Saber Jalilpiran
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Saber Jalilpiran has a total of 29 co-authors. Here are the top co-authors by number of shared publications:
- Sophie LaRochelle
Université Laval
8 shared publications - Jacques Lefebvre
National Research Council Canada
7 shared publications Younès Messaddeq
3 shared publications- Anees Mehaboob2 shared publications
- Firat Ertac Durak
Kutahya Dumlupinar Universitesi
2 shared publications Lixian Wang
Canada research center, Huawei Technologies Canada, Ottawa, ON, Canada
2 shared publications
Latest Publications
- 18 May 2026
- Published by Optica Publishing Group in Optics Letters
- Vol. 51 (11) , 3012-3015
Drawing-induced improvement of amplification in bismuth-doped phosphosilicate fibers
This study investigates drawing-induced effects on bismuth active centers (BACs) and optical amplification in Bi-doped phosphosilicate fibers operating in E and S bands. A twofold increase in BAC-related active absorption was observed, while the unsaturable loss remained nearly constant over a 100 °C drawing temperature. Unitary gain (dB/m) was found to increase linearly with drawing temperature, reaching ∼0.4 dB/m under bi-directional pumping when using 390 mW. With this pumping configuration, the amplifier’s unsaturated peak gain was close to 35 dB using an optimum fiber length less than 100 m, demonstrating efficient amplification with high Bi concentration in those fibers.
- 18 May 2026
- Published by Optica Publishing Group in Optics Letters
- Vol. 51 (11) , 3012-3015
Drawing-induced improvement of amplification in bismuth-doped phosphosilicate fibers
This study investigates drawing-induced effects on bismuth active centers (BACs) and optical amplification in Bi-doped phosphosilicate fibers operating in E and S bands. A twofold increase in BAC-related active absorption was observed, while the unsaturable loss remained nearly constant over a 100 °C drawing temperature. Unitary gain (dB/m) was found to increase linearly with drawing temperature, reaching ∼0.4 dB/m under bi-directional pumping when using 390 mW. With this pumping configuration, the amplifier’s unsaturated peak gain was close to 35 dB using an optimum fiber length less than 100 m, demonstrating efficient amplification with high Bi concentration in those fibers.
- 16 October 2025
- Published by Elsevier in Optical Fiber Technology
- Vol. 95
Rare-earth co-doping for improved power efficiency in extended L-band erbium-doped fiber amplifiers
- 16 October 2025
- Published by Elsevier in Optical Fiber Technology
- Vol. 95
Rare-earth co-doping for improved power efficiency in extended L-band erbium-doped fiber amplifiers
- 18 September 2025
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 15 (10) , 2510
High-bismuth-content phospho-silicate fiber for optical amplification
We report a fiber fabrication process combining modified chemical vapor deposition and solution doping, which maximizes material retention to produce bismuth-doped fibers with high doping content. With a detectable amount of Bi at the 0.1 wt.% level, fabricated fibers exhibit low levels of background and unsaturable loss. Moreover, a flat and broad absorption profile is obtained and is attributed to a balanced level of phosphorus and silica-related bismuth active centers (BACs). Our photoluminescence results suggest excitation-dependent emission spectra, including broad luminescence under 808 and 980 nm pump wavelengths. The BPFs present a flat gain spectrum, free from OH-related absorption, reaching 34 dB peak gain with 100 nm bandwidth (>20 dB) and a noise figure (NF) in the range of 3.7 - 5.7 dB over the E- and S-band.
- 18 September 2025
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 15 (10) , 2510
High-bismuth-content phospho-silicate fiber for optical amplification
We report a fiber fabrication process combining modified chemical vapor deposition and solution doping, which maximizes material retention to produce bismuth-doped fibers with high doping content. With a detectable amount of Bi at the 0.1 wt.% level, fabricated fibers exhibit low levels of background and unsaturable loss. Moreover, a flat and broad absorption profile is obtained and is attributed to a balanced level of phosphorus and silica-related bismuth active centers (BACs). Our photoluminescence results suggest excitation-dependent emission spectra, including broad luminescence under 808 and 980 nm pump wavelengths. The BPFs present a flat gain spectrum, free from OH-related absorption, reaching 34 dB peak gain with 100 nm bandwidth (>20 dB) and a noise figure (NF) in the range of 3.7 - 5.7 dB over the E- and S-band.
