Michael Malaki
Research Subjects
Michael Malaki has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Andreas Beyer
Faculty of Physics and Materials Science Center, Philipps-Universität Marburg, Hans-Meerwein Str. 6, Marburg, HE, 35037, Germany
3 shared publications - Jean Philippe Beaupain
Fraunhofer Institute for Ceramic Technologies and Systems IKTS, Winterbergstraße 28, 01277 Dresden, Germany
2 shared publications Johannes Haust
Marburg Center for Quantum Materials and Sustainable Technology (mar.quest) and Department of Physics
2 shared publicationsKerstin Volz
Materials Sciences Center (WZMW) and Department of Physics Philipps University of Marburg Hans Meerwein Strasse 6 35032 Marburg Germany
2 shared publications- Anja Henss
Justus Liebig University Giessen Heinrich-Buff-Ring 16
1 shared publication Anuj Pokle
Materials Sciences Center (WZMW) and Department of Physics, Philipps University Marburg, Hans Meerwein Strasse 6, 35032 Marburg, Germany
1 shared publication
Latest Publications
- Open Access
- 16 May 2025
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 37 (11) , 3993-4004
Effect of a Two-Step Temperature-Swing Synthesis on Coarse-Grained LiNiO2 Secondary Particles Characterized by Scanning Transmission Electron Microscopy
To enhance the range of electric vehicles, research is focused on increasing the nickel content in cathode active materials (CAM), which leads to higher practically achievable specific capacities. As a result, the material LiNiO2 (LNO) has attracted significant interest. In this study, a two-step temperature swing synthesis is employed to produce LNO secondary particles with large primary grains as CAM for solid-state batteries (SSBs). The synthesis involves sintering the material at 800 °C for 1 h, followed by an annealing step at a lower temperature for 6 h. Different batches of annealed LNO, using temperatures of 600 and 700 °C, are compared with unannealed LNO, utilizing various transmission electron microscopy (TEM) techniques. The annealing step contributes to smoother particle surfaces, reduced residual lithium species on particle surfaces, and increased lithium occupancy in the crystal lattice, resulting in higher discharge capacity during the initial cycles. However, higher annealing temperatures also lead to the formation of a thin rock-salt layer on the surface and internal misorientation, likely caused by thermal residual stress during cooling. These effects are more pronounced in the sample annealed at 700 °C compared to 600 °C. Despite the potential drawbacks associated with these factors, LNO annealed at 700 °C achieves the highest discharge capacity, indicating that the benefits of annealing outweigh its disadvantages, at least during the initial cycles.
- 16 May 2025
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 37 (11) , 3993-4004
Open AccessEffect of a Two-Step Temperature-Swing Synthesis on Coarse-Grained LiNiO2 Secondary Particles Characterized by Scanning Transmission Electron Microscopy
To enhance the range of electric vehicles, research is focused on increasing the nickel content in cathode active materials (CAM), which leads to higher practically achievable specific capacities. As a result, the material LiNiO2 (LNO) has attracted significant interest. In this study, a two-step temperature swing synthesis is employed to produce LNO secondary particles with large primary grains as CAM for solid-state batteries (SSBs). The synthesis involves sintering the material at 800 °C for 1 h, followed by an annealing step at a lower temperature for 6 h. Different batches of annealed LNO, using temperatures of 600 and 700 °C, are compared with unannealed LNO, utilizing various transmission electron microscopy (TEM) techniques. The annealing step contributes to smoother particle surfaces, reduced residual lithium species on particle surfaces, and increased lithium occupancy in the crystal lattice, resulting in higher discharge capacity during the initial cycles. However, higher annealing temperatures also lead to the formation of a thin rock-salt layer on the surface and internal misorientation, likely caused by thermal residual stress during cooling. These effects are more pronounced in the sample annealed at 700 °C compared to 600 °C. Despite the potential drawbacks associated with these factors, LNO annealed at 700 °C achieves the highest discharge capacity, indicating that the benefits of annealing outweigh its disadvantages, at least during the initial cycles.
- Open Access
- 22 September 2023
- Published by Wiley in Advanced Materials Interfaces
- Vol. 10 (35)
Probing the Interface Evolution in Co‐sintered All‐Phosphate Cathode‐Solid Electrolyte Composites
To achieve cohesive interfaces of solid components in next‐generation Li‐ion batteries (LIBs) composed of oxide cathodes and solid electrolytes (SEs) high‐temperature sintering is necessary which leads to material degradation and phase decompositions. Thermochemically compatible components can address these issues. In this work, advanced electron microscopy techniques are employed to investigate the structural and chemical evolution taking place at the interfaces between a LiFePO4 (LFP) cathode and an in‐house optimized Li1.3Al0.3Ti1.7(PO4)3 (LATP) SE co‐sintered between 650 °C – 850 °C. While the LFP particles exhibit excellent structural stability, the LATP particles phase transforms at elevated temperatures. At 650 °C, FeLi anti‐site defect is observed at the LFP grain boundaries. Between 750 and 850 °C, the LATP (R‐3c) transforms into two orthorhombic phases (Pbca and Pbcn) of the type Li1.3+xAl0.3FexTi1.7‐x(PO4)3 depending on Fe substitution while forming the cohesive interfaces. The discharge capacity of the composite decreases from 148 mAh g−1 at 650 °C to 130 mAh g‐1 at 850 °C confirming that the new phases are still electrochemically active. This study provides a spatially resolved insight into the formation of cohesive interfaces highlighting the advantage of employing components with similar anionic structures for further improvements in LIBs.
- 22 September 2023
- Published by Wiley in Advanced Materials Interfaces
- Vol. 10 (35)
Open AccessProbing the Interface Evolution in Co‐sintered All‐Phosphate Cathode‐Solid Electrolyte Composites
To achieve cohesive interfaces of solid components in next‐generation Li‐ion batteries (LIBs) composed of oxide cathodes and solid electrolytes (SEs) high‐temperature sintering is necessary which leads to material degradation and phase decompositions. Thermochemically compatible components can address these issues. In this work, advanced electron microscopy techniques are employed to investigate the structural and chemical evolution taking place at the interfaces between a LiFePO4 (LFP) cathode and an in‐house optimized Li1.3Al0.3Ti1.7(PO4)3 (LATP) SE co‐sintered between 650 °C – 850 °C. While the LFP particles exhibit excellent structural stability, the LATP particles phase transforms at elevated temperatures. At 650 °C, FeLi anti‐site defect is observed at the LFP grain boundaries. Between 750 and 850 °C, the LATP (R‐3c) transforms into two orthorhombic phases (Pbca and Pbcn) of the type Li1.3+xAl0.3FexTi1.7‐x(PO4)3 depending on Fe substitution while forming the cohesive interfaces. The discharge capacity of the composite decreases from 148 mAh g−1 at 650 °C to 130 mAh g‐1 at 850 °C confirming that the new phases are still electrochemically active. This study provides a spatially resolved insight into the formation of cohesive interfaces highlighting the advantage of employing components with similar anionic structures for further improvements in LIBs.
- 11 April 2022
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 5 (4) , 4651-4663
Advanced Analytical Characterization of Interface Degradation in Ni-Rich NCM Cathode Co-Sintered with LATP Solid Electrolyte
- 11 April 2022
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 5 (4) , 4651-4663
Advanced Analytical Characterization of Interface Degradation in Ni-Rich NCM Cathode Co-Sintered with LATP Solid Electrolyte