Doaa F. Baamer
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Doaa F. Baamer has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Afaf Almasoudi
Chemistry Department, Faculty of Science, King Abdulaziz University, Jeddah P.O. Box 42734, Saudi Arabia
4 shared publications - Omar Makram Ali
Department of Chemistry, Taraba University College, Taraba Branch, Taif University, P.O. Box 11099, Taif 21944, Saudi Arabia
4 shared publications - Abdallah Shanableh
Research Institute of Sciences and Engineering, University of Sharjah
3 shared publications - Javier Fernandez-Garcia
IQS School of Engineering, Universitat Ramon Llull, Via Augusta 390, 08017 Barcelona, Spain
3 shared publications - Muhammad Imran Khan
Research Institute of Sciences and Engineering (RISE), University of Sharjah, Sharjah 27272, United Arab Emirates
3 shared publications - Muhammad Khalid Nazir
Institute of Chemical Sciences, Bahauddin Zakariya University, Multan 60800, Pakistan
2 shared publications
Latest Publications
- Open Access
Synergistic Effect of NiAl-Layered Double Hydroxide and Cu-MOF for the Enhanced Photocatalytic Degradation of Methyl Orange and Antibacterial Properties
This study synthesized NiAl-layered double hydroxide (LDH)/Cu-MOF photocatalyst using a simple impregnation method involving NiAl-LDH and Cu-MOF. The successful synthesis was confirmed through Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), scanning electron microscopy (SEM), zeta potential measurements, thermogravimetric analysis (TGA), ultraviolet diffuse reflectance spectroscopy (UV-DRS), N2 adsorption at −196 °C, and electrochemical impedance spectroscopy (EIS). Photocatalysts based on NiAl-LDH, Cu-MOF, and NiAl-LDH/Cu-MOF were used to remove methyl orange (MO) dye from contaminated water. The impact of various factors, including pH, dye concentration, and photocatalyst amount, on MO degradation efficiency was assessed. FTIR analysis was conducted both before and after dye degradation. The optimal degradation conditions were a photocatalyst dose of 25 mg and a pH of 3. Kinetic studies indicated that the degradation of MO dye onto NiAl-LDH/Cu-MOF followed a pseudo-first-order and an L–H or Langmuir–Hinshelwood model. The value of R2 = 0.94 confirms the validity of pseudo-first-order and Langmuir–Hinshelwood (L–H) kinetic models for the photocatalytic degradation of MO dye. This study highlights the importance of developing novel photocatalysts with improved degradation efficiency to protect the water environment. Antibacterial activity was also performed with antibacterial sensibility testing by disk diffusion to determine minimal inhibitory and bactericidal concentrations. In short, NiAl-LDH/Cu-MOF can be helpful for various biomedical and industrial applications.
Open AccessSynergistic Effect of NiAl-Layered Double Hydroxide and Cu-MOF for the Enhanced Photocatalytic Degradation of Methyl Orange and Antibacterial Properties
This study synthesized NiAl-layered double hydroxide (LDH)/Cu-MOF photocatalyst using a simple impregnation method involving NiAl-LDH and Cu-MOF. The successful synthesis was confirmed through Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), scanning electron microscopy (SEM), zeta potential measurements, thermogravimetric analysis (TGA), ultraviolet diffuse reflectance spectroscopy (UV-DRS), N2 adsorption at −196 °C, and electrochemical impedance spectroscopy (EIS). Photocatalysts based on NiAl-LDH, Cu-MOF, and NiAl-LDH/Cu-MOF were used to remove methyl orange (MO) dye from contaminated water. The impact of various factors, including pH, dye concentration, and photocatalyst amount, on MO degradation efficiency was assessed. FTIR analysis was conducted both before and after dye degradation. The optimal degradation conditions were a photocatalyst dose of 25 mg and a pH of 3. Kinetic studies indicated that the degradation of MO dye onto NiAl-LDH/Cu-MOF followed a pseudo-first-order and an L–H or Langmuir–Hinshelwood model. The value of R2 = 0.94 confirms the validity of pseudo-first-order and Langmuir–Hinshelwood (L–H) kinetic models for the photocatalytic degradation of MO dye. This study highlights the importance of developing novel photocatalysts with improved degradation efficiency to protect the water environment. Antibacterial activity was also performed with antibacterial sensibility testing by disk diffusion to determine minimal inhibitory and bactericidal concentrations. In short, NiAl-LDH/Cu-MOF can be helpful for various biomedical and industrial applications.
