Latest Publications

  • Back-End of Line Compatible Hf0.5Zr0.5O2 With ZrO2 Seed Layer for Enhanced Ferroelectricity

    by Yin-Chi Liu, Yu-Chun Li, Ze-Yu Gu, Xin-Long Zhou, Teng Huang, Ze-Hui Li, Tian-Tian Pi, Yan-Fei Li, Shi-Jin Ding, Lin Chen, et al.

    In this letter, four ferroelectric (FE) capacitors with thickness dependent ZrO 2 seed layer (SL) were designed and fabricated at a low annealing temperature below 350 °C. By modulating the thickness of ZrO 2 SL, it is demonstrated that the FE capacitor with 1 nm ZrO 2 SL exhibits a superior remnant polarization (2 Pr ) of 44.1 μC/cm 2 under 3 MV/cm at 1 kHz and 2 Pr of 17.6 μC/cm 2 after 10 9 cycles at 3 MV/cm. It is found that the 1 nm ZrO 2 SL provides more growth sites for the Hf 0.5 Zr 0.5 O 2 (HZO) thin films, and enhances the ratio of the ferroelectric phases during crystallization, thereby leading to enhancement of its ferroelectricity and reliability. This work provides a robust solution to improve both ferroelectricity and endurance for future ferroelectric device compatible with back end of line (BEOL) process.


  • High-Performance a-IGZO TFT Fabricated With Ultralow Thermal Budget via Microwave Annealing

    by Tiantian Pi, Dongqi Xiao, Hui Yang, Gang He, Xiaohan Wu, Wenjun Liu, David Wei Zhang, Shi-Jin Ding

    In this work, we report high-performance amorphous indium gallium zinc oxide (a-IGZO) thin-film transistors (TFTs) with atomic layer deposited Al 2 O 3 dielectric processed at a minimal temperature of 189.6 °C via microwave annealing (MWA). The a-IGZO TFT with MWA exhibits an improvement of 57% in subthreshold swing (SS) compared with the unannealed device; meanwhile, it retains high field-effect mobility of up to 29.2 cm 2 /(V $\cdot $ s) and large switching ratio of >10 8 . Moreover, the SS of the device was further reduced through a two-step MWA treatment. It is believed that MWA treatment effectively reduces the density of trap states associated with oxygen vacancies, promotes the formation of lattice oxygen, and thus improves the quality of IGZO film. MWA with low thermal budget shows great potential in applications of the back-end of line (BEOL)-compatible oxide devices.