Igor Igorevich Bezsonov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Igor Igorevich Bezsonov has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Timothy Norman Lambert
Department of Photovoltaics and Materials Technology, Sandia National Laboratories, Albuquerque, NM 87185, USA
2 shared publications Calvin D. Quilty
Sandia National Laboratories
1 shared publication- Calvin D. Quilty
Sandia National Laboratories (SNL-NM), Albuquerque, NM (United States)
1 shared publication Cassidy Tran
Department of Chemistry and Biochemistry University of California Santa Cruz California USA
1 shared publication- Cheng Zhu
Lawrence Livermore National Laboratory Livermore California USA
1 shared publication Christopher Hendricks
Naval Surface Warfare Center Carderock Division
1 shared publication
Latest Publications
- 27 October 2026
- Published by Wiley in Advanced Materials
Copper Surface Engineering Enables Uniform Zn Plating in Zn Batteries at Unity N/P Ratio
Zinc (Zn) metal plating is notoriously sensitive to interfacial inefficiencies under Zn‐limited conditions, where small losses of active Zn rapidly lead to premature cell failure. Here, we demonstrate a surface reconstruction strategy for copper (Cu) current collectors that enables exceptional performance at a negative‐to‐positive (N/P) capacity ratio of 1.0. By chemically etching Cu to create a sacrificial cuprous chloride (γ‐CuCl) interface, we obtained a micro‐textured Cu substrate with increased electrochemical surface area (ECSA). Upon initial electrochemical reduction, γ‐CuCl converts to metallic Cu while releasing Cl − ions into the local interfacial region of the electrolyte. Density functional theory calculations indicate that localized Cl − ions favorably regulate Zn 2+ adsorption energy while suppressing the hydrogen evolution reaction. Benefitting from the synergistic combination of enhanced ECSA and dynamic Cl − mediated interfacial engineering, Zn//Cu cells achieve stable plating/stripping cycling for 1654 h (69 days). Notably, Zn//MnO 2 full cells using 3D‐printed etched Cu substrate assembled under a nominal N/P ratio of 1.0 (determined by a reversible capacity at 10 mA cm −2 ) deliver a remarkable device volumetric capacity of 53.5 mAh cm −3 . Under high‐rate cycling (80 mA cm −2 ), the cell retains 70% of initial capacity over 500 cycles. This performance represents a benchmark for Zn reversibility under extreme material‐limited conditions.
- 27 October 2026
- Published by Wiley in Advanced Materials
Copper Surface Engineering Enables Uniform Zn Plating in Zn Batteries at Unity N/P Ratio
Zinc (Zn) metal plating is notoriously sensitive to interfacial inefficiencies under Zn‐limited conditions, where small losses of active Zn rapidly lead to premature cell failure. Here, we demonstrate a surface reconstruction strategy for copper (Cu) current collectors that enables exceptional performance at a negative‐to‐positive (N/P) capacity ratio of 1.0. By chemically etching Cu to create a sacrificial cuprous chloride (γ‐CuCl) interface, we obtained a micro‐textured Cu substrate with increased electrochemical surface area (ECSA). Upon initial electrochemical reduction, γ‐CuCl converts to metallic Cu while releasing Cl − ions into the local interfacial region of the electrolyte. Density functional theory calculations indicate that localized Cl − ions favorably regulate Zn 2+ adsorption energy while suppressing the hydrogen evolution reaction. Benefitting from the synergistic combination of enhanced ECSA and dynamic Cl − mediated interfacial engineering, Zn//Cu cells achieve stable plating/stripping cycling for 1654 h (69 days). Notably, Zn//MnO 2 full cells using 3D‐printed etched Cu substrate assembled under a nominal N/P ratio of 1.0 (determined by a reversible capacity at 10 mA cm −2 ) deliver a remarkable device volumetric capacity of 53.5 mAh cm −3 . Under high‐rate cycling (80 mA cm −2 ), the cell retains 70% of initial capacity over 500 cycles. This performance represents a benchmark for Zn reversibility under extreme material‐limited conditions.
