Wenbin Deng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Wenbin Deng has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Yunhui Mei
School of Electrical Engineering, Tiangong University, Tianjin, China
2 shared publications - Changsheng Ma
Department of Radiation Physics, Shandong Cancer Hospital and Institute, Shandong First Medical University and Shandong Academy of Medical Sciences, Jinan, China
1 shared publication - Gaojia Zhu
School of Electrical Engineering, Tiangong University, Tianjin, China
1 shared publication - Guo-Quan Lu
Department of Materials Science and Engineering, Virginia Polytechnic Institute and State University, Blacksburg, USA
1 shared publication - Longnv Li
School of Electrical Engineering, Tiangong University, Tianjin, China
1 shared publication Lu Wang
School of Mechanical Engineering, Tiangong University, Tianjin, China
1 shared publication
Latest Publications
- 1 October 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Emerging and Selected Topics in Power Electronics
- Vol. 9 (4) , 4887-4896
A Way to Reduce Leakage Current and Improve Reliability of Wire-Bonds for 300-A Multichip SiC Hybrid Modules
In this paper, pressureless sintering of nanosilver paste is proposed to enhance the reliability of wire-bonds with SiC chips by both alleviating thermo-mechanical stresses and enhancing thermal coupling of bonding wires and chips. A multichip 1200-V/300-A SiC hybrid module with six Si IGBTs and twelve SiC Schottky Barrier Diodes (SBDs) is demonstrated. The lifetime of the wire-bonds with the SiC SBD bonded by the pressureless sintered nanosilver is 27.9% longer than that by the high-temperature solder under the power cycling with the constant temperature swing. The lifetime of the wire-bonds with the IGBT also bonded by the pressureless sintered nanosilver is 46.2% longer than that by the high-temperature solder under the power cycling with the constant conduction current. Furthermore, not only the cost of 1700-V SiC SBDs is quite similar with that of 1200-V ones, but also the leakage current of the 1200-V/300-A SiC hybrid module can be reduced greatly using 1700-V SiC SBDs as free-wheeling diodes instead of regular 1200-V ones. Considering the much larger leakage current of a SiC SBD compared to that of a Si PiN diode. It is feasible to use a SiC SBD with the higher blocking voltage to reduce the significant leakage current of the free-wheeling SBD with almost no cost increase.
- 1 October 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Emerging and Selected Topics in Power Electronics
- Vol. 9 (4) , 4887-4896
A Way to Reduce Leakage Current and Improve Reliability of Wire-Bonds for 300-A Multichip SiC Hybrid Modules
In this paper, pressureless sintering of nanosilver paste is proposed to enhance the reliability of wire-bonds with SiC chips by both alleviating thermo-mechanical stresses and enhancing thermal coupling of bonding wires and chips. A multichip 1200-V/300-A SiC hybrid module with six Si IGBTs and twelve SiC Schottky Barrier Diodes (SBDs) is demonstrated. The lifetime of the wire-bonds with the SiC SBD bonded by the pressureless sintered nanosilver is 27.9% longer than that by the high-temperature solder under the power cycling with the constant temperature swing. The lifetime of the wire-bonds with the IGBT also bonded by the pressureless sintered nanosilver is 46.2% longer than that by the high-temperature solder under the power cycling with the constant conduction current. Furthermore, not only the cost of 1700-V SiC SBDs is quite similar with that of 1200-V ones, but also the leakage current of the 1200-V/300-A SiC hybrid module can be reduced greatly using 1700-V SiC SBDs as free-wheeling diodes instead of regular 1200-V ones. Considering the much larger leakage current of a SiC SBD compared to that of a Si PiN diode. It is feasible to use a SiC SBD with the higher blocking voltage to reduce the significant leakage current of the free-wheeling SBD with almost no cost increase.