Lifang Mei
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Lifang Mei has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
Dongbing Yan
College of Mechanical and Automotive Engineering, Xiamen University of Technology, Xiamen, China
6 shared publicationsYu Liang
College of Mechanical and Automotive Engineering, Xiamen University of Technology, Xiamen, China
4 shared publicationsLong Lin
College of Mechanical and Automotive Engineering, Xiamen University of Technology, Xiamen, China
3 shared publicationsShanming Luo
College of Marine Equipment and Mechanical Engineering, Jimei University, Xiamen, China
3 shared publications- Dongbing Yan
College of Mechanical and Automotive Engineering, Xiamen University of Technology 1 , Xiamen 361024, China
2 shared publications Qingying Dai
College of Mechanical and Automotive Engineering, Xiamen University of Technology, Xiamen, China
2 shared publications
Latest Publications
- 8 August 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (39) , 41019-41038
Impact of Pre-formed Surface Texture on Laser Clad NiCoCrAlY Coatings’ Thermal Stress and Properties
- 8 August 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (39) , 41019-41038
Impact of Pre-formed Surface Texture on Laser Clad NiCoCrAlY Coatings’ Thermal Stress and Properties
- 24 March 2026
- Published by Laser Institute of America in Journal of Laser Applications
- Vol. 38 (2)
Effects of different active agents on the dynamic features and joint performance of full/partial-penetration laser welding of stainless-steel thick plates
This paper systematically investigates the effects of oxide active agents (SiO2, TiO2, Cr2O3), a rare earth active agent (CeO2), and a fluoride active agent (NaF) on the dynamic behavior of metal vapor/plasma, deep penetration keyholes, and the molten pool during laser full/partial-penetration welding of stainless-steel thick plates. This effectively suppresses the violent ejection of metal vapor/plasma, keyhole oscillation, and deformation, enhancing welding stability and increasing penetration depth. Among these, coating with a Cr2O3 active agent in the full-penetration welded state and coating with a SiO2 active agent in the partial-penetration welded state exhibited the most significant suppression effects on metal vapor/plasma ejection. Compared to samples without active agent coating, these treatments reduced ejection by 11.33% and 24.7%, respectively. Additionally, microstructure, mechanical properties, and elemental analysis indicate that active agents have a relatively limited impact on the microstructure and properties of full-penetration welded, while significantly improving those of the partial-penetration welded. The Cr2O3 active agent demonstrates the most pronounced effect, increasing tensile strength by 9.17%, compared to uncoated specimens. It also refines grain size and reduces the heat-affected zone. In contrast, the NaF active agent showed no significant effect on improving weld bead formation quality. This indicates that adding suitable active agents enhances welding stability and quality by regulating fluid behavior such as Marangoni convection. This study provides a solid experimental foundation for the theoretical development and industrial application of thick-plate laser welding technology.
- 24 March 2026
- Published by Laser Institute of America in Journal of Laser Applications
- Vol. 38 (2)
Effects of different active agents on the dynamic features and joint performance of full/partial-penetration laser welding of stainless-steel thick plates
This paper systematically investigates the effects of oxide active agents (SiO2, TiO2, Cr2O3), a rare earth active agent (CeO2), and a fluoride active agent (NaF) on the dynamic behavior of metal vapor/plasma, deep penetration keyholes, and the molten pool during laser full/partial-penetration welding of stainless-steel thick plates. This effectively suppresses the violent ejection of metal vapor/plasma, keyhole oscillation, and deformation, enhancing welding stability and increasing penetration depth. Among these, coating with a Cr2O3 active agent in the full-penetration welded state and coating with a SiO2 active agent in the partial-penetration welded state exhibited the most significant suppression effects on metal vapor/plasma ejection. Compared to samples without active agent coating, these treatments reduced ejection by 11.33% and 24.7%, respectively. Additionally, microstructure, mechanical properties, and elemental analysis indicate that active agents have a relatively limited impact on the microstructure and properties of full-penetration welded, while significantly improving those of the partial-penetration welded. The Cr2O3 active agent demonstrates the most pronounced effect, increasing tensile strength by 9.17%, compared to uncoated specimens. It also refines grain size and reduces the heat-affected zone. In contrast, the NaF active agent showed no significant effect on improving weld bead formation quality. This indicates that adding suitable active agents enhances welding stability and quality by regulating fluid behavior such as Marangoni convection. This study provides a solid experimental foundation for the theoretical development and industrial application of thick-plate laser welding technology.
