Cheng-Gong Zhang
Research Subjects
Cheng-Gong Zhang has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
Xue-Yan Dong
Qilu Zhongke
4 shared publicationsXin-Lei Li
Qilu Zhongke
3 shared publicationsXing-Wei Yan
Qilu Zhongke
3 shared publicationsZhong-Zheng Chen
Qilu Zhongke
3 shared publicationsZi-Lei Liu
Institute of Optical Physics and Engineering Technology
3 shared publicationsHao-Zhu Wang
Qilu Zhongke
2 shared publications
Latest Publications
- 17 August 2026
- Published by Optica Publishing Group in Applied Optics
- Vol. 65 (24) , 8408-8411
High-power nanosecond green laser with efficient second-harmonic generation
High-power nanosecond green lasers are widely used in precision machining due to their small heat-affected zone, excellent beam quality, and high process controllability. In this work, second-harmonic generation (SHG) of a high-power nanosecond laser was demonstrated employing type-I noncritical phase matching (NCPM) in an LBO crystal. An average output power of 200 W at 532 nm was achieved from a 1064 nm fundamental beam with an average input power of 363 W, corresponding to an SHG conversion efficiency of 55.1%. The green laser operated at a repetition rate of 20 kHz with a pulse width of 63.1 ns and a beam quality factor M 2 of 2.33. Thermal simulation revealed a temperature gradient of 0.47°C within the LBO crystal. This research presents a green light source of high stability, suitable for machining high-reflectivity materials such as diamond.
- 17 August 2026
- Published by Optica Publishing Group in Applied Optics
- Vol. 65 (24) , 8408-8411
High-power nanosecond green laser with efficient second-harmonic generation
High-power nanosecond green lasers are widely used in precision machining due to their small heat-affected zone, excellent beam quality, and high process controllability. In this work, second-harmonic generation (SHG) of a high-power nanosecond laser was demonstrated employing type-I noncritical phase matching (NCPM) in an LBO crystal. An average output power of 200 W at 532 nm was achieved from a 1064 nm fundamental beam with an average input power of 363 W, corresponding to an SHG conversion efficiency of 55.1%. The green laser operated at a repetition rate of 20 kHz with a pulse width of 63.1 ns and a beam quality factor M 2 of 2.33. Thermal simulation revealed a temperature gradient of 0.47°C within the LBO crystal. This research presents a green light source of high stability, suitable for machining high-reflectivity materials such as diamond.
- 14 November 2025
- Published by Optica Publishing Group in Applied Optics
- Vol. 64 (33) , 10077-10081
High-power and high-beam-quality acousto-optic Q -switched hybrid-cavity slab laser
We propose a high-power, high-beam-quality hybrid-cavity acousto-optic (AO) Q -switched slab laser. This laser employs a large-area-pumped Nd:YAG slab laser crystal and is based on a hybrid resonator cavity combining stable and off-axis unstable modes, incorporating large-aperture acousto-optic Q -switching technology to achieve direct output of high-power nanosecond lasers. By establishing a rate equation for acousto-optic Q -switching in the Nd:YAG slab laser oscillator, we simulate and optimize the laser performance, effectively enhancing the laser conversion efficiency. Furthermore, we design a hybrid cooling temperature control structure for the slab crystal, effectively suppressing the thermal lensing effect along the thickness direction of the crystal. The experimental results demonstrate that the output power of the laser reaches 3062 W at a pump power of 9800 W, with an optical-to-optical conversion efficiency of 31%, a pulse width of 46 ns, a single-pulse energy of 153.1 mJ, and beam quality factors of M x 2 ≤4.8 and M y 2 ≤3.5. The hybrid-cavity acousto-optic Q -switching design simplifies the optical path structure, reduces the number of components in the cavity, and effectively minimizes the laser volume. Additionally, this laser shows broad application potential in the field of laser cleaning, achieving a cleaning grade of Sa 2.5 and an efficiency of 25m 2 /h when used for line-laser rust removal on Q235 carbon steel with an initial rust grade of C.
