Kusdianto Kusdianto
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Kusdianto Kusdianto has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
- Sugeng Winardi
Chemical Engineering Department, Institut Teknologi Sepuluh Nopember, Kampus ITS Sukolilo, Surabaya 60111, Indonesia
6 shared publications - Manabu Shimada
Chemical Engineering Program, Graduate School of Advanced Science and Engineering, Hiroshima University, 4-1, Kagamiyama 1-chome, Higashi-Hiroshima 739-8527, Hiroshima, Japan
3 shared publications - Meditha Hudandini
Chemical Engineering Program, Graduate School of Advanced Science and Engineering, Hiroshima University, 1-4-1, Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan
3 shared publications - Masaru Kubo
Chemical Engineering Program, Graduate School of Advanced Science and Engineering, Hiroshima University, 1-4-1, Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan
2 shared publications Nurdiana Ratna Puri
Department of Chemical Engineering, Institut Teknologi Sepuluh Nopember, Kampus ITS Sukolilo, Surabaya 60111, Indonesia
2 shared publicationsSuci Madhania
Institut Teknologi Sepuluh Nopember Surabaya
2 shared publications
Latest Publications
- 17 March 2025
- Published by Springer Nature
- p. 197-205
Scale-Up of Bubble Column Reactor for Carbon Mineralization with Precipitated CaCO3 Product
- 17 March 2025
- Published by Springer Nature
- p. 197-205
Scale-Up of Bubble Column Reactor for Carbon Mineralization with Precipitated CaCO3 Product
- 18 February 2025
- Published by Springer Nature
- p. 189-201
Battery Pack Cooling Phenomenon at Varied Air Cooling Temperature Using Computational Fluid Dynamics
- 18 February 2025
- Published by Springer Nature
- p. 189-201
Battery Pack Cooling Phenomenon at Varied Air Cooling Temperature Using Computational Fluid Dynamics
- Open Access
Gas-Phase Fabrication and Photocatalytic Activity of TiO2 and TiO2–CuO Nanoparticulate Thin Films
CuO-loaded TiO2 nanomaterials have applications in pollutant degradation via photocatalysis. However, the existing methods of fabricating these nanomaterials involve liquid-phase processes, which require several steps and typically generate liquid waste. In this study, TiO2 and TiO2–CuO nanoparticulate thin films were successfully fabricated through a one-step gas-phase approach involving a combination of plasma-enhanced chemical vapor deposition and physical vapor deposition. The resulting films consisted of small, spherical TiO2 nanoparticles with observable CuO on the TiO2 surface. Upon annealing in air, the TiO2 nanoparticles were crystallized, and CuO was completely oxidized. The photocatalytic activity of TiO2–CuO/H2O2, when introduced into the rhodamine 6G degradation system, was substantially enhanced under both ultraviolet and visible light irradiation. Moreover, this study highlights the influence of pH on the photocatalytic activity; TiO2–CuO/H2O2 exhibited the highest photocatalytic activity at pH 13, with a reaction rate constant of 0.99 h−1 cm−2 after 180 min of visible light irradiation. These findings could facilitate the development of nanoparticulate thin films for enhanced pollutant degradation in wastewater treatment.
Open AccessGas-Phase Fabrication and Photocatalytic Activity of TiO2 and TiO2–CuO Nanoparticulate Thin Films
CuO-loaded TiO2 nanomaterials have applications in pollutant degradation via photocatalysis. However, the existing methods of fabricating these nanomaterials involve liquid-phase processes, which require several steps and typically generate liquid waste. In this study, TiO2 and TiO2–CuO nanoparticulate thin films were successfully fabricated through a one-step gas-phase approach involving a combination of plasma-enhanced chemical vapor deposition and physical vapor deposition. The resulting films consisted of small, spherical TiO2 nanoparticles with observable CuO on the TiO2 surface. Upon annealing in air, the TiO2 nanoparticles were crystallized, and CuO was completely oxidized. The photocatalytic activity of TiO2–CuO/H2O2, when introduced into the rhodamine 6G degradation system, was substantially enhanced under both ultraviolet and visible light irradiation. Moreover, this study highlights the influence of pH on the photocatalytic activity; TiO2–CuO/H2O2 exhibited the highest photocatalytic activity at pH 13, with a reaction rate constant of 0.99 h−1 cm−2 after 180 min of visible light irradiation. These findings could facilitate the development of nanoparticulate thin films for enhanced pollutant degradation in wastewater treatment.
