    Hydrogen-Induced Cracking Susceptibility of API 5L X100 Steel Welded Joint

    by Chunyan Yan, Lingchuan Zhou, Qianwen Zhou, Tiancheng Yao, Xinyi Liu, Qiqing Lu

    Hydrogen-induced cracking (HIC) is a possible failure mode of high-strength pipeline steel welded joints. The HIC susceptibility of shielded metal arc-welded joint of X100 pipeline steel was investigated using the slow strain rate tensile test (SSRT) under current densities of 2 mA/cm2, 5 mA/cm2, 10 mA/cm2, 20 mA/cm2, and 30 mA/cm2. Hydrogen diffusion behavior, distribution of microstructures, and inclusions in the welded joint were also surveyed and characterized. The SSRT results indicated that the welded joint exhibited a higher hydrogen embrittlement index than the base metal (BM) under the same current density, showing a higher HIC sensitivity than the BM. The weld metal (WM) showed a lower hydrogen diffusivity (5.38 × 10−5 cm2·s−1) than the BM (6.23 × 10−5 cm2·s−1). The martensite–austenite (M-A) constituent area fraction in the WM was higher than that in the coarse-grained heat-affected zone (CGHAZ), fine-grained HAZ (FGHAZ), and BM. The inclusion amount in the WM was larger than that in the BM. In addition, the high HIC vulnerability of the X100 steel welded joint was also associated with a coarse grain size in the WM.

  • Open Access

    Effect of Quenching Temperature on Microstructure and Hydrogen-Induced Cracking Susceptibility in S355 Steel

    by Chunyan Yan, Shenglin Zhang, Lingchuan Zhou, Zhanpeng Tian, Mengdie Shen, Xinyi Liu

    S355 steels are widely used in various applications. However, they may be affected by hydrogen, which can induce hydrogen-induced cracking (HIC). The effects of the quenching temperature (Twq) on the microstructure variation and HIC susceptibility of S355 steel was investigated by microstructural characterization, hydrogen permeation (HP) test, slow strain rate tensile (SSRT) test, hydrogen microprint technique (HMT) test, and hydrogen-charged cracking test. The results indicate that the microstructure of the treated specimens consisted of predominantly lath martensite (LM) and small amounts of lath bainite (LB) for the Twq of 950 °C and 1000 °C, while the microstructure of the treated specimens mainly consisted of LM for the Twq of 1050 °C and 1100 °C. The results indicate that as the Twq increased, the sample treated at 950 °C exhibited a minimum hydrogen embrittlement index (Iz), while the sample treated at 1050 °C exhibited the maximum Iz. The hydrogen diffusion coefficient was relatively low, while the hydrogen concentration and trap density were relatively high for the Twq of 1050 °C. The lath interfaces in martensite were effective hydrogen traps with high hydrogen-trapping efficiency. Hydrogen-induced cracks were significantly affected by hydrogen trapping at martensitic lath interfaces, exhibiting a basically transgranular fracture.


  • Open Access

    Research on Hydrogen-Induced Induced Cracking Sensitivity of X80 Pipeline Steel under Different Heat Treatments

    by Chen Wu, Chunyan Yan, Shenglin Zhang, Lingchuan Zhou, Mengdie Shen, Zhanpeng Tian

    X80 pipeline steel has played a vital role in oil and gas transportation in recent years. However, hydrogen-related issues frequently lead to pipeline failures during service, resulting in significant losses of properties and lives. Three heat treatment processes (furnace cooling (FC), air cooling (AC), and water cooling (WC)) were carried out to investigate the effect of different microstructures on hydrogen-induced cracking (HIC) susceptibility of X80 pipeline steel. The WC sample demonstrated the highest hydrogen embrittlement index, registering at 21.9%, while the AC and FC samples exhibited progressively lower values of 15.45% and 10.98%, respectively. Under equivalent hydrogen charging durations, crack dimensions with a maximum length exceeding 30 μm in the WC sample generally exceed those in the FC sample and AC sample. The variation is attributed to the difference in microstructures of the samples, predominantly lath bainite (LB) in water-cooled samples, granular bainite (GB) in air-cooled samples, and ferrite/pearlite (F/P) in FC samples. The research results demonstrate that the sensitivity of lath bainite (LB) to HIC is significantly higher than that of pearlite, ferrite, and granular bainite (GB). The presence of a large amount of martensite/austenite (M/A) constituents within bainite results in a multitude of hydrogen trap sites. HIC cracks in bainite generally propagate along the profiles of M/A constituents, showing both intergranular and transgranular cracking modes.


  • Open Access

    Weld Formation, Microstructure Evolution and Mechanical Property of Laser-Arc Hybrid Welded AZ31B Magnesium Alloy

    by Sibo Wang, Chunyan Yan, Zhengjia Gu

    Laser-arc hybrid welding of AZ31B magnesium alloy was carried out in this paper, and the effects of welding parameters (laser power, welding speed, welding current) on weld formation, microstructure evolution and mechanical property were studied. The results showed that laser-arc hybrid welding can inhibit the undercut defect during laser welding on the one hand, and enhance the arc stability on the other hand. The penetration depth and width showed no significant relation with the total heat input, but were linear related to the laser heat input and the arc heat input, respectively. The average grain size of the equiaxed grains was closely related to the heat input. The higher the heat input was, the larger the grains. The optimized welding parameters were laser power of 3.5 kW, welding speed of 1.8 m/min and welding current of 100 A. In this case, the weld was free of undercut and pores, and the tensile strength and elongation rate reached 190 MPa and 12%, respectively.