  • Distinct liquefaction resistance of Fujian sand under the combined effect of asymmetric cyclic loads and fabric anisotropy

    by Shihao Zhang, Wenke Li, Huari Tang, Songtao Li, Yongchao Zhu, Wei Li

    Fabric anisotropy and load asymmetry can both significantly influence the mechanical behavior of sand. To clarify the coupled influence of fabric anisotropy and load asymmetry on liquefaction characteristics, sand specimens with different bedding angles were loaded by cyclic loadings of different degrees of asymmetry under undrained triaxial conditions. The influences of fabric anisotropy on the liquefaction characteristics under different degrees of loading asymmetry were identified through comprehensive analyses of excess pore water pressure generation, axial strain development, and energy dissipation during the cyclic loading. The results indicate that under a symmetric cyclic load, the liquefaction resistance of sand increases with increasing bedding angle. However, when the loading asymmetry increases and exceeds a certain degree, the larger bedding angle leads to lower liquefaction resistance.

  • Simulation analysis of thermal resistance asphalt pavement based on cooling function

    by Shihao Zhang, Yilei Hu, Zhengqi Zhang, Datong Guo, Songtao Li, Baolin Wang

    To improve the high-temperature stability of asphalt pavement, a thermally resistant asphalt mixture was prepared in this study, where part of the mineral aggregates was replaced with ceramsite (CE) and floating beads (FBs) featuring low thermal conductivity. The results indicate that the recommended thermal conductivity coefficient of the upper layer is 1.39 ∼ 1.94 W (m·K) −1 , and that of the middle course is 0.83 ∼ 1.94 W (m·K) −1 for cooling performance. In terms of rutting resistance, the recommended thermal conductivity coefficient of the upper layer is 0.28 ∼ 1.94 W (m·K) −1 , and that of the middle course is 1.39 ∼ 1.94 W (m·K) −1 . For urban light-load roads, the recommended mixing ratio of CE is 50% ∼ 75% for the upper layer and FB is 25% ∼ 50% for the middle course. For heavy-load roads, the recommended mixing ratio of CE is 50% ∼ 75% for the upper layer, and either CE or FB is 50% ∼ 75% for the middle course. Within 24 h, the settlement and uplift displacement values of the composite thermally resistant pavement are reduced by 0.01028 mm and 0.00668 mm, respectively, compared with those of the conventional asphalt mixture pavement.

  • Open Access

    Mechanical Analysis of Preventing Reflection Cracks Based on Stress Absorbing Layer

    by Lingjie Han, Shihao Zhang, Zhengqi Zhang, Taotao Gao

    After asphalt concrete overlay, the reflection crack in the old pavement remains a great challenge. In order to overcome this problem, here, we report the effect of stress absorbing layer on the reflection crack. First, the concrete measures to prevent and reduce reflection cracks at home and abroad are analyzed. Then, the mechanism of the generation and development of reflection cracks is studied, the functional characteristics of stress absorbing layer are analyzed, and the principle of antireflection crack is clarified. Further, the effects of modulus thickness and porosity of stress absorbing layer on the stress of pavement structure layer are discussed. Finally, the effect of the stress absorbing layer on preventing reflective cracks is analyzed by numerical simulation. The analyses show that the stress absorbing layer is a thin asphalt concrete layer with good fatigue resistance and low modulus between the old pavement and asphalt pavement, which delays the expansion of pavement reflection cracks. The stress absorbing layer should have high elasticity and low temperature flexibility, water damage resistance, and interlayer bonding. The simulation results suggest that the modulus of the stress absorbing layer should be 400 MPa∼600 MPa, and the thickness should be 1 cm∼2.5 cm. When the thickness of the stress absorption layer is 2.5 cm, the values of tensile stress σX, equivalent stress σMises and maximum shear stress τMax are 31.7%, 29.2%, and 25.7% lower than those of the layer without addition, respectively. The results demonstrate that the effect of stress reduction is obvious, which plays an important role in preventing or reducing the occurrence of reflective cracks. The designed void ratio of the mixture is between 1% and 2.5% for the indoor permeability resistance test. We believe that these findings have certain guiding significance for theoretical analysis and engineering application of stress absorbing layer.