Qingyou Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Qingyou Liu has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
- Shujun Jia
Central Iron and Steel Research Institute Co., Ltd., Beijing, China
5 shared publications - Ba Li
Central Iron and Steel Research Institute Co., Ltd., Beijing 100081, China
4 shared publications - Bing Wang
Department of Structural Steels, Central Iron and Steel Research Institute Co., Ltd., Beijing 100081, China
3 shared publications - Shubiao Yin
Faculty of Metallurgy and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, China
2 shared publications - Ba Li
Institute for Structural Steels, Central Iron and Steel Research Institute Co., Ltd., Beijing 100081, China
1 shared publication - Feilong Wang
State Key Laboratory of New Metal Materials, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication
Latest Publications
- Open Access
Tempering Temperature-Dependent Microstructural Evolution and Mechanical Properties of Seamless Pipeline Steel for Deepwater Applications
An ultra-low-Mn steel (MS) incorporating multiple alloying additions was designed for seamless pipes used in deepwater oil and gas transportation to eliminate through-wall microstructural banding and optimize the strength–toughness balance. Using a conventional pipeline steel (BS) as a reference, the effects of tempering temperature on the microstructure and mechanical properties of both steels were systematically investigated over 600–700 °C. The evolution of microstructural banding and the strengthening mechanisms were examined using optical microscopy, scanning electron microscopy, electron backscatter diffraction, electron probe microanalysis, transmission electron microscopy, and physicochemical phase analysis. The results indicated that through-wall microstructural banding originated from pearlite bands associated with C and Mn segregation during piercing and rolling. These bands persisted through subsequent heat treatment and could promote local hydrogen accumulation, thereby increasing susceptibility to hydrogen-induced cracking (HIC). Substantially reducing the Mn content while increasing the combined contents of Cr, Ni, and Mo and the microalloying additions of Nb, V, and Ti, together with appropriate heat treatment, reduced microstructural banding and produced a fine, uniform microstructure throughout the pipe wall. MS exhibited greater strength–toughness balance than BS across the entire tempering temperature range, with the optimum strength–toughness balance achieved at 660–680 °C. The favorable strength–toughness balance of MS was attributed to the combined effects of microstructural homogenization, dislocation recovery, grain-boundary evolution, and strengthening by nanoscale compound (Mo, Nb, Ti, V)C precipitates during tempering. The highest fraction of fine, dispersed precipitates was obtained at 660 °C, effectively compensating for recovery-induced matrix softening and maintaining a high strength level.
Open AccessTempering Temperature-Dependent Microstructural Evolution and Mechanical Properties of Seamless Pipeline Steel for Deepwater Applications
An ultra-low-Mn steel (MS) incorporating multiple alloying additions was designed for seamless pipes used in deepwater oil and gas transportation to eliminate through-wall microstructural banding and optimize the strength–toughness balance. Using a conventional pipeline steel (BS) as a reference, the effects of tempering temperature on the microstructure and mechanical properties of both steels were systematically investigated over 600–700 °C. The evolution of microstructural banding and the strengthening mechanisms were examined using optical microscopy, scanning electron microscopy, electron backscatter diffraction, electron probe microanalysis, transmission electron microscopy, and physicochemical phase analysis. The results indicated that through-wall microstructural banding originated from pearlite bands associated with C and Mn segregation during piercing and rolling. These bands persisted through subsequent heat treatment and could promote local hydrogen accumulation, thereby increasing susceptibility to hydrogen-induced cracking (HIC). Substantially reducing the Mn content while increasing the combined contents of Cr, Ni, and Mo and the microalloying additions of Nb, V, and Ti, together with appropriate heat treatment, reduced microstructural banding and produced a fine, uniform microstructure throughout the pipe wall. MS exhibited greater strength–toughness balance than BS across the entire tempering temperature range, with the optimum strength–toughness balance achieved at 660–680 °C. The favorable strength–toughness balance of MS was attributed to the combined effects of microstructural homogenization, dislocation recovery, grain-boundary evolution, and strengthening by nanoscale compound (Mo, Nb, Ti, V)C precipitates during tempering. The highest fraction of fine, dispersed precipitates was obtained at 660 °C, effectively compensating for recovery-induced matrix softening and maintaining a high strength level.