- Open Access
Synthesis, Magnetic, and Photocatalytic Activity of Polypyrrole-Based TiO2–Fe Catalyst for Wastewater Treatment
The primary aim of this study is to investigate the degradation efficacy of the Ppy/TiO2-Fe photocatalyst for MB dye in an aqueous solution. Firstly, the direct addition of TiO2 and Fe was done to prepare Ppy/TiO2-Fe photocatalyst. Fourier transformation infrared spectroscopy, XRD, SEM, BET surface area analysis, and magnetization tests established the formation of the Ppy/TiO2-Fe photocatalyst. The crystallite sizes of TiO2, Fe-TiO2, and Ppy/TiO2-Fe photocatalyst were estimated to be 24.99 nm, 21.94 nm, and 21.84 nm, respectively. For the synthesis confirmation, the FTIR spectrum confirmed the existence of Ti-O, Fe-O, and Ppy-related bonds. While comparing the SEM images, the impact of polypyrrole on the particle shape was observed with less aggregation and increased surface roughness. The VSM analysis revealed that incorporating polypyrrole (Ppy) into Fe-TiO2 significantly enhances its magnetic properties, with Ppy/TiO2-Fe exhibiting superparamagnetic behavior, characterized by a higher saturation magnetization (Ms) of 33.11 emu/g and a lower coercivity (Hc) of 0.160 Oe, compared to Fe-TiO2’s Ms of 1.09 emu/g and Hc of 341.39 Oe. The N2 sorption desorption, with a specific surface area of 2.25 × 102 m2/g, is beneficial for photocatalytic activity. The concentration of dye, amount of catalyst, pH, and temperature were studied to evaluate the photocatalytic efficiency of the synthesized Ppy/TiO2-Fe photocatalyst under different conditions. The findings revealed a degradation efficiency of 91.92%. The degradation rate reached 91.92% under optimal conditions within 120 min and could be fitted well by first-order kinetics. The photocatalytic efficiency was also evaluated for the scavenger, and the concentration of H2O2 and the reusability of the catalyst were demonstrated. Based on the observed results, the Ppy/TiO2-Fe photocatalyst could be applied more effectively and efficiently to photocatalytic degradation of organic dyes in wastewater treatment.
Open AccessSynthesis, Magnetic, and Photocatalytic Activity of Polypyrrole-Based TiO2–Fe Catalyst for Wastewater Treatment
The primary aim of this study is to investigate the degradation efficacy of the Ppy/TiO2-Fe photocatalyst for MB dye in an aqueous solution. Firstly, the direct addition of TiO2 and Fe was done to prepare Ppy/TiO2-Fe photocatalyst. Fourier transformation infrared spectroscopy, XRD, SEM, BET surface area analysis, and magnetization tests established the formation of the Ppy/TiO2-Fe photocatalyst. The crystallite sizes of TiO2, Fe-TiO2, and Ppy/TiO2-Fe photocatalyst were estimated to be 24.99 nm, 21.94 nm, and 21.84 nm, respectively. For the synthesis confirmation, the FTIR spectrum confirmed the existence of Ti-O, Fe-O, and Ppy-related bonds. While comparing the SEM images, the impact of polypyrrole on the particle shape was observed with less aggregation and increased surface roughness. The VSM analysis revealed that incorporating polypyrrole (Ppy) into Fe-TiO2 significantly enhances its magnetic properties, with Ppy/TiO2-Fe exhibiting superparamagnetic behavior, characterized by a higher saturation magnetization (Ms) of 33.11 emu/g and a lower coercivity (Hc) of 0.160 Oe, compared to Fe-TiO2’s Ms of 1.09 emu/g and Hc of 341.39 Oe. The N2 sorption desorption, with a specific surface area of 2.25 × 102 m2/g, is beneficial for photocatalytic activity. The concentration of dye, amount of catalyst, pH, and temperature were studied to evaluate the photocatalytic efficiency of the synthesized Ppy/TiO2-Fe photocatalyst under different conditions. The findings revealed a degradation efficiency of 91.92%. The degradation rate reached 91.92% under optimal conditions within 120 min and could be fitted well by first-order kinetics. The photocatalytic efficiency was also evaluated for the scavenger, and the concentration of H2O2 and the reusability of the catalyst were demonstrated. Based on the observed results, the Ppy/TiO2-Fe photocatalyst could be applied more effectively and efficiently to photocatalytic degradation of organic dyes in wastewater treatment.