- 1 February 2026
- Published by Pleiades Publishing Ltd in Fluid Dynamics
- Vol. 61 (1) , 10
Simulation and Analysis of Flow Field Evolution and Particle Dynamics in the Molding Cavity of Solid CO2
The gas-solid two-phase flow characteristics within the compression cavity of a solid carbon dioxide (CO2) molding machine are investigated using numerical simulation. Initially, based on computational fluid dynamics (CFD), the effects of varying inlet inclination angles (0–60°) on the flow field structure within the cavity are analyzed, with a particular focus on examining the evolution of the velocity field, the pressure distribution, and the gas trajectory patterns. Subsequently, the discrete phase model (DPM) is applied to track the motion of snowflake-shaped dry ice particles, enabling a detailed examination of particle spatial distribution under flow interactions. Results indicate that an increase in the inlet inclination angle significantly enhances the main flow diffusion within the cavity, improving particle phase dispersion uniformity. However, further increases in the angle lead to a concomitant rise in the static pressure gradients, raising the risk of high-pressure injection events. An analysis of gas motion trajectories shows that, at the 45 and 60° inlet angles, the flow field exhibits a typical vortex-diffusion composite pattern. The primary gas flow forms stable spiral trajectories that enhance particle dispersion, while secondary flows effectively reduce particle deposition at the cavity bottom. In terms of the particle distribution, particles accumulate near the exhaust hole at the angle of 45°, increasing the cavitation risk, whereas at the angle of 60°, they concentrate primarily on the right side while maintaining optimal dispersion uniformity throughout the cavity. Comprehensive evaluation identifies the angle of 60° as the optimal inlet inclination for aerodynamic performance. This work provides critical theoretical foundation and engineering guidance for the aerodynamic optimization of solid CO2 molding equipment.
- 1 February 2026
- Published by Pleiades Publishing Ltd in Fluid Dynamics
- Vol. 61 (1) , 10
Simulation and Analysis of Flow Field Evolution and Particle Dynamics in the Molding Cavity of Solid CO2
The gas-solid two-phase flow characteristics within the compression cavity of a solid carbon dioxide (CO2) molding machine are investigated using numerical simulation. Initially, based on computational fluid dynamics (CFD), the effects of varying inlet inclination angles (0–60°) on the flow field structure within the cavity are analyzed, with a particular focus on examining the evolution of the velocity field, the pressure distribution, and the gas trajectory patterns. Subsequently, the discrete phase model (DPM) is applied to track the motion of snowflake-shaped dry ice particles, enabling a detailed examination of particle spatial distribution under flow interactions. Results indicate that an increase in the inlet inclination angle significantly enhances the main flow diffusion within the cavity, improving particle phase dispersion uniformity. However, further increases in the angle lead to a concomitant rise in the static pressure gradients, raising the risk of high-pressure injection events. An analysis of gas motion trajectories shows that, at the 45 and 60° inlet angles, the flow field exhibits a typical vortex-diffusion composite pattern. The primary gas flow forms stable spiral trajectories that enhance particle dispersion, while secondary flows effectively reduce particle deposition at the cavity bottom. In terms of the particle distribution, particles accumulate near the exhaust hole at the angle of 45°, increasing the cavitation risk, whereas at the angle of 60°, they concentrate primarily on the right side while maintaining optimal dispersion uniformity throughout the cavity. Comprehensive evaluation identifies the angle of 60° as the optimal inlet inclination for aerodynamic performance. This work provides critical theoretical foundation and engineering guidance for the aerodynamic optimization of solid CO2 molding equipment.
- 13 March 2025
- Published by Springer Nature in Applied Physics B
- Vol. 131 (4) , 1-27
Effect of longitudinal alternating magnetic field on the dynamic behaviour and joint properties of laser scanning welding of T2 red copper
- 13 March 2025
- Published by Springer Nature in Applied Physics B
- Vol. 131 (4) , 1-27
Effect of longitudinal alternating magnetic field on the dynamic behaviour and joint properties of laser scanning welding of T2 red copper
- 25 March 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (5) , 3827-3842
Performance Study and Heat Treatment Analysis of Selective Laser Melting SiC/18Ni300 Martensitic Mold Steel Composites
- 25 March 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (5) , 3827-3842
Performance Study and Heat Treatment Analysis of Selective Laser Melting SiC/18Ni300 Martensitic Mold Steel Composites
- 13 March 2024
- Published by Elsevier in Optics & Laser Technology
- Vol. 175
Numeric simulation and experimental study in magnetic field-assisted laser scanning welding of T2 red copper
- 13 March 2024
- Published by Elsevier in Optics & Laser Technology
- Vol. 175
Numeric simulation and experimental study in magnetic field-assisted laser scanning welding of T2 red copper
- 12 January 2024
- Published by Laser Institute of America in Journal of Laser Applications
- Vol. 36 (1)
Experimental study on magnetic field-assisted laser scanning welding of T2 copper
The study employed laser scanning welding technology for butt welding experiments on red copper, investigating the behavior of metal vapor plumes, plasma, and metal spatter during the welding process, as well as the quality and electrical conductivity of the resulting joints by varying the polarity and strength of the applied magnetic field. The results showed that the polarity of the magnetic field had a minor effect on welding performance, with the main influencing factor being the strength of the magnetic field. As the magnetic field strength increased, the formation volume and ejection intensity of metal vapor plumes and plasma exhibited an initial decrease followed by an increase, similarly affecting the weld seam morphology, mechanical properties, and electrical conductivity. At 120 mT magnetic strength, metal vapor and plasma formation are minimized, and metal spattering is eliminated, thereby enhancing welding stability; the weld seam was uniformly formed with no significant defects; the cross-sectional weld was even without obvious undulations; on one side of the weld zone, columnar crystals were extremely fine, and the center of the weld consisted of numerous equiaxed crystals with a few columnar crystals perpendicular to the horizontal direction, while the equiaxed crystals on the other side of the weld zone were denser; the sample joints achieved peak hardness and tensile strength at 70.9 HV and 202 MPa, showing increases of 17.2% and 14.8%, respectively, over nonmagnetic conditions; the weldment’s conductivity peaked at 79.58 mS/m, 36.5% higher than without a magnetic field, reaching 97.9% of the parent material’s.