- Open Access
Effect of Heat Input on the Hydrogen Embrittlement Sensitivity of CGHAZ of X60 Pipeline Steel
In the coarse grain heat-affected zone (CGHAZ) of welded pipe steel joints, hydrogen damage is a key factor limiting the high-pressure hydrogen transportation performance of the pipeline. This study employed multi-dimensional characterization methods (including microstructure, mechanical properties, and hydrogen distribution) to investigate the influence of welding heat input on the hydrogen embrittlement (HE) sensitivity of X60 pipeline steel in the CGHAZ. The results showed that as the heat input increased, the grains in the CGHAZ became coarser, and the microstructure changed from bainitic ferrite (BF) to granular bainite (GB) and polygonal ferrite (PF). Among them, the BF + GB composite structure had the best resistance to HE (HE sensitivity was 29.8%). At low heat input, the reversible hydrogen distribution occurred at the interfaces between the grain boundaries and the BF blocks, while at high heat input, it would accumulate around the martensite/austenite (M/A) constituents. For the 16 kJ/cm heat input experimental steel, the increase in Σ3 grain boundary density accelerated hydrogen diffusion and reduced its enrichment, thereby resulting in the lowest HE sensitivity.
Open AccessEffect of Heat Input on the Hydrogen Embrittlement Sensitivity of CGHAZ of X60 Pipeline Steel
In the coarse grain heat-affected zone (CGHAZ) of welded pipe steel joints, hydrogen damage is a key factor limiting the high-pressure hydrogen transportation performance of the pipeline. This study employed multi-dimensional characterization methods (including microstructure, mechanical properties, and hydrogen distribution) to investigate the influence of welding heat input on the hydrogen embrittlement (HE) sensitivity of X60 pipeline steel in the CGHAZ. The results showed that as the heat input increased, the grains in the CGHAZ became coarser, and the microstructure changed from bainitic ferrite (BF) to granular bainite (GB) and polygonal ferrite (PF). Among them, the BF + GB composite structure had the best resistance to HE (HE sensitivity was 29.8%). At low heat input, the reversible hydrogen distribution occurred at the interfaces between the grain boundaries and the BF blocks, while at high heat input, it would accumulate around the martensite/austenite (M/A) constituents. For the 16 kJ/cm heat input experimental steel, the increase in Σ3 grain boundary density accelerated hydrogen diffusion and reduced its enrichment, thereby resulting in the lowest HE sensitivity.
- Open Access
Hydrogen Embrittlement Sensitivity of X70 Welded Pipe Under a High-Pressure Pure Hydrogen Environment
With the rapid development of hydrogen pipelines, their safety issues have become increasingly prominent. In order to evaluate the properties of pipeline materials under a high-pressure hydrogen environment, this study investigates the hydrogen embrittlement sensitivity of X70 welded pipe in a 10 MPa high-pressure hydrogen environment, using slow strain rate testing (SSRT) and low-cycle fatigue (LCF) analysis. The microstructure, slow tensile and fatigue fracture morphology of base metal (BM) and weld metal (WM) were characterized and analyzed by means of ultra-depth microscope, scanning electron microscope (SEM), electron backscattering diffraction (EBSD), and transmission electron microscope (TEM). Results indicate that while the high-pressure hydrogen environment has minimal impact on ultimate tensile strength (UTS) for both BM and WM, it significantly decreases reduction of area (RA) and elongation (EL), with RA reduction in WM exceeding that in BM. Under the nitrogen environment, the slow tensile fracture of X70 pipeline steel BM and WM is a typical ductile fracture, while under the high-pressure hydrogen environment, the unevenness of the slow tensile fracture increased, and a large number of microcracks appeared on the fracture surface and edges, with the fracture mode changing to ductile fracture + quasi-cleavage fracture. In addition, the high-pressure hydrogen environment reduces the fatigue life of the BM and WM of X70 pipeline steel, and the fatigue life of the WM decreases more than that of the BM as well. Compared to the nitrogen environment, the fatigue fracture specimens of BM and WM in the hydrogen environment showed quasi-cleavage fracture patterns, and the fracture area in the instantaneous fracture zone (IFZ) was significantly reduced. Compared with the BM of X70 pipeline steel, although the effective grain size of the WM is smaller, WM’s microstructure, with larger Martensite/austenite (M/A) constituents and MnS and Al-rich oxides, contributes to a heightened embrittlement sensitivity. In contrast, the second-phase precipitation of nanosized Nb, V, and Ti composite carbon-nitride in the BM acts as an effective irreversible hydrogen trap, which can significantly reduce the hydrogen embrittlement sensitivity.
