MHMarion Herrmann

Marion Herrmann

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Marion Herrmann has a total of 15 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Direct laser active brazing of 316Ti to alumina

    by Jian Feng, Marion Herrmann, Antonio Hurtado

    This work addresses the challenges in brazing thermohydraulic sealings involving dissimilar materials, specifically 316Ti stainless steel and alumina, which have significantly different coefficients of thermal expansion (CTEs) and elastic constants. Traditional brazing methods require complex interlayers or extensive metallization steps, leading to issues such as dimensional changes, braze voids, and inadequate corrosion resistance due to prolonged high‐temperature exposure. A novel laser‐based brazing technique utilizing a diode laser is introduced to create high‐quality, localized joints while preserving the integrity of the parent materials. The study systematically optimizes laser process parameters using finite‐element modeling and the Taguchi method to achieve the desired bead geometry and thermal stress distribution with minimal heat input. Comparative analysis between laser active brazing (LAB) and conventional furnace brazing was conducted through metallography, shear testing, and autoclave testing. Results indicate that LAB parameters significantly affect bead thickness and shear strength, with laser‐brazed joints demonstrating superior quality and stability post‐autoclave testing compared with furnace‐brazed joints. The thermodynamic and kinetic aspects of the brazing process were also analyzed. In conclusion, the LAB method for brazing 316Ti to alumina proves to be a successful and efficient alternative, with joint properties meeting or exceeding those of traditional furnace brazing.


  • Open Access

    Active Brazing for Energy Devices Sealing

    by Jian Feng, Marion Herrmann, Anne-Maria Reinecke, Antonio Hurtado

    The pursuit of reliable energy devices sealing solutions stands as a paramount engineering challenge for ensuring energy safety and dependability. This review focuses on an examination of recent scientific publications, primarily within the last decade, with a central aim to grasp and apply critical concepts relevant to the efficient design and specification of brazements for ceramic–metal active-brazed assemblies, emphasizing the sealing of energy devices. The goal is to establish robust and enduring joints capable of withstanding water-vapor and hydrogen environments. The review commences with a concise recapitulation of the fundamental principles of active brazing, followed by an in-depth exploration of material selection, illustrated using water-vapor-resistant sensors as illustrative examples. Furthermore, the review presents practical solutions for the sealing of energy devices while also scrutinizing the factors that exert significant influence on the deterioration of these active-brazed connections. Ultimately, the review culminates in a comprehensive discussion of emerging trends and developments in active brazing techniques for energy-related applications.


  • Open Access

    Laser beam decontamination of metallic surfaces with a pulsed (150 W) Nd:YAG laser

    by Anne-Maria Reinecke, Margret Acker, Steffen Taut, Marion Herrmann, Wolfgang Lippmann, Antonio Hurtado


  • Open Access

    Investigations of Graphite Particle Interaction with Metallic Surfaces

    by Andreas Andris, Felix Fischer, Marion Herrmann, Wolfgang Lippmann, Antonio Hurtado

    Previous studies on the safety of gas-cooled high-temperature reactors (HTR) have analyzed the corrosion and oxidation behavior of the primary circuit components under normal and accident conditions. Through the use of graphite components, graphite particles can be formed by mechanical and chemical means whose influence on the structural change of metal surfaces must be analyzed in a comprehensive manner. The dust resuspension and deposition in tank geometry (DRESDEN-TANK) test facility was set up to thermally anneal metallic samples (Alloy 800H, Inconel 617) loaded with graphite particles under typical HTR conditions (helium, 750 °C, 6 MPa) for the investigation of interactions over a long-term range. In addition to the carrying out of a description of the processes occurring on the material surface, the gaseous reaction products have been analyzed. The results show that the presence of graphite particles in the near-surface layer has a significant impact on corrosion processes due to thermally-induced interactions. In this case iron and chromium are degraded in the metallic alloys, which leads to a structural change in the near-surface layer. Furthermore, the graphite particles significantly influence the formation of the oxide layers on the alloys; for example, they influence the formation speed of the layer and the layer height. The originally deposited particles thus exhibit a chemically-altered composition and a different geometric shape.


  • Rare earth (RE: Nd, Dy, Ho, Y, Yb, and Sc) aluminosilicates for joining silicon carbide components

    by Marion Herrmann, Sarfraz Ahmad, Wolfgang Lippmann, Hans‐Jürgen Seifert, Antonio Hurtado

    Six different types of glass 12.18 RE 2 O 3 ‐22 Al 2 O 3 ‐65.82 SiO 2 (mol %) where RE : Nd, Dy, Ho, Y, Yb, and Sc were tested for joining silicon carbide (SiC) components. The different types of glass vary in their thermal properties but they are similar in their behavior for the joining process when a laser‐based heating technology was used. The quality of the joints was characterized by microscopic analysis, mechanical tests, and measurements of tightness. Annealing experiments were conducted at temperatures in the range of the glass transition and crystallization allowing an assessment of the compositions for usability as glass and as glass‐ceramic interlayers. Five of the investigated compositions can be recommended for application up to temperatures of 900°C. The Y‐ and Yb‐based compositions guarantee a high joint quality at temperatures up to 1200°C. The high temperature assessment was based on tightness and microstructural analyses of the joints after the annealing procedures. The results can be transferred to joining processes with lower heating and cooling rates.