- 12 January 2024
- Published by Laser Institute of America in Journal of Laser Applications
- Vol. 36 (1)
Experimental study on magnetic field-assisted laser scanning welding of T2 copper
The study employed laser scanning welding technology for butt welding experiments on red copper, investigating the behavior of metal vapor plumes, plasma, and metal spatter during the welding process, as well as the quality and electrical conductivity of the resulting joints by varying the polarity and strength of the applied magnetic field. The results showed that the polarity of the magnetic field had a minor effect on welding performance, with the main influencing factor being the strength of the magnetic field. As the magnetic field strength increased, the formation volume and ejection intensity of metal vapor plumes and plasma exhibited an initial decrease followed by an increase, similarly affecting the weld seam morphology, mechanical properties, and electrical conductivity. At 120 mT magnetic strength, metal vapor and plasma formation are minimized, and metal spattering is eliminated, thereby enhancing welding stability; the weld seam was uniformly formed with no significant defects; the cross-sectional weld was even without obvious undulations; on one side of the weld zone, columnar crystals were extremely fine, and the center of the weld consisted of numerous equiaxed crystals with a few columnar crystals perpendicular to the horizontal direction, while the equiaxed crystals on the other side of the weld zone were denser; the sample joints achieved peak hardness and tensile strength at 70.9 HV and 202 MPa, showing increases of 17.2% and 14.8%, respectively, over nonmagnetic conditions; the weldment’s conductivity peaked at 79.58 mS/m, 36.5% higher than without a magnetic field, reaching 97.9% of the parent material’s.
- 12 December 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 130 (3-4) , 1693-1708
Theoretical and experimental research on nanosecond laser cleaning of SiO2 particles on silicon wafer surface
- 12 December 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 130 (3-4) , 1693-1708
Theoretical and experimental research on nanosecond laser cleaning of SiO2 particles on silicon wafer surface
- Open Access
- 1 July 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (7) , 076506
Dynamic behavior of molten pool flow field for active laser welded-thick stainless steel plates
By combining numerical simulation and experimental investigation, this paper intensively investigated the influence rules of adding three active agents (SiO2, TiO2 and NaF) on the dynamic behaviors of flow field in the laser welding 304 stainless steel thick plate pool. First of all, the mathematical model of the activating laser welding stainless steel thick plate was constructed to numerically investigate the impact of active agents on the fluid flow in the pool. Secondly, based on the tungsten particle tracing principle test, the high speed camera system was adopted for real-time monitoring to investigate the mechanism of action of the active agents on the flow field in the pool. The results suggested that, the active agents partially affected the mode of fluid flow. The velocity vector from both sides of the pool to the center occurred on the pool surface, while vortex from the pool margin to the center occurred on the pool cross section. The phenomenon that the tracing tungsten particles moving from the pool margin to the center, it shows that the flow direction of the fluid changed after coating with the active agent, the fluid flew from the pool margin to the center. At the same time, the coating of active agents changed the flow velocity of fluid inside the pool, and SiO2 active agent has the most significant increase effect, the maximum velocity of fluid flow on the upper surface, the longitudinal and cross sections at the same position of the SiO2 active agent coated specimen increased by 25.8%, 8% and 33.8%, respectively, compared with that without the active agents.
- 1 July 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (7) , 076506
Open AccessDynamic behavior of molten pool flow field for active laser welded-thick stainless steel plates
By combining numerical simulation and experimental investigation, this paper intensively investigated the influence rules of adding three active agents (SiO2, TiO2 and NaF) on the dynamic behaviors of flow field in the laser welding 304 stainless steel thick plate pool. First of all, the mathematical model of the activating laser welding stainless steel thick plate was constructed to numerically investigate the impact of active agents on the fluid flow in the pool. Secondly, based on the tungsten particle tracing principle test, the high speed camera system was adopted for real-time monitoring to investigate the mechanism of action of the active agents on the flow field in the pool. The results suggested that, the active agents partially affected the mode of fluid flow. The velocity vector from both sides of the pool to the center occurred on the pool surface, while vortex from the pool margin to the center occurred on the pool cross section. The phenomenon that the tracing tungsten particles moving from the pool margin to the center, it shows that the flow direction of the fluid changed after coating with the active agent, the fluid flew from the pool margin to the center. At the same time, the coating of active agents changed the flow velocity of fluid inside the pool, and SiO2 active agent has the most significant increase effect, the maximum velocity of fluid flow on the upper surface, the longitudinal and cross sections at the same position of the SiO2 active agent coated specimen increased by 25.8%, 8% and 33.8%, respectively, compared with that without the active agents.