Guoqi Han
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Guoqi Han has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Yang Han
College of Civil Engineering, Kashi University, Kashi 844008, China
3 shared publications - Dongqiao Li
College of Civil Engineering, Henan University of Technology, Zhengzhou 450001, China
2 shared publications - Zhishuan Lv
College of Civil Engineering, Kashi University, Kashi 844008, China
2 shared publications - Hao Wang
College of Civil Engineering, Kashi University, Kashi 844008, China
1 shared publication - Junfeng Duan
School of Intelligent Construction, Zhengzhou University of Industrial Technology, Zhengzhou 451100, China
1 shared publication - Xueyu Ge
Kashi University
1 shared publication
Latest Publications
- Open Access
Experimental Study on the Mechanical Properties of Crumb Rubber Concrete after Elevated Temperature
To reduce the environmental damage caused by waste rubber, crumb rubber concrete (CRC) was prepared by replacing some fine aggregates with crumb rubber. The effects of elevated temperature as well as crumb rubber content on the mechanical properties of the prepared CRC were studied. The crumb rubber contents were 0%, 10%, and 20%, while CRC was subjected to atmospheric temperatures (AT) of 300 °C, 500 °C, and 700 °C. The concrete without crumb rubber content was used as the control group at the atmospheric temperature. The mass loss, thermal conductivity characteristics, compressive strength, splitting tensile strength, axial compressive strength, elastic modulus, and stress-strain characteristics of CRC at elevated temperatures were studied. The experimental results show that: (1) With the increase in crumb rubber content and temperature, the cracks on the surface of the specimen gradually widen while the mass loss of the specimen increases. (2) With the increase in crumb rubber content and temperature, the cube compressive strength, splitting tensile strength, axial compressive strength, and elastic modulus of CRC decrease, yet the plastic failure characteristics of CRC are more obvious. (3) The influences of elevated temperature on strength and elastic modulus are as follows: splitting tensile strength > elastic modulus > axial compressive strength > cubic compressive strength. (4) With the increase in temperature, the stress-strain curve of the CRC tends to flatten, the peak stress decreases, and the corresponding peak strain significantly increases. With the increase in crumb rubber content, there is a great decrease in peak stress, yet the corresponding peak strain is basically the same. The use of CRC can be prioritized in applications that increase toughness rather than strength.
Open AccessExperimental Study on the Mechanical Properties of Crumb Rubber Concrete after Elevated Temperature
To reduce the environmental damage caused by waste rubber, crumb rubber concrete (CRC) was prepared by replacing some fine aggregates with crumb rubber. The effects of elevated temperature as well as crumb rubber content on the mechanical properties of the prepared CRC were studied. The crumb rubber contents were 0%, 10%, and 20%, while CRC was subjected to atmospheric temperatures (AT) of 300 °C, 500 °C, and 700 °C. The concrete without crumb rubber content was used as the control group at the atmospheric temperature. The mass loss, thermal conductivity characteristics, compressive strength, splitting tensile strength, axial compressive strength, elastic modulus, and stress-strain characteristics of CRC at elevated temperatures were studied. The experimental results show that: (1) With the increase in crumb rubber content and temperature, the cracks on the surface of the specimen gradually widen while the mass loss of the specimen increases. (2) With the increase in crumb rubber content and temperature, the cube compressive strength, splitting tensile strength, axial compressive strength, and elastic modulus of CRC decrease, yet the plastic failure characteristics of CRC are more obvious. (3) The influences of elevated temperature on strength and elastic modulus are as follows: splitting tensile strength > elastic modulus > axial compressive strength > cubic compressive strength. (4) With the increase in temperature, the stress-strain curve of the CRC tends to flatten, the peak stress decreases, and the corresponding peak strain significantly increases. With the increase in crumb rubber content, there is a great decrease in peak stress, yet the corresponding peak strain is basically the same. The use of CRC can be prioritized in applications that increase toughness rather than strength.
- Open Access
- 14 March 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (6) , 5160
Numerical Simulation of Assembly Process and Sealing Reliability of T-Rubber Gasket Pipe Joints
Underground pipelines are vital parts to urban water supply, gas supply, and other lifeline systems, affecting the sustainable development of cities to a great extent. The pipeline joint, which is a weak link, may be seriously damaged during natural disasters such as earthquakes. The failure of pipe joints can cause leakage accidents, resulting in system failure and interruption, and even some secondary disasters. Herein, based on uniaxial and plane tensile test results of a T-rubber gasket material, the assembly process and sealing performance of a T-rubber gasket joint of a ductile iron pipe are numerically simulated using the Ogden third-order strain energy density function to fit the material constant. The simulation accounts for severe nonlinearities, including large deformations, hyperelasticity, and complex contacts. The effects of the assembly friction coefficient, assembly depth, and radial clearance deviation of the socket and spigot on the seal contact pressure are analyzed. The results suggest that the entire history of the deformation and stress variations during assembly can be clearly visualized and accurately calculated. For the different friction coefficients, the assembly depth corresponding to the sliding friction condition of the spigot pipe was 74 mm, while the minimum pushing force required to assemble the T-rubber gasket joint of a DN300 ductile iron pipe was 6.8 kN at the ideal situation with a friction coefficient of 0. The effective contact pressure of the rubber gasket seepage surface under various operating conditions is much higher than the normal pressure of municipal pipelines, thus indicating that the rubber gasket joint exhibits the ideal sealing performance. Furthermore, a certain deviation, which is about 20 mm, is allowed for the assembly depth of the rubber gasket joint such that the axial displacement of the pipe joint can be adapted under an earthquake or ground displacement.
