Young-Ho Kim
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Young-Ho Kim has a total of 103 co-authors. Here are the top co-authors by number of shared publications:
Jae-Yong Park
7 shared publicationsDong Joo Choi
Division of Materials Science & Engineering, Hanyang University, Seoul, Korea
6 shared publicationsKey-One Ahn
Department of Materials Science and Engineering, Hanyang University, 04763, Korea
5 shared publicationsSun-Chul Kim
Division of Materials Science & Engineering, Hanyang University, Seoul, Korea
5 shared publicationsSung Woo Ma
5 shared publicationsWonil Seo
Joining R&D Group, Korea Institute of Industrial Technology, Incheon, Republic of Korea
5 shared publications
Latest Publications
- 27 March 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (14) , 11002-11016
Microstructure and shear strength of Au-20wt%Sn solder joints fabricated by thermo-compression bonding for LED packages
- 27 March 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (14) , 11002-11016
Microstructure and shear strength of Au-20wt%Sn solder joints fabricated by thermo-compression bonding for LED packages
- 1 May 2021
- Published by American Scientific Publishers in Journal of Nanoelectronics and Optoelectronics
- Vol. 16 (5) , 723-730
Electromagnetic Interference Shielding from the Back-Side Metallization of the Chip in Fan-Out Wafer Level Package
Shielding against electromagnetic interference (EMI) is becoming increasingly important as electronics such as wearable devices, sensors, IoT, and smartphones become smaller, faster, and weigh less. Package level EMI shielding has several advantages over board level shielding, such as a higher packaging density and better design flexibility. We developed a new fan-out package structure using back-side under bump metallurgy (UBM) and a substrate (or metal carrier) to improve the thermal characteristics and reduce die shift. UBM and the substrate (or metal carrier), which consisted of highly conductive metals, is effective for EMI shielding. We study EMI shielding effects of UBM and the substrate (or metal carrier). To determine the EMI shielding of the UBM structures, Ti (17 nm thick) and Cu (70 nm thick) were sequentially deposited on a glass substrate using a direct-current (DC) magnetron sputtering system. Then Cu was electroplated or Ni-P was electroless plated with various thicknesses up to 10 µm. Samples were measured under 100 MHz and 1 GHz with 0 dB conditions using a spectra analyzer, which is a near-field measurement equipment. In unpatterened UBM, increase in the Cu or Ni thickness resulted in further enhanced EMI shielding. When the thickness of Cu UBM or Ni-P UBM was bigger than 5 µm or 3 µm, respectively, the UBM exhibited good EMI shielding. A double layer of Cu strips was formed on the back side of the chip to enhance EMI shielding. The larger the overlap between the Cu strip and the upper and lower layers, the better the EMI shielding effect. When this overlap was larger than 0.5 mm, the EMI SE was similar to that of a single unpatterned Cu layer. We demonstrated good EMI shielding in the double-layered structure with a large overlap width between the upper and lower Cu strips, and expect better moisture release in such structures.
- 1 May 2021
- Published by American Scientific Publishers in Journal of Nanoelectronics and Optoelectronics
- Vol. 16 (5) , 723-730
Electromagnetic Interference Shielding from the Back-Side Metallization of the Chip in Fan-Out Wafer Level Package
Shielding against electromagnetic interference (EMI) is becoming increasingly important as electronics such as wearable devices, sensors, IoT, and smartphones become smaller, faster, and weigh less. Package level EMI shielding has several advantages over board level shielding, such as a higher packaging density and better design flexibility. We developed a new fan-out package structure using back-side under bump metallurgy (UBM) and a substrate (or metal carrier) to improve the thermal characteristics and reduce die shift. UBM and the substrate (or metal carrier), which consisted of highly conductive metals, is effective for EMI shielding. We study EMI shielding effects of UBM and the substrate (or metal carrier). To determine the EMI shielding of the UBM structures, Ti (17 nm thick) and Cu (70 nm thick) were sequentially deposited on a glass substrate using a direct-current (DC) magnetron sputtering system. Then Cu was electroplated or Ni-P was electroless plated with various thicknesses up to 10 µm. Samples were measured under 100 MHz and 1 GHz with 0 dB conditions using a spectra analyzer, which is a near-field measurement equipment. In unpatterened UBM, increase in the Cu or Ni thickness resulted in further enhanced EMI shielding. When the thickness of Cu UBM or Ni-P UBM was bigger than 5 µm or 3 µm, respectively, the UBM exhibited good EMI shielding. A double layer of Cu strips was formed on the back side of the chip to enhance EMI shielding. The larger the overlap between the Cu strip and the upper and lower layers, the better the EMI shielding effect. When this overlap was larger than 0.5 mm, the EMI SE was similar to that of a single unpatterned Cu layer. We demonstrated good EMI shielding in the double-layered structure with a large overlap width between the upper and lower Cu strips, and expect better moisture release in such structures.
