Keqiang Xie
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Keqiang Xie has a total of 45 co-authors. Here are the top co-authors by number of shared publications:
- Shicong Yang
Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, China
6 shared publications - Wenhui Ma
School of Engineering, Yunnan University, Kunming, China
6 shared publications - Kuixian Wei
Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming, China
5 shared publications Shiyu Yan
Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, Yunnan, China; National Engineering Laboratory for Vacuum Metallurgy, Kunming 650093, Yunnan, China
3 shared publicationsWentao Ji
Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, Yunnan, China; National Engineering Laboratory for Vacuum Metallurgy, Kunming 650093, Yunnan, China
3 shared publications- Dandan Wu
State Key Laboratory of Complex Nonferrous Metal Resources Clean Utilization, Kunming University of Science and Technology, Kunming, People’s Republic of China
2 shared publications
Latest Publications
- 15 July 2025
- Published by Springer Nature in Silicon
- p. 1-13
Experimental Study on the Sedimentation of Silicon Particles Under the Interference of Flocculants
- 15 July 2025
- Published by Springer Nature in Silicon
- p. 1-13
Experimental Study on the Sedimentation of Silicon Particles Under the Interference of Flocculants
- Open Access
Study on Vanadium Leaching from Vanadium and Ferro-Titanium Concentrate Using Calcified Roasting Pellets and Sulfuric Acid at Constant pH
This study proposed a selective leaching method to address the challenge of excessive iron (Fe) leaching during a sulfuric acid treatment of magnetite pellets, which complicates the subsequent extraction and precipitation of vanadium (V). The approach involved constant-pH sulfuric acid leaching of calcined and roasted vanadium–titanium (V–Ti) magnetite pellets to enhance V recovery while minimizing Fe dissolution. A comparison between constant-pH leaching and conventional heap leaching was conducted. The results showed that, under optimal leaching conditions, the V leaching rate remained largely unchanged, while the Fe leaching rate was significantly reduced compared with conventional heap leaching. Specifically, under optimal conditions—acid concentration of 2 mol/L, liquid–solid ratio of 1:3, temperature of 90 °C, and leaching time of 360 h—the V leaching rate reached 72.21%, while the Fe leaching rate remained as low as 0.91%. Additionally, the valence states of V and Fe in the pellets before and after leaching, as well as the main phase compositions during the leaching process, were analyzed. The results indicated that the primary phases in the calcined and roasted pellets remain unchanged before and after leaching, and most of the V and nearly all divalent Fe were effectively leached.
Open AccessStudy on Vanadium Leaching from Vanadium and Ferro-Titanium Concentrate Using Calcified Roasting Pellets and Sulfuric Acid at Constant pH
This study proposed a selective leaching method to address the challenge of excessive iron (Fe) leaching during a sulfuric acid treatment of magnetite pellets, which complicates the subsequent extraction and precipitation of vanadium (V). The approach involved constant-pH sulfuric acid leaching of calcined and roasted vanadium–titanium (V–Ti) magnetite pellets to enhance V recovery while minimizing Fe dissolution. A comparison between constant-pH leaching and conventional heap leaching was conducted. The results showed that, under optimal leaching conditions, the V leaching rate remained largely unchanged, while the Fe leaching rate was significantly reduced compared with conventional heap leaching. Specifically, under optimal conditions—acid concentration of 2 mol/L, liquid–solid ratio of 1:3, temperature of 90 °C, and leaching time of 360 h—the V leaching rate reached 72.21%, while the Fe leaching rate remained as low as 0.91%. Additionally, the valence states of V and Fe in the pellets before and after leaching, as well as the main phase compositions during the leaching process, were analyzed. The results indicated that the primary phases in the calcined and roasted pellets remain unchanged before and after leaching, and most of the V and nearly all divalent Fe were effectively leached.