- 14 November 2025
- Published by Optica Publishing Group in Applied Optics
- Vol. 64 (33) , 10077-10081
High-power and high-beam-quality acousto-optic Q -switched hybrid-cavity slab laser
We propose a high-power, high-beam-quality hybrid-cavity acousto-optic (AO) Q -switched slab laser. This laser employs a large-area-pumped Nd:YAG slab laser crystal and is based on a hybrid resonator cavity combining stable and off-axis unstable modes, incorporating large-aperture acousto-optic Q -switching technology to achieve direct output of high-power nanosecond lasers. By establishing a rate equation for acousto-optic Q -switching in the Nd:YAG slab laser oscillator, we simulate and optimize the laser performance, effectively enhancing the laser conversion efficiency. Furthermore, we design a hybrid cooling temperature control structure for the slab crystal, effectively suppressing the thermal lensing effect along the thickness direction of the crystal. The experimental results demonstrate that the output power of the laser reaches 3062 W at a pump power of 9800 W, with an optical-to-optical conversion efficiency of 31%, a pulse width of 46 ns, a single-pulse energy of 153.1 mJ, and beam quality factors of M x 2 ≤4.8 and M y 2 ≤3.5. The hybrid-cavity acousto-optic Q -switching design simplifies the optical path structure, reduces the number of components in the cavity, and effectively minimizes the laser volume. Additionally, this laser shows broad application potential in the field of laser cleaning, achieving a cleaning grade of Sa 2.5 and an efficiency of 25m 2 /h when used for line-laser rust removal on Q235 carbon steel with an initial rust grade of C.
- 19 August 2025
- Published by Optica Publishing Group in Applied Optics
- Vol. 64 (25) , 7298-7303
Pulsed laser milling process of CVD single crystal diamond
Chemical vapor deposition (CVD) diamond has high thermal conductivity and a low coefficient of thermal expansion, making it a good thermal conductive material. However, conventional processing methods are often difficult to balance processing quality while pursuing high efficiency. In view of this, this study focuses on the milling of CVD single crystal diamond using nanosecond and picosecond laser technology, aiming to optimize its processing accuracy and efficiency. By systematically investigating the effects of laser incidence angle, pulse width, and spot size on the milling angle of diamond. It is found that the slope angle of the machined surface can be effectively reduced by decreasing the laser incidence angle, shortening the pulse width, and reducing the spot size. With an average power of 200 W, a pulse width of 12 ps, a spot diameter of 60 µm, an incidence angle of 3°, and a scanning speed of 30 mm/s, the milling angle of diamond can be optimized to 1.30°, and at the same time, the surface roughness Sa is 0.42 µm, the maximum height difference of the surface Sz is 2.76 µm, and the machining efficiency reaches 32.57mm3/h. When the pulse width is adjusted to 150 ns and the rest of the parameters are kept unchanged, the milling angle of diamond is 2.45°, the Sa is 0.45 µm, the Sz is 2.88 µm, and the machining efficiency is improved to 66.10mm3/h. The present study proposes a high-efficiency and low-damage machining strategy for chip bonding diamond, which provides an important reference for the application of diamond in the field of microelectronics encapsulation.