Open AccessHydrogen Embrittlement Sensitivity of X70 Welded Pipe Under a High-Pressure Pure Hydrogen Environment
With the rapid development of hydrogen pipelines, their safety issues have become increasingly prominent. In order to evaluate the properties of pipeline materials under a high-pressure hydrogen environment, this study investigates the hydrogen embrittlement sensitivity of X70 welded pipe in a 10 MPa high-pressure hydrogen environment, using slow strain rate testing (SSRT) and low-cycle fatigue (LCF) analysis. The microstructure, slow tensile and fatigue fracture morphology of base metal (BM) and weld metal (WM) were characterized and analyzed by means of ultra-depth microscope, scanning electron microscope (SEM), electron backscattering diffraction (EBSD), and transmission electron microscope (TEM). Results indicate that while the high-pressure hydrogen environment has minimal impact on ultimate tensile strength (UTS) for both BM and WM, it significantly decreases reduction of area (RA) and elongation (EL), with RA reduction in WM exceeding that in BM. Under the nitrogen environment, the slow tensile fracture of X70 pipeline steel BM and WM is a typical ductile fracture, while under the high-pressure hydrogen environment, the unevenness of the slow tensile fracture increased, and a large number of microcracks appeared on the fracture surface and edges, with the fracture mode changing to ductile fracture + quasi-cleavage fracture. In addition, the high-pressure hydrogen environment reduces the fatigue life of the BM and WM of X70 pipeline steel, and the fatigue life of the WM decreases more than that of the BM as well. Compared to the nitrogen environment, the fatigue fracture specimens of BM and WM in the hydrogen environment showed quasi-cleavage fracture patterns, and the fracture area in the instantaneous fracture zone (IFZ) was significantly reduced. Compared with the BM of X70 pipeline steel, although the effective grain size of the WM is smaller, WM’s microstructure, with larger Martensite/austenite (M/A) constituents and MnS and Al-rich oxides, contributes to a heightened embrittlement sensitivity. In contrast, the second-phase precipitation of nanosized Nb, V, and Ti composite carbon-nitride in the BM acts as an effective irreversible hydrogen trap, which can significantly reduce the hydrogen embrittlement sensitivity.
- Open Access
Revealing the Corrosion Resistance Mechanism of Plain Carbon Steel Micro-Alloyed by La in Simulated Industrial Atmosphere
Plain carbon steel is the most widely applied steel in current engineering construction. With the increased application property needs, the service life of plain carbon steel has been severely tested. As one of the most destructive failure modes, corrosion resistance of carbon steel has attracted wide attention. Rare earth La, as the microalloying element, was employed in plain carbon steel, Q355, to improve its corrosion resistance. As the content of La increased, the microstructure was refined. The fraction of pearlite decreased, while the content of acicular increased. Within the La addition of 230 ppm, the tensile strength and impact energy were jointly improved. Furthermore, the microalloying element of La modified the inclusion types and refined the inclusion size. The modified microstructure and inclusions by La co-improved the corrosion resistance. The formula of effective La content was proposed to estimate the effect of La on corrosion. As the effective content of La increased, the relative corrosion rate decreased. La3+ promoted the protective rust layer to increase corrosion resistance.
Open AccessRevealing the Corrosion Resistance Mechanism of Plain Carbon Steel Micro-Alloyed by La in Simulated Industrial Atmosphere
Plain carbon steel is the most widely applied steel in current engineering construction. With the increased application property needs, the service life of plain carbon steel has been severely tested. As one of the most destructive failure modes, corrosion resistance of carbon steel has attracted wide attention. Rare earth La, as the microalloying element, was employed in plain carbon steel, Q355, to improve its corrosion resistance. As the content of La increased, the microstructure was refined. The fraction of pearlite decreased, while the content of acicular increased. Within the La addition of 230 ppm, the tensile strength and impact energy were jointly improved. Furthermore, the microalloying element of La modified the inclusion types and refined the inclusion size. The modified microstructure and inclusions by La co-improved the corrosion resistance. The formula of effective La content was proposed to estimate the effect of La on corrosion. As the effective content of La increased, the relative corrosion rate decreased. La3+ promoted the protective rust layer to increase corrosion resistance.