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (6) , 900
(Invited) Investigations into the Electrochemical Cycling of Zinc-Based Batteries
Metallic Zn is a nearly ideal anode for grid applications owing to its low cost ( ca. 2 USD kg −1 ), existing supply chain, environmental benignity, relative safety, and high stability in water [−0.76 V vs standard hydrogen electrode (SHE)]. The high theoretical capacity (2e − @ 820 mAh g −1 and 5855 mA h cm −3 ), and overall low polarizability (6 × 10 −8 Ω m) further motivate Zn-based battery development as alternatives to lead acid and lithium-ion batteries, despite their considerably lower operating voltages (< 2V).Despite many recent advances, the high-capacity utilization of Zn for thousands of cycles remains a challenge, with cycle life typically obtained at the expense of energy density. We recently began investigating the ability to cycle zinc-based electrodes in both alkaline and mildly acidic electrolytes. In each electrolyte, a dissolution precipitation reaction occurs upon cycling, cycling between metallic Zn and its soluble oxidized species: either zincate [Zn(OH) 4 2- ] in alkaline or Zn 2+ , in acidic electrolytes, with further chemical reactions leading to the formation of ZnO or Zinc hydroxy ‘ate’ species, respectively. In this talk we will cover approaches to stabilize the Zn conversion reactions and extend battery life in alkaline and/or acidic electrolytes with an emphasis on low-cost electrode additives, oxide-based formulations, new electrolyte formulations and/or the use of ion selective separators. Our emphasis is on cycling at high areal and volumetric capacities, properties that are requisite to take studies from the laboratory and adapt them to a commercial battery technology to support grid storage applications. Finally, we will highlight a recent project on the effect of pressure on the cycling behavior of zinc and other conversion cathode materials and the development of a new US-based Zinc battery consortium. This material is based upon work supported by the U.S. Department of Energy, Office of Electricity (OE), Energy Storage Division. This work was performed, in part, at the Center for Integrated Nanotechnologies, an Office of Science User Facility operated for the U.S. Department of Energy (DOE) Office of Science. Sandia National Laboratories is a multi-program laboratory managed and operated by National Technology and Engineering Solutions of Sandia, LLC, a wholly owned subsidiary of Honeywell International, Inc., for the U.S. Department of Energy’s National Nuclear Security Administration under contract DE-NA-0003525. This paper describes objective technical results and analysis. Any subjective views or opinions that might be expressed in the paper do not necessarily represent the views of the U.S. Department of Energy or the United States Government.
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (6) , 900
(Invited) Investigations into the Electrochemical Cycling of Zinc-Based Batteries
Metallic Zn is a nearly ideal anode for grid applications owing to its low cost ( ca. 2 USD kg −1 ), existing supply chain, environmental benignity, relative safety, and high stability in water [−0.76 V vs standard hydrogen electrode (SHE)]. The high theoretical capacity (2e − @ 820 mAh g −1 and 5855 mA h cm −3 ), and overall low polarizability (6 × 10 −8 Ω m) further motivate Zn-based battery development as alternatives to lead acid and lithium-ion batteries, despite their considerably lower operating voltages (< 2V).Despite many recent advances, the high-capacity utilization of Zn for thousands of cycles remains a challenge, with cycle life typically obtained at the expense of energy density. We recently began investigating the ability to cycle zinc-based electrodes in both alkaline and mildly acidic electrolytes. In each electrolyte, a dissolution precipitation reaction occurs upon cycling, cycling between metallic Zn and its soluble oxidized species: either zincate [Zn(OH) 4 2- ] in alkaline or Zn 2+ , in acidic electrolytes, with further chemical reactions leading to the formation of ZnO or Zinc hydroxy ‘ate’ species, respectively. In this talk we will cover approaches to stabilize the Zn conversion reactions and extend battery life in alkaline and/or acidic electrolytes with an emphasis on low-cost electrode additives, oxide-based formulations, new electrolyte formulations and/or the use of ion selective separators. Our emphasis is on cycling at high areal and volumetric capacities, properties that are requisite to take studies from the laboratory and adapt them to a commercial battery technology to support grid storage applications. Finally, we will highlight a recent project on the effect of pressure on the cycling behavior of zinc and other conversion cathode materials and the development of a new US-based Zinc battery consortium. This material is based upon work supported by the U.S. Department of Energy, Office of Electricity (OE), Energy Storage Division. This work was performed, in part, at the Center for Integrated Nanotechnologies, an Office of Science User Facility operated for the U.S. Department of Energy (DOE) Office of Science. Sandia National Laboratories is a multi-program laboratory managed and operated by National Technology and Engineering Solutions of Sandia, LLC, a wholly owned subsidiary of Honeywell International, Inc., for the U.S. Department of Energy’s National Nuclear Security Administration under contract DE-NA-0003525. This paper describes objective technical results and analysis. Any subjective views or opinions that might be expressed in the paper do not necessarily represent the views of the U.S. Department of Energy or the United States Government.
