Ana Júlia Smolinski Gouveia
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ana Júlia Smolinski Gouveia has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Mônica Regina Garcez
Civil Engineering Post-Graduation Program: Construction and Infrastructure, Federal University of Rio Grande Do Sul, Porto Alegre, Brazil
2 shared publications - Alessandro Simas Franchetto
Universidade Federal do Rio Grande do Sul, Brasil
1 shared publication - Fabiana Ziegler
Núcleo orientado para a inovação da construção (NORIE), Escola de Engenharia, Universidade Federal do Rio Grande do Sul, Porto Alegre, Brasil
1 shared publication - Kennedy Queiros Pessoa
Núcleo orientado para a inovação da construção (NORIE), Escola de Engenharia, Universidade Federal do Rio Grande do Sul, Porto Alegre, Brasil
1 shared publication - Rayara Pinto Costa
Universidade Federal do Rio Grande do Sul, Brasil
1 shared publication - Silvana Da Dalt
Universidade Federal do Rio Grande do Sul
1 shared publication
Latest Publications
- Open Access
- 2 May 2026
- Published by Springer Nature in Journal of Building Pathology and Rehabilitation
- Vol. 11 (3) , 154
Improving self-compacting concrete performance at high temperature with red ceramic waste filler
The high content of fine materials required in self-compacting concrete to ensure flowability reduces matrix porosity, thereby increasing vulnerability to deterioration and heat-induced spalling at high temperatures. This paper investigates the unconventional use of red ceramic waste as a replacement for limestone filler in self-compacting concrete, leveraging its porous structure to attenuate thermo-hydro-mechanical effects and mitigate heat-induced spalling. Residual compressive strength, modulus of elasticity, mass loss, homogeneity, capillary absorption, and evidence of heat-induced spalling were monitored in conventional and self-compacting concrete conditioned specimens after exposure to temperatures ranging from 200 °C to 800 °C at 1 °C/min. Heat-induced spalling was simulated by subjecting unconditioned specimens to a high heating rate to 1000 °C at 27 °C/min, thereby replicating severe thermal loading conditions. The self-compacting mixture with red ceramic waste fulfilled flowability and stability requirements at the fresh state. Replacing limestone filler with red ceramic waste enhanced residual mechanical performance, particularly in the 200 °C to 600 °C range, highlighting the beneficial role of the waste’s porous structure in mitigating thermo-hydro-mechanical damage. Although incorporating red ceramic waste did not entirely prevent heat-induced spalling at a high heating rate, it significantly reduced damage severity compared to limestone filler. Furthermore, self-compacting mixtures with red ceramic waste as a filler required 3% (C30) to 10% (C40) less cement, offering a potential reduction in the concrete carbon footprint and contributing to circular economy principles through the valorization of industrial waste.
- 2 May 2026
- Published by Springer Nature in Journal of Building Pathology and Rehabilitation
- Vol. 11 (3) , 154
Open AccessImproving self-compacting concrete performance at high temperature with red ceramic waste filler
The high content of fine materials required in self-compacting concrete to ensure flowability reduces matrix porosity, thereby increasing vulnerability to deterioration and heat-induced spalling at high temperatures. This paper investigates the unconventional use of red ceramic waste as a replacement for limestone filler in self-compacting concrete, leveraging its porous structure to attenuate thermo-hydro-mechanical effects and mitigate heat-induced spalling. Residual compressive strength, modulus of elasticity, mass loss, homogeneity, capillary absorption, and evidence of heat-induced spalling were monitored in conventional and self-compacting concrete conditioned specimens after exposure to temperatures ranging from 200 °C to 800 °C at 1 °C/min. Heat-induced spalling was simulated by subjecting unconditioned specimens to a high heating rate to 1000 °C at 27 °C/min, thereby replicating severe thermal loading conditions. The self-compacting mixture with red ceramic waste fulfilled flowability and stability requirements at the fresh state. Replacing limestone filler with red ceramic waste enhanced residual mechanical performance, particularly in the 200 °C to 600 °C range, highlighting the beneficial role of the waste’s porous structure in mitigating thermo-hydro-mechanical damage. Although incorporating red ceramic waste did not entirely prevent heat-induced spalling at a high heating rate, it significantly reduced damage severity compared to limestone filler. Furthermore, self-compacting mixtures with red ceramic waste as a filler required 3% (C30) to 10% (C40) less cement, offering a potential reduction in the concrete carbon footprint and contributing to circular economy principles through the valorization of industrial waste.
- Open Access
- 1 January 2022
- Published by Alconpat Internacional in Revista ALCONPAT
- Vol. 12 (1) , 47 – 60
Previsão da vida útil de estruturas de concreto com base em modelos para avanço da frente de carbonatação
Este artigo busca avaliar a variabilidade na previsão da vida útil de estruturas de concreto através de quatro modelos que estimam o avanço natural da frente de carbonatação. Os resultados mostram que há variabilidade na frente de carbonatação estimada. Os modelos de Possan (2010) e Ekolu (2018) apresentam valores estimados próximos aos medidos, enquanto Ho e Lewis (1987) e Bob e Affana (1993) tendem, respectivamente, a subestimar e superestimar a frente natural de carbonatação. Somente concretos sem adição de materiais cimentícios suplementares foram considerados, por limitações dos modelos. A resistência à compressão, concentração de CO2 e umidade relativa do ar têm influência significativa nos resultados e a variabilidade depende de quais parâmetros são considerados nos modelos
- 1 January 2022
- Published by Alconpat Internacional in Revista ALCONPAT
- Vol. 12 (1) , 47 – 60
Open AccessPrevisão da vida útil de estruturas de concreto com base em modelos para avanço da frente de carbonatação
Este artigo busca avaliar a variabilidade na previsão da vida útil de estruturas de concreto através de quatro modelos que estimam o avanço natural da frente de carbonatação. Os resultados mostram que há variabilidade na frente de carbonatação estimada. Os modelos de Possan (2010) e Ekolu (2018) apresentam valores estimados próximos aos medidos, enquanto Ho e Lewis (1987) e Bob e Affana (1993) tendem, respectivamente, a subestimar e superestimar a frente natural de carbonatação. Somente concretos sem adição de materiais cimentícios suplementares foram considerados, por limitações dos modelos. A resistência à compressão, concentração de CO2 e umidade relativa do ar têm influência significativa nos resultados e a variabilidade depende de quais parâmetros são considerados nos modelos