Ramandeep Mandia
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ramandeep Mandia has a total of 29 co-authors. Here are the top co-authors by number of shared publications:
- David J. Smith
Department of Physics, Arizona State University 2 , Tempe, Arizona 85287
3 shared publications - Arpit Nandi
Center for Device Thermography and Reliability, University of Bristol, Bristol BS8 1TL, UK
2 shared publications - David Cherns
HH Wills Physics Laboratory
2 shared publications Kelly Woo
2 shared publications- Martin Kuball
University of Bristol
2 shared publications Mohamadali Malakoutian
2 shared publications
Latest Publications
- 19 November 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 43 (6)
Material and electrical characterization of ultrawide bandgap BN/AlN metal-insulator-semiconductor (MIS) Schottky diodes
Devices based on ultrawide bandgap heterostructures are attracting increased attention for applications that require high fields or high-temperature environments. In this article, we demonstrate an ultrawide bandgap BN/AlN metal-insulator-semiconductor Schottky diode on single-crystal AlN substrates, where the AlN epilayers were grown via metalorganic chemical vapor deposition, and the BN layer was deposited using microwave plasma chemical vapor deposition. The BN/AlN heterostructure was characterized by x-ray photoelectron spectroscopy, transmission electron microscopy, and electron-energy-loss spectroscopy. Capacitance-frequency measurements indicated a low interface state density of 0.67–3.55 × 1011 eV−1 cm−2 at the BN/AlN interface. At forward bias, the device showed good rectifying behavior. At reverse bias, 2D variable range hopping and trap-assisted tunneling were found to be the dominant mechanisms. This work provides valuable guidance for developing ultrawide bandgap nitride heterostructures.
- 19 November 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 43 (6)
Material and electrical characterization of ultrawide bandgap BN/AlN metal-insulator-semiconductor (MIS) Schottky diodes
Devices based on ultrawide bandgap heterostructures are attracting increased attention for applications that require high fields or high-temperature environments. In this article, we demonstrate an ultrawide bandgap BN/AlN metal-insulator-semiconductor Schottky diode on single-crystal AlN substrates, where the AlN epilayers were grown via metalorganic chemical vapor deposition, and the BN layer was deposited using microwave plasma chemical vapor deposition. The BN/AlN heterostructure was characterized by x-ray photoelectron spectroscopy, transmission electron microscopy, and electron-energy-loss spectroscopy. Capacitance-frequency measurements indicated a low interface state density of 0.67–3.55 × 1011 eV−1 cm−2 at the BN/AlN interface. At forward bias, the device showed good rectifying behavior. At reverse bias, 2D variable range hopping and trap-assisted tunneling were found to be the dominant mechanisms. This work provides valuable guidance for developing ultrawide bandgap nitride heterostructures.
- 10 October 2025
- Published by International Union of Crystallography (IUCr) in Journal of Applied Crystallography
- Vol. 58 (6) , 1936-1946
(Pseudo-)symmetry-driven coherent interfaces and texture in epitaxial β-Ga 2 O 3 thin films on (001) diamond
Epitaxial β-Ga 2 O 3 films grown on (001) diamond substrates with a β-(Al/Ga) 2 O 3 buffer layer exhibit strong texture with multiple rotational domain variants sharing a common growth axis. This texture is attributed to two interrelated structural and geometrical factors: (1) pseudo-symmetry about the growth direction due to the high symmetry of the oxygen sublattice which results in close interplanar spacings of different lattice planes that determine the in-plane lattice mismatch, and hence two different crystallographic relationships and types of domain variants; (2) the lack of higher-order symmetry in the C 2/ m monoclinic structure of β-Ga 2 O 3 and the higher symmetry of the diamond substrate that leads to various subvariants. The microstructure of the films consists predominantly of domain clusters, with domains rotated by either ∼60° or 120° (±10°) relative to each other about the growth axis ∼[ 1 02]. Some domain boundaries (DBs), visible near edge-on in cross-sectional and plan-view projections, exhibit a high degree of coherency. These highly coherent DBs with small lattice rotation and/or distortion near the DB are observed where small in-plane and off-plane DB lattice mismatch is expected. Larger lattice mismatch between domains is accommodated by relatively large lattice rotation and/or distortion near the DB, as well as changes in DB structure and shape. Understanding the origin of texture and the characteristics of common planar defects in β-Ga 2 O 3 will offer insights into their impact on thermal and electrical transport properties and enable effective microstructural optimization for successful integration into future power electronics.
