Barsha Marandi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Barsha Marandi has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Kali Sanjay
Hydro & Electrometallurgy Department, CSIR-Institute of Minerals and Materials Technology, Bhubaneswar, India
2 shared publications - Manickam Minakshi
Engineering and Energy, Murdoch University, WA 6150, Australia
2 shared publications - Tondepu Subbaiah
Vignan's Foundation for Science, Technology and Research
2 shared publications - Abdul Rauf Sheik
CSIR-Institute of Minerals and Materials Technology, Bhubaneswar 751013, India
1 shared publication - Chinmaya Kumar Sarangi
CSIR-Institute of Minerals and Materials Technology, Bhubaneswar 751013, India
1 shared publication - Malay Kumar Ghosh
Hydro & Electrometallurgy Department, CSIR-Institute of Minerals and Materials Technology, Bhubaneswar, India
1 shared publication
Latest Publications
- Open Access
- 3 August 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (15) , 11919
Recovery of Tellurium from Waste Anode Slime Containing High Copper and High Tellurium of Copper Refineries
Tellurium is used in cadmium tellurium-based solar cells. Mercury cadmium telluride is used as a sensing material for thermal imaging devices. High-purity tellurium is used in alloys for electronic applications. It is one of the important raw materials for solar energy applications. It is used as an alloying element in the production of low-carbon steel and copper alloys. Tellurium catalysts are used chiefly for the oxidation of organic compounds and as vulcanizing/accelerating agents in the processing of rubber compounds. Even though several researchers tried to recover tellurium from different raw materials, there is no attempt to develop a process flow sheet to recover tellurium from waste anode slime having a high tellurium concentration. In this study, optimum conditions were developed to recover Te and Cu from anode slime with the composition Cu: 31.8%, Te: 24.7%, and As: 0.96%. The unit operations involved are leaching, purification, and electro winning. The optimum conditions for producing Te at a recovery of 90% are found to be roasting of anode slime at 450 °C without the addition of soda ash followed by leaching in 1 M NaOH at 10% pulp density for 2 h. The purity of Te metal achieved was up to 99.99%, which could provide a sustainable energy future. The major impurities of the tellurium are observed to be in the order: Se > Sb > As > Cu.
- 3 August 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (15) , 11919
Open AccessRecovery of Tellurium from Waste Anode Slime Containing High Copper and High Tellurium of Copper Refineries
Tellurium is used in cadmium tellurium-based solar cells. Mercury cadmium telluride is used as a sensing material for thermal imaging devices. High-purity tellurium is used in alloys for electronic applications. It is one of the important raw materials for solar energy applications. It is used as an alloying element in the production of low-carbon steel and copper alloys. Tellurium catalysts are used chiefly for the oxidation of organic compounds and as vulcanizing/accelerating agents in the processing of rubber compounds. Even though several researchers tried to recover tellurium from different raw materials, there is no attempt to develop a process flow sheet to recover tellurium from waste anode slime having a high tellurium concentration. In this study, optimum conditions were developed to recover Te and Cu from anode slime with the composition Cu: 31.8%, Te: 24.7%, and As: 0.96%. The unit operations involved are leaching, purification, and electro winning. The optimum conditions for producing Te at a recovery of 90% are found to be roasting of anode slime at 450 °C without the addition of soda ash followed by leaching in 1 M NaOH at 10% pulp density for 2 h. The purity of Te metal achieved was up to 99.99%, which could provide a sustainable energy future. The major impurities of the tellurium are observed to be in the order: Se > Sb > As > Cu.
- Open Access
- 13 January 2022
- Published by MDPI AG in Sustainability
- Vol. 14 (2) , 880
Ionic Mass Transfer at Point Electrodes Located at Cathode Support Plate in an Electrorefining Cell in Presence of Rectangular Turbulent Promoters
Current density plays a major role in deciding the plant size, current efficiency, and energy consumption in electrorefining cells. In general, operating current density will be 40% of the limiting current density. Forced circulation of the electrolyte in the presence of promoters improves the mass transfer coefficient. In the present study, rectangular turbulence promoters are fitted at the bottom side of the cell to improve the mass transfer coefficient at the cathode support plate. The limiting current density technique is used to measure the mass transfer coefficient. The variables covered in the present study are the effects of flow rate, promoter height, and spacing among the promoters. The electrolyte consists of copper sulfate and sulphuric acid. At a regulated flow rate, the electrolyte is pumped from the recirculation tank to the cell through an intermediate overhead tank. The limiting current density increased with an increasing flow rate in the presence of promoters, and thus the overall mass transfer coefficient on the cathode support plate also improved. With an increase in the flow rate of the electrolyte from 6.67 × 10−6 to 153.33 m3/s, limiting current density increased from 356.8 to 488.8 A/m2 for spacing of 0.30 m, with a promoter height of 0.01 m. However, it is noteworthy that when the promoter height is increased from 0.01 to 0.07 m, the overall mass transfer coefficient is found to increase up to 60%, but with the further increase in the promoter height to 0.30 m the mass transfer coefficient starts to decrease. Therefore, the optimized cell parameters are established in this work. The current sustainable concept of employing rectangular turbulence promoters will bring benefits to any precious metal refining or electrowinning tank house electrolytes.
- 13 January 2022
- Published by MDPI AG in Sustainability
- Vol. 14 (2) , 880
Open AccessIonic Mass Transfer at Point Electrodes Located at Cathode Support Plate in an Electrorefining Cell in Presence of Rectangular Turbulent Promoters
Current density plays a major role in deciding the plant size, current efficiency, and energy consumption in electrorefining cells. In general, operating current density will be 40% of the limiting current density. Forced circulation of the electrolyte in the presence of promoters improves the mass transfer coefficient. In the present study, rectangular turbulence promoters are fitted at the bottom side of the cell to improve the mass transfer coefficient at the cathode support plate. The limiting current density technique is used to measure the mass transfer coefficient. The variables covered in the present study are the effects of flow rate, promoter height, and spacing among the promoters. The electrolyte consists of copper sulfate and sulphuric acid. At a regulated flow rate, the electrolyte is pumped from the recirculation tank to the cell through an intermediate overhead tank. The limiting current density increased with an increasing flow rate in the presence of promoters, and thus the overall mass transfer coefficient on the cathode support plate also improved. With an increase in the flow rate of the electrolyte from 6.67 × 10−6 to 153.33 m3/s, limiting current density increased from 356.8 to 488.8 A/m2 for spacing of 0.30 m, with a promoter height of 0.01 m. However, it is noteworthy that when the promoter height is increased from 0.01 to 0.07 m, the overall mass transfer coefficient is found to increase up to 60%, but with the further increase in the promoter height to 0.30 m the mass transfer coefficient starts to decrease. Therefore, the optimized cell parameters are established in this work. The current sustainable concept of employing rectangular turbulence promoters will bring benefits to any precious metal refining or electrowinning tank house electrolytes.