- Open Access
Facile Synthesis of Sodium Alginate (SA)-Based Quaternary Bio-Nanocomposite (SA@Co-Zn-Ce) for Antioxidant Activity and Photocatalytic Degradation of Reactive Red 24
This study introduces a new strategy for the environmentally friendly catalytic degradation of Reactive Red 24 (RR24) dye using sunlight. We developed a cost-effective quaternary nanocomposite by immobilizing a sodium alginate biopolymer over bioengineered Co-Zn-Ce nanoparticles, forming an SA@Co–Zn–Ce nanocomposite (where SA means sodium alginate). This composite also demonstrated an exceptional antioxidant potential of approximately 89%, attributed to the synergistic effect of sodium alginate and green-synthesized Co–Zn–Ce nanoparticles (biosynthesized using Ocimum sanctum leaf extract as a reducing agent). Scanning electron microscopy revealed grain sizes of 28.6 nm for Co–Zn–Ce NPs and 25.59 nm for SA@Co–Zn–Ce nanocomposites (NCs). X-ray diffraction showed particle sizes of 16.87 nm and 15.43 nm, respectively. Co–Zn–Ce NPs exhibited a zeta potential of 1.99 mV, whereas the sodium alginate-anchored Co–Zn–Ce showed −7.99 mV. This indicated the entrapment of negatively charged ions from sodium alginate, altering the surface charge characteristics and enhancing the photocatalytic degradation of RR24. Dynamic light scattering revealed an average particle size of approximately 81 nm for SA@Co–Zn–Ce NCs, with the larger size due to the influence of water molecules in the colloidal solution affecting hydrodynamic diameter measurement. The SA@Co–Zn–Ce NCs exhibited a CO2 adsorption capacity of 3.29 mmol/g at 25 °C and 4.76 mmol/g at 40 °C, indicating temperature-dependent variations in adsorption capabilities. The specific surface area of Co–Zn–Ce oxide NPs, measured using Brunauer–Emmett–Teller (BET) analysis, was found to be 167.346 m2/g, whereas the SA@Co–Zn–Ce oxide nanocomposite showed a surface area of 24.14 m2/g. BJH analysis revealed average pore diameters of 34.60 Å for Co–Zn–Ce oxide NPs and 9.26 Å for SA@Co–Zn–Ce oxide NCs. Although the immobilization of sodium alginate on Co–Zn–Ce oxide NPs did not increase the adsorption sites and porosity of the composite, as evidenced by the N2 adsorption–desorption isotherms, the SA@Co–Zn–Ce oxide NCs still demonstrated a high photocatalytic degradation efficiency of RR24.