- 10 October 2025
- Published by International Union of Crystallography (IUCr) in Journal of Applied Crystallography
- Vol. 58 (6) , 1936-1946
(Pseudo-)symmetry-driven coherent interfaces and texture in epitaxial β-Ga 2 O 3 thin films on (001) diamond
Epitaxial β-Ga 2 O 3 films grown on (001) diamond substrates with a β-(Al/Ga) 2 O 3 buffer layer exhibit strong texture with multiple rotational domain variants sharing a common growth axis. This texture is attributed to two interrelated structural and geometrical factors: (1) pseudo-symmetry about the growth direction due to the high symmetry of the oxygen sublattice which results in close interplanar spacings of different lattice planes that determine the in-plane lattice mismatch, and hence two different crystallographic relationships and types of domain variants; (2) the lack of higher-order symmetry in the C 2/ m monoclinic structure of β-Ga 2 O 3 and the higher symmetry of the diamond substrate that leads to various subvariants. The microstructure of the films consists predominantly of domain clusters, with domains rotated by either ∼60° or 120° (±10°) relative to each other about the growth axis ∼[ 1 02]. Some domain boundaries (DBs), visible near edge-on in cross-sectional and plan-view projections, exhibit a high degree of coherency. These highly coherent DBs with small lattice rotation and/or distortion near the DB are observed where small in-plane and off-plane DB lattice mismatch is expected. Larger lattice mismatch between domains is accommodated by relatively large lattice rotation and/or distortion near the DB, as well as changes in DB structure and shape. Understanding the origin of texture and the characteristics of common planar defects in β-Ga 2 O 3 will offer insights into their impact on thermal and electrical transport properties and enable effective microstructural optimization for successful integration into future power electronics.
- Open Access
- 1 July 2025
- Published by AIP Publishing in APL Materials
- Vol. 13 (7)
Adherent β-Ga2O3 thin films on single crystal diamond (001) substrates enabled by (AlxGa1−x)2O3 buffer layers
Diamond is an attractive substrate choice for the growth of gallium oxide for high-power device applications due to its high thermal conductivity. However, the cubic crystal structure of diamond is very different from that of monoclinic β-Ga2O3. Adding to the complexity, there is a large surface energy difference between the two materials, and a high-temperature oxide environment is required for Ga2O3 growth. Here, we demonstrate a viable pathway that enables thick adherent Ga2O3 layers to be grown epitaxially on diamond (001) substrates, using metal–organic chemical vapor deposition. This growth is achieved using an intermediary (Al0.06Ga0.94)2O3 (AGO6) buffer layer. Omission of the strain management buffer results in Ga2O3 films that exfoliate into membranes for thicknesses greater than about 500 nm. Implementation of the buffer layer allows for the alleviation of the excess strain energy developed within the grown film and assists in improving film quality, increasing grain size, reducing dislocations, and providing epitaxially textured thin films relative to layers without the buffer. Adherent 750-nm-thick β-Ga2O3 epitaxial layers have been achieved using the AGO6 buffer, with a full-width at half-maximum of 1.36° and a root-mean-square roughness of 6.24 nm. The thermal conductivity of the β-Ga2O3 thin films with and without the AGO6 buffer was measured to be 6.0–6.5 W/mK. Thus, integration of the monoclinic gallium oxide with the diamond cubic substrate using the intermediary buffer layer improves the crystal quality but does not impact the thermal conductivity, suggesting the future feasibility of using diamond substrates for a wide range of Ga2O3 device applications.
- 1 July 2025
- Published by AIP Publishing in APL Materials
- Vol. 13 (7)
Open AccessAdherent β-Ga2O3 thin films on single crystal diamond (001) substrates enabled by (AlxGa1−x)2O3 buffer layers
Diamond is an attractive substrate choice for the growth of gallium oxide for high-power device applications due to its high thermal conductivity. However, the cubic crystal structure of diamond is very different from that of monoclinic β-Ga2O3. Adding to the complexity, there is a large surface energy difference between the two materials, and a high-temperature oxide environment is required for Ga2O3 growth. Here, we demonstrate a viable pathway that enables thick adherent Ga2O3 layers to be grown epitaxially on diamond (001) substrates, using metal–organic chemical vapor deposition. This growth is achieved using an intermediary (Al0.06Ga0.94)2O3 (AGO6) buffer layer. Omission of the strain management buffer results in Ga2O3 films that exfoliate into membranes for thicknesses greater than about 500 nm. Implementation of the buffer layer allows for the alleviation of the excess strain energy developed within the grown film and assists in improving film quality, increasing grain size, reducing dislocations, and providing epitaxially textured thin films relative to layers without the buffer. Adherent 750-nm-thick β-Ga2O3 epitaxial layers have been achieved using the AGO6 buffer, with a full-width at half-maximum of 1.36° and a root-mean-square roughness of 6.24 nm. The thermal conductivity of the β-Ga2O3 thin films with and without the AGO6 buffer was measured to be 6.0–6.5 W/mK. Thus, integration of the monoclinic gallium oxide with the diamond cubic substrate using the intermediary buffer layer improves the crystal quality but does not impact the thermal conductivity, suggesting the future feasibility of using diamond substrates for a wide range of Ga2O3 device applications.