- 19 August 2025
- Published by Optica Publishing Group in Applied Optics
- Vol. 64 (25) , 7298-7303
Pulsed laser milling process of CVD single crystal diamond
Chemical vapor deposition (CVD) diamond has high thermal conductivity and a low coefficient of thermal expansion, making it a good thermal conductive material. However, conventional processing methods are often difficult to balance processing quality while pursuing high efficiency. In view of this, this study focuses on the milling of CVD single crystal diamond using nanosecond and picosecond laser technology, aiming to optimize its processing accuracy and efficiency. By systematically investigating the effects of laser incidence angle, pulse width, and spot size on the milling angle of diamond. It is found that the slope angle of the machined surface can be effectively reduced by decreasing the laser incidence angle, shortening the pulse width, and reducing the spot size. With an average power of 200 W, a pulse width of 12 ps, a spot diameter of 60 µm, an incidence angle of 3°, and a scanning speed of 30 mm/s, the milling angle of diamond can be optimized to 1.30°, and at the same time, the surface roughness Sa is 0.42 µm, the maximum height difference of the surface Sz is 2.76 µm, and the machining efficiency reaches 32.57mm3/h. When the pulse width is adjusted to 150 ns and the rest of the parameters are kept unchanged, the milling angle of diamond is 2.45°, the Sa is 0.45 µm, the Sz is 2.88 µm, and the machining efficiency is improved to 66.10mm3/h. The present study proposes a high-efficiency and low-damage machining strategy for chip bonding diamond, which provides an important reference for the application of diamond in the field of microelectronics encapsulation.
- 3 April 2024
- Published by Optica Publishing Group in Applied Optics
- Vol. 63 (11) , 2863-2867
4.4 kW Nd:YAG slab amplifier with a high repetition frequency and high beam quality
Using the self-developed fused indium wetting technology and planar waveguide, the uniform heat dissipation of the slab crystal and uniform pumping of the pump light were achieved, respectively. Based on the master oscillator power amplification (MOPA) scheme, the power was then amplified when the seed light source passed through the Nd:YAG slab crystal three times. Additionally, the image transfer system that we added to the amplified optical path achieved high beam quality. Finally, we obtained a rectangular pulsed laser with an output average power of 4461 W, a repetition frequency of 20 kHz, a pulse width of 62 ns, an optical-to-optical conversion efficiency of 26.8%, and a beam quality of β x =7.0 and β y =7.7.
- 3 April 2024
- Published by Optica Publishing Group in Applied Optics
- Vol. 63 (11) , 2863-2867
4.4 kW Nd:YAG slab amplifier with a high repetition frequency and high beam quality
Using the self-developed fused indium wetting technology and planar waveguide, the uniform heat dissipation of the slab crystal and uniform pumping of the pump light were achieved, respectively. Based on the master oscillator power amplification (MOPA) scheme, the power was then amplified when the seed light source passed through the Nd:YAG slab crystal three times. Additionally, the image transfer system that we added to the amplified optical path achieved high beam quality. Finally, we obtained a rectangular pulsed laser with an output average power of 4461 W, a repetition frequency of 20 kHz, a pulse width of 62 ns, an optical-to-optical conversion efficiency of 26.8%, and a beam quality of β x =7.0 and β y =7.7.
- 27 January 2022
- Published by Wiley in Physica Status Solidi (b)
- Vol. 259 (4)
Monolayer NbNSe with High Fermi Velocity and Anisotropic Properties
2D materials with high carrier mobility and anisotropy have attracted extensive research interest. The single‐layer NbNSe has anisotropic elasticity, and the Young's modulus is up to 106 N m−1. The Fermi velocity is as high as 3.5 × 105 m s−1, and the transition between semiconductor and metallic states can be achieved by applying a uniaxial tensile strain of 2%. In addition, anisotropic electron transport properties indicate that currents along the b direction can reach 12.4 μA under a bias voltage of 2.0 V. These findings provide a physical basis for the design and synthesis of a new 2D material.
- 27 January 2022
- Published by Wiley in Physica Status Solidi (b)
- Vol. 259 (4)
Monolayer NbNSe with High Fermi Velocity and Anisotropic Properties
2D materials with high carrier mobility and anisotropy have attracted extensive research interest. The single‐layer NbNSe has anisotropic elasticity, and the Young's modulus is up to 106 N m−1. The Fermi velocity is as high as 3.5 × 105 m s−1, and the transition between semiconductor and metallic states can be achieved by applying a uniaxial tensile strain of 2%. In addition, anisotropic electron transport properties indicate that currents along the b direction can reach 12.4 μA under a bias voltage of 2.0 V. These findings provide a physical basis for the design and synthesis of a new 2D material.
