YPYurii I. Pochivalov

Yurii I. Pochivalov

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Yurii I. Pochivalov has a total of 37 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Scanning Tunneling Microscopy of Intermediate Transformation Structures in Electric Arc Surfacing Modified with Titanium Carbonitrides on Pipe Steel

    by Kuznetsov Pavel, Galchenko Nina, Pochivalov Yury

    In the present paper, the structure of electric arc coatings modified with nanodispersed titanium carbonitride additives on low-carbon pipe steel is studied using optical, scanning tunneling, and transmission electron microscopy. The obtained “substrate-modified surface” compositions are tested for fracture toughness, and the derived test results are compared with the data for the compositions formed using commercial electrodes. It is found that the introduction of titanium carbonitride nanoparticles with the estimated content from 0.15 to 1 wt% refines the ferrite–pearlite structure. Scanning tunneling microscopy reveals acicular and lamellar structures in local regions of ferrite grains, which, by morphological features, are identified as lower bainite and acicular ferrite. It is concluded that the increase in fracture toughness of the “substrate-modified surface” composition is of a complex nature. First of all, this increase is associated with grain refinement, while the formation of intermediate transformation structures plays a secondary role.

  • Structure Formation and Mechnical Properties of Low-Carbon Steel After Lengthwise and Cross Rolling

    by A. I. Gordienko, Yu. I. Pochivalov, I. V. Vlasov, I. P. Mishin


  • Open Access

    The effects of high-energy influence on the structure and fatigue life of VT6 titanium alloy and its welded joint

    by A. S. Smirnova, Yu. I. Pochivalov, V. E. Panin, A. V. Nasonovskaya, A. G. Malikov, A. M. Orishich

    In this study, a new surface treatment method was applied to laser welded joints of a high-strength VT6 titanium alloy. After welding, the welded joints were exposed to high energy electric pulse treatment in combination with ultrasonic forging. Ultrasonic forging creates a high-defect structure with high curvature of the crystal lattice in the surface layer, as evidenced by the appearance of extinction contours. The total number of cycles to failure is 8,700 for the samples untreated after welding and 29,400 for the treated samples, which indicates a significant increase in the fatigue life of the welded joint.


  • Open Access

    Effect of ultrasonic forging of surface layers on the fatigue failure of a VT8-1 titanium alloy welded joint

    by A. Smirnova, Yu. Pochivalov

    The paper studies the effect of ultrasonic forging of the surface layers of linear friction welded joints of the VT8-1 titanium alloy on their fatigue life. Low-cycle fatigue tests report a 2.5-fold increase in the service life of the welded joint after ultrasonic forging of its surface layers. The fractographic analysis of the fracture surfaces shows that, after ultrasonic forging, cracks initiate from the lateral surface of a specimen and have a radial front without river markings and with scarcely visible tear ridges. The microrelief of the initiation and growth zone of the main crack indicates a more ductile pattern of the fatigue crack growth in the material after ultrasonic forging. Ultrasonic forging of the surface layers of the VT8-1 welded joint increases its fatigue life and presents an effective method for improving the service life of welded joints, thus excluding a complex thermomechanical treatment.

  • The structure and mechanical properties of welded joints of 17Mn1Si steel subjected to pulsed mechanical-electrophysical treatment

    by S. V. Panin, I. V. Vlasov, R. V. Stankevich, A. S. Smirnova, A. V. Yakovlev, Yu. I. Pochivalov, D. V. Valuev

    The structure and mechanical properties of specimens of welded joints of the 17Mn1Si pipe steel after modification by means of surface ultrasonic impact and combined pulsed mechano-electrophysical treatments is studied. The research was carried out on specimens cut from steel plates having an integral joint both in the heat-affected zone and directly in the weld. It is shown that the proposed treatment methods provide hardening of the surface layer, as well as an increase in tensile strength under static tension. The toughness of the specimens a) without welding (as supplied state), b) with a weld, and c) after modification of the surface layer was tested at room temperature and negative one, T = −70 °C. The differences revealed in the structure and deformation behavior of the specimens subjected to different treatment methods are shown and discussed.