- 7 April 2025
- Published by Elsevier in Acta Materialia
- Vol. 292
Structural and chemical transitions in diamond/dielectric/Si heterostructures
- 7 April 2025
- Published by Elsevier in Acta Materialia
- Vol. 292
Structural and chemical transitions in diamond/dielectric/Si heterostructures
- Open Access
- 24 July 2024
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 30 (Supplement)
Understanding Interface Transitions in Polycrystalline Diamond/Dielectric Interlayer/Si Heterostructures Using STEM-EELS
Polycrystalline (PC) diamond films grown on semiconductor devices that are prone to premature failure due to self-heating have recently shown great improvement in channel/junction temperature reduction without compromising the device electrical performance [ 1]. The enhanced heat transfer coefficient to the heat sink is attributed to the exceptionally low thermal boundary resistance (TBR) of the interface and the very high thermal conductivity (TC) of PC diamond [ 2-4]. In this study, we have characterized diamond nucleation and growth on Si with several different dielectric interlayers, with the goal of maximizing the phonon transport by improving the quality and adhesion of the as-grown diamond layers [ 2]. Samples for cross-sectional TEM study were prepared using a Thermo Fisher Helios 5UX Dualbeam system, often followed by a final argon-ion-milling with a Gatan PIPS-II. The cross-sectional geometry and interface abruptness of these heterostructures were analyzed with an FEI-Philips CM 200 at 200 kV and a Talos L120C at 120 kV, and chemical composition was measured using scanning transmission electron microscope (STEM) imaging and electron-energy-loss spectroscopy (EELS) with a JEOL ARM200F operated at 200kV. Phase-contrast imaging was used to provide information about the preferred growth directions of the PC-diamond grains, while STEM-EELS was employed to assess the interfacial chemical non-abruptness.
- 24 July 2024
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 30 (Supplement)
Open AccessUnderstanding Interface Transitions in Polycrystalline Diamond/Dielectric Interlayer/Si Heterostructures Using STEM-EELS
Polycrystalline (PC) diamond films grown on semiconductor devices that are prone to premature failure due to self-heating have recently shown great improvement in channel/junction temperature reduction without compromising the device electrical performance [ 1]. The enhanced heat transfer coefficient to the heat sink is attributed to the exceptionally low thermal boundary resistance (TBR) of the interface and the very high thermal conductivity (TC) of PC diamond [ 2-4]. In this study, we have characterized diamond nucleation and growth on Si with several different dielectric interlayers, with the goal of maximizing the phonon transport by improving the quality and adhesion of the as-grown diamond layers [ 2]. Samples for cross-sectional TEM study were prepared using a Thermo Fisher Helios 5UX Dualbeam system, often followed by a final argon-ion-milling with a Gatan PIPS-II. The cross-sectional geometry and interface abruptness of these heterostructures were analyzed with an FEI-Philips CM 200 at 200 kV and a Talos L120C at 120 kV, and chemical composition was measured using scanning transmission electron microscope (STEM) imaging and electron-energy-loss spectroscopy (EELS) with a JEOL ARM200F operated at 200kV. Phase-contrast imaging was used to provide information about the preferred growth directions of the PC-diamond grains, while STEM-EELS was employed to assess the interfacial chemical non-abruptness.
- 5 May 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (9) , 5843-5852
Energetics and structure of the B‐type solid solution in the Nd 2 O 3 –Y 2 O 3 system
The system Nd 2 O 3 –Y 2 O 3 contains solid‐solution phases with several different structures. Single‐phase B‐type (Nd 1− x Y x ) 2 O 3 solid solutions in the range of were formed at 1873 K and retained on cooling to ambient temperature. They showed a linear composition dependence of lattice parameters, enabling extrapolation to x = 0 and 1 for comparison with the structures of the stable endmembers. A positive enthalpy of formation from A‐type Nd 2 O 3 and C‐type Y 2 O 3 determined using oxide melt solution calorimetry indicated entropic stabilization of the B‐type phase. A positive interaction parameter for mixing in the B‐type solid solution, Ω 47.46 ± 4.04 kJ/mol, was obtained by fitting the data using a regular solution model. This value is significantly more positive than that obtained by previous phase diagram analysis using the CalPhaD approach. Exsolution into two B‐type phases is predicted to occur below 1427 K, making it unimportant for the equilibrium phase relations that will be dominated by other structures at low temperature.
