Cheng-Yuan Hung
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Cheng-Yuan Hung has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Chien-Ming Kang
Huayi Dental Laboratory, Taipei 10491, Taiwan
1 shared publication - Dan-Jae Lin
Department of Biomedical Engineering, College of Biomedical Engineering, China Medical University, Taichung 40402, Taiwan
1 shared publication - Sheng-Wei Feng
School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei 110301, Taiwan
1 shared publication - Shogo Iwaguro
Division of Dental Technician, Department of Clinical Practice and Support, Hiroshima University Hospital, Hiroshima 734-8551, Japan
1 shared publication - Tzu-Yu Peng
School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei 110301, Taiwan
1 shared publication
Latest Publications
- Open Access
- 24 October 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (21) , 12783
Innovation Glass-Ceramic Spray Deposition Technology Improving the Adhesive Performance for Zirconium-Based Dental Restorations
Glass-ceramic spray deposition (GCSD) is a novel technique for coating lithium disilicate (LD) glass-ceramics onto zirconia through simple tempering steps. GCSD has been proven to improve the bonding of zirconia to resin cement, but the effect of etching time on GCSD and the long-term durability of the bond achieved remain unknown. The effects of air abrasion with aluminum particles (ABB) and air abrasion (GAB) or etching with 5.0% hydrogen fluoride (HF) for 20, 60, 90, and 120 s (G20, G60, G90, and G120) on the resin cement–zirconia bond were studied. LD was included as a control (LDG). The microstructure, sub-micron roughness, wettability, and phase changes of samples were analyzed. After resin cement was bonded to zirconia, half of the samples were subjected to thermocycling (5000 cycles at 5–55 °C). The bond strengths of the samples were determined in shear bond strength (SBS) tests (n = 10 per group). An LD structure can be formed on zirconia after GCSD and proper etching processes, which result in high roughness and a hydrophilic nature. GCSD and HF etching significantly improved SBS, with G90 and G120 samples with pre- or post-thermocycling exhibiting SBS values comparable to those of LDG (p > 0.760). The surface characteristics of the LD layer are influenced by the etching time and affect the SBS of the bond of zirconia to resin cement. HF etching for 90–120 s after GCSD results in zirconia with SBS and bond durability comparable to LD.
- 24 October 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (21) , 12783
Open AccessInnovation Glass-Ceramic Spray Deposition Technology Improving the Adhesive Performance for Zirconium-Based Dental Restorations
Glass-ceramic spray deposition (GCSD) is a novel technique for coating lithium disilicate (LD) glass-ceramics onto zirconia through simple tempering steps. GCSD has been proven to improve the bonding of zirconia to resin cement, but the effect of etching time on GCSD and the long-term durability of the bond achieved remain unknown. The effects of air abrasion with aluminum particles (ABB) and air abrasion (GAB) or etching with 5.0% hydrogen fluoride (HF) for 20, 60, 90, and 120 s (G20, G60, G90, and G120) on the resin cement–zirconia bond were studied. LD was included as a control (LDG). The microstructure, sub-micron roughness, wettability, and phase changes of samples were analyzed. After resin cement was bonded to zirconia, half of the samples were subjected to thermocycling (5000 cycles at 5–55 °C). The bond strengths of the samples were determined in shear bond strength (SBS) tests (n = 10 per group). An LD structure can be formed on zirconia after GCSD and proper etching processes, which result in high roughness and a hydrophilic nature. GCSD and HF etching significantly improved SBS, with G90 and G120 samples with pre- or post-thermocycling exhibiting SBS values comparable to those of LDG (p > 0.760). The surface characteristics of the LD layer are influenced by the etching time and affect the SBS of the bond of zirconia to resin cement. HF etching for 90–120 s after GCSD results in zirconia with SBS and bond durability comparable to LD.