Wenqing Jia
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Wenqing Jia has a total of 68 co-authors. Here are the top co-authors by number of shared publications:
- Chaoliang Xu
Material Engineering Technology Center, Suzhou Nuclear Power Research Institute, Suzhou 215004, China
4 shared publications Qiwei Quan
4 shared publicationsXiangbing Liu
4 shared publicationsBin Li
3 shared publicationsMiao Fu
3 shared publications- Wangjie Qian
Material Engineering Technology Center, Suzhou Nuclear Power Research Institute, Suzhou 215004, China
3 shared publications
Latest Publications
- 3 March 2026
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 626
The evolution of NiMnSi clusters in RPV steels under proton irradiation: The effect of Ni
- 3 March 2026
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 626
The evolution of NiMnSi clusters in RPV steels under proton irradiation: The effect of Ni
- Open Access
- 20 February 2026
- Published by Elsevier in SSRN Electronic Journal
Altering nanostructure and mechanical property evolution by annealing mitigation treatment of long-term aged cast duplex stainless steel
In order to explore lifespan extension methods for key nuclear power plant components, this study systematically investigates the evolution of spinodal decomposition (SD) nanostructures and corresponding mechanical properties of the long-term aged Z3CN20-09M cast duplex stainless steel (CDSS) during re-aging following an annealing mitigation treatment (AMT). Microstructure and nanostructure characterization was conducted using electron back scatter diffraction, x-ray diffraction, transmission electron microscopy and small-angle neutron scattering. Nanoindentation was employed to correlate the structural features with the mechanical responses of ferrite and austenite. The results indicate that AMT at 550 °C for 1 h effectively dissolves the SD nanostructures and restores the toughness of ferrite in the 13000 h-aged alloy to levels comparable to that of the as-cast condition. SD kinetics and associated toughness degradation are markedly retarded during re-aging, which is attributed to the reduced thermodynamic driving force and atomic diffusion rates, caused by the residual SD nanostructures, Ni-rich clusters and limited vacancy concentration after long-term aging and AMT. Thus, AMT can significantly extend the lifespan of CDSS components at reactor operating temperatures. Quantitative constitutive relationships were established to describe the non-linear dependence of mechanical properties on the characteristic parameters of SD nanostructures, enabling a predictive correlation between nanostructural evolution and mechanical performance. The study provides a mechanistic understanding of the relationship between mechanical properties and nanostructures of the re-aged CDSS after AMT, which contributes to the development of optimized thermal treatment strategies for the service life extension of nuclear power plant components.
- 20 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessAltering nanostructure and mechanical property evolution by annealing mitigation treatment of long-term aged cast duplex stainless steel
In order to explore lifespan extension methods for key nuclear power plant components, this study systematically investigates the evolution of spinodal decomposition (SD) nanostructures and corresponding mechanical properties of the long-term aged Z3CN20-09M cast duplex stainless steel (CDSS) during re-aging following an annealing mitigation treatment (AMT). Microstructure and nanostructure characterization was conducted using electron back scatter diffraction, x-ray diffraction, transmission electron microscopy and small-angle neutron scattering. Nanoindentation was employed to correlate the structural features with the mechanical responses of ferrite and austenite. The results indicate that AMT at 550 °C for 1 h effectively dissolves the SD nanostructures and restores the toughness of ferrite in the 13000 h-aged alloy to levels comparable to that of the as-cast condition. SD kinetics and associated toughness degradation are markedly retarded during re-aging, which is attributed to the reduced thermodynamic driving force and atomic diffusion rates, caused by the residual SD nanostructures, Ni-rich clusters and limited vacancy concentration after long-term aging and AMT. Thus, AMT can significantly extend the lifespan of CDSS components at reactor operating temperatures. Quantitative constitutive relationships were established to describe the non-linear dependence of mechanical properties on the characteristic parameters of SD nanostructures, enabling a predictive correlation between nanostructural evolution and mechanical performance. The study provides a mechanistic understanding of the relationship between mechanical properties and nanostructures of the re-aged CDSS after AMT, which contributes to the development of optimized thermal treatment strategies for the service life extension of nuclear power plant components.
