Chunhua Wei
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Chunhua Wei has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Hongqun Tang
School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
2 shared publications - Biao Huang
State Key Laboratory of Featured Metal Materials and Life-cycle Safety for Composite Structures, Guangxi University, Nanning 530004, China
1 shared publication - Chuanchao Meng
State Key Laboratory of Featured Metal Materials and Life-cycle Safety for Composite Structures, School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Jianqiang Wu
Guangxi Key Laboratory of Processing for Nonferrous Metals and Featured Materials, Center of Ecological Collaborative Innovation for Aluminium Industry in Guangxi, School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication - Junsheng Wang
School of Materials Science and Engineering, Beijing Institute of Technology, Beijing, China
1 shared publication - Lingyou Wen
Guangxi Key Laboratory of Processing for Nonferrous Metals and Featured Materials, Center of Ecological Collaborative Innovation for Aluminum Industry in Guangxi, School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China
1 shared publication
Latest Publications
- Open Access
Insights into Poisoning Mechanism of Zr by First Principle Calculation on Adhesion Work and Adsorption Energy between TiB2, Al3Ti, and Al3Zr
Al-Ti-B intermediate alloys are widely used as grain refiners in aluminum alloys owing to the presence of Al3Ti and TiB2 phases. However, the existence of Zr in aluminum alloy melts often results in coarse grain size, leading to Al-Ti-B failure called Zr poisoning. There are three kinds of poisoning mechanisms related to TiB2, Al3Ti, and a combination of TiB2 and Al3Ti for Zr. First, Zr forms ZrB2 or Ti2Zr with TiB2 in Al-Ti-B to reduce the nucleation ability. Second, Zr existing in the aluminum melt with a high melting point Al3Zr then attracts Ti to reduce the dispersion of Ti as a growth inhibitor. Third, Zr reacts with Al3Ti on TiB2 surface to form Al3Zr, thereby increasing the degree of mismatch with Al and diminishing the refiner’s ability as a nucleation substrate. To gain a better understanding of the mechanism of Zr poisoning, the first principle was used in this study to calculate the adhesion works (ZrB2//Al3Ti), (Ti2Zr//Al3Ti), (Al3Zr//Al3Ti), (Al3Ti//Al), (TiB2//Al3Zr), and (Al3Zr//Al), as well as the surface energy of Al3Zr and adsorption energies of Al to Al3Ti or Al3Zr. The results demonstrated that Zr poisoning originated from the second guess. Zr element exiting in aluminum melt led to the formation of an Al3Zr (001) surface. The interfacial adhesion work of Al3Zr (001)//Al3Ti (001) was not weaker than that of TiB2//Al3Ti. As a result, Al3Zr first combined with Al3Ti to significantly decline the adsorption of Al3Ti (001) on Al, losing its role as a nucleating agent and grain coarsening. Overall, to prevent failure of the grain refiner in Zr containing aluminum melt, the adhesion work interface between the generated phase of the grain refiner and Al3Zr must remain lower to avoid the combination of the generated phase of grain refiner with Al3Zr. In sum, these findings look promising for evaluating future effects of grain refinement in Zr containing aluminum melt.
Open AccessInsights into Poisoning Mechanism of Zr by First Principle Calculation on Adhesion Work and Adsorption Energy between TiB2, Al3Ti, and Al3Zr
Al-Ti-B intermediate alloys are widely used as grain refiners in aluminum alloys owing to the presence of Al3Ti and TiB2 phases. However, the existence of Zr in aluminum alloy melts often results in coarse grain size, leading to Al-Ti-B failure called Zr poisoning. There are three kinds of poisoning mechanisms related to TiB2, Al3Ti, and a combination of TiB2 and Al3Ti for Zr. First, Zr forms ZrB2 or Ti2Zr with TiB2 in Al-Ti-B to reduce the nucleation ability. Second, Zr existing in the aluminum melt with a high melting point Al3Zr then attracts Ti to reduce the dispersion of Ti as a growth inhibitor. Third, Zr reacts with Al3Ti on TiB2 surface to form Al3Zr, thereby increasing the degree of mismatch with Al and diminishing the refiner’s ability as a nucleation substrate. To gain a better understanding of the mechanism of Zr poisoning, the first principle was used in this study to calculate the adhesion works (ZrB2//Al3Ti), (Ti2Zr//Al3Ti), (Al3Zr//Al3Ti), (Al3Ti//Al), (TiB2//Al3Zr), and (Al3Zr//Al), as well as the surface energy of Al3Zr and adsorption energies of Al to Al3Ti or Al3Zr. The results demonstrated that Zr poisoning originated from the second guess. Zr element exiting in aluminum melt led to the formation of an Al3Zr (001) surface. The interfacial adhesion work of Al3Zr (001)//Al3Ti (001) was not weaker than that of TiB2//Al3Ti. As a result, Al3Zr first combined with Al3Ti to significantly decline the adsorption of Al3Ti (001) on Al, losing its role as a nucleating agent and grain coarsening. Overall, to prevent failure of the grain refiner in Zr containing aluminum melt, the adhesion work interface between the generated phase of the grain refiner and Al3Zr must remain lower to avoid the combination of the generated phase of grain refiner with Al3Zr. In sum, these findings look promising for evaluating future effects of grain refinement in Zr containing aluminum melt.
- Open Access
An Investigation into Microstructures and Mechanical Properties of 1060 Pure Aluminum during Submerged Friction Stir Processing at a High Rotating Speed
In this work, 1060 pure aluminum was subjected to high rotating speed submerged friction stir processing (HRS-SFSP). The heat cycle curve of the processing area was measured by K-type thermocouple and temperature recorder. The microstructure, grain size, texture, and tensile fracture of the processing area were analyzed by electron backscattered diffraction and scanning electron microscopy. The results show that the HRS-SFSP caused severe plastic deformation of 1060 aluminum and produced fine recrystallized grains. The minimum average grain size was 0.686 μm at the 2-pass. In addition, the dislocation density in the stirred region was greatly reduced and the high angle grain boundaries (HAGBs) were dominant. The texture strength of pure aluminum increased with the increase in processing passes. The maximum hardness of 66.3 HV and ultimate tensile strength of 95.2 MPa were obtained at 1-pass, which were 86% and 33.9% higher than those of the base material, respectively. The hardness and strength of the stirring zone (SZ) decreased with the increase in the number of processing passes. Therefore, HRS-SFSP pure aluminum can obtain high strength and hardness while maintaining good plasticity.
Open AccessAn Investigation into Microstructures and Mechanical Properties of 1060 Pure Aluminum during Submerged Friction Stir Processing at a High Rotating Speed
In this work, 1060 pure aluminum was subjected to high rotating speed submerged friction stir processing (HRS-SFSP). The heat cycle curve of the processing area was measured by K-type thermocouple and temperature recorder. The microstructure, grain size, texture, and tensile fracture of the processing area were analyzed by electron backscattered diffraction and scanning electron microscopy. The results show that the HRS-SFSP caused severe plastic deformation of 1060 aluminum and produced fine recrystallized grains. The minimum average grain size was 0.686 μm at the 2-pass. In addition, the dislocation density in the stirred region was greatly reduced and the high angle grain boundaries (HAGBs) were dominant. The texture strength of pure aluminum increased with the increase in processing passes. The maximum hardness of 66.3 HV and ultimate tensile strength of 95.2 MPa were obtained at 1-pass, which were 86% and 33.9% higher than those of the base material, respectively. The hardness and strength of the stirring zone (SZ) decreased with the increase in the number of processing passes. Therefore, HRS-SFSP pure aluminum can obtain high strength and hardness while maintaining good plasticity.