Mathews Lima dos Santos
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Mathews Lima dos Santos has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Tiago Felipe de Abreu Santos
Universidade Federal de Pernambuco
5 shared publications - Renato Alexandre Costa de Santana
Department of Mechanical Engineering, Federal University of Campina Grande, Campina Grande, Brazil
4 shared publications - Ivan Bezerra de Mello Picchi
Department of Mechanical Engineering, Universidade Federal de Pernambuco, Recife, Brazil
3 shared publications - Theophilo Moura Maciel
Universidade Federal de Campina Grande, Brasil
3 shared publications - Edwar Andrés Torres López
Universidad de Antioquía
2 shared publications - Guilherme Gadelha de Sousa Figueiredo
Department of Mechanical Engineering SOLDAMAT Research Group Universidade Federal de Pernambuco Arquitetura Av. Recife Pernambuco Brazil
2 shared publications
Latest Publications
- 22 January 2026
- Published by Elsevier in Surfaces and Interfaces
- Vol. 83
Influence of cold-wire GTAW parameters on bead geometry in austenitic stainless steel coatings
- 22 January 2026
- Published by Elsevier in Surfaces and Interfaces
- Vol. 83
Influence of cold-wire GTAW parameters on bead geometry in austenitic stainless steel coatings
- Open Access
Influence of Centerline Segregation Region on the Hydrogen Embrittlement Susceptibility of API 5L X80 Pipeline Steels
The influence of the centerline segregation region (CSR) on the hydrogen embrittlement (HE) of two different API 5L X80 pipeline steel plates was investigated. The novelty of this work was to establish relationships between the CSR, microstructure, and distribution of localized fragile particles on HE susceptibility and on fracture morphology. This work intended to establish a relationship between centerline segregation and HE susceptibility in high-strength low-alloy steels submitted to inhomogeneous transformations. Microscopy, hydrogen permeation, and slow strain rate (SSR) tests were used to investigate hydrogen-related degradation. The solution used on the charging cell of the permeation tests—and on the SSR test cell—was 0.5 mol L−1 H2SO4 + 10 mg L−1 As2O3, and in the oxidation cell, 0.1 M NaOH was used as a solution. The CSR led the thicker plate to present the highest HE index (0.612) in analyses carried out in the mid-thickness; however, the same plate showed the lowest HE index in near-surface tests. The presence of hydrogen changed the fracture morphology from ductile to a brittle and ductile feature; this occurred due to the interaction with localized fragile particles and the significant reduction of the shear stress necessary for the dislocation movement.
Open AccessInfluence of Centerline Segregation Region on the Hydrogen Embrittlement Susceptibility of API 5L X80 Pipeline Steels
The influence of the centerline segregation region (CSR) on the hydrogen embrittlement (HE) of two different API 5L X80 pipeline steel plates was investigated. The novelty of this work was to establish relationships between the CSR, microstructure, and distribution of localized fragile particles on HE susceptibility and on fracture morphology. This work intended to establish a relationship between centerline segregation and HE susceptibility in high-strength low-alloy steels submitted to inhomogeneous transformations. Microscopy, hydrogen permeation, and slow strain rate (SSR) tests were used to investigate hydrogen-related degradation. The solution used on the charging cell of the permeation tests—and on the SSR test cell—was 0.5 mol L−1 H2SO4 + 10 mg L−1 As2O3, and in the oxidation cell, 0.1 M NaOH was used as a solution. The CSR led the thicker plate to present the highest HE index (0.612) in analyses carried out in the mid-thickness; however, the same plate showed the lowest HE index in near-surface tests. The presence of hydrogen changed the fracture morphology from ductile to a brittle and ductile feature; this occurred due to the interaction with localized fragile particles and the significant reduction of the shear stress necessary for the dislocation movement.
