Yanfang Qin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yanfang Qin has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Jining He
Tianjin Key Laboratory of Materials Laminating Fabrication and Interface Control Technology, School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China
3 shared publications - Hongjian Zhao
Hebei Key Laboratory of New Functional Materials, School of Materials Science and Engineering, Hebei University of Technology, Tianjin, China
2 shared publications - Jiawei Fan
Key Lab for New Type of Functional Materials in Hebei Province, School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China
2 shared publications - Baoqiang Li
Key Lab for New Type of Functional Materials in Hebei Province, School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China
1 shared publication - Guanya Fu
Key Lab for New Type of Functional Materials in Hebei Province, School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China
1 shared publication - Hongjian Zhao
Tianjin Key Laboratory of Materials Laminating Fabrication and Interface Control Technology, School of Materials Science and Engineering, Hebei University of Technology, Tianjin, China
1 shared publication
Latest Publications
- Open Access
Oxidation and Heat Shock Resistance of Plasma-Sprayed TiC-CoNi Composite Coatings at 900 °C
In this work, the TiC-reinforced CoNi alloy coatings were prepared by the plasma spraying method. Their microstructure, high-temperature oxidation, and thermal shock resistance at 900 °C were studied. The results showed that the CoNi alloy coating exhibited a single phase (c-Co-Ni-Cr-Mo). After adding Ti-graphite mixed powders, the sprayed coating exhibited TiC and TiO2 phases, besides the c-Co-Ni-Cr-Mo matrix phase. For CoNi alloy coating, the main oxidation products were Cr2O3 and CoCr2O4 (NiCr2O4). For TiC-CoNi alloy coating, the main oxidation products were the TiO2 phase, coupled with Cr2O3 and CoCr2O4 (NiCr2O4) phases. The content of oxides increased with the oxidation time. The oxidation weight gain of the TiC-CoNi composite coating was slightly higher than that of the CoNi alloy coating. The formation of TiC could improve the thermal shock resistance of the CoNi alloy coating.
Open AccessOxidation and Heat Shock Resistance of Plasma-Sprayed TiC-CoNi Composite Coatings at 900 °C
In this work, the TiC-reinforced CoNi alloy coatings were prepared by the plasma spraying method. Their microstructure, high-temperature oxidation, and thermal shock resistance at 900 °C were studied. The results showed that the CoNi alloy coating exhibited a single phase (c-Co-Ni-Cr-Mo). After adding Ti-graphite mixed powders, the sprayed coating exhibited TiC and TiO2 phases, besides the c-Co-Ni-Cr-Mo matrix phase. For CoNi alloy coating, the main oxidation products were Cr2O3 and CoCr2O4 (NiCr2O4). For TiC-CoNi alloy coating, the main oxidation products were the TiO2 phase, coupled with Cr2O3 and CoCr2O4 (NiCr2O4) phases. The content of oxides increased with the oxidation time. The oxidation weight gain of the TiC-CoNi composite coating was slightly higher than that of the CoNi alloy coating. The formation of TiC could improve the thermal shock resistance of the CoNi alloy coating.
- Open Access
High-Temperature Heat Treatment of Plasma Sprayed Ti–Si–C–Mo Coatings
In this work, the effect of 800 °C and 1100 °C post-heat treatment on the plasma spraying of Ti–Si–C–xMo (x = 1.0, 1.5) composite coatings was investigated. The composite coatings were composed of TiC, Ti3SiC2, Ti5Si3 and Mo5Si3 reacted phases. After heat treatment, the Ti3SiC2 and Mo5Si3 phases increased. The coating microhardness decreased by 16% and 18% for Ti–Si–C–1.0Mo and Ti–Si–C–1.5Mo coatings, respectively, after heat treatment at 1100 °C. Fracture toughness increased by 16% for the Ti–Si–C–1.5Mo coating after heat treatment at 1100 °C, which was mainly due to the heat treatment promoting Ti3SiC2 formation, healing micro-cracks, reducing the internal stress and making the microstructure dense. The coating friction coefficient before and after heat -treatment was between 0.4 and 0.6. After heat treatment, the wear amount of the coating was first reduced and then increased, and the minimum wear loss occurred after heat treatment at 800 °C. The wear mechanism was mixed abrasive wear, adhesive wear and tribo-oxidation wear.
Open AccessHigh-Temperature Heat Treatment of Plasma Sprayed Ti–Si–C–Mo Coatings
In this work, the effect of 800 °C and 1100 °C post-heat treatment on the plasma spraying of Ti–Si–C–xMo (x = 1.0, 1.5) composite coatings was investigated. The composite coatings were composed of TiC, Ti3SiC2, Ti5Si3 and Mo5Si3 reacted phases. After heat treatment, the Ti3SiC2 and Mo5Si3 phases increased. The coating microhardness decreased by 16% and 18% for Ti–Si–C–1.0Mo and Ti–Si–C–1.5Mo coatings, respectively, after heat treatment at 1100 °C. Fracture toughness increased by 16% for the Ti–Si–C–1.5Mo coating after heat treatment at 1100 °C, which was mainly due to the heat treatment promoting Ti3SiC2 formation, healing micro-cracks, reducing the internal stress and making the microstructure dense. The coating friction coefficient before and after heat -treatment was between 0.4 and 0.6. After heat treatment, the wear amount of the coating was first reduced and then increased, and the minimum wear loss occurred after heat treatment at 800 °C. The wear mechanism was mixed abrasive wear, adhesive wear and tribo-oxidation wear.
- 25 August 2022
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 31 (8) , 2280-2299
A Review of TiCN Coating Prepared by Reaction Plasma Spraying
- 25 August 2022
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 31 (8) , 2280-2299
A Review of TiCN Coating Prepared by Reaction Plasma Spraying