- 1 January 2022
- Published by Elsevier in Physica E: Low-dimensional Systems and Nanostructures
- Vol. 135, 114971
Intrinsic direct bandgap semiconductor with high stability, strong anisotropy and controllable edge position in BrHfN monolayer
- 1 January 2022
- Published by Elsevier in Physica E: Low-dimensional Systems and Nanostructures
- Vol. 135, 114971
Intrinsic direct bandgap semiconductor with high stability, strong anisotropy and controllable edge position in BrHfN monolayer
- 6 March 2019
- Published by Cambridge University Press (CUP) in Geological Magazine
- Vol. 156 (9) , 1587-1604
Detrital zircon U–Pb geochronology and geochemistry of late Neoproterozoic – early Cambrian sedimentary rocks in the Cathaysia Block: constraint on its palaeo-position in Gondwana supercontinent
We present updated U–Pb ages and Hf isotopic compositions of detrital zircons and whole-rock geochemical data to investigate the provenance and tectonic setting of late Neoproterozoic and early Cambrian sandstones from the Cathaysia Block, in order to offer new constraints on its tectonic evolution and its palaeo-position within the supercontinent. The source rocks for the studied sandstones were dominated by felsic–intermediate materials with moderate weathering history. U–Pb dating results show major populations atc. 2500 Ma, 1000–900 Ma and 870–716 Ma with subordinate peaks at 655–532 Ma, consistent with the global Neoarchean continental crust growth, assembly and break-up of Rodinia, and Pan-African Event associated with the formation of Gondwana. Zircon U–Pb ages and Hf isotopic data suggest that most derived from exotic terranes once connected to the Cathaysia Block. Using whole-rock geochemical analysis, it was determined that the studied sedimentary rocks were deposited in a passive continental margin and the Cathaysia and Yangtze blocks were part of the same continent; no Cambrian ocean existed between them. Compiling a detrital zircon dataset from Qiangtang, northern India, the Lhasa Terrane and Western Australia, the Cathaysia Block seems to be more similar to the Qiangtang and western part of the northern India margin, instead of having a direct connection with the Lhasa Terrane and Western Australia in the Gondwana reconstruction during the late Neoproterozoic and Cambrian eons.
- 6 March 2019
- Published by Cambridge University Press (CUP) in Geological Magazine
- Vol. 156 (9) , 1587-1604
Detrital zircon U–Pb geochronology and geochemistry of late Neoproterozoic – early Cambrian sedimentary rocks in the Cathaysia Block: constraint on its palaeo-position in Gondwana supercontinent
We present updated U–Pb ages and Hf isotopic compositions of detrital zircons and whole-rock geochemical data to investigate the provenance and tectonic setting of late Neoproterozoic and early Cambrian sandstones from the Cathaysia Block, in order to offer new constraints on its tectonic evolution and its palaeo-position within the supercontinent. The source rocks for the studied sandstones were dominated by felsic–intermediate materials with moderate weathering history. U–Pb dating results show major populations atc. 2500 Ma, 1000–900 Ma and 870–716 Ma with subordinate peaks at 655–532 Ma, consistent with the global Neoarchean continental crust growth, assembly and break-up of Rodinia, and Pan-African Event associated with the formation of Gondwana. Zircon U–Pb ages and Hf isotopic data suggest that most derived from exotic terranes once connected to the Cathaysia Block. Using whole-rock geochemical analysis, it was determined that the studied sedimentary rocks were deposited in a passive continental margin and the Cathaysia and Yangtze blocks were part of the same continent; no Cambrian ocean existed between them. Compiling a detrital zircon dataset from Qiangtang, northern India, the Lhasa Terrane and Western Australia, the Cathaysia Block seems to be more similar to the Qiangtang and western part of the northern India margin, instead of having a direct connection with the Lhasa Terrane and Western Australia in the Gondwana reconstruction during the late Neoproterozoic and Cambrian eons.