- 14 March 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (6) , 5160
Open AccessNumerical Simulation of Assembly Process and Sealing Reliability of T-Rubber Gasket Pipe Joints
Underground pipelines are vital parts to urban water supply, gas supply, and other lifeline systems, affecting the sustainable development of cities to a great extent. The pipeline joint, which is a weak link, may be seriously damaged during natural disasters such as earthquakes. The failure of pipe joints can cause leakage accidents, resulting in system failure and interruption, and even some secondary disasters. Herein, based on uniaxial and plane tensile test results of a T-rubber gasket material, the assembly process and sealing performance of a T-rubber gasket joint of a ductile iron pipe are numerically simulated using the Ogden third-order strain energy density function to fit the material constant. The simulation accounts for severe nonlinearities, including large deformations, hyperelasticity, and complex contacts. The effects of the assembly friction coefficient, assembly depth, and radial clearance deviation of the socket and spigot on the seal contact pressure are analyzed. The results suggest that the entire history of the deformation and stress variations during assembly can be clearly visualized and accurately calculated. For the different friction coefficients, the assembly depth corresponding to the sliding friction condition of the spigot pipe was 74 mm, while the minimum pushing force required to assemble the T-rubber gasket joint of a DN300 ductile iron pipe was 6.8 kN at the ideal situation with a friction coefficient of 0. The effective contact pressure of the rubber gasket seepage surface under various operating conditions is much higher than the normal pressure of municipal pipelines, thus indicating that the rubber gasket joint exhibits the ideal sealing performance. Furthermore, a certain deviation, which is about 20 mm, is allowed for the assembly depth of the rubber gasket joint such that the axial displacement of the pipe joint can be adapted under an earthquake or ground displacement.
- Open Access
Experimental Study on Toughness of Engineered Cementitious Composites with Desert Sand
In this paper, engineered cementitious composites (ECCs) were prepared with desert sand instead of ordinary sand, and the toughness properties of the ECCs were studied. The particle size of the desert sand was 0.075–0.3 mm, which is defined as ultrafine sand. The ordinary sand was sieved into one control group with a size of 0.075–0.3 mm and three other reference groups. Together with the desert sand group, a total of five groups of ECC specimens were created. Through a uniaxial tensile test, three-point bending test and single-seam tensile test on the ECC specimens, the influence of aggregate particle size and sand type on the ECC tensile strength, deformation capacity, initial crack strength, cement-matrix-fracture toughness, multiple cracking characteristics and strain-hardening properties were studied. The experimental results show that the 28d tensile strain of the four groups of the ordinary sand specimens was 8.13%, 4.37%, 4.51% and 4.23%, respectively, which exceeded 2% and satisfied the requirements for the minimum strain of the ECCs. It is easier to achieve the ECC strain hardening with sand with a fine particle size; thus, a particle size below 0.3 mm is preferred when preparing the ECCs to achieve a high toughness. The multiple cracking performance (MCP) and the pseudostrain hardening (PSH) of desert sand and ordinary sand with a 0.075–0.3 mm grain size were 2.88 and 2.33, and 8.76 and 8.17, respectively, all of which meet the strength criteria and energy criteria and have similar properties. The tensile strength and tensile deformation of the desert sand group were 4.97 MPa and 6.78%, respectively, and the deformation capacity and strain–strengthening performance were outstanding. It is verified that it is feasible to use desert sand instead of ordinary sand to prepare the ECCs.
Open AccessExperimental Study on Toughness of Engineered Cementitious Composites with Desert Sand
In this paper, engineered cementitious composites (ECCs) were prepared with desert sand instead of ordinary sand, and the toughness properties of the ECCs were studied. The particle size of the desert sand was 0.075–0.3 mm, which is defined as ultrafine sand. The ordinary sand was sieved into one control group with a size of 0.075–0.3 mm and three other reference groups. Together with the desert sand group, a total of five groups of ECC specimens were created. Through a uniaxial tensile test, three-point bending test and single-seam tensile test on the ECC specimens, the influence of aggregate particle size and sand type on the ECC tensile strength, deformation capacity, initial crack strength, cement-matrix-fracture toughness, multiple cracking characteristics and strain-hardening properties were studied. The experimental results show that the 28d tensile strain of the four groups of the ordinary sand specimens was 8.13%, 4.37%, 4.51% and 4.23%, respectively, which exceeded 2% and satisfied the requirements for the minimum strain of the ECCs. It is easier to achieve the ECC strain hardening with sand with a fine particle size; thus, a particle size below 0.3 mm is preferred when preparing the ECCs to achieve a high toughness. The multiple cracking performance (MCP) and the pseudostrain hardening (PSH) of desert sand and ordinary sand with a 0.075–0.3 mm grain size were 2.88 and 2.33, and 8.76 and 8.17, respectively, all of which meet the strength criteria and energy criteria and have similar properties. The tensile strength and tensile deformation of the desert sand group were 4.97 MPa and 6.78%, respectively, and the deformation capacity and strain–strengthening performance were outstanding. It is verified that it is feasible to use desert sand instead of ordinary sand to prepare the ECCs.