HZHaoyu Zuo

Haoyu Zuo

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Haoyu Zuo has a total of 13 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Study of the Design and Mechanical Properties of the Mix Proportion for Desulfurization Gypsum–Fly Ash Flowable Lightweight Soil

    by Xianglong Zuo, Shen Zuo, Jin Li, Ning Hou, Haoyu Zuo, Tiancheng Zhou

    In order to solve the global problem of bridge head jumping caused by the insufficient compaction of the roadbed in the transition section of highways and bridges, a desulfurization gypsum–fly ash flowable lightweight soil without vibration, capable of self-compaction, low bulk density, and economic and environmental protection, has been developed. This study selected low-grade cement, industrial waste (fly ash and desulfurization gypsum), and Yellow River silt as the raw materials for the design of the mix ratio of a desulfurization gypsum–fly ash flow-state lightweight soil mix. Through multiple indoor experiments, the influence of cement content, silt content, and the fly ash/desulfurization gypsum quality ratio on its fluidity and mechanical properties was systematically studied. The stress–strain relationship under uniaxial compression was analyzed and the strength formation mechanism was revealed through scanning electron microscopy (SEM). The results show that the mechanical properties of the prepared desulfurization gypsum–fly ash flowable lightweight soil meet the engineering requirements. Increasing both the cement and fly ash content results in the decreased fluidity of the desulfurization gypsum and fluidized fly ash. However, as the mass ratio of fly ash to desulfurization gypsum increases, the fluidity reaches its maximum when the mass ratio of fly ash to desulfurization gypsum is 2:1. Based on the stress–strain relationship test results, a uniaxial compressive constitutive model of the desulfurization gypsum–fly ash flowable lightweight soil was proposed. The model was fitted and analyzed with the test results, and the correlation was greater than 0.96. The high degree of agreement showed that desulfurization gypsum can promote the disintegration of fly ash, thereby increasing the specific surface area. This provides more contact points, promotes the hardening process, and enhances the interlocking force between particles and the formation of cementitious substances, further enhancing strength.


  • Open Access

    Identification Fluidity Method to Determine Suitability of Weathered and River Sand for Constructions Purposes

    by Haoyu Zuo, Jin Li, Li Zhu, Degang Cheng, De Chang

    At present, in order to comply with the development of the “the Belt and Road Initiatives”, the country is accelerating the pace of construction and increasing the demand for construction river sand. However, the quality of construction river sand is uncontrollable, and its shape is very similar to that of weathered sand. Therefore, using inferior weathered sand and mixed sand as inferior substitute sand in the market is prohibited, resulting in an increase in the difficulty coefficient of quality control of concrete fine aggregate in actual projects. This lays hidden dangers for the construction quality of the project. It is urgent to improve the quality control, testing, and detection process of river sand. Due to the long-term weathering of weathered sand, its density is small, and there are many pores, which leads to the material’s water absorption rate is higher than that of standard sand and river sand during fluidity tests. This paper takes this as a breakthrough point, reveals the variation law of fluidity loss under different variables, and explores a method for effectively screening low-quality sand and gravel. Through the silt content test (screening and washing method), the low-quality sand is preliminarily screened out, the mortar ratio is designed, and the fluidity test is carried out to compare the difference in fluidity loss of different types of mortar; determine the loss threshold range (mobility loss ≤ 15 mm) according to the mobility test results of the control group, and determine the qualification standard by comparing the measured mobility loss of the unknown sample with the loss threshold range. When the mobility loss is within the loss threshold range, the sample is qualified river sand. Otherwise, it is weathered sand or chowder sand. This method establishes a complete detection scheme for distinguishing weathered sand and river sand through mud content tests and mobility loss tests, solves the difficult problem of river sand quality control in engineering applications, and effectively eliminates the phenomenon of using low-quality weathered sand as river sand in the sand and gravel material market, thus avoiding congenital defects in concrete homogeneity.


  • Open Access

    Dynamic Strain Response of Hot-Recycled Asphalt Pavement under Dual-Axle Accelerated Loading Conditions

    by Jin Li, Yingyong Li, Chongsheng Xin, Haoyu Zuo, Ping An, Shen Zuo, Peng Liu

    Accelerated pavement testing (APT) is an effective method to study the long-term performance of pavement. Therefore, the dynamic strain behavior analysis of asphalt pavement has important guiding significance in the study of pavement failure modes. To explore the dynamic response of a high-content plant-mixed hot-reclaimed asphalt mixture under a dynamic load of vehicles, a full-scale test road was paved, and ALT biaxial accelerated loading test equipment was used to simulate the dynamic loads of vehicles. Based on parameters such as axle load, temperature, speed, and loading times, the development law for the bottom strain of the three pavement structures was analyzed. The test results show that the most unfavorable position of the asphalt pavement load is located just below the centerline of the wheel track on one side, and the damage effect of a single double-axle wheel load is far greater than that of two single-axle wheel loads. Then, the longitudinal tensile strain of the pavement bottom always maintains the alternating state of compression-tension and compression. The longitudinal tensile strain of the pavement bottom is larger than the transverse tensile strain, and transverse fatigue cracks appear first. Under normal temperature conditions, the bottom tensile strains of the three composite pavement structures under different axial loads are close, and the pavement performance of the hot-recycled asphalt pavement of structure A and structure B can meet the specification requirements. The relationship between the bottom strain and axle load is nonlinear and is directly related to the tire ground pressure, and the difference in the tensile and compressive strain values of the bottom of the three composite pavement structures is small. Under high temperature conditions, the bottom layer temperature of structure A and structure B is lower than that of structure C, and the thermal heat transfer efficiency of hot-recycled asphalt pavement is lower than that of ordinary asphalt pavement. Additionally, the longitudinal tensile strain is about 1–1.5 times that of the transverse tensile strain. Based on the Boltzmann function, the accumulative tensile strain prediction model was established to reflect the relationship between the cumulative strain at the bottom and the number of loads.