- 25 October 2025
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 261, 94-102
Evolution of NiMnSi clusters in RPV steel under proton irradiation
- 25 October 2025
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 261, 94-102
Evolution of NiMnSi clusters in RPV steel under proton irradiation
- 22 September 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 618
The evolution of NiMnSi clusters in RPV steels under proton irradiation: The effect of Cu
- 22 September 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 618
The evolution of NiMnSi clusters in RPV steels under proton irradiation: The effect of Cu
- 6 August 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 616
Effects of proton irradiation on microstructures and Cr/Zr interface mechanics of Cr-coated Zr-1Nb cladding
- 6 August 2025
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 616
Effects of proton irradiation on microstructures and Cr/Zr interface mechanics of Cr-coated Zr-1Nb cladding
- Open Access
Effect of Constant Cyclic Stress Coupling on the Fatigue Behavior of 304LN Stainless Steel
The stress state of the primary circuit main pipeline is very complex mixed constant stress and periodic cyclic stress during the operation of nuclear power plants, which often affects the failure behavior of the stainless steel (SS) pipe. The fatigue behavior of 304LN SS under mixed constant stress and cyclic stress was investigated, and it was found that the coupling effect of constant stress and cyclic stress has a significant collaborative acceleration on the fatigue behavior. The research results showed that the cracks in the 304LN SS did not propagate even after 78 days under both constant load conditions of 5 KN and 7.5 KN, while the crack growth rate (CGR) of the specimen increased by about an order of magnitude when coupled with a cyclic fatigue load. The fatigue life of 304LN SS was the longest under 200 °C high-temperature water, and its life was roughly the same under 250 °C and 300 °C water. In a 300 °C high-temperature water environment, the fatigue life under the coupling of constant stress and cyclic fatigue stress is significantly lower than that under symmetric cyclic stress alone. There is a synergistic acceleration effect on the fatigue life of 304LN SS when constant stress is coupled with periodic cyclic stress, which is attributed to the combined effect of a corrosion environment and mechanical factors.
Open AccessEffect of Constant Cyclic Stress Coupling on the Fatigue Behavior of 304LN Stainless Steel
The stress state of the primary circuit main pipeline is very complex mixed constant stress and periodic cyclic stress during the operation of nuclear power plants, which often affects the failure behavior of the stainless steel (SS) pipe. The fatigue behavior of 304LN SS under mixed constant stress and cyclic stress was investigated, and it was found that the coupling effect of constant stress and cyclic stress has a significant collaborative acceleration on the fatigue behavior. The research results showed that the cracks in the 304LN SS did not propagate even after 78 days under both constant load conditions of 5 KN and 7.5 KN, while the crack growth rate (CGR) of the specimen increased by about an order of magnitude when coupled with a cyclic fatigue load. The fatigue life of 304LN SS was the longest under 200 °C high-temperature water, and its life was roughly the same under 250 °C and 300 °C water. In a 300 °C high-temperature water environment, the fatigue life under the coupling of constant stress and cyclic fatigue stress is significantly lower than that under symmetric cyclic stress alone. There is a synergistic acceleration effect on the fatigue life of 304LN SS when constant stress is coupled with periodic cyclic stress, which is attributed to the combined effect of a corrosion environment and mechanical factors.
- Open Access
Magnetic Indicator for Evaluating Cu Clustering and Hardening Effect in RPV Model Alloy
The reactor pressure vessel (RPV) is a critical barrier in nuclear power plants, but its embrittlement during service poses a significant safety challenge. This study investigated the effects of Cu-enriched clusters on the mechanical and magnetic properties of Fe-0.9 wt.%Cu model alloys through thermal aging. Using Vickers hardness tests, Magnetic Barkhausen Noise (MBN) detection, and Atom Probe Tomography (APT), the study aimed to establish a quantitative correlation between MBN signals, Vickers hardness, and Cu-enriched clusters, facilitating the non-destructive testing of RPV embrittlement. Experimental results showed that the hardness and MBN parameters (RMS and Vpp values) changed significantly with aging time. The hardness increased rapidly in the early stage (under-aged), followed by a plateau and then a decreasing trend (over-aged). In contrast, MBN parameters decreased initially and then increased. APT analysis revealed that Cu-enriched clusters increase in size to 4.60 nm and coalesced during aging, with their number density peaking to 3.76 × 1023 m−3 before declining. An inverse linear correlation was found between MBN signals and the combined factor Nd2Rg (product of the number density squared and the mean radius of Cu-enriched clusters). This correlation was consistent across both under-aged and over-aged states, suggesting that MBN signals can serve as applicable indicators for the non-destructive evaluation of RPV steel embrittlement.
