Wen Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Wen Wang has a total of 99 co-authors. Here are the top co-authors by number of shared publications:
Kuaishe Wang
School of Metallurgical Engineering, National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an University of Architecture and Technology, Xi’an, P.R. China
8 shared publications- Kuaishe Wang
School of Metallurgy Engineering, Xi’an University of Architecture and Technology, Xi’an, China
7 shared publications Fengming Qiang
School of Metallurgical Engineering, National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an University of Architecture and Technology, Xi’an, P.R. China
6 shared publicationsPeng Han
School of Metallurgical Engineering, National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an University of Architecture and Technology, Xi’an, P.R. China
6 shared publicationsKe Qiao
School of Metallurgical Engineering, National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an University of Architecture and Technology, Xi’an, P.R. China
5 shared publications- Ke Qiao
School of Metallurgical Engineering, National and Local Joint Engineering Research Center for Functional Materials Processing, Xi’an University of Architecture and Technology, Xi’an, China
5 shared publications
Latest Publications
- 6 August 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (38) , 39241-39266
Recent Progress in TiC Particle-Modified Aluminum Matrix Composites Fabricated by Selective Laser Melting: Processes, Microstructures, and Properties
- 6 August 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (38) , 39241-39266
Recent Progress in TiC Particle-Modified Aluminum Matrix Composites Fabricated by Selective Laser Melting: Processes, Microstructures, and Properties
- Open Access
- 30 March 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (5) , 2528-2546
Microstructure, Tensile Properties, and Superplasticity of the Large-Area Fine-Grained Ti–6Al–4V Alloy Sheets Prepared by Multi-pass Friction Stir Processing
- 30 March 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (5) , 2528-2546
Open AccessMicrostructure, Tensile Properties, and Superplasticity of the Large-Area Fine-Grained Ti–6Al–4V Alloy Sheets Prepared by Multi-pass Friction Stir Processing
- Open Access
- 21 November 2025
- Published by Springer Nature in Advanced Composites and Hybrid Materials
- Vol. 8 (6)
Microstructure evolution and mechanical properties of high entropy alloy reinforced titanium matrix composites processed by cold spray-friction stir processing composite additive manufacturing
- 21 November 2025
- Published by Springer Nature in Advanced Composites and Hybrid Materials
- Vol. 8 (6)
Open AccessMicrostructure evolution and mechanical properties of high entropy alloy reinforced titanium matrix composites processed by cold spray-friction stir processing composite additive manufacturing
- 24 October 2025
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (6) , 7080-7095
Large-Area AA6061 Alloy Sheets Prepared via Multi-pass Particles-Based Additive Friction Stir Deposition
- 24 October 2025
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (6) , 7080-7095
Large-Area AA6061 Alloy Sheets Prepared via Multi-pass Particles-Based Additive Friction Stir Deposition
- 26 May 2025
- Published by Springer Nature in Journal of Materials Science
- Vol. 60 (21) , 8870-8889
Hot deformation behavior and microstructural evolution of as-cast TC4 titanium alloy
- 26 May 2025
- Published by Springer Nature in Journal of Materials Science
- Vol. 60 (21) , 8870-8889
Hot deformation behavior and microstructural evolution of as-cast TC4 titanium alloy
- Open Access
Coupled Temperature–Flow Field and Microstructure Numerical Simulation of the Solidification Process for Cu-3Ti-0.2Fe Alloy
This work investigates the time-dependent changes in temperature, flow, and solidification microstructure under various cooling conditions. The mechanism of the effects of different pouring temperatures on the morphology and evolution of the solidification microstructure is explored. During gradual cooling, the temperature distribution remained consistent and the solid–liquid interface extended to its furthest extent. In contrast, water cooling generated the most pronounced temperature gradient at the solidification front, which was conducive to the development of columnar grains. Specifically, the maximum solidification rates at the center of the casting under the water-cooled copper mold, copper mold, and ceramic mold conditions were 2.71 mm/s, 1.45 mm/s, and 0.95 mm/s, respectively, with water cooling achieving the fastest rate. In the early stages of solidification, the flow velocity at the casting center was relatively high, and during slow cooling, the molten material tended to flow toward the surface. When air cooling was applied, the molten material at the center migrated outward, while under water cooling, the fluid moved in an upward direction. At a heat transfer coefficient of 100 W/(m2·K), the alloy primarily formed equiaxed grains; however, at 5000 W/(m2·K), the proportion of columnar grains increased significantly, and the average grain area expanded from 3.664 × 10−6 m2 to 4.441 × 10−6 m2. Additionally, as the pouring temperature increased from 1100 °C to 1200 °C, the number of grains decreased, while the average radius grew from 1.665 × 10−3 m to 1.820 × 10−3 m, resulting in a reduced fraction of equiaxed grains. This study provides valuable theoretical insights for optimizing the solidification process of this particular alloy.