- 15 February 2024
- Published by Trans Tech Publications, Ltd. in Nano Hybrids and Composites
- Vol. 42, 39-47
Effect of Gas Flowrate on the Properties and Photocatalytic Activity of ZnO-Ag Nanocomposite Materials Prepared by Flame Pyrolysis
It is well known that adding the appropriate amount of Ag to semiconductor materials can enhance photocatalytic performance. In our previous study, the addition of Ag nanoparticles to ZnO enhanced the photocatalytic activity. The best photocatalytic performance was obtained when Ag content was 5 wt%. However, the effect of a carrier gas flow rate has not been investigated. The objective of this study is to investigate the effect of carrier gas flow rate on the morphology of the ZnO-Ag nanocomposites as well as the photocatalytic activity of the produced nanocomposites. ZnO-Ag nanocomposite was fabricated by a one-step process using flame pyrolysis and the produced nanocomposites were characterized by a scanning electron microscope (SEM) and X-Ray Diffraction (XRD) analysis. The photocatalytic performance was evaluated by measuring the degradation of methylene blue under UV light irradiation. SEM images indicated that the morphology of ZnO-Ag nanocomposites has a spherical shape with a particle diameter of around 65 nm. Moreover, increasing the flow rate will increase the particle size of the produced nanocomposites. The photocatalytic test was determined based on the rate constant of MB degradation efficiency under UV light irradiation, where the photocatalytic activity decreased when the carrier gas increased. Finally, the produced nanocomposites were also tested several times (recycling test), where photocatalytic performance showed that the degradation value of methylene blue for each recycle did not vary much with the variable before being recycled.
- 15 February 2024
- Published by Trans Tech Publications, Ltd. in Nano Hybrids and Composites
- Vol. 42, 39-47
Effect of Gas Flowrate on the Properties and Photocatalytic Activity of ZnO-Ag Nanocomposite Materials Prepared by Flame Pyrolysis
It is well known that adding the appropriate amount of Ag to semiconductor materials can enhance photocatalytic performance. In our previous study, the addition of Ag nanoparticles to ZnO enhanced the photocatalytic activity. The best photocatalytic performance was obtained when Ag content was 5 wt%. However, the effect of a carrier gas flow rate has not been investigated. The objective of this study is to investigate the effect of carrier gas flow rate on the morphology of the ZnO-Ag nanocomposites as well as the photocatalytic activity of the produced nanocomposites. ZnO-Ag nanocomposite was fabricated by a one-step process using flame pyrolysis and the produced nanocomposites were characterized by a scanning electron microscope (SEM) and X-Ray Diffraction (XRD) analysis. The photocatalytic performance was evaluated by measuring the degradation of methylene blue under UV light irradiation. SEM images indicated that the morphology of ZnO-Ag nanocomposites has a spherical shape with a particle diameter of around 65 nm. Moreover, increasing the flow rate will increase the particle size of the produced nanocomposites. The photocatalytic test was determined based on the rate constant of MB degradation efficiency under UV light irradiation, where the photocatalytic activity decreased when the carrier gas increased. Finally, the produced nanocomposites were also tested several times (recycling test), where photocatalytic performance showed that the degradation value of methylene blue for each recycle did not vary much with the variable before being recycled.
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3073 (1)
Preliminary design precipitated calcium carbonate from blast furnace gas and steel slag plant
The steel industries account for 6% of the world’s CO2 emissions. The number of emissions will continue to increase as the steel industry in Indonesia grows. Ge
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3073 (1)
Preliminary design precipitated calcium carbonate from blast furnace gas and steel slag plant
The steel industries account for 6% of the world’s CO2 emissions. The number of emissions will continue to increase as the steel industry in Indonesia grows. Ge
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3073 (1)
Parameters influencing stable colloidal ZnO from zinc acetate dihydrate using sol-gel method
Studies on several factors influencing the stability of ZnO colloids were discussed in this paper. Parameters such as colloidal and LiOH concentrations were exp
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3073 (1)
Parameters influencing stable colloidal ZnO from zinc acetate dihydrate using sol-gel method
Studies on several factors influencing the stability of ZnO colloids were discussed in this paper. Parameters such as colloidal and LiOH concentrations were exp
- Open Access
Photocatalytic Activity of ZnO/Ag Nanoparticles Fabricated by a Spray Pyrolysis Method with Different O2:N2 Carrier Gas Ratios and Ag Contents
Wastewaters of the textile industry, e.g., those generated in Gresik, Indonesia, are a possible threat to the environment and should be treated before disposal. Photodegradation is a more promising method to overcome this problem than conventional methods such as biodegradation. ZnO is widely used for photodegradation due to its unique physical and chemical properties and stability. In this study, Ag was loaded onto ZnO, which is non-toxic and inexpensive, can improve the electron–hole separation, and has a significant catalytic potential. Pristine ZnO and ZnO-Ag nanoparticles were fabricated by an ultrasonic spray pyrolysis system at different Ag contents (1, 5, and 10 wt%). The carrier gas ratio (O2:N2) was also changed (1:0, 1:2, 1:1, 2:1, and 0:1) to examine its effects on the nanoparticle characteristics. The nanoparticle characteristics were examined using X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and Brunauer, Emmett, and Teller (BET) specific surface area. The results were interpreted in relation to photodegradation under UV light irradiation. An increase in the ZnO-Ag activity compared with pristine ZnO was observed at a carrier gas ratio of 0:1 with reaction rate constants of 0.0059 and 0.0025 min−1, respectively.
