John Otieno Odhiambo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
John Otieno Odhiambo has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
Akira Otsu
Department of Mechanical and Aerospace Engineering, Tottori University Graduate School of Engineering, Tottori, Japan
1 shared publication- Li-Fu Yi
Department of Mechanical and Aerospace Engineering, Tottori University Graduate School of Engineering, Tottori, Japan
1 shared publication Motoshi Yoshida
Department of Mechanical and Aerospace Engineering, Tottori University Graduate School of Engineering, Tottori, Japan
1 shared publicationTetsuhiko Onda
Department of Mechanical and Aerospace Engineering, Tottori University Graduate School of Engineering, Tottori, Japan
1 shared publication- Zhong-Chun Chen
Department of Mechanical and Aerospace Engineering, Graduate School of Engineering, Tottori University
1 shared publication
Latest Publications
- 30 March 2022
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 56 (13) , 1987-2001
Microstructure and tensile properties of in-situ synthesized and hot-extruded aluminum-matrix composites reinforced with hybrid submicron-sized ceramic particles
Aluminum-matrix composites (AMCs) reinforced with submicron-sized ceramic particles of Al2O3, TiB2 and TiC were in-situ synthesized by reactive sintering of Al, TiO2, and B4C powder mixtures and further densified by hot-extrusion process. The reaction mechanisms for formation of the reinforcing particles, extrusion behavior, microstructure, and tensile properties of the AMCs have been investigated. The reactions of TiO2 and B4C with molten Al were a stepwise process, and there were many intermediate phases including oxygen deficient titanium oxides (Ti3O5, Ti2O3, and TiO), Al4C3, AlB2, and Al3Ti, before the expected reinforcing particles of Al2O3, TiB2, and TiC were formed. The results showed that hot-extrusion process was an effective means to densify reactive-sintered porous composites, and dense AMCs can be obtained through hot-extrusion in a temperature range of 480–550°C. The microstructure of the resulting AMCs was characterized by fine reinforcing ceramic phases with an average particle size of 0.24 μm, which were homogeneously distributed in Al matrix. Furthermore, no significant change in particle sizes could be found after extrusion, and ceramic particle content and extrusion temperature have small influences on the average particle sizes of the reinforcing phases. The presence of these sub-micron hybrid ceramic particles resulted in significant enhancements in yield and tensile strength of the AMCs. The yield strength improvement is mostly due to the coefficient of thermal expansion (CTE) mismatch between the ceramic particles and Al matrix, followed by Orowan strengthening, while the relative contributions of grain refinement and load-bearing effects are much smaller.
- 30 March 2022
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 56 (13) , 1987-2001
Microstructure and tensile properties of in-situ synthesized and hot-extruded aluminum-matrix composites reinforced with hybrid submicron-sized ceramic particles
Aluminum-matrix composites (AMCs) reinforced with submicron-sized ceramic particles of Al2O3, TiB2 and TiC were in-situ synthesized by reactive sintering of Al, TiO2, and B4C powder mixtures and further densified by hot-extrusion process. The reaction mechanisms for formation of the reinforcing particles, extrusion behavior, microstructure, and tensile properties of the AMCs have been investigated. The reactions of TiO2 and B4C with molten Al were a stepwise process, and there were many intermediate phases including oxygen deficient titanium oxides (Ti3O5, Ti2O3, and TiO), Al4C3, AlB2, and Al3Ti, before the expected reinforcing particles of Al2O3, TiB2, and TiC were formed. The results showed that hot-extrusion process was an effective means to densify reactive-sintered porous composites, and dense AMCs can be obtained through hot-extrusion in a temperature range of 480–550°C. The microstructure of the resulting AMCs was characterized by fine reinforcing ceramic phases with an average particle size of 0.24 μm, which were homogeneously distributed in Al matrix. Furthermore, no significant change in particle sizes could be found after extrusion, and ceramic particle content and extrusion temperature have small influences on the average particle sizes of the reinforcing phases. The presence of these sub-micron hybrid ceramic particles resulted in significant enhancements in yield and tensile strength of the AMCs. The yield strength improvement is mostly due to the coefficient of thermal expansion (CTE) mismatch between the ceramic particles and Al matrix, followed by Orowan strengthening, while the relative contributions of grain refinement and load-bearing effects are much smaller.