- Open Access
- 16 May 2025
- Published by Springer Nature in Research Square
Experimental study on the sedimentation of silicon particles under the interference of flocculants
Silicon separation represents the initial step in the recovery of silicon from diamond wire saw silicon waste slurry. In the current recovery process, the relatively low recovery rate indicates an inadequacy in silicon separation. This article primarily focuses on the sedimentation of particle groups and delves into the interference sedimentation mechanism of particle swarms. The experimental results reveal that the optimal flocculant for promoting interference sedimentation is CPAM (Cationic Polyacrylamide). For 3.72 µm silicon particles, the effect is optimal when the CPAM concentration is set at 0.2% and the addition rate is 17%. And 0.59 µm silicon particles require a higher concentration of 0.4% concentration and 17% addition rate for CPAM, to make the particles settle. And by comparing the particle size results, it can be seen that the 0.59 µm silicon particles have more surface voids and tiny particles on the flocs, and a larger total contact area, requiring more flocculant addition. Therefore, the contact performance between particles and flocculants determines the effective level of flocculants. To enhance the contact performance between flocculants and particles, a certain proportion of PDDA was added while adding the optimal proportion of CPAM. The experimental results showed that the addition of PDDA could reduce the contact angle between particles and CPAM, improve the overall hydrophilicity of the suspension, and make it easier for CPAM to contact with silicon particles. Moreover, 0.5% PDDA was required for 3.72 µm silicon particles, and 1.5% PDDA was required for 0.59 µm silicon particles. Under these conditions, the flocculation speed and sedimentation efficiency of particles were improved.
- 16 May 2025
- Published by Springer Nature in Research Square
Open AccessExperimental study on the sedimentation of silicon particles under the interference of flocculants
Silicon separation represents the initial step in the recovery of silicon from diamond wire saw silicon waste slurry. In the current recovery process, the relatively low recovery rate indicates an inadequacy in silicon separation. This article primarily focuses on the sedimentation of particle groups and delves into the interference sedimentation mechanism of particle swarms. The experimental results reveal that the optimal flocculant for promoting interference sedimentation is CPAM (Cationic Polyacrylamide). For 3.72 µm silicon particles, the effect is optimal when the CPAM concentration is set at 0.2% and the addition rate is 17%. And 0.59 µm silicon particles require a higher concentration of 0.4% concentration and 17% addition rate for CPAM, to make the particles settle. And by comparing the particle size results, it can be seen that the 0.59 µm silicon particles have more surface voids and tiny particles on the flocs, and a larger total contact area, requiring more flocculant addition. Therefore, the contact performance between particles and flocculants determines the effective level of flocculants. To enhance the contact performance between flocculants and particles, a certain proportion of PDDA was added while adding the optimal proportion of CPAM. The experimental results showed that the addition of PDDA could reduce the contact angle between particles and CPAM, improve the overall hydrophilicity of the suspension, and make it easier for CPAM to contact with silicon particles. Moreover, 0.5% PDDA was required for 3.72 µm silicon particles, and 1.5% PDDA was required for 0.59 µm silicon particles. Under these conditions, the flocculation speed and sedimentation efficiency of particles were improved.
- Open Access
Silicon Extraction from a Diamond Wire Saw Silicon Slurry with Flotation and the Flotation Interface Behavior
Diamond wire saw silicon slurry (DWSSS) is a waste resource produced during the process of solar-grade silicon wafer preparation with diamond wire sawing. The DWSSS contains 6N grade high-purity silicon and offers a promising resource for high-purity silicon recycling. The current process for silicon extraction recovery from DWSSS presents the disadvantages of lower recovery and secondary pollution. This study focuses on the original DWSSS as the target and proposes flotation for efficiently extracting silicon. The experimental results indicate that the maximal recovery of silicon reached 98.2% under the condition of a dodecylamine (DDA) dosage of 0.6 g·L−1 and natural pH conditions within 24 min, and the flotation conforms to the first-order rate model. Moreover, the mechanism of the interface behavior between DWSSS and DDA revealed that DDA is adsorbed on the surface of silicon though adsorption, and the floatability of silicon is improved. The DFT calculation indicates that DDA can be spontaneously adsorbed with the silicon. The present study demonstrates that flotation is an efficient method for extracting silicon from DWSSS and provides an available option for silicon recovery.
