Ivica Kladarić
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ivica Kladarić has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Andrijana Milinović
Mechanical Engineering Faculty in Slavonski Brod, University of Slavonski Brod, Trg Ivane Brlić-Mažuranić 2, 35000 Slavonski Brod, Croatia
2 shared publications - Božidar Matijević
Faculty of Mechanical Engineering and Naval Architecture, University of Zagreb, Ivana Lucica 5, 10000 Zagreb, Croatia
1 shared publication - Danko Ćorić
Faculty of Mechanical Engineering and Naval Architecture, University of Zagreb, Ivana Lucica 5, 10000 Zagreb, Croatia
1 shared publication - Josip Stojšić
Mechanical Engineering Faculty in Slavonski Brod, University of Slavonski Brod, 35000 Slavonski Brod, Croatia
1 shared publication - Stjepan Golubić
Polytechnic of Bjelovar, Bjelovar University of Applied Sciences, Trg Eugena Kvaternika 4, 43000 Bjelovar, Croatia
1 shared publication
Latest Publications
- Open Access
The Influence of Applying PVD Coatings on Adhesion Wear Resistance of Quenching and Tempering Steels
The article examines the effect of different types of two-layer nanostructured coatings (cVIc and nACVIc) deposited on three types of steel substrates, 45S20, C45E, and 42CrMo4, to determine the resistance to adhesive wear of the substrate/coating system. The samples underwent different heat treatments, including normalising, quenching, and quenching and tempering, followed by PVD (physical vapour deposition) treatment at temperatures of 450 °C (cVIc) and 460 °C (nACVIc). The thickness of the cVIc layers for all three steels ranged from 0.9 to 3.4 μm, while the thickness of the nACVIc layers on all steels was slightly greater, ranging from 1.9 to 3.1 μm. Tribological tests were conducted using the pin-on-disc method, and the results were statistically analysed. Results indicate that steel grade, heat treatment, and PVD coating significantly affect adhesive wear resistance, with the type of PVD coating showing the strongest influence. For all three steels, quenched and uncoated samples exhibited the lowest adhesion wear index values. Normalised and quenched with or without tempering steels coated with cVIc layer exhibit higher resistance to adhesive wear due to better adhesion of the layer compared to the nACVIc coating.
Open AccessThe Influence of Applying PVD Coatings on Adhesion Wear Resistance of Quenching and Tempering Steels
The article examines the effect of different types of two-layer nanostructured coatings (cVIc and nACVIc) deposited on three types of steel substrates, 45S20, C45E, and 42CrMo4, to determine the resistance to adhesive wear of the substrate/coating system. The samples underwent different heat treatments, including normalising, quenching, and quenching and tempering, followed by PVD (physical vapour deposition) treatment at temperatures of 450 °C (cVIc) and 460 °C (nACVIc). The thickness of the cVIc layers for all three steels ranged from 0.9 to 3.4 μm, while the thickness of the nACVIc layers on all steels was slightly greater, ranging from 1.9 to 3.1 μm. Tribological tests were conducted using the pin-on-disc method, and the results were statistically analysed. Results indicate that steel grade, heat treatment, and PVD coating significantly affect adhesive wear resistance, with the type of PVD coating showing the strongest influence. For all three steels, quenched and uncoated samples exhibited the lowest adhesion wear index values. Normalised and quenched with or without tempering steels coated with cVIc layer exhibit higher resistance to adhesive wear due to better adhesion of the layer compared to the nACVIc coating.
- Open Access
Evaluation of Boride Layers on C70W2 Steel Using a New Approach to Characterization of Boride Layers
In this study, boride layers on C70W2 steel, obtained by boronizing at temperatures ranging from 870 to 970 °C and durations from 4 to 8 h, were investigated. The characterization of the layers was carried out using a new approach based on the change in the volume fraction of the boride phase. Analysis of the change in volume fraction showed that an increase in temperature and duration resulted in thicker layers, with temperature having a greater influence. Based on the volume fraction of the boride phase, the layer is divided into compact and toothed parts. With increasing temperature, the thicknesses of both parts of the layer increased. The thickness of the toothed part was the highest after 6 h of boronizing and further prolongation of boronizing led to a decrease in the thickness. Regression equations were estimated for the prediction of the volume fraction of the boride phase, the thickness of the compact part, and that of the toothed part of the boride layer as a function of the boronizing parameters. This study has shown that characterization based on the volume fraction of the boride phase offers advantages over the conventional method based on the average thickness of the layer.
Open AccessEvaluation of Boride Layers on C70W2 Steel Using a New Approach to Characterization of Boride Layers
In this study, boride layers on C70W2 steel, obtained by boronizing at temperatures ranging from 870 to 970 °C and durations from 4 to 8 h, were investigated. The characterization of the layers was carried out using a new approach based on the change in the volume fraction of the boride phase. Analysis of the change in volume fraction showed that an increase in temperature and duration resulted in thicker layers, with temperature having a greater influence. Based on the volume fraction of the boride phase, the layer is divided into compact and toothed parts. With increasing temperature, the thicknesses of both parts of the layer increased. The thickness of the toothed part was the highest after 6 h of boronizing and further prolongation of boronizing led to a decrease in the thickness. Regression equations were estimated for the prediction of the volume fraction of the boride phase, the thickness of the compact part, and that of the toothed part of the boride layer as a function of the boronizing parameters. This study has shown that characterization based on the volume fraction of the boride phase offers advantages over the conventional method based on the average thickness of the layer.