- 21 October 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 129 (7-8) , 3073-3092
Parametric study and response optimization for the wire + arc additive manufacturing of 316LSi via pulsed GMAW
- 21 October 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 129 (7-8) , 3073-3092
Parametric study and response optimization for the wire + arc additive manufacturing of 316LSi via pulsed GMAW
- 10 August 2023
- Published by Springer Nature in Welding in the World
- Vol. 67 (11) , 2571-2587
Microstructure characterization of the weld cladding of clad steel plate A516 GR.70 - AISI 904L by electroslag strip cladding using Inconel 625 strip
- 10 August 2023
- Published by Springer Nature in Welding in the World
- Vol. 67 (11) , 2571-2587
Microstructure characterization of the weld cladding of clad steel plate A516 GR.70 - AISI 904L by electroslag strip cladding using Inconel 625 strip
- 1 January 2023
- Published by Even3 in Anais Do Congresso Internacional de Engenharia Mecânica E Industrial
- Vol. 1
PROJETO FUTURAS CIENTISTAS E OS DESAFIOS NO ENSINO DE ENGENHARIA
Anais do Congresso Internacional de Engenharia Mecânica e Industrial (2764-4294) - Projeto Futuras Cientistas E Os Desafios No Ensino De Engenharia
- 1 January 2023
- Published by Even3 in Anais Do Congresso Internacional de Engenharia Mecânica E Industrial
- Vol. 1
PROJETO FUTURAS CIENTISTAS E OS DESAFIOS NO ENSINO DE ENGENHARIA
Anais do Congresso Internacional de Engenharia Mecânica e Industrial (2764-4294) - Projeto Futuras Cientistas E Os Desafios No Ensino De Engenharia
- Open Access
- 1 January 2022
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 27
Uma Contribuição para o Entendimento da Influência das Tensões Residuais na Fragilização por Hidrogênio em Aços API 5L
Resumo Materiais, quando sob carregamento em ambientes agressivos, como é o caso dos aços de tubulações no setor de petróleo e gás, estão sujeitos à fragilização por hidrogênio devido às condições ambientais. A susceptibilidade do tubo a tal fragilização está diretamente relacionada, entre outros fatores, ao nível de tensões residuais presentes; e impõe ao material severas e danosas reduções de propriedades mecânicas. Nesse contexto, devido à necessidade cada vez mais frequente de evitar falhas catastróficas que conduzem a perdas irreparáveis para os seres humanos e o ambiente, são destinados maciços investimentos para o aprimoramento das propriedades mecânicas e grandes esforços para compreender os mecanismos que levam aos danos causados pelo hidrogênio. A compreensão do efeito das tensões residuais originadas pelos diferentes processos ao qual o aço é submetido ainda é bastante escassa e nem sempre há uma unanimidade entre pesquisadores. Diante desta problemática, o presente trabalho, através de uma revisão bibliográfica, objetiva oferecer uma abordagem de como as tensões residuais podem afetar o nível de fragilização nos aços API 5L, bem como uma melhor compreensão dos mecanismos e dos fatores que facilitam a dissolução do hidrogênio na rede cristalina destes materiais.
- 1 January 2022
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 27
Open AccessUma Contribuição para o Entendimento da Influência das Tensões Residuais na Fragilização por Hidrogênio em Aços API 5L
Resumo Materiais, quando sob carregamento em ambientes agressivos, como é o caso dos aços de tubulações no setor de petróleo e gás, estão sujeitos à fragilização por hidrogênio devido às condições ambientais. A susceptibilidade do tubo a tal fragilização está diretamente relacionada, entre outros fatores, ao nível de tensões residuais presentes; e impõe ao material severas e danosas reduções de propriedades mecânicas. Nesse contexto, devido à necessidade cada vez mais frequente de evitar falhas catastróficas que conduzem a perdas irreparáveis para os seres humanos e o ambiente, são destinados maciços investimentos para o aprimoramento das propriedades mecânicas e grandes esforços para compreender os mecanismos que levam aos danos causados pelo hidrogênio. A compreensão do efeito das tensões residuais originadas pelos diferentes processos ao qual o aço é submetido ainda é bastante escassa e nem sempre há uma unanimidade entre pesquisadores. Diante desta problemática, o presente trabalho, através de uma revisão bibliográfica, objetiva oferecer uma abordagem de como as tensões residuais podem afetar o nível de fragilização nos aços API 5L, bem como uma melhor compreensão dos mecanismos e dos fatores que facilitam a dissolução do hidrogênio na rede cristalina destes materiais.