Open AccessFacile Synthesis of Sodium Alginate (SA)-Based Quaternary Bio-Nanocomposite (SA@Co-Zn-Ce) for Antioxidant Activity and Photocatalytic Degradation of Reactive Red 24
This study introduces a new strategy for the environmentally friendly catalytic degradation of Reactive Red 24 (RR24) dye using sunlight. We developed a cost-effective quaternary nanocomposite by immobilizing a sodium alginate biopolymer over bioengineered Co-Zn-Ce nanoparticles, forming an SA@Co–Zn–Ce nanocomposite (where SA means sodium alginate). This composite also demonstrated an exceptional antioxidant potential of approximately 89%, attributed to the synergistic effect of sodium alginate and green-synthesized Co–Zn–Ce nanoparticles (biosynthesized using Ocimum sanctum leaf extract as a reducing agent). Scanning electron microscopy revealed grain sizes of 28.6 nm for Co–Zn–Ce NPs and 25.59 nm for SA@Co–Zn–Ce nanocomposites (NCs). X-ray diffraction showed particle sizes of 16.87 nm and 15.43 nm, respectively. Co–Zn–Ce NPs exhibited a zeta potential of 1.99 mV, whereas the sodium alginate-anchored Co–Zn–Ce showed −7.99 mV. This indicated the entrapment of negatively charged ions from sodium alginate, altering the surface charge characteristics and enhancing the photocatalytic degradation of RR24. Dynamic light scattering revealed an average particle size of approximately 81 nm for SA@Co–Zn–Ce NCs, with the larger size due to the influence of water molecules in the colloidal solution affecting hydrodynamic diameter measurement. The SA@Co–Zn–Ce NCs exhibited a CO2 adsorption capacity of 3.29 mmol/g at 25 °C and 4.76 mmol/g at 40 °C, indicating temperature-dependent variations in adsorption capabilities. The specific surface area of Co–Zn–Ce oxide NPs, measured using Brunauer–Emmett–Teller (BET) analysis, was found to be 167.346 m2/g, whereas the SA@Co–Zn–Ce oxide nanocomposite showed a surface area of 24.14 m2/g. BJH analysis revealed average pore diameters of 34.60 Å for Co–Zn–Ce oxide NPs and 9.26 Å for SA@Co–Zn–Ce oxide NCs. Although the immobilization of sodium alginate on Co–Zn–Ce oxide NPs did not increase the adsorption sites and porosity of the composite, as evidenced by the N2 adsorption–desorption isotherms, the SA@Co–Zn–Ce oxide NCs still demonstrated a high photocatalytic degradation efficiency of RR24.
- Open Access
Novel Starch-Modified NiCrMn-LDH-Based Composite for Photocatalytic Degradation of Reactive Orange 13
Water pollution has become a great challenge today. To address this problem regarding wastewater treatment by removing toxic synthetic dyes from wastewater, this research focused on the synthesis of a novel starch-modified NiCrMn-layered double hydroxide composite through the coprecipitation method and applied it as a photocatalyst for the degradation of reactive orange 13 dye. The synthesized photocatalyst was characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), Brunauer–Emmett–Teller (BET), point of zero charges (PZC), dynamic light scattering (DLS), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC) and Zeta potential techniques. These techniques revealed different characteristics of photocatalysts, like surface and structural properties. According to BET analysis, the final composite had 2.5 × 102 m2/g BET-specific surface area with a 45.56 nm pore radius value, and the overall composite found as mesoporous. Similarly, in DLS analysis, bare NiCrMn-LDH had 404 nm hydrodynamic size, which increased for the final starch composite up to 667 nm. Zeta potential value changed from −14.56 mV to 0.95 mV after the incorporation of starch with NiCrMn-LDH. They confirmed the incorporation of starch with trimetallic NiCrMn-layered double hydroxide (2:1:2). Starch association improved the properties of the photocatalyst like surface area. Different parameters like pH value, initial dye concentration, photocatalyst dose, hydrogen peroxide concentration, effect of sacrificial reagent, and effect of inorganic anions were studied for degradation of RO13. Overall, the photocatalysis process for RO13 followed pseudo-first-order kinetics. Photocatalytic degradation reactions for reactive orange 13 were conducted with an initial dye concentration of 10 mg/L, photocatalyst dosage of 20 mg/50 mL, and pH value at 3 in the presence of sunlight, resulting in an impressive degradation removal rate of 86.68%. This remarkable degradation ability of the photocatalyst for reactive orange 13 proves this composite was highly efficient.