Open AccessSilicon Extraction from a Diamond Wire Saw Silicon Slurry with Flotation and the Flotation Interface Behavior
Diamond wire saw silicon slurry (DWSSS) is a waste resource produced during the process of solar-grade silicon wafer preparation with diamond wire sawing. The DWSSS contains 6N grade high-purity silicon and offers a promising resource for high-purity silicon recycling. The current process for silicon extraction recovery from DWSSS presents the disadvantages of lower recovery and secondary pollution. This study focuses on the original DWSSS as the target and proposes flotation for efficiently extracting silicon. The experimental results indicate that the maximal recovery of silicon reached 98.2% under the condition of a dodecylamine (DDA) dosage of 0.6 g·L−1 and natural pH conditions within 24 min, and the flotation conforms to the first-order rate model. Moreover, the mechanism of the interface behavior between DWSSS and DDA revealed that DDA is adsorbed on the surface of silicon though adsorption, and the floatability of silicon is improved. The DFT calculation indicates that DDA can be spontaneously adsorbed with the silicon. The present study demonstrates that flotation is an efficient method for extracting silicon from DWSSS and provides an available option for silicon recovery.
- Open Access
Review of Silicon Recovery from Diamond Wire Saw Silicon Powder Waste Based on Hydrometallurgical Process
The photovoltaic (PV) industry is developing rapidly to support energy transformation and emission reduction. In the whole PV industry chain, diamond wire saw silicon powder (DWSSP) waste is the most promising secondary resource for recycling high-purity silicon. DWSSP mainly contains metal impurities, and the treatment process based on hydrometallurgy can effectively remove metal impurities. The current DWSSP recovery process was divided into three categories: direct acid leaching, pyrometallurgy followed by acid leaching, and acid leaching followed by pyrometallurgy. This paper gives a comprehensive overview of these three purification processes from the aspects of impurity removal and recovery yield. The results suggest that acid leaching followed by pyrometallurgy is currently the most effective process for removing metal impurities from DWSSP. Moreover, this study underscores the potential for enhancing the purity of reclaimed silicon through the application of external field reinforcement, oxygen-regulated acid leaching, and surfactant-facilitated organic acid leaching and points out the development direction for promoting silicon recovery from DWSSP.
Open AccessReview of Silicon Recovery from Diamond Wire Saw Silicon Powder Waste Based on Hydrometallurgical Process
The photovoltaic (PV) industry is developing rapidly to support energy transformation and emission reduction. In the whole PV industry chain, diamond wire saw silicon powder (DWSSP) waste is the most promising secondary resource for recycling high-purity silicon. DWSSP mainly contains metal impurities, and the treatment process based on hydrometallurgy can effectively remove metal impurities. The current DWSSP recovery process was divided into three categories: direct acid leaching, pyrometallurgy followed by acid leaching, and acid leaching followed by pyrometallurgy. This paper gives a comprehensive overview of these three purification processes from the aspects of impurity removal and recovery yield. The results suggest that acid leaching followed by pyrometallurgy is currently the most effective process for removing metal impurities from DWSSP. Moreover, this study underscores the potential for enhancing the purity of reclaimed silicon through the application of external field reinforcement, oxygen-regulated acid leaching, and surfactant-facilitated organic acid leaching and points out the development direction for promoting silicon recovery from DWSSP.
