JLJaekwon Lee

Jaekwon Lee

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jaekwon Lee has a total of 14 co-authors. Here are the top co-authors by number of shared publications:

  • Can Bayram

    University of Illinois at Urbana-Champaign

    9 shared publications
  • Andrey E. Mironov

    Department of Electrical and Computer Engineering, University of Illinois 1 , Urbana, Illinois 61801, USA

    3 shared publications
  • Y. C. Chiu

    Department of Electrical and Computer Engineering, The Grainger College of Engineering, University of Illinois at Urbana-Champaign, Illinois 61801, USA and Nick Holonyak, Jr., Micro and Nanotechnology Laboratory, The Grainger College of Engineering, University of Illinois at Urbana-Champaign , Illinois 61801

    3 shared publications
  • Zhuoran Han

    Department of Electrical and Computer Engineering, Grainger College of Engineering, University of Illinois 1 , Urbana, Illinois 61801

    3 shared publications
  • Anik Mazumder

    Department of Electrical and Computer Engineering, Grainger College of Engineering, University of Illinois 1 , Urbana, Illinois 61801

    2 shared publications
  • Hubert N. Elly

    School of Electrical and Computer Engineering, Georgia Institute of Technology, Atlanta, GA, USA

    2 shared publications

Latest Publications

  • Ultrafast vertical photoconductive intrinsic diamond switch with high current (17.1 A at 1 kV)

    by Hubert Elly, Eric Cheng, Anik Mazumder, Zhuoran Han, Jaekwon Lee, Andrey Mironov, Can Bayram

    This Letter reports on a vertical, bulk-conducting photoconductive semiconductor switch (PCSS) fabricated on an intrinsic Type IIa single-crystal diamond substrate. Under near-bandgap excitation at 225 nm with a 20 μJ pulse, a strong photocurrent response of 17.1 A at 1 kV DC bias magnitude is obtained by (i) tuning the optical trigger wavelength to the “matched-absorption” window (224–235 nm) near the band edge, where the optical penetration depth becomes comparable to the 500 μm substrate thickness, and (ii) choosing the bias polarity ensuring electron-dominant conduction, given that electrons have a higher mobility than holes in diamond. The PCSS has an area-normalized responsivity of 54.2 mA W−1 cm−2 and an effective on-resistance of 8.48 Ω, with a fast 90%–10% transient fall time of 25 ns, attributed to carrier sweep-out. These results support vertical, bulk-conducting intrinsic diamond PCSS as a promising platform for high-power optical switching and provide new insight into intrinsic photoconductivity in diamond.

  • Efficiency cliff in scaling InGaN light-emitting diodes down to submicron

    by J. Lee, Y. C. Chiu, C. Bayram

    The top-down submicron fabrication of blue-emitting light-emitting diodes on Qromis Substrate Technology substrates is reported. Light-emitting diodes with mesa sizes as small as 250 × 250 nm2 show ideal forward voltage and low leakage current density. It is observed that sidewall treatment and passivation methods used in micro-light-emitting diodes (2–20 μm) do not lead to the same level of sidewall recombination suppression for submicron ones (<1 μm), as evidenced by a ∼70% decrease in peak external quantum efficiencies when mesa sizes are scaled from 2 μm down to 250 nm. This is attributed to the lateral carrier diffusion being comparable to the mesa size, regardless of the sidewall passivation and recovery. The results call for rethinking the impact of sidewalls in emerging top-down fabricated (sub)micrometer-light-emitting diodes.


  • Efficiency droop contributors in InGaN green light emitting diodes

    by P. Thirasuntrakul, J. Li, J. Lee, Y. C. Chiu, C. Bayram

    Here, efficiency droop contributors (i.e., inherent Auger–Meitner recombination, polarization-induced effects, thermal effects, and light extraction) in InGaN green light emitting diodes (LEDs) are decoupled and quantified. First, a modified ABC model is developed, and external quantum efficiency measurements are taken under constant and pulsed currents (EQEConstant and EQEPulsed, respectively). The LED internal quantum efficiency with and without thermal effects (IQEConstantABC and IQEPulsedABC, respectively) is extracted using the modified model. Then, using Raman spectroscopy, the LED junction temperature is extracted. Finally, using the optical-electrical model (OEM), the polarization- and temperature-independent LED internal quantum efficiency (IQEOEM) is calculated from the modified ABC model and the extracted junction temperature. By comparing external (EQEConstant) and the three internal quantum efficiencies (IQEConstantABC, IQEPulsedABC, and IQEOEM), the impacts of inherent Auger–Meitner recombination, polarization-induced effects, thermal effects, and light extraction on the efficiency droop are decoupled and quantified. It is found that inherent Auger–Meitner recombination-induced droop is approximately 49% of the total efficiency droop in commercial green LEDs, while polarization-induced effects contribute about 35%, and thermal droop accounts for nearly 16%. These findings suggest, to quash the green gap, it is critical to search for materials and device designs with low inherent Auger–Meitner coefficients and polarization fields, respectively.


  • Record performance in intrinsic, impurity-free lateral diamond photoconductive semiconductor switches

    by Zhuoran Han, Jaekwon Lee, Anik Mazumder, Hubert Elly, Stephen Messing, Andrey Mironov, Can Bayram

    Photoconductive semiconductor switches (PCSSs) are fabricated on type IIa diamond substrates with varying boron and nitrogen impurity levels (<1014–1016 cm−3). The photoresponse of lateral PCSS is reported over the incident laser wavelength range (212–240 nm), energy per pulse (5–65 μJ), and DC bias (−1.2 to +1.2 kV). The PCSS device with the lowest boron and nitrogen impurity concentration achieves the highest normalized responsivity of 9.1 × 10−8 A-cm/W-V, peak photocurrent of 8.0 A, and on/off ratio of 2.3 × 1011 at a DC bias of +1.2 kV with the potential for even higher currents at increased DC bias. All PCSS display fast rise times (<3 ns), limited by the laser's rise time. However, photoresponse measurements reveal that higher impurity levels reduce the photocurrent and decrease the on/off ratio. These results highlight the performance advantages of using low background concentration type IIa diamond substrates for PCSS fabrication and present a promising route toward advanced high-power, high-speed diamond-based switches.