- 20 November 2020
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (1) , 1042-1051
Growth of intermetallic compounds and brittle fracture behavior of Sn-Ag-Cu/ENIG joint with columnar Ni-P layer
- 20 November 2020
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (1) , 1042-1051
Growth of intermetallic compounds and brittle fracture behavior of Sn-Ag-Cu/ENIG joint with columnar Ni-P layer
- 12 August 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (17) , 15889-15896
Void fraction of a Sn–Ag–Cu solder joint underneath a chip resistor and its effect on joint strength and thermomechanical reliability
- 12 August 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (17) , 15889-15896
Void fraction of a Sn–Ag–Cu solder joint underneath a chip resistor and its effect on joint strength and thermomechanical reliability
- 1 August 2019
- Published by Elsevier in Microelectronic Engineering
- Vol. 216, 110973
Joint properties and reliability of Cu/Sn-Ag pillar bumps via low-temperature thermo-compression bonding
- 1 August 2019
- Published by Elsevier in Microelectronic Engineering
- Vol. 216, 110973
Joint properties and reliability of Cu/Sn-Ag pillar bumps via low-temperature thermo-compression bonding
- 8 May 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (11) , 10550-10559
Shear strength between Sn–3.0Ag–0.5Cu solders and Cu substrate after two solid-state aging processes for fan-out package process applications
- 8 May 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (11) , 10550-10559
Shear strength between Sn–3.0Ag–0.5Cu solders and Cu substrate after two solid-state aging processes for fan-out package process applications
- 11 March 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (8) , 7645-7653
Electromigration reliability of Sn–3.0Ag–0.5Cu/Cu–Zn solder joints
- 11 March 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (8) , 7645-7653
Electromigration reliability of Sn–3.0Ag–0.5Cu/Cu–Zn solder joints
- 1 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1937-1941
The Reliability and the Effect of NCA Trapping in Thermo-Compression Flip-Chip Solder Joints Fabricated Using Sn-Ag Solder Capped 40 µm Pitch Cu Pillar Bumps and Low Temperature Curable Non-Conductive Adhesive (NCA)
The effects of nonconductive adhesive (NCA) trapping on the reliability of low-temperature (150°C) thermo-compression (TC)-bonded flip-chip joints were investigated in this study. Both rough and smooth Cu pads were employed to investigate the effects of surface roughness on NCA trapping, with Sn-Ag solder-capped Cu pillar bumps bonded onto the Cu pads via low-temperature TC bonding. The NCA trapping in the rough Cu pad sample was much greater than that in the smooth Cu pad sample after TC bonding. In addition, the NCA trapping increased with decreasing bonding pressure. The electrical resistance for both the rough and smooth Cu pad samples increased after preconditioning (moisture sensitive level 3) and thermal cycling (-55°C/125°C) reliability tests. The high electrical resistance of the rough Cu pad sample was due to the crack propagation caused by the expansion of the trapped NCA. The reliability of the flip chip joint increased with increasing bonding pressure increased and decreasing surface roughness.
- 1 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1937-1941
The Reliability and the Effect of NCA Trapping in Thermo-Compression Flip-Chip Solder Joints Fabricated Using Sn-Ag Solder Capped 40 µm Pitch Cu Pillar Bumps and Low Temperature Curable Non-Conductive Adhesive (NCA)
The effects of nonconductive adhesive (NCA) trapping on the reliability of low-temperature (150°C) thermo-compression (TC)-bonded flip-chip joints were investigated in this study. Both rough and smooth Cu pads were employed to investigate the effects of surface roughness on NCA trapping, with Sn-Ag solder-capped Cu pillar bumps bonded onto the Cu pads via low-temperature TC bonding. The NCA trapping in the rough Cu pad sample was much greater than that in the smooth Cu pad sample after TC bonding. In addition, the NCA trapping increased with decreasing bonding pressure. The electrical resistance for both the rough and smooth Cu pad samples increased after preconditioning (moisture sensitive level 3) and thermal cycling (-55°C/125°C) reliability tests. The high electrical resistance of the rough Cu pad sample was due to the crack propagation caused by the expansion of the trapped NCA. The reliability of the flip chip joint increased with increasing bonding pressure increased and decreasing surface roughness.
- 1 November 2017
- Published by Elsevier in Microelectronics Reliability
- Vol. 78, 220-226
Adhesion of NCF to oxidized Si wafers after oxygen plasma treatment
- 1 November 2017
- Published by Elsevier in Microelectronics Reliability
- Vol. 78, 220-226
Adhesion of NCF to oxidized Si wafers after oxygen plasma treatment
- 1 November 2017
- Published by Elsevier in Microelectronics Reliability
- Vol. 78, 1-10
Degradation of adhesion between Cu and epoxy-based dielectric during exposure to hot humid environments
- 1 November 2017
- Published by Elsevier in Microelectronics Reliability
- Vol. 78, 1-10
Degradation of adhesion between Cu and epoxy-based dielectric during exposure to hot humid environments