- 22 October 2024
- Published by Springer Nature in Silicon
- Vol. 17 (1) , 39-49
Quantum Chemical Simulation for the Adsorption Behavior of Silicon in Water and Surface Property Study
- 22 October 2024
- Published by Springer Nature in Silicon
- Vol. 17 (1) , 39-49
Quantum Chemical Simulation for the Adsorption Behavior of Silicon in Water and Surface Property Study
- 26 October 2023
- Published by Springer Nature in Silicon
- Vol. 16 (2) , 867-875
Study on the Separation and Sedimentation Performance of Silicon from Diamond Wire Saw Silicon Powder Slurry
- 26 October 2023
- Published by Springer Nature in Silicon
- Vol. 16 (2) , 867-875
Study on the Separation and Sedimentation Performance of Silicon from Diamond Wire Saw Silicon Powder Slurry
- Open Access
Purification of Waste Graphite from Crucibles Used in Photovoltaic Crystallization by an Alkali-Acid Method
The photovoltaic industry generates large amounts of waste graphite (WG) that contains useful metals that can be recycled into high-value products. This study elucidated the impurity elements and their existence states in WG, analyzed and verified the source of the main impurity phase SiC, and determined the SiC content to be 4.66%. WG was purified using an alkaline-acid method, whose optimal process parameters were a solid alkali ratio of 3, calcination temperature of 600 °C, calcination time of 120 min, HCl concentration of 1 M, and acid leaching time of 40 min. Under these conditions, a graphite product with a fixed carbon content of 98.45% was obtained. Impurities were determined to migrate via three pathways: (1) Most main elements (Al, K, and Si) in silicates were removed by alkaline roasting, while the remaining elements were dissolved in acid. (2) Impurities containing metal elements such as Fe, Mg, Ca, and Zn were decomposed in NaOH to form hydroxides or oxides that were dissolved in HCl. (3) Silicon carbide impurities were removed by the alkaline-acid method without decomposition and often existed with graphite in the acid-leaching slag.
Open AccessPurification of Waste Graphite from Crucibles Used in Photovoltaic Crystallization by an Alkali-Acid Method
The photovoltaic industry generates large amounts of waste graphite (WG) that contains useful metals that can be recycled into high-value products. This study elucidated the impurity elements and their existence states in WG, analyzed and verified the source of the main impurity phase SiC, and determined the SiC content to be 4.66%. WG was purified using an alkaline-acid method, whose optimal process parameters were a solid alkali ratio of 3, calcination temperature of 600 °C, calcination time of 120 min, HCl concentration of 1 M, and acid leaching time of 40 min. Under these conditions, a graphite product with a fixed carbon content of 98.45% was obtained. Impurities were determined to migrate via three pathways: (1) Most main elements (Al, K, and Si) in silicates were removed by alkaline roasting, while the remaining elements were dissolved in acid. (2) Impurities containing metal elements such as Fe, Mg, Ca, and Zn were decomposed in NaOH to form hydroxides or oxides that were dissolved in HCl. (3) Silicon carbide impurities were removed by the alkaline-acid method without decomposition and often existed with graphite in the acid-leaching slag.
- Open Access
Vanadium–Titanium Magnetite Concentrate, Calcium–Magnesium Composite Roasting and Sulfuric Acid Leaching for Vanadium Extraction from Pellets
This paper investigated a pellet ore production process in which vanadium was extracted from vanadium and titanium magnetite concentrates using sulfuric acid leaching. Calcium and magnesium were added to the iron ore concentrate during pellet production to produce calcium vanadate and magnesium vanadate after roasting. The pellets were leached with sulfuric acid solution to extract V5+. The resulting pellets had a compressive strength of 3375 N after primary roasting, a good pellet morphology after acid leaching, and simple liquid–solid separation. Under the optimal experimental conditions, the vanadium leaching rate in the pellets reached 77.86%, while the iron leaching rate was only 1.17%. The pellets did not fragment, which was an improvement upon existing vanadium extraction methods. The strength of the pellets after vanadium extraction decreased to 563 N, but after secondary roasting, the compressive strength of the pellets reached 2578 N, which was suitable for blast furnace ironmaking. The roasting and acid leaching experiments showed that the vanadium extraction process resulted in suitable pellet properties. The use of low compound additives can effectively improve the leaching effect, while avoiding the previous problems of too many additives, pellet iron grade reduction, or the pursuit of high vanadium extraction rate pellet breakage and serious high secondary use process costs.