Open AccessMagnetic Indicator for Evaluating Cu Clustering and Hardening Effect in RPV Model Alloy
The reactor pressure vessel (RPV) is a critical barrier in nuclear power plants, but its embrittlement during service poses a significant safety challenge. This study investigated the effects of Cu-enriched clusters on the mechanical and magnetic properties of Fe-0.9 wt.%Cu model alloys through thermal aging. Using Vickers hardness tests, Magnetic Barkhausen Noise (MBN) detection, and Atom Probe Tomography (APT), the study aimed to establish a quantitative correlation between MBN signals, Vickers hardness, and Cu-enriched clusters, facilitating the non-destructive testing of RPV embrittlement. Experimental results showed that the hardness and MBN parameters (RMS and Vpp values) changed significantly with aging time. The hardness increased rapidly in the early stage (under-aged), followed by a plateau and then a decreasing trend (over-aged). In contrast, MBN parameters decreased initially and then increased. APT analysis revealed that Cu-enriched clusters increase in size to 4.60 nm and coalesced during aging, with their number density peaking to 3.76 × 1023 m−3 before declining. An inverse linear correlation was found between MBN signals and the combined factor Nd2Rg (product of the number density squared and the mean radius of Cu-enriched clusters). This correlation was consistent across both under-aged and over-aged states, suggesting that MBN signals can serve as applicable indicators for the non-destructive evaluation of RPV steel embrittlement.
- Open Access
Study on Corrosion Fatigue Behavior of 304L Austenite Stainless Steel in 325 °C High-Temperature Water Environment
The fatigue crack growth behavior of 304L austenitic stainless steel (SS) in a 325 °C high-temperature and high-pressure water environment were investigated by a corrosion fatigue test system, by electron back scatter diffraction (EBSD), and by a transmission electron microscope (TEM). The experimental results indicated that the crack growth rate (CGR) of 304L SS increases with increasing the stress intensity factor, stress level, and fatigue frequency (f). Compared to dissolved hydrogen (DH) in a high-temperature water environment, dissolved oxygen (DO) significantly enhances the CGR by about an order of magnitude higher. The crack tip of 304L SS after the corrosion fatigue test under higher stress levels is sharper, with more secondary cracks on the fracture surface, while the crack tip under lower stress levels is blunter with relatively fewer secondary cracks. The oxidation behavior at the crack tip was analyzed under different loading and water chemistry conditions, and a related effect on the crack tip and CGR was clarified.
Open AccessStudy on Corrosion Fatigue Behavior of 304L Austenite Stainless Steel in 325 °C High-Temperature Water Environment
The fatigue crack growth behavior of 304L austenitic stainless steel (SS) in a 325 °C high-temperature and high-pressure water environment were investigated by a corrosion fatigue test system, by electron back scatter diffraction (EBSD), and by a transmission electron microscope (TEM). The experimental results indicated that the crack growth rate (CGR) of 304L SS increases with increasing the stress intensity factor, stress level, and fatigue frequency (f). Compared to dissolved hydrogen (DH) in a high-temperature water environment, dissolved oxygen (DO) significantly enhances the CGR by about an order of magnitude higher. The crack tip of 304L SS after the corrosion fatigue test under higher stress levels is sharper, with more secondary cracks on the fracture surface, while the crack tip under lower stress levels is blunter with relatively fewer secondary cracks. The oxidation behavior at the crack tip was analyzed under different loading and water chemistry conditions, and a related effect on the crack tip and CGR was clarified.