Open AccessNovel Starch-Modified NiCrMn-LDH-Based Composite for Photocatalytic Degradation of Reactive Orange 13
Water pollution has become a great challenge today. To address this problem regarding wastewater treatment by removing toxic synthetic dyes from wastewater, this research focused on the synthesis of a novel starch-modified NiCrMn-layered double hydroxide composite through the coprecipitation method and applied it as a photocatalyst for the degradation of reactive orange 13 dye. The synthesized photocatalyst was characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), Brunauer–Emmett–Teller (BET), point of zero charges (PZC), dynamic light scattering (DLS), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC) and Zeta potential techniques. These techniques revealed different characteristics of photocatalysts, like surface and structural properties. According to BET analysis, the final composite had 2.5 × 102 m2/g BET-specific surface area with a 45.56 nm pore radius value, and the overall composite found as mesoporous. Similarly, in DLS analysis, bare NiCrMn-LDH had 404 nm hydrodynamic size, which increased for the final starch composite up to 667 nm. Zeta potential value changed from −14.56 mV to 0.95 mV after the incorporation of starch with NiCrMn-LDH. They confirmed the incorporation of starch with trimetallic NiCrMn-layered double hydroxide (2:1:2). Starch association improved the properties of the photocatalyst like surface area. Different parameters like pH value, initial dye concentration, photocatalyst dose, hydrogen peroxide concentration, effect of sacrificial reagent, and effect of inorganic anions were studied for degradation of RO13. Overall, the photocatalysis process for RO13 followed pseudo-first-order kinetics. Photocatalytic degradation reactions for reactive orange 13 were conducted with an initial dye concentration of 10 mg/L, photocatalyst dosage of 20 mg/50 mL, and pH value at 3 in the presence of sunlight, resulting in an impressive degradation removal rate of 86.68%. This remarkable degradation ability of the photocatalyst for reactive orange 13 proves this composite was highly efficient.
- Open Access
Synthesis and Characterization of Green ZnO@polynaniline/Bentonite Tripartite Structure (G.Zn@PN/BE) as Adsorbent for As (V) Ions: Integration, Steric, and Energetic Properties
A green ZnO@polynaniline/bentonite composite (G.Zn@PN/BE) was synthesized as an enhanced adsorbent for As (V) ions. Its adsorption properties were assessed in comparison with the integrated components of bentonite (BE) and polyaniline/bentonite (PN/BE) composites. The G.Zn@PN/BE composite achieved an As (V) retention capacity (213 mg/g) higher than BE (72.7 mg/g) and PN/BE (119.8 mg/g). The enhanced capacity of G.Zn@PN/BE was studied using classic (Langmuir) and advanced equilibrium (monolayer model of one energy) models. Considering the steric properties, the structure of G.Zn@PN/BE demonstrated a higher density of active sites (Nm = 109.8 (20 °C), 108.9 (30 °C), and 67.8 mg/g (40 °C)) than BE and PN/BE. This declared the effect of the integration process in inducing the retention capacity by increasing the quantities of the active sites. The number of adsorbed As (V) ions per site (1.76 up to 2.13) signifies the retention of two or three ions per site by a multi-ionic mechanism. The adsorption energies (from −3.07 to −3.26 kJ/mol) suggested physical retention mechanisms (hydrogen bonding and dipole bonding forces). The adsorption energy, internal energy, and free enthalpy reflected the exothermic, feasible, and spontaneous nature of the retention process. The structure is of significant As (V) uptake capacity in the existence of competitive anions or metal ions.
Open AccessSynthesis and Characterization of Green ZnO@polynaniline/Bentonite Tripartite Structure (G.Zn@PN/BE) as Adsorbent for As (V) Ions: Integration, Steric, and Energetic Properties
A green ZnO@polynaniline/bentonite composite (G.Zn@PN/BE) was synthesized as an enhanced adsorbent for As (V) ions. Its adsorption properties were assessed in comparison with the integrated components of bentonite (BE) and polyaniline/bentonite (PN/BE) composites. The G.Zn@PN/BE composite achieved an As (V) retention capacity (213 mg/g) higher than BE (72.7 mg/g) and PN/BE (119.8 mg/g). The enhanced capacity of G.Zn@PN/BE was studied using classic (Langmuir) and advanced equilibrium (monolayer model of one energy) models. Considering the steric properties, the structure of G.Zn@PN/BE demonstrated a higher density of active sites (Nm = 109.8 (20 °C), 108.9 (30 °C), and 67.8 mg/g (40 °C)) than BE and PN/BE. This declared the effect of the integration process in inducing the retention capacity by increasing the quantities of the active sites. The number of adsorbed As (V) ions per site (1.76 up to 2.13) signifies the retention of two or three ions per site by a multi-ionic mechanism. The adsorption energies (from −3.07 to −3.26 kJ/mol) suggested physical retention mechanisms (hydrogen bonding and dipole bonding forces). The adsorption energy, internal energy, and free enthalpy reflected the exothermic, feasible, and spontaneous nature of the retention process. The structure is of significant As (V) uptake capacity in the existence of competitive anions or metal ions.