Open AccessPhotocatalytic Activity of ZnO/Ag Nanoparticles Fabricated by a Spray Pyrolysis Method with Different O2:N2 Carrier Gas Ratios and Ag Contents
Wastewaters of the textile industry, e.g., those generated in Gresik, Indonesia, are a possible threat to the environment and should be treated before disposal. Photodegradation is a more promising method to overcome this problem than conventional methods such as biodegradation. ZnO is widely used for photodegradation due to its unique physical and chemical properties and stability. In this study, Ag was loaded onto ZnO, which is non-toxic and inexpensive, can improve the electron–hole separation, and has a significant catalytic potential. Pristine ZnO and ZnO-Ag nanoparticles were fabricated by an ultrasonic spray pyrolysis system at different Ag contents (1, 5, and 10 wt%). The carrier gas ratio (O2:N2) was also changed (1:0, 1:2, 1:1, 2:1, and 0:1) to examine its effects on the nanoparticle characteristics. The nanoparticle characteristics were examined using X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and Brunauer, Emmett, and Teller (BET) specific surface area. The results were interpreted in relation to photodegradation under UV light irradiation. An increase in the ZnO-Ag activity compared with pristine ZnO was observed at a carrier gas ratio of 0:1 with reaction rate constants of 0.0059 and 0.0025 min−1, respectively.
- Open Access
- 1 September 2022
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 2344 (1) , 012010
Effect of SiO2 Content on Photocatalytic Activities of ZnO/Ag/SiO2 Nanocomposites Prepared by Spray Pyrolysis
Spray pyrolysis is a method for preparing nanocomposite materials in the gas phase. Due to the ease with which the temperature in the furnace can be controlled, this method can produce more uniform nanoparticle sizes. This method can be used to synthesize ZnO nanoparticles. Additionally, due to the photocatalytic properties of the synthesized particles, they are used to decompose synthetic dye waste. Due to electron-hole recombination, ZnO’s photocatalytic properties are limited. A doping process with various metals was used to enhance the photocatalytic properties of ZnO nanoparticles. Ag is one of these metals. The addition of Ag metal to ZnO nanoparticles results in the formation of nanocomposites with preferable photocatalytic properties. However, the addition of Ag results in the aggregation of the obtained particles. As a result, the ZnO particles must be trapped in a matrix (for example, SiO2) to inhibit particle growth. This research aims to determine the effect of the SiO2 composition on the characteristics and photocatalytic properties of ZnO/Ag/SiO2 nanocomposite synthesized via spray pyrolysis. SEM (Scanning Electron Microscope) analysis was used to determine the morphology of the nanocomposites, XRD (X-ray Diffraction) analysis was used to determine the purity and degree of crystallization, FTIR (Fourier-transform Infrared) analysis was used to determine the functional groups, and UV-Vis Spectrophotometer analysis was used to determine the photocatalytic characteristics. According to the analysis results, the optimal photocatalytic activity was obtained at 1% SiO2, with a degradation rate of up to 47% of methylene blue and a rate constant (k) of 0.0086 L/min under UV light irradiation.
- 1 September 2022
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 2344 (1) , 012010
Open AccessEffect of SiO2 Content on Photocatalytic Activities of ZnO/Ag/SiO2 Nanocomposites Prepared by Spray Pyrolysis
Spray pyrolysis is a method for preparing nanocomposite materials in the gas phase. Due to the ease with which the temperature in the furnace can be controlled, this method can produce more uniform nanoparticle sizes. This method can be used to synthesize ZnO nanoparticles. Additionally, due to the photocatalytic properties of the synthesized particles, they are used to decompose synthetic dye waste. Due to electron-hole recombination, ZnO’s photocatalytic properties are limited. A doping process with various metals was used to enhance the photocatalytic properties of ZnO nanoparticles. Ag is one of these metals. The addition of Ag metal to ZnO nanoparticles results in the formation of nanocomposites with preferable photocatalytic properties. However, the addition of Ag results in the aggregation of the obtained particles. As a result, the ZnO particles must be trapped in a matrix (for example, SiO2) to inhibit particle growth. This research aims to determine the effect of the SiO2 composition on the characteristics and photocatalytic properties of ZnO/Ag/SiO2 nanocomposite synthesized via spray pyrolysis. SEM (Scanning Electron Microscope) analysis was used to determine the morphology of the nanocomposites, XRD (X-ray Diffraction) analysis was used to determine the purity and degree of crystallization, FTIR (Fourier-transform Infrared) analysis was used to determine the functional groups, and UV-Vis Spectrophotometer analysis was used to determine the photocatalytic characteristics. According to the analysis results, the optimal photocatalytic activity was obtained at 1% SiO2, with a degradation rate of up to 47% of methylene blue and a rate constant (k) of 0.0086 L/min under UV light irradiation.