- 5 May 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (9) , 5843-5852
Energetics and structure of the B‐type solid solution in the Nd 2 O 3 –Y 2 O 3 system
The system Nd 2 O 3 –Y 2 O 3 contains solid‐solution phases with several different structures. Single‐phase B‐type (Nd 1− x Y x ) 2 O 3 solid solutions in the range of were formed at 1873 K and retained on cooling to ambient temperature. They showed a linear composition dependence of lattice parameters, enabling extrapolation to x = 0 and 1 for comparison with the structures of the stable endmembers. A positive enthalpy of formation from A‐type Nd 2 O 3 and C‐type Y 2 O 3 determined using oxide melt solution calorimetry indicated entropic stabilization of the B‐type phase. A positive interaction parameter for mixing in the B‐type solid solution, Ω 47.46 ± 4.04 kJ/mol, was obtained by fitting the data using a regular solution model. This value is significantly more positive than that obtained by previous phase diagram analysis using the CalPhaD approach. Exsolution into two B‐type phases is predicted to occur below 1427 K, making it unimportant for the equilibrium phase relations that will be dominated by other structures at low temperature.
- Open Access
Texture Selection Mechanisms during Recrystallization and Grain Growth of a Magnesium-Erbium-Zinc Alloy
Binary and ternary Mg-1%Er/Mg-1%Er-1%Zn alloys were rolled and subsequently subjected to various heat treatments to study texture selection during recrystallization and following grain growth. The results revealed favorable texture alterations in both alloys and the formation of a unique ±40° transvers direction (TD) recrystallization texture in the ternary alloy. While the binary alloy underwent a continuous alteration of its texture and grain size throughout recrystallization and grain growth, the ternary alloy showed a rapid rolling (RD) to transvers direction (TD) texture transition occurring during early stages of recrystallization. Targeted electron back scatter diffraction (EBSD) analysis of the recrystallized fraction unraveled a selective growth behavior of recrystallization nuclei with TD tilted orientations that is likely attributed to solute drag effect on the mobility of specific grain boundaries. Mg-1%Er-1%Zn additionally exhibited a stunning microstructural stability during grain growth annealing. This was attributed to a fine dispersion of dense nanosized particles in the matrix that impeded grain growth by Zener drag. The mechanical properties of both alloys were determined by uniaxial tensile tests combined with EBSD assisted slip trace analysis at 5% tensile strain to investigate non-basal slip behavior. Owing to synergic alloying effects on solid solution strengthening and slip activation, as well as precipitation hardening, the ternary Mg-1%Er-1%Zn alloy demonstrated a remarkable enhancement in the yield strength, strain hardening capability, and failure ductility, compared with the Mg-1%Er alloy.
Open AccessTexture Selection Mechanisms during Recrystallization and Grain Growth of a Magnesium-Erbium-Zinc Alloy
Binary and ternary Mg-1%Er/Mg-1%Er-1%Zn alloys were rolled and subsequently subjected to various heat treatments to study texture selection during recrystallization and following grain growth. The results revealed favorable texture alterations in both alloys and the formation of a unique ±40° transvers direction (TD) recrystallization texture in the ternary alloy. While the binary alloy underwent a continuous alteration of its texture and grain size throughout recrystallization and grain growth, the ternary alloy showed a rapid rolling (RD) to transvers direction (TD) texture transition occurring during early stages of recrystallization. Targeted electron back scatter diffraction (EBSD) analysis of the recrystallized fraction unraveled a selective growth behavior of recrystallization nuclei with TD tilted orientations that is likely attributed to solute drag effect on the mobility of specific grain boundaries. Mg-1%Er-1%Zn additionally exhibited a stunning microstructural stability during grain growth annealing. This was attributed to a fine dispersion of dense nanosized particles in the matrix that impeded grain growth by Zener drag. The mechanical properties of both alloys were determined by uniaxial tensile tests combined with EBSD assisted slip trace analysis at 5% tensile strain to investigate non-basal slip behavior. Owing to synergic alloying effects on solid solution strengthening and slip activation, as well as precipitation hardening, the ternary Mg-1%Er-1%Zn alloy demonstrated a remarkable enhancement in the yield strength, strain hardening capability, and failure ductility, compared with the Mg-1%Er alloy.