  • Modification of structure and impact toughness of 17Mn1Si pipe steel welded joints by pulsed mechanical-electrophysical treatment

    by I. V. Vlasov, R. V. Stankevich, A. S. Smirnova, A. V. Yakovlev, Yu. I. Pochivalov, D. V. Valuev, S. V. Panin

    The structure and mechanical properties of welded joints of 17Mn1Si pipe steel after modification by means of surface ultrasonic impact straining as well as combined pulsed mechanical-electrophysical treatments have been studied. Welded joint specimens were cut out of steel plates from the heat affected zone and from the center of the weld. It is shown that the proposed treatment technique ensures hardening of the surface layer, as well as increasing the yield strength under static tension. Impact toughness tests for the specimens (i) without a weld (as supplied state), (ii) with a welded joint, and (iii) after the modifications by two techniques were carried out at a room and negative T = −70°C temperatures. The differences in the structure and deformation behavior of the specimens subjected to different kinds of treatment are revealed and discussed.

  • Strength properties of 17Mn1Si steel welded joints subjected to pulsed mechanical-electrophysical treatment

    by A. S. Smirnova, I. V. Vlasov, R. V. Stankevich, A. V. Yakovlev, Yu. I. Pochivalov, D. V. Valuev, S. V. Panin

    The structure, mechanical properties and deformation behavior of welded joints of 17Mn1Si pipe steel modified by means of surface ultrasonic impact straining and combined pulsed mechanical-electrophysical treatments have been studied. Welded steel plates of 10 mm thickness were used for specimens’ preparation. In doing so, their gauge length comprised of the heat affected zone and directly the weld region. It is shown that the proposed treatment techniques provide hardening of the surface layer, as well as increase in tensile strength. The revealed differences in the structure modification and deformation behavior of the specimens subjected to different treatment methods are illustrated and discussed.

  • The effect of advanced ultrasonic forging on fatigue fracture mechanisms of welded Ti-6A1-4V alloy

    by A. Smirnova, Yu. Pochivalov, V. Panin, S. Panin, A. Eremin, A. Gorbunov

    The current study is devoted to application of advanced postwelding ultrasonic forging to joints formed by laser welding of Ti-6A1-4V alloy in order to enhance their mechanical properties and fatigue durability. Low cycle fatigue tests were performed via digital image correlation technique used to obtain strain fields and in situ characterization of deformation, crack growth and fracture. Fracture surfaces were studied by SEM analysis accompanied with calculation of fracture patterns percentage. The fatigue tests demonstrate the high increase in the number of cycles until fracture (from 17 000 to 32 000 cycles) which could be explained by high ductility of welded material after treatment. This leads to lower fatigue crack growth rate due to higher energy dissipation. The obtained effect is attributable only for small cracks on micro-/mesoscales and fails to play a significant role for macro cracks.


  • The structure and mechanical properties of VT23 laser-welded joints

    by A. S. Smirnova, V. E. Panin, Yu. I. Pochivalov, A. V. Gorbunov, A. G. Malikov, A. M. Orishich

    The structure and mechanical properties of welded joints the of VT23 titanium alloy produced by laser welding with subsequent thermomechanical treatment (TMP1 and TMP2) including ultrasonic mechanical forging are investigated. The results have shown that the fatigue life of welded joints in TMP2 multiply increases compared with the fatigue life of the welded connection samples in the delivery. The structure of a welded joint formed by laser welding has a gradient highly non-equilibrium coarse-grained structure based on the α-phase. The structure with defect density monotonically decreases with the increasing distance from the surface into the material. As follows from the presented data, the fatigue life of the VT23 titanium alloy has increased more than threefold.


  • Strain localization of commercially pure titanium subjected to ultrasonic impact treatment followed by uniaxial tension

    by Alexey Panin, Marina Kazachenok, Anna Kozelskaya, Olga Perevalova, Ruslan Balokhonov, Varvara Romanova, Yurii Pochivalov

    It was demonstrated that the ultrasonic impact treatment results in the gradient microstructure of the surface layer of commercially pure titanium composed of nanosized nonequiaxial α-Ti grains, underlying course α-grains with banded substructure and deformation twins, and subjacent layer characterized by the presence of a few twins and extinction contours within the course grains. The effect of ultrasonic impact treatment on the mechanical behavior of titanium specimen under tension was revealed theoretically and experimentally Using optical and atomic force microscopes it was shown that the fine-grained surface layer impede dislocation motion causing the initiation and propagation of shear bands oriented along the direction of maximum shear stresses. The fine structure of shear bands was studied by transmission electron microscopy.