Qibing Lv
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Qibing Lv has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Jiao Zhang
School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, China
3 shared publicationsXiao Wang
School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, China
3 shared publicationsJiarong Deng
Key Laboratory of Advanced Technologies of Materials, Ministry of Education, School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, China
2 shared publicationsRui Ma
School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, Sichuan, P.R. China
2 shared publicationsXin Liu
Key Laboratory of Advanced Technologies of Materials, Ministry of Education, School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, China
2 shared publicationsBo Yang
Key Laboratory of Advanced Technologies of Materials, Ministry of Education, School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu, China
1 shared publication
Latest Publications
- 10 August 2024
- Published by Springer Nature in Welding in the World
- Vol. 68 (10) , 2735-2749
Simulation of nonuniform heating induced by alternating-current rail flash butt welding at the end face
- 10 August 2024
- Published by Springer Nature in Welding in the World
- Vol. 68 (10) , 2735-2749
Simulation of nonuniform heating induced by alternating-current rail flash butt welding at the end face
- 18 January 2024
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 77 (4) , 1161-1171
Numerical Model of Rail Flash Welding Liquid Bridge Heating Process
- 18 January 2024
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 77 (4) , 1161-1171
Numerical Model of Rail Flash Welding Liquid Bridge Heating Process
- Open Access
Effect of Normalising Process on the Corrosion Behaviour of U75V Rail Flash Butt Welded Joints in a Marine Environment
U75V rail steel is widely used in railways in China, including train tunnels in mountain and subsea projects, where it suffers from selective corrosion near welded joints. To ensure adequate railway service life, this study examines the effect of the normalisation process on the electrochemical behaviour of U75V rail-welded joints (URWJs) manufactured by flash butt welding (FBW) using potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS). Corrosion morphology and elemental distribution analyses were performed to investigate the corrosion behaviour. The results show that the grains within the joints became finer and more homogeneous after normalisation, with a lower corrosion rate and higher corrosion resistance. It is demonstrated that fewer corrosion products were formed on the surface of the normalised joints after electrochemical test, and the corrosion resistance of the URWJs improved, owing to the formation of denser passivation films caused by normalisation. These mechanisms of corrosion response help explain corrosion failure in railway lines, as well as also help optimise the welding process and normalising processes to obtain a corrosion-resistant microstructure and ensure the quality of welded joints.
Open AccessEffect of Normalising Process on the Corrosion Behaviour of U75V Rail Flash Butt Welded Joints in a Marine Environment
U75V rail steel is widely used in railways in China, including train tunnels in mountain and subsea projects, where it suffers from selective corrosion near welded joints. To ensure adequate railway service life, this study examines the effect of the normalisation process on the electrochemical behaviour of U75V rail-welded joints (URWJs) manufactured by flash butt welding (FBW) using potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS). Corrosion morphology and elemental distribution analyses were performed to investigate the corrosion behaviour. The results show that the grains within the joints became finer and more homogeneous after normalisation, with a lower corrosion rate and higher corrosion resistance. It is demonstrated that fewer corrosion products were formed on the surface of the normalised joints after electrochemical test, and the corrosion resistance of the URWJs improved, owing to the formation of denser passivation films caused by normalisation. These mechanisms of corrosion response help explain corrosion failure in railway lines, as well as also help optimise the welding process and normalising processes to obtain a corrosion-resistant microstructure and ensure the quality of welded joints.
- 30 January 2022
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 120 (1-2) , 173-183
Numerical simulation of end face heating in alternating current flash butt welding based on electrical–thermal bidirectional coupling
- 30 January 2022
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 120 (1-2) , 173-183
Numerical simulation of end face heating in alternating current flash butt welding based on electrical–thermal bidirectional coupling
- 16 September 2020
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 111 (9) , 780-787
Effects of rail flash-butt welding and post-weld heat treatment processes meeting different national standards on residual stresses of welded joints
This study investigates residual stresses of the welded joint heat-affected zone for the processes that meet the Chinese and European standards of field rail welding. Furthermore, this study investigates the factory rail welding process and different normalizing methods in China. According to the residual stresses data and the Debye ring test result, the residual stresses distribution of the welded joint meets the Chinese standard and uses induction normalizing treatment resulting in the best service performance and an improvement in grain size uniformity. In the absence of a normalizing process, the ideal welding process that meets the Chinese standard is actually inferior to that which meets the European standard, with regard to a uniform distribution of the residual stresses of the welded joint.
- 16 September 2020
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 111 (9) , 780-787
Effects of rail flash-butt welding and post-weld heat treatment processes meeting different national standards on residual stresses of welded joints
This study investigates residual stresses of the welded joint heat-affected zone for the processes that meet the Chinese and European standards of field rail welding. Furthermore, this study investigates the factory rail welding process and different normalizing methods in China. According to the residual stresses data and the Debye ring test result, the residual stresses distribution of the welded joint meets the Chinese standard and uses induction normalizing treatment resulting in the best service performance and an improvement in grain size uniformity. In the absence of a normalizing process, the ideal welding process that meets the Chinese standard is actually inferior to that which meets the European standard, with regard to a uniform distribution of the residual stresses of the welded joint.
- 15 July 2019
- Published by Springer Nature in Journal of Materials Research
- Vol. 34 (19) , 3351-3360
Extrusion behavior of impurities in upsetting process of rail flash butt welding based on finite element method
- 15 July 2019
- Published by Springer Nature in Journal of Materials Research
- Vol. 34 (19) , 3351-3360
Extrusion behavior of impurities in upsetting process of rail flash butt welding based on finite element method