Open AccessCoupled Temperature–Flow Field and Microstructure Numerical Simulation of the Solidification Process for Cu-3Ti-0.2Fe Alloy
This work investigates the time-dependent changes in temperature, flow, and solidification microstructure under various cooling conditions. The mechanism of the effects of different pouring temperatures on the morphology and evolution of the solidification microstructure is explored. During gradual cooling, the temperature distribution remained consistent and the solid–liquid interface extended to its furthest extent. In contrast, water cooling generated the most pronounced temperature gradient at the solidification front, which was conducive to the development of columnar grains. Specifically, the maximum solidification rates at the center of the casting under the water-cooled copper mold, copper mold, and ceramic mold conditions were 2.71 mm/s, 1.45 mm/s, and 0.95 mm/s, respectively, with water cooling achieving the fastest rate. In the early stages of solidification, the flow velocity at the casting center was relatively high, and during slow cooling, the molten material tended to flow toward the surface. When air cooling was applied, the molten material at the center migrated outward, while under water cooling, the fluid moved in an upward direction. At a heat transfer coefficient of 100 W/(m2·K), the alloy primarily formed equiaxed grains; however, at 5000 W/(m2·K), the proportion of columnar grains increased significantly, and the average grain area expanded from 3.664 × 10−6 m2 to 4.441 × 10−6 m2. Additionally, as the pouring temperature increased from 1100 °C to 1200 °C, the number of grains decreased, while the average radius grew from 1.665 × 10−3 m to 1.820 × 10−3 m, resulting in a reduced fraction of equiaxed grains. This study provides valuable theoretical insights for optimizing the solidification process of this particular alloy.
- Open Access
- 15 May 2025
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 38 (8) , 1436-1452
Amelioration of Mechanical Properties of Rolled Mg-4.5Al-2.5Zn Alloy by Cryogenic Cycling Treatment
- 15 May 2025
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 38 (8) , 1436-1452
Open AccessAmelioration of Mechanical Properties of Rolled Mg-4.5Al-2.5Zn Alloy by Cryogenic Cycling Treatment
- Open Access
Insight into Grain Refinement Mechanisms of WC Cemented Carbide with Al0.5CoCrFeNiTi0.5 Binder
High-entropy alloys (HEA) as a kind of new binder for cemented carbide have garnered significant attention. In this work, WC/(17~25 wt.%)Al0.5CoCrFeNiTi0.5 cemented carbides were prepared by hot pressing sintering (HPS), and the reactions between WC powder and Al0.5CoCrFeNiTi0.5 powder during hot pressing sintering were elucidated. It found that different from traditional Co binder, the Al0.5CoCrFeNiTi0.5 binder effectively inhibited WC grain growth. During HPS, the decomposed W and C atoms from WC diffused into the Al0.5CoCrFeNiTi0.5 binder, reacted with the elements in the binder, and then formed the M(Co, Fe, Ni)3W3C phase. The back-diffusion of W and C atoms to WC grains was restricted by the Al0.5CoCrFeNiTi0.5 alloy and inhibited them from re-precipitating onto the large undissolved WC grains. As a result, the average size of WC grains in the cemented carbides was less than 200 nm. This work bright new insight into the grain refinement mechanisms of WC cemented carbide with HEA binder and provide a guidance for designing performance-stable WC/HEA cemented carbide and promoting their application.
Open AccessInsight into Grain Refinement Mechanisms of WC Cemented Carbide with Al0.5CoCrFeNiTi0.5 Binder
High-entropy alloys (HEA) as a kind of new binder for cemented carbide have garnered significant attention. In this work, WC/(17~25 wt.%)Al0.5CoCrFeNiTi0.5 cemented carbides were prepared by hot pressing sintering (HPS), and the reactions between WC powder and Al0.5CoCrFeNiTi0.5 powder during hot pressing sintering were elucidated. It found that different from traditional Co binder, the Al0.5CoCrFeNiTi0.5 binder effectively inhibited WC grain growth. During HPS, the decomposed W and C atoms from WC diffused into the Al0.5CoCrFeNiTi0.5 binder, reacted with the elements in the binder, and then formed the M(Co, Fe, Ni)3W3C phase. The back-diffusion of W and C atoms to WC grains was restricted by the Al0.5CoCrFeNiTi0.5 alloy and inhibited them from re-precipitating onto the large undissolved WC grains. As a result, the average size of WC grains in the cemented carbides was less than 200 nm. This work bright new insight into the grain refinement mechanisms of WC cemented carbide with HEA binder and provide a guidance for designing performance-stable WC/HEA cemented carbide and promoting their application.
- 13 August 2024
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 37 (11) , 1947-1960
Microstructure Evolution and Recrystallized Behavior of Friction Stir Welding Twin-Induced Plasticity Steel
- 13 August 2024
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 37 (11) , 1947-1960
Microstructure Evolution and Recrystallized Behavior of Friction Stir Welding Twin-Induced Plasticity Steel