Mohd Shahriman Adenan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Mohd Shahriman Adenan has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Baljit Singh Bhathal Singh
Faculty of Mechanical Engineering, Universiti Teknologi Mara, Shah Alam 40450, Selangor, Malaysia
1 shared publication - Hui Leng Choo
School of Engineering, Taylor’s University, Subang Jaya, Malaysia
1 shared publication - John Ryan Cortez Dizon
Design, Research, Extension in Additive Manufacturing (DR3AM) Center, Bataan Peninsula State University (Main Campus), City of Balanga, Philippines
1 shared publication Juri Saedon
Faculty of Mechanical Engineering, Universiti Teknologi MARA, Shah Alam, Malaysia
1 shared publication- Mohammad Kamil Sued
Fakulti Teknologi dan Kejuruteraan Industri dan Pembuatan, Universiti Teknikal Malaysia Melaka, Hang Tuah Jaya, 76100 Durian Tunggal, Melaka, Malaysia
1 shared publication Mohd Afzan Mohd Anuar
Faculty of Mechanical Engineering, Universiti Teknologi MARA, Shah Alam, Malaysia
1 shared publication
Latest Publications
- Open Access
Defect Evolution, Texture Modification, and T6 Response of LPBF AA7075 Reinforced with AlCoCrFeNi2.1 Eutectic HEA Particles
Laser powder bed fusion (LPBF) of AA7075 is severely constrained by a narrow process window and susceptibility to defect formation (hot cracking and porosity), which often dominates performance. In this study, 5 wt.% AlCoCrFeNi2.1 high-entropy alloy (HEA) particles, volumetric energy density (VED = 74–222 J·mm−3), and subsequent T6 heat treatment were systematically investigated to reveal their combined effects on defect structure, crystallographic texture/substructure, and tensile behaviour. Quantitative EBSD shows a measurable grain refinement in the as-built state (average grain size 13.44 → 11.80 µm, ~12%) accompanied by a pronounced weakening of the fibre texture (maximum MRD 4.94 → 2.38), indicating disrupted epitaxial growth and a more dispersed orientation distribution. After T6, the reinforced alloy retains a higher low-angle boundary fraction (31.62% vs. 24.17% in unreinforced AA7075) and a higher kernel average misorientation (0.80° vs. 0.60°), consistent with particle-stabilised substructure retention and retarded recovery. Across all VEDs, AA7075-HEA exhibits higher microhardness (compared with AA7075, the addition of HEA increases the hardness by roughly 20–50 HV) and tensile strength, with the intermediate VED (140.74 J·mm−3, T6 states) yielding the best performance. While macroscopic cracking is not fully eliminated, the results clarify that HEA-enabled texture/substructure modifications can contribute to enhanced defect tolerance and are more effectively translated into tensile performance when the as-built defect severity is controlled. These findings provide quantitative insights into defect–microstructure–property coupling in LPBF AA7075-HEA composites from as-built to T6 states.
Open AccessDefect Evolution, Texture Modification, and T6 Response of LPBF AA7075 Reinforced with AlCoCrFeNi2.1 Eutectic HEA Particles
Laser powder bed fusion (LPBF) of AA7075 is severely constrained by a narrow process window and susceptibility to defect formation (hot cracking and porosity), which often dominates performance. In this study, 5 wt.% AlCoCrFeNi2.1 high-entropy alloy (HEA) particles, volumetric energy density (VED = 74–222 J·mm−3), and subsequent T6 heat treatment were systematically investigated to reveal their combined effects on defect structure, crystallographic texture/substructure, and tensile behaviour. Quantitative EBSD shows a measurable grain refinement in the as-built state (average grain size 13.44 → 11.80 µm, ~12%) accompanied by a pronounced weakening of the fibre texture (maximum MRD 4.94 → 2.38), indicating disrupted epitaxial growth and a more dispersed orientation distribution. After T6, the reinforced alloy retains a higher low-angle boundary fraction (31.62% vs. 24.17% in unreinforced AA7075) and a higher kernel average misorientation (0.80° vs. 0.60°), consistent with particle-stabilised substructure retention and retarded recovery. Across all VEDs, AA7075-HEA exhibits higher microhardness (compared with AA7075, the addition of HEA increases the hardness by roughly 20–50 HV) and tensile strength, with the intermediate VED (140.74 J·mm−3, T6 states) yielding the best performance. While macroscopic cracking is not fully eliminated, the results clarify that HEA-enabled texture/substructure modifications can contribute to enhanced defect tolerance and are more effectively translated into tensile performance when the as-built defect severity is controlled. These findings provide quantitative insights into defect–microstructure–property coupling in LPBF AA7075-HEA composites from as-built to T6 states.
- 18 February 2022
- Published by Springer Nature in MRS Communications
- Vol. 12 (2) , 194-200
Simulation and verification of grain size prediction on SS316L GMAW process
- 18 February 2022
- Published by Springer Nature in MRS Communications
- Vol. 12 (2) , 194-200
Simulation and verification of grain size prediction on SS316L GMAW process