- Open Access
Effect of Heating Rate on the Photocatalytic Activity of Ag–TiO2 Nanocomposites by One-Step Process via Aerosol Routes
Ag–TiO2 nanocomposite films, based of Ag and TiO2 nanoparticles, were fabricated in a one-step aerosol route employing the simultaneous plasma-enhanced chemical vapor deposition and physical vapor deposition systems. The as-fabricated films were subjected to different heating rates (3 to 60 °C/min) with a constant annealing temperature of 600 °C to observe the significant changes in the properties (e.g., nanoparticle size, crystalline size, crystallite phase, surface area) toward the photocatalytic performance. The photocatalytic activity was evaluated by the measurement of the degradation of a methylene blue aqueous solution under UV light irradiation, and the results revealed that it gradually increased with the increase in the heating rate, caused by the increased Brunauer–Emmett–Teller (BET) specific surface area and total pore volume.
Open AccessEffect of Heating Rate on the Photocatalytic Activity of Ag–TiO2 Nanocomposites by One-Step Process via Aerosol Routes
Ag–TiO2 nanocomposite films, based of Ag and TiO2 nanoparticles, were fabricated in a one-step aerosol route employing the simultaneous plasma-enhanced chemical vapor deposition and physical vapor deposition systems. The as-fabricated films were subjected to different heating rates (3 to 60 °C/min) with a constant annealing temperature of 600 °C to observe the significant changes in the properties (e.g., nanoparticle size, crystalline size, crystallite phase, surface area) toward the photocatalytic performance. The photocatalytic activity was evaluated by the measurement of the degradation of a methylene blue aqueous solution under UV light irradiation, and the results revealed that it gradually increased with the increase in the heating rate, caused by the increased Brunauer–Emmett–Teller (BET) specific surface area and total pore volume.
- Open Access
- 15 June 2020
- Published by Penerbit UTM Press in Malaysian Journal of Fundamental and Applied Sciences
- Vol. 16 (3) , 258-263
Deposition of ultrasonic nebulized aerosols onto a hydrophilic surface
The effect of chemical treatment of a metallic substrate on the deposition of aerosols generated by an ultrasonic nebulizer was investigated. A single substrate with areas having different “level” of hydrophilicity (or hydrophobicity) was used as a model surface. The treated (more hydrophilic) area became more negatively-charged based on a surface electric potential meter. A low-pressure analysis method (electron-microscope image) and ordinary pressure methods (Raman spectroscopy and X-ray fluorescence) analytical results indicated that in comparison with the untreated area, the treated area trapped more particles in the case of the deposition of “wet” aerosols. In the case of the deposition of more “dry” aerosols, the untreated area trapped more particles rather than that of the treated one. The efficiency of particles deposition not only depended on the degree of hydrophilicity (or hydrophobicity) of the surface but also due to the conditions (wet or dry) of incoming aerosols.
- 15 June 2020
- Published by Penerbit UTM Press in Malaysian Journal of Fundamental and Applied Sciences
- Vol. 16 (3) , 258-263
Open AccessDeposition of ultrasonic nebulized aerosols onto a hydrophilic surface
The effect of chemical treatment of a metallic substrate on the deposition of aerosols generated by an ultrasonic nebulizer was investigated. A single substrate with areas having different “level” of hydrophilicity (or hydrophobicity) was used as a model surface. The treated (more hydrophilic) area became more negatively-charged based on a surface electric potential meter. A low-pressure analysis method (electron-microscope image) and ordinary pressure methods (Raman spectroscopy and X-ray fluorescence) analytical results indicated that in comparison with the untreated area, the treated area trapped more particles in the case of the deposition of “wet” aerosols. In the case of the deposition of more “dry” aerosols, the untreated area trapped more particles rather than that of the treated one. The efficiency of particles deposition not only depended on the degree of hydrophilicity (or hydrophobicity) of the surface but also due to the conditions (wet or dry) of incoming aerosols.