Open AccessVanadium–Titanium Magnetite Concentrate, Calcium–Magnesium Composite Roasting and Sulfuric Acid Leaching for Vanadium Extraction from Pellets
This paper investigated a pellet ore production process in which vanadium was extracted from vanadium and titanium magnetite concentrates using sulfuric acid leaching. Calcium and magnesium were added to the iron ore concentrate during pellet production to produce calcium vanadate and magnesium vanadate after roasting. The pellets were leached with sulfuric acid solution to extract V5+. The resulting pellets had a compressive strength of 3375 N after primary roasting, a good pellet morphology after acid leaching, and simple liquid–solid separation. Under the optimal experimental conditions, the vanadium leaching rate in the pellets reached 77.86%, while the iron leaching rate was only 1.17%. The pellets did not fragment, which was an improvement upon existing vanadium extraction methods. The strength of the pellets after vanadium extraction decreased to 563 N, but after secondary roasting, the compressive strength of the pellets reached 2578 N, which was suitable for blast furnace ironmaking. The roasting and acid leaching experiments showed that the vanadium extraction process resulted in suitable pellet properties. The use of low compound additives can effectively improve the leaching effect, while avoiding the previous problems of too many additives, pellet iron grade reduction, or the pursuit of high vanadium extraction rate pellet breakage and serious high secondary use process costs.
- Open Access
Study on the Properties of Vanadium Pellets Extracted from Vanadium Titanium Magnetite Concentrate by Calcium Roasting and Acid Leaching
In this study, a clean pellet production method of calcium roasting and sulfuric acid leaching of vanadium from vanadium and titanium magnetite concentrates is proposed, which can effectively separate vanadium and iron, and the pellets after acid leaching and vanadium extraction can be used as raw material for iron making after secondary roasting. During the experiment, only 2% Ca(OH)2 was added as the calcifier to make pellets, and vanadium was extracted by acid leaching after calcination. Under the optimum conditions, the vanadium leaching rate was 74.51%, and the iron leaching rate was only 1.05%. After secondary roasting, the compressive strength of the pellets was 2358 N, and the qualification rate was 97%. Additionally, after acid leaching and vanadium extraction, the impurities in the pellet were partially removed, and the iron content of the pellet increased by 6.6%, which is more conducive to subsequent ironmaking. The roasting and acid leaching experiments show that based on the production of iron smelting pellets, the use of pellets can better extract vanadium from the titanium magnetite concentrate, while avoiding the problems of excessive additives to reduce the iron grade of pellets. Or the pursuit of high vanadium extraction rate pellets, which can be seriously damaged and difficult to use later. This process can perform a comprehensive utilization of vanadium titanium magnetite, and has certain guiding significance for industrial production.
Open AccessStudy on the Properties of Vanadium Pellets Extracted from Vanadium Titanium Magnetite Concentrate by Calcium Roasting and Acid Leaching
In this study, a clean pellet production method of calcium roasting and sulfuric acid leaching of vanadium from vanadium and titanium magnetite concentrates is proposed, which can effectively separate vanadium and iron, and the pellets after acid leaching and vanadium extraction can be used as raw material for iron making after secondary roasting. During the experiment, only 2% Ca(OH)2 was added as the calcifier to make pellets, and vanadium was extracted by acid leaching after calcination. Under the optimum conditions, the vanadium leaching rate was 74.51%, and the iron leaching rate was only 1.05%. After secondary roasting, the compressive strength of the pellets was 2358 N, and the qualification rate was 97%. Additionally, after acid leaching and vanadium extraction, the impurities in the pellet were partially removed, and the iron content of the pellet increased by 6.6%, which is more conducive to subsequent ironmaking. The roasting and acid leaching experiments show that based on the production of iron smelting pellets, the use of pellets can better extract vanadium from the titanium magnetite concentrate, while avoiding the problems of excessive additives to reduce the iron grade of pellets. Or the pursuit of high vanadium extraction rate pellets, which can be seriously damaged and difficult to use later. This process can perform a comprehensive utilization of vanadium titanium magnetite, and has certain guiding significance for industrial production.