Latest Publications

  • Open Access

    Applications of soft biomaterials based on organic and hybrid thin films deposited from the vapor phase

    by Sophie Marcelja, Lisanne Demelius, Taher Abu Ali, Margherita Aghito, Fabian Muralter, Gabriel Hernandez Rodriguez, Marianne Kräuter, Katrin Unger, Lukas Wolfsberger, Anna Maria Coclite

    Soft biomaterials are a crucial component in several application fields. They are used, for example, in biomedical implants, biosensors, drug delivery systems as well as in tissue engineering. In parallel to extensive ongoing efforts to synthesize new materials, the development of means to tailor the materials’ surface properties and thus their interaction with the environment is an important field of research. This has led to the emergence of several surface modification techniques that enable the exploitation of biomaterials in a broader range of technologies. In particular, the use of functional thin films can enable a plethora of biomedical applications by combining advantageous bulk properties of the substrate (e.g. flexibility, lightweight, structural strength) with tailored surface properties of the thin film (e.g. enhancing/prevention of cell proliferation, controlled drug release). For some biomedical applications, thin films can also be the main functional components, e.g. in biosensors. The present review focuses on recent developments in the applications of soft biomaterials based on thin films deposited from the vapor phase. In the field of soft biomaterials, the possibility of depositing from the vapor phase—without the need for any solvents—offers the unprecedented benefit that no toxic leachables are included in the biomaterial. Further, due to the complete lack of solvents and chemicals overall being used in small quantities only, depositing thin films from the vapor phase can be a more sustainable choice than other techniques that are commonly used.


  • Open Access

    Vapor Deposited Zeolitic Imidazolate Framework-8 Derived from Porous ZnO Thin Films

    by Marianne Kräuter, Katrin Unger, Roland Resel, Anna Maria Coclite

    In recent years, the vapor deposition of zeolitic imidazolate framework-8 (ZIF-8) has gained high attraction due to its good scalability, conformality, and thickness control. The present study provides new fundamental insights regarding the vapor deposition of ZIF-8 from zinc oxide (ZnO). During synthesis, ZnO thin films with different percentages of open porosity (14.5%–24%) were subjected to a 2-methylimidazole vapor for different conversion times (20 min–24 h). For the first time, the impact of the porosity of ZnO thin films onto the converted ZIF-8 is investigated. Grazing incidence X-ray diffraction reveals randomly oriented crystallites of ZIF-8, which already appear after 20 min of conversion. The thickness, roughness, and average particle height of the ZIF-8 layers increase with the conversion time, reaching values up to (172 ± 20) nm, (29 ± 3) nm, and (113 ± 8) nm, respectively, for ZIF-8 obtained from ZnO with 14.5% open porosity. At long conversion times (i.e., 24 h), the results hint at greater precursor porosities resulting in lower thicknesses of ZIF-8, as the thickness, roughness, and average particle height for ZIF-8 obtained from 24%-porous ZnO show values of (132 ± 20) nm, (25 ± 3) nm and (80 ± 8) nm, respectively. Additionally, the potential of the ZIF-8 layers as a photocatalyst for the degradation of the organic dye methylene blue was studied. The ZIF-8 enhances the degradation by approximately 8% when compared to degradation without a photocatalyst.


  • Open Access

    Tuning the Porosity of Piezoelectric Zinc Oxide Thin Films Obtained from Molecular Layer-Deposited “Zincones”

    by Marianne Kräuter, Taher Abu Ali, Barbara Stadlober, Roland Resel, Katrin Unger, Anna Maria Coclite

    Porous zinc oxide (ZnO) thin films were synthesized via the calcination of molecular layer-deposited (MLD) “zincone” layers. The effect of the MLD process temperature (110 °C, 125 °C) and of the calcination temperature (340 °C, 400 °C, 500 °C) on the chemical, morphological, and crystallographic properties of the resulting ZnO was thoroughly investigated. Spectroscopic ellipsometry reveals that the thickness of the calcinated layers depends on the MLD temperature, resulting in 38–43% and 52–56% of remaining thickness for the 110 °C and 125 °C samples, respectively. Ellipsometric porosimetry shows that the open porosity of the ZnO thin films depends on the calcination temperature as well as on the MLD process temperature. The maximum open porosity of ZnO derived from zincone deposited at 110 °C ranges from 14.5% to 24%, rising with increasing calcination temperature. Compared with the 110 °C samples, the ZnO obtained from 125 °C zincone yields a higher porosity for low calcination temperatures, namely 18% for calcination at 340 °C; and up to 24% for calcination at 500 °C. Additionally, the porous ZnO thin films were subjected to piezoelectric measurements. The piezoelectric coefficient, d33, was determined to be 2.8 pC/N, demonstrating the potential of the porous ZnO as an, e.g., piezoelectric sensor or energy harvester.


  • Open Access

    Influence of Precursor Density and Conversion Time on the Orientation of Vapor-Deposited ZIF-8

    by Marianne Kräuter, Alexander John Cruz, Timothée Stassin, Sabina Rodríguez-Hermida, Rob Ameloot, Roland Resel, Anna Maria Coclite

    ZIF-8 was synthesized by subjecting ZnO thin films deposited via plasma-enhanced atomic layer deposition to a 2-methylimidazole vapor. The impact of the conversion time as well as the density and thickness of the ZnO precursor on the resulting ZIF-8 layers were investigated. Grazing Incidence X-ray diffraction reveals a preferred (100) or (111) orientation of the ZIF-8 crystals, depending on thickness and density of the precursor, and with a more prominent orientation at longer conversion times. The onset of crystallization occurs after 20 min of conversion for the less dense precursor, compared to 40 min for the denser one. The ZIF-8 thickness and roughness increase with conversion time. The final thickness of the ZIF-8 layer depends on the thickness and density of the precursor layer, and can be up to 15-fold higher than the precursor thickness.