability of Concrete

    by Ahmed Abdelrahman Elshami

    This paper presents the experimental approach and the first results obtained as a result of the effect of five Sources of mixing water on produce more durable concrete . Five types of water were used, namely simulated acid rain (AR), Rain water (RW), tap water (TW), Zamzam water (ZW) and sea water (SW) as mixing water for ordinary portland cement concrete (OPCC). The durability of these different types of water were tested toward their capacity to prevent the rebar corrosion. The results of workability, pH value, compressive strength, chlorides penetration and microstructure of different specimens mixed with each type of water were compared with those mixed with tap water (TW). In the present research, the effect of five sources of mixing water on durability of concrete mixes was investigated, incorporating different contents of silica fume. Chloride profile, gas permeability, Compressive Strength, Energy Dispersive X-Ray Analysis EDX, scanning electron microscope SEM, and water porosity tests are used for this propose

  • Open Access

    Effects of Five Sources of Mixing Water on Durability of Concrete

    by Ahmed. A. Elshami

    This paper presents the experimental approach and the first results obtained as a result of the effect of five Sources of mixing water on produce more durable concrete. Five types of water were used, namely simulated acid rain (AR), Rain water (RW), tap water (TW), Zamzam water (ZW) and sea water (SW) as mixing water for ordinary portland cement concrete OPCC. The durability of these different types of water were tested toward their capacity to prevent the rebar corrosion. The results of workability, pH value, compressive strength, chlorides penetration and microstructure of different specimens mixed with each type of water were compared with those mixed with tap water (TW).

  • Open Access

    Microstructure characterization of sustainable light weight concrete using trapped air additions.

    by Said Maaty, Ahmed Elshami, Fryal Kamel

    Light-weight aggregate and trapped air additions (TAD) affect concrete performance and lead to the production of light-weight concrete (LWC). In this research, fourteen mixes were designed to study the effects of TAD type and content and pozzolanic material (PZ) type on the microstructure characterization of concrete. Aluminum powder (AP) and lightcrete (LC) were used as TAD with content equal to (0%, 0.25%, 0.50%, 0.57%). The PZ included silica fume (SF) and fly ash (FA) with a content equal to 10% of the weight of cement. Tests were performed for compressive strength, density, SEM, EDS, XRD, and TGA/DTG. The results show that compressive strength and density are reduced as TAD ratios are increased.


  • Open Access

    Experimentally evaluation of high-performance concrete mixes used for tunnels and containing silica fume and polypropylene fiber after exposed to high temperatures

    by Mohamed Elmesiri, Mohamed Fawzy Ahmed, Mohamed Bneni, Ahmed ElShami, Seleem Ahmad

    This work introduces an experimental study to evaluate the effect of elevated temperatures on the mechanical properties of high-performance concrete (HPC) mix with changes in Water-Cementitious ratios, W/(C+SF), Silica Fume percent, SF, and Polypropylene, PP, fiber contents. This mix was typically designed to satisfy the requirements of tunnel concrete. The compressive and indirect tensile strengths were measured at room temperature, RT, and after exposure to 400°C and 800°C. Moreover, SEM micrograph and EDS spot analysis tests were done to evaluate the effect of elevated temperatures. Fifteen mixes of HPC with different ratios of W/(C+SF), SF, and PP fiber were tested. According to the test results, the compressive strength values of design mixes increased significantly after exposure to 400°C. Moreover, using SF = 10%, the results indicated remarkable improvements in the compressive strength at 400°C and 800°C, in the case of the W/(C+SF) ratio of 0.31. On the other hand, the highest effect of the presence of PP fibers was 0.211, depending on variable ratios of the W/(C+SF) ratio and the SF content. In the case of PP=0.106 and SF=10%, the mass loss was higher at exposure to temperatures of 800°C.

  • Bacterial sustainable concrete for repair and rehabilitation of structural cracks

    by Seleem S. E. Ahmad, Mohamed.A.R. Elmahdy, A.A Elshami, El-Shikh M. Yousry

    Self-healing concrete is an advanced, sustainable technique that has the potential to reduce maintenance costs by automatically repairing cracks. Some Bacillus species produce a urease enzyme to precipitate calcite during biomineralization, which can act as a binding filling material. This study investigated the effects of bacteria type, content and concentration, and nutrient content on the properties of self-healing concrete, especially at the age of 90 days. Bacillus Sphaericus and Bacillus Megaterium were introduced into the concrete at two concentrations, 2 × 108 and 2 × 109 (CFU/ml), and different percentages of bacteria were selected using calcium lactate as a nutrient material. Tests were performed for compressive strength, SEM, EDS, water permeability, rapid chloride permeability, and TGA/DTG. The results show significant development in compressive strength and microstructure characterization of concrete, especially with Bacillus Megaterium using a 2.5% bacterial proportion with a concentration of 2 × 109 CFU/ml and 1% of calcium lactate.