Shweta Tomer
Research Subjects
Shweta Tomer has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
Vandana
3 shared publicationsAbhishek Kumar
Natl Phys Lab, Adv Mat & Devices Metrol Div, PV Metrol Grp, New Delhi 110012, India
2 shared publications- Abhishek Kumar
Academy of Scientific and Innovative Research (AcSIR), Ghaziabad, India
2 shared publications Meenakshi Devi
Natl Phys Lab, Adv Mat & Devices Metrol Div, PV Metrol Grp, New Delhi 110012, India
2 shared publications- Meenakshi Devi
Photovoltaic Metrology Division, CSIR-National Physical Laboratory, New Delhi, India
2 shared publications - Preetam Singh
CSIR-National Physical Laboratory, Dr K S Krishnan Marg, New Delhi, 110012, India
2 shared publications
Latest Publications
- 29 February 2024
- Published by Elsevier in Surfaces and Interfaces
- Vol. 47
Study of silicon surface passivation by ZnOx/AlOx stack prepared using super-cycle approach in thermal ALD process
- 29 February 2024
- Published by Elsevier in Surfaces and Interfaces
- Vol. 47
Study of silicon surface passivation by ZnOx/AlOx stack prepared using super-cycle approach in thermal ALD process
- 1 August 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 13 (5) , 691-698
High-Quality Silicon Surface Passivation by Thermal-ALD Deposited Hafnium Oxide Films
Excellent silicon surface passivation is achieved by atomic layer deposition (ALD) grown hafnium oxide (HfO x ) films on silicon surfaces (both n-type and p-type). It is inferred from the study that the silicon surface passivation by HfO x thin films is a film-thickness-dependent quality and a minimum film thickness of ∼2 nm is essential to passivate the silicon surface. A good level of surface passivation (surface recombination velocity, SRV< 20 cm/s) can be achieved for film thickness, d >5 nm. However, the best results are obtained for hydrogen-annealed, ∼8.5-nm-thin HfO x films. SRV as low as 3.5 cm/s (effective minority carrier lifetime, τ eff ∼5 ms) and 4.4 cm/s (τ eff ∼4 ms) are realized on p-type and n-type silicon surfaces, respectively. The injection level dependence of τ eff reveals that HfO x films provide better passivation for n-type silicon compared to p-type silicon at low injection levels. Hydrogen present in the annealing ambient first saturates the dangling bonds at the film/silicon interface and then affects the oxide charge density. Effective oxide charge density is positive in HfO x /n-Si samples and negative in HfO x /p-Si samples. This creates an accumulation condition near the silicon surface for both substrate-type situations and is responsible for effective passivation in both types of substrates. Thus, our study demonstrates that ALD-grown HfO x films offer excellent passivation for silicon surfaces.
- 1 August 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 13 (5) , 691-698
High-Quality Silicon Surface Passivation by Thermal-ALD Deposited Hafnium Oxide Films
Excellent silicon surface passivation is achieved by atomic layer deposition (ALD) grown hafnium oxide (HfO x ) films on silicon surfaces (both n-type and p-type). It is inferred from the study that the silicon surface passivation by HfO x thin films is a film-thickness-dependent quality and a minimum film thickness of ∼2 nm is essential to passivate the silicon surface. A good level of surface passivation (surface recombination velocity, SRV< 20 cm/s) can be achieved for film thickness, d >5 nm. However, the best results are obtained for hydrogen-annealed, ∼8.5-nm-thin HfO x films. SRV as low as 3.5 cm/s (effective minority carrier lifetime, τ eff ∼5 ms) and 4.4 cm/s (τ eff ∼4 ms) are realized on p-type and n-type silicon surfaces, respectively. The injection level dependence of τ eff reveals that HfO x films provide better passivation for n-type silicon compared to p-type silicon at low injection levels. Hydrogen present in the annealing ambient first saturates the dangling bonds at the film/silicon interface and then affects the oxide charge density. Effective oxide charge density is positive in HfO x /n-Si samples and negative in HfO x /p-Si samples. This creates an accumulation condition near the silicon surface for both substrate-type situations and is responsible for effective passivation in both types of substrates. Thus, our study demonstrates that ALD-grown HfO x films offer excellent passivation for silicon surfaces.
- 21 July 2023
- Published by Elsevier in Surfaces and Interfaces
- Vol. 41
ALD deposited bipolar HfOx films for silicon surface passivation
- 21 July 2023
- Published by Elsevier in Surfaces and Interfaces
- Vol. 41
ALD deposited bipolar HfOx films for silicon surface passivation
- 24 August 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (24) , 36556-36569
Heterostructure nanoarchitectonics with ZnO/SnO2 for ultrafast and selective detection of CO gas at low ppm levels
- 24 August 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (24) , 36556-36569
Heterostructure nanoarchitectonics with ZnO/SnO2 for ultrafast and selective detection of CO gas at low ppm levels
- 24 September 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (6) , 1614-1623
Silicon Surface Passivation by Atomic Layer Deposited Hafnium Oxide Films: Trap States Investigation Using Constant Voltage Stress Studies
Excellent silicon surface passivation is demonstrated by the HfO $_\text{x}$ film deposited using optimized atomic layer deposition (ALD) process. For pristine films, surface recombination velocity (SRV) as low as ∼29 cm/s is achieved. The highest effective lifetime of 3 ms, corresponding to SRV of ∼5 cm/s, is achieved for hydrogen ambient annealed films. Capacitance–voltage and conductance–voltage measurements confirm that the pristine film consists of positive fixed charges, which remain of the same type or change polarity depending on the postdeposition annealing ambient. Constant voltage stress (CVS) measurements reveal that acceptor-like trap states are present in the film. These trap states are intrinsic in nature and are incorporated in the film structure during ALD growth. CVS study gives an insight to the change in fixed charge polarity in nitrogen ambient annealing, which is not the case in hydrogen ambient. The reduction in surface recombination losses is explained as a combined effect of field and chemical passivation where former dominates in nitrogen and later is dominant in hydrogen ambient annealed films.- 24 September 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (6) , 1614-1623
Silicon Surface Passivation by Atomic Layer Deposited Hafnium Oxide Films: Trap States Investigation Using Constant Voltage Stress Studies
Excellent silicon surface passivation is demonstrated by the HfO $_\text{x}$ film deposited using optimized atomic layer deposition (ALD) process. For pristine films, surface recombination velocity (SRV) as low as ∼29 cm/s is achieved. The highest effective lifetime of 3 ms, corresponding to SRV of ∼5 cm/s, is achieved for hydrogen ambient annealed films. Capacitance–voltage and conductance–voltage measurements confirm that the pristine film consists of positive fixed charges, which remain of the same type or change polarity depending on the postdeposition annealing ambient. Constant voltage stress (CVS) measurements reveal that acceptor-like trap states are present in the film. These trap states are intrinsic in nature and are incorporated in the film structure during ALD growth. CVS study gives an insight to the change in fixed charge polarity in nitrogen ambient annealing, which is not the case in hydrogen ambient. The reduction in surface recombination losses is explained as a combined effect of field and chemical passivation where former dominates in nitrogen and later is dominant in hydrogen ambient annealed films.