  • Open Access

    High Field Transport in (Ultra) Wide Bandgap Semiconductors: Diamond Versus Cubic GaN

    by Jaekwon Lee, Can Bayram, Jean-Pierre Leburton

    We provide an analysis of nonlinear transport in diamond and cubic GaN (c-GaN) with emphasis on the different types of optical phonon scattering [i.e., optical deformation potential (ODP) scattering versus polar optic phonon (POP) scattering] limiting the carrier velocity. Both types of carrier mobilities and carrier saturation (peak) velocities in diamond and c-GaN as functions of different doping types and concentrations are obtained by directly solving the Boltzmann equation. Our model indicates that the nonrandomizing nature of POP scattering causes carrier temperature cooling, resulting in higher carrier drift velocity than with ODP scattering. This effect, in addition to the small carrier effective masses and large optical phonon energies, is responsible for the higher peak velocities in c-GaN, compared to carrier drift velocity in diamond.


  • Open Access

    High Current Density Diamond Photoconductive Semiconductor Switches With a Buried, Metallic Conductive Channel

    by Zhuoran Han, Jaekwon Lee, Stephen Messing, Thomas Reboli, Andrey Mironov, Can Bayram

    Laterally configured diamond photoconductive semiconductor switches (PCSS) with a buried, metallic p+ current channel are reported. Above bandgap ( $\lambda \le 226$ nm) optical triggering enables responsivity of over 130 mA/W. The use of low-impurity semi-insulating diamond as an active absorption layer enables fast rise and fall times (~2 ns) and on/off ratios greater than 1011. The PCSS excited with a laser energy of 20 nJ per pulse passes a high current density (44 A/cm) under a DC bias of 60 V, thanks to the buried metallic p+ current channel. The reported devices promise high current carrying capacity without the need for filamenting while leveraging the excellent optical, electronic, and thermal properties of diamond.


  • Green-emitting cubic GaN/In0.16Ga0.84N/GaN quantum well with 32% internal quantum efficiency at room temperature

    by J. Lee, C. Bayram

    Structural and optical properties of a green-emitting cubic (i.e., zinc blende) GaN/In0.16Ga0.84N/GaN single quantum well structure are reported. The active layer is grown on a phase-pure (i.e., 100%) cubic GaN enabled on a 1 × 1 cm2 U-grooved silicon (100) through aspect ratio phase trapping. Energy dispersive x-ray spectroscopy combined with room temperature cathodoluminescence reveals 522 nm green light emission at room temperature with only 16.0% ± 1.6% of indium content, which is ∼30% less than the amount of indium needed in a traditional green-emitting hexagonal (i.e., wurtzite) well. Temperature-dependent behavior of the green emission, such as activation energy, s-shaped peak energy shift, and linewidth, is reported. Cathodoluminescence at 8 and 300 K reveals an internal quantum efficiency of 32.0% ± 0.6%, which is higher than any reported value for cubic wells. Overall, phase-pure cubic active layers on phase transition cubic GaN are shown to be promising for green and longer wavelength emitters.


  • Design tradeoffs between traditional hexagonal and emerging cubic InXGa(1–X)N/GaN-based green light-emitting diodes

    by Jaekwon Lee, Jean-Pierre Leburton, Can Bayram

    Here, we report on the design tradeoffs between traditional hexagonal and emerging cubic InXGa(1−X)N/GaN-based green (520nm≤λ≤550nm) light-emitting diodes with special emphasis on the electron blocking layer, number of quantum wells, and thicknesses of quantum wells and barriers. We identified three crucial design rules for cubic green light-emitting diodes: (1) no need for an electron blocking layer; (2) use of a wide quantum well; and (3) choice of thin quantum barriers in multi-quantum well light-emitting diode designs. These design rules increase the internal quantum efficiency of cubic green light-emitting diodes by ∼30.5% under 100A/cm2 injection with respect to traditional designs. Overall, the design rules of cubic light-emitting diodes and their differentiating nature from the traditional, hexagonal ones are crucial for the advent of next-generation cubic light-emitting diodes.


  • Open Access

    Structural and optical properties of cubic GaN on U-grooved Si (100)

    by J. Lee, Y. C. Chiu, M. A. Johar, C. Bayram

    Cubic GaN epitaxy on large-area U-grooved silicon (100) dies is demonstrated by metalorganic chemical vapor deposition, and its structural and optical properties are reported. Scanning electron, atomic force, and transmission electron microscopy studies reveal that cubic GaN shows no discernible threading dislocations and a low stacking fault density of 3.27 ± 0.18 × 104 cm−1. Temperature-dependent photoluminescence studies reveal as-grown cubic GaN band edge emission internal quantum efficiency as 25.6% ± 0.9%. Selective etching of the low-temperature AlN buffer layer, SiO2 sidewalls, and hexagonal-phase GaN is demonstrated, which increases the cubic GaN band edge emission internal quantum efficiency to 31.6% ± 0.8%. This increase is attributed to the decrease in the radiative recombination lifetime via the removal of defective hexagonal-phase GaN. Overall, cubic GaN on U-grooved silicon with high structural and optical quality is reported, promising its suitability for next-generation devices.