- Open Access
Effect of Nb Addition and Heat Input on Heat-Affected Zone Softening in High-Strength Low-Alloy Steel
The effect of both Nb content and heat input on the softening phenomenon of the heat-affected zone (HAZ) of low-alloy high-strength steel was studied through welding thermal simulation experiments. The microstructure evolution, density variation of geometrically necessary dislocation, microhardness distribution and the second phase precipitation behavior in HAZ was characterized and analyzed by combining the optical microscope, scanning electron microscope, high-resolution transmission electron microscope with microhardness tests. The results showed that the softening appeared in the fine-grain HAZ (FGHAZ) of the low-alloy high-strength steel with the polygonal ferrite and bainite microstructure. With an increase in Nb content, the FGHAZ softening was inhibited even with high heat input; however, the hardness shows little variation. On the one hand, the increase in the Nb content increased the volume fraction of high-strength bainite in the FGHAZ. On the other hand, the remarkable strengthening was produced by the equally distributed precipitation nanoparticles. As a result, the two factors were the main reason for the solution of the FGHAZ softening problem in the low-alloyed high-strength steel with the mixed microstructure of ferrite and bainite.
Open AccessEffect of Nb Addition and Heat Input on Heat-Affected Zone Softening in High-Strength Low-Alloy Steel
The effect of both Nb content and heat input on the softening phenomenon of the heat-affected zone (HAZ) of low-alloy high-strength steel was studied through welding thermal simulation experiments. The microstructure evolution, density variation of geometrically necessary dislocation, microhardness distribution and the second phase precipitation behavior in HAZ was characterized and analyzed by combining the optical microscope, scanning electron microscope, high-resolution transmission electron microscope with microhardness tests. The results showed that the softening appeared in the fine-grain HAZ (FGHAZ) of the low-alloy high-strength steel with the polygonal ferrite and bainite microstructure. With an increase in Nb content, the FGHAZ softening was inhibited even with high heat input; however, the hardness shows little variation. On the one hand, the increase in the Nb content increased the volume fraction of high-strength bainite in the FGHAZ. On the other hand, the remarkable strengthening was produced by the equally distributed precipitation nanoparticles. As a result, the two factors were the main reason for the solution of the FGHAZ softening problem in the low-alloyed high-strength steel with the mixed microstructure of ferrite and bainite.
- Open Access
Effect of V Content and Heat Input on HAZ Softening of Deep-Sea Pipeline Steel
In this paper, the welding thermal cycle process of deep-sea pipeline steel was investigated by welding thermal simulation. The microstructure evolution, crystallology and second-phase precipitation behavior of the soft zone of the heat-affected zone (HAZ) were characterized and analyzed by combining scanning electron microscopy, electron back-scattered diffraction, transmission electron microscopy and hardness testing. The results show that HAZ softening appeared in the fine-grained zone with a peak temperature of 900–1000 °C for deep-sea pipeline steel, the base metal microstructure of which was the polygonal ferrite and acicular ferrite. Using V microalloying and low welding heat input could effectively decrease the softening of the HAZ fine-grained region, which was achieved by reducing the effective grain size, increasing the proportion of the dislocation substructures, and precipitating the nanoscale second-phase particles.
Open AccessEffect of V Content and Heat Input on HAZ Softening of Deep-Sea Pipeline Steel
In this paper, the welding thermal cycle process of deep-sea pipeline steel was investigated by welding thermal simulation. The microstructure evolution, crystallology and second-phase precipitation behavior of the soft zone of the heat-affected zone (HAZ) were characterized and analyzed by combining scanning electron microscopy, electron back-scattered diffraction, transmission electron microscopy and hardness testing. The results show that HAZ softening appeared in the fine-grained zone with a peak temperature of 900–1000 °C for deep-sea pipeline steel, the base metal microstructure of which was the polygonal ferrite and acicular ferrite. Using V microalloying and low welding heat input could effectively decrease the softening of the HAZ fine-grained region, which was achieved by reducing the effective grain size, increasing the proportion of the dislocation substructures, and precipitating the nanoscale second-phase particles.