Dan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Dan Li has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Guxia Wang
School of Chemistry and Chemical Engineering, North Minzu University, Yinchuan 750021, China
1 shared publication - Jinying Yuan
Key Lab of Organic Optoelectronics and Molecular Engineering of Ministry of Education, Department of Chemistry, Tsinghua University, Beijing 100084, P. R. China
1 shared publication Jinzhao Ji
Key Laboratory of Organic OptoElectronics and Molecular Engineering, Department of Chemistry, Tsinghua University, Beijing 100084, P. R. China
1 shared publication- Jun Yan
School of Materials Science and Engineering, North Minzu University, Yinchuan 750021, China
1 shared publication Min Zeng
Key Laboratory of Organic OptoElectronics and Molecular Engineering, Department of Chemistry, Tsinghua University, Beijing 100084, P. R. China
1 shared publicationNan Liu
School of Life Sciences, Tsinghua University, Beijing 100084, P. R. China
1 shared publication
Latest Publications
- 23 February 2023
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 25 (6) , 2427-2437
Ultrafast and continuous synthesis of phase change nanocapsules using salt-accelerated microwave-assisted polymerization
Using nanoencapsulated phase change materials (NanoPCMs) for thermal energy storage has great application prospects in addressing the mismatch issues between energy supply and demand. However, the rapid, large-scale preparation of NanoPCMs is a challenge. Here, we developed a facile, efficient, green, and continuous method for the ultrafast preparation of NanoPCMs for energy storage using microwave-assisted polymerization with cross-linked poly(methyl methacrylate) and the PCM n-octadecane utilized as the shell and core materials, respectively. Sodium chloride (NaCl) acted as a microwave sensitizer and synergized with emulsifier to control the particle size of the NanoPCMs. Through orthogonal experiments, we investigated the effects of microwave power, temperature, and polymerization time on the properties of the NanoPCMs. The optimum conditions were 1.0 wt% NaCl, 60 °C, 10 min, and 600 W. The resulting NanoPCMs with uniform, spherical, core–shell structures were successfully utilized as thermal energy storage materials. The encapsulation efficiency was 50.8% and the NanoPCMs exhibited a particle size of ca. 95 nm, a high latent heat storage capacity of ca. 114.9 J g−1, and good thermal stability. In particular, the reaction time was greatly reduced from 12 h to 10 min, 100 times faster than conventional hydrothermal polymerization. Based on these parameters, the continuous, efficient production of microwave-assisted NanoPCMs was realized through reactor design, laying a foundation for the commercial production of NanoPCMs.
- 23 February 2023
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 25 (6) , 2427-2437
Ultrafast and continuous synthesis of phase change nanocapsules using salt-accelerated microwave-assisted polymerization
Using nanoencapsulated phase change materials (NanoPCMs) for thermal energy storage has great application prospects in addressing the mismatch issues between energy supply and demand. However, the rapid, large-scale preparation of NanoPCMs is a challenge. Here, we developed a facile, efficient, green, and continuous method for the ultrafast preparation of NanoPCMs for energy storage using microwave-assisted polymerization with cross-linked poly(methyl methacrylate) and the PCM n-octadecane utilized as the shell and core materials, respectively. Sodium chloride (NaCl) acted as a microwave sensitizer and synergized with emulsifier to control the particle size of the NanoPCMs. Through orthogonal experiments, we investigated the effects of microwave power, temperature, and polymerization time on the properties of the NanoPCMs. The optimum conditions were 1.0 wt% NaCl, 60 °C, 10 min, and 600 W. The resulting NanoPCMs with uniform, spherical, core–shell structures were successfully utilized as thermal energy storage materials. The encapsulation efficiency was 50.8% and the NanoPCMs exhibited a particle size of ca. 95 nm, a high latent heat storage capacity of ca. 114.9 J g−1, and good thermal stability. In particular, the reaction time was greatly reduced from 12 h to 10 min, 100 times faster than conventional hydrothermal polymerization. Based on these parameters, the continuous, efficient production of microwave-assisted NanoPCMs was realized through reactor design, laying a foundation for the commercial production of NanoPCMs.
- 19 May 2022
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 13 (23) , 3529-3538
Customizable nano-sized colloidal tetrahedra by polymerization-induced particle self-assembly (PIPA)
Colloidal molecules (CMs) are colloidal clusters with molecule-like symmetry and architecture, generated from the self-assembly of nanoparticles with attractive patches. However, the large-scale preparation of patchy nanoparticles remains challenging. Here, we synthesize CH4-like colloidal tetrahedra (CTs) in a scalable way by aqueous polymerization-induced particle self-assembly (PIPA), where isotropic diblock copolymer spheres are used as seeds. During PIPA, the newly formed third block aggregates into attractive patches, which bridge the isotropic spheres together to form CTs in situ, as a result of surface energy minimization. This approach surpasses previous reports in its scalability, high yield and versatility. For example, the purity of as-prepared CTs reaches 78.3% at a concentration of 100 g L−1, which allows the 3D reconstruction of the tetrahedral structure by single particle electron microscopy analysis. The versatility of PIPA is illustrated by preparing CMs of tunable size, valency and various chemical structures. In addition, the architecture of the CMs can be manipulated after the PIPA process simply by the addition of ethanol, for example, the CTs can be transformed into ladder-like structures, paving a new avenue to access hierarchical nanoscale self-assemblies.
- 19 May 2022
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 13 (23) , 3529-3538
Customizable nano-sized colloidal tetrahedra by polymerization-induced particle self-assembly (PIPA)
Colloidal molecules (CMs) are colloidal clusters with molecule-like symmetry and architecture, generated from the self-assembly of nanoparticles with attractive patches. However, the large-scale preparation of patchy nanoparticles remains challenging. Here, we synthesize CH4-like colloidal tetrahedra (CTs) in a scalable way by aqueous polymerization-induced particle self-assembly (PIPA), where isotropic diblock copolymer spheres are used as seeds. During PIPA, the newly formed third block aggregates into attractive patches, which bridge the isotropic spheres together to form CTs in situ, as a result of surface energy minimization. This approach surpasses previous reports in its scalability, high yield and versatility. For example, the purity of as-prepared CTs reaches 78.3% at a concentration of 100 g L−1, which allows the 3D reconstruction of the tetrahedral structure by single particle electron microscopy analysis. The versatility of PIPA is illustrated by preparing CMs of tunable size, valency and various chemical structures. In addition, the architecture of the CMs can be manipulated after the PIPA process simply by the addition of ethanol, for example, the CTs can be transformed into ladder-like structures, paving a new avenue to access hierarchical nanoscale self-assemblies.