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (6) , 592
Strain and Temperature Behavior of Lithium-Ion 18650 Cylindrical Batteries
Modern technology, from portable electronics to electric vehicles, is increasingly reliant on lithium-ion batteries for energy storage, but their use poses safety concerns, namely due to the risk of thermal runaway [1]. This process results in toxic off-gassing, smoke, fire, and explosions, causing damage to property and endangering people. Therefore, early detection of thermal runaway is critical. Voltage, current, and temperature sensors are used to monitor batteries and identify the onset of thermal runaway, but these have limitations. For example, the heat generated inside the battery will take time to be detected due to the low thermal conductivity of polymers and other battery components. Past studies have measured the stress generated in each electrode during cycling [2] and investigated the volumetric expansion of batteries during cycling [3,4]. Therefore, strain measurement of cells could provide insight into the reversible and irreversible phenomenon inside of a battery in real time. To this end, strain and temperature response of a commercially available high capacity (3.4 Ah) 18650 lithium-ion battery were investigated in this study. Strain measurements were conducted while cycling in a temperature-controlled environment. During battery cycling the maximum strain was recorded at 100% state-of-charge (4.2V) in the hoop direction at the center of the battery. Strain was returned to a baseline value upon discharge. In all the cycling scenarios, the electrochemical reaction peaks coincided with change in strain response. Repeated measurements across multiple cycles and multiple identical cells have produced similar strain behavior. The results from this study indicate that strain measurements on a battery’s surface are directly correlated to the reversible electrochemical behavior of a battery, and therefore be used as a diagnostics tool for battery operation to detect irreversible phenomenon. This presentation will describe the methods of strain measurement as well as potential applications of this technique as a diagnostic or early fault detection tool. Figure 1: Middle hoop strain and battery potential during a full cycle. Figure 1
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (6) , 592
Strain and Temperature Behavior of Lithium-Ion 18650 Cylindrical Batteries
Modern technology, from portable electronics to electric vehicles, is increasingly reliant on lithium-ion batteries for energy storage, but their use poses safety concerns, namely due to the risk of thermal runaway [1]. This process results in toxic off-gassing, smoke, fire, and explosions, causing damage to property and endangering people. Therefore, early detection of thermal runaway is critical. Voltage, current, and temperature sensors are used to monitor batteries and identify the onset of thermal runaway, but these have limitations. For example, the heat generated inside the battery will take time to be detected due to the low thermal conductivity of polymers and other battery components. Past studies have measured the stress generated in each electrode during cycling [2] and investigated the volumetric expansion of batteries during cycling [3,4]. Therefore, strain measurement of cells could provide insight into the reversible and irreversible phenomenon inside of a battery in real time. To this end, strain and temperature response of a commercially available high capacity (3.4 Ah) 18650 lithium-ion battery were investigated in this study. Strain measurements were conducted while cycling in a temperature-controlled environment. During battery cycling the maximum strain was recorded at 100% state-of-charge (4.2V) in the hoop direction at the center of the battery. Strain was returned to a baseline value upon discharge. In all the cycling scenarios, the electrochemical reaction peaks coincided with change in strain response. Repeated measurements across multiple cycles and multiple identical cells have produced similar strain behavior. The results from this study indicate that strain measurements on a battery’s surface are directly correlated to the reversible electrochemical behavior of a battery, and therefore be used as a diagnostics tool for battery operation to detect irreversible phenomenon. This presentation will describe the methods of strain measurement as well as potential applications of this technique as a diagnostic or early fault detection tool. Figure 1: Middle hoop strain and battery potential during a full cycle. Figure 1