- 9 December 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Photonics Technology Letters
- Vol. 37 (2) , 69-72
Hybrid Pumping for Optimized Electrical Power Usage in Cladding-Pumped L-Band Amplifiers
We investigate reducing pump power requirements in super L-band erbium/ytterbium co-doped fiber amplifiers. We examine several pump configurations and find good trade-offs in performance and power when employing a hybrid pumping scheme that combines forward 915 nm cladding-pumping with backward 1480 nm core-pumping. Using experimental measurements with hybrid pumping, we train a neural network model to predict gain and noise figure. With the fast and precise neural network model, we examine the effect on performance (gain, noise figure and total electrical power consumption) as we vary the percentage of power dedicated to cladding vs. core pumping.
- 9 December 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Photonics Technology Letters
- Vol. 37 (2) , 69-72
Hybrid Pumping for Optimized Electrical Power Usage in Cladding-Pumped L-Band Amplifiers
We investigate reducing pump power requirements in super L-band erbium/ytterbium co-doped fiber amplifiers. We examine several pump configurations and find good trade-offs in performance and power when employing a hybrid pumping scheme that combines forward 915 nm cladding-pumping with backward 1480 nm core-pumping. Using experimental measurements with hybrid pumping, we train a neural network model to predict gain and noise figure. With the fast and precise neural network model, we examine the effect on performance (gain, noise figure and total electrical power consumption) as we vary the percentage of power dedicated to cladding vs. core pumping.
- 2 October 2024
- Published by Optica Publishing Group in Optics Letters
- Vol. 49 (20) , 5715-5718
Analysis of signal excited-state absorption for improving extended L-band erbium-doped fibers
The precise characterization of signal excited-state absorption (ESA) in erbium-doped fibers (EDFs) is achieved through an ON/OFF pumping scheme, using a supercontinuum source in conjunction with a bandpass tunable filter to generate the input signal. Normalizing the ESA profile, by the value of the ESA peak, allows sample comparisons independent of their erbium concentration. This method directly assesses the impact of ESA on the net gain within the 1600–1730 nm range, providing a significant means to study how to expand the gain bandwidth toward longer wavelengths. As an illustrative application, we investigate the effect of chemical elements, such as Er, Al, and Ba, and their concentrations on ESA. We then optimize the Al content to enhance erbium solubility without inadvertently inducing detrimental ESA effects. This advancement in the ESA characterization presents substantial advantages for the pursuit of efficient extended L-band erbium-doped fiber amplifiers (EDFAs).
- 2 October 2024
- Published by Optica Publishing Group in Optics Letters
- Vol. 49 (20) , 5715-5718
Analysis of signal excited-state absorption for improving extended L-band erbium-doped fibers
The precise characterization of signal excited-state absorption (ESA) in erbium-doped fibers (EDFs) is achieved through an ON/OFF pumping scheme, using a supercontinuum source in conjunction with a bandpass tunable filter to generate the input signal. Normalizing the ESA profile, by the value of the ESA peak, allows sample comparisons independent of their erbium concentration. This method directly assesses the impact of ESA on the net gain within the 1600–1730 nm range, providing a significant means to study how to expand the gain bandwidth toward longer wavelengths. As an illustrative application, we investigate the effect of chemical elements, such as Er, Al, and Ba, and their concentrations on ESA. We then optimize the Al content to enhance erbium solubility without inadvertently inducing detrimental ESA effects. This advancement in the ESA characterization presents substantial advantages for the pursuit of efficient extended L-band erbium-doped fiber amplifiers (EDFAs).
- 12 February 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in Journal of Lightwave Technology
- Vol. 42 (10) , 3835-3843
Improving Extended L-Band Fiber Amplifiers Using Er3+: Y3+ Co-Doped Silicate With Optimized Alumino-Phospho-Silicate Glass Matrix
Fiber amplifiers operating in the L-band can benefit from further extending their gain bandwidth and improving overall operation costs. This work addresses both aspects through an optimization of the host matrix using phosphorus/aluminum (P/Al) as glass modifier and secondly through the use of yttrium as an alternative co-dopant to ytterbium. Fiber samples were fabricated using the modified chemical vapor deposition (MCVD) and solution doping technique. Using a maximum amount of phosphorus consistent with a flat refractive index profile, we find the optimum alumino-phospho-silicate glass matrix. The achieved amplifier exhibits a large gain amplification ranging from 15 to 25 dB, with its peak gain occurring at 1610 nm when pumped with a total power of 1.4 W at 978 nm. The maximum noise figure was 6.3 dB, while the gain ripple within the wavelength range of 1575 to 1626 nm was 76%. Moreover, we have obtained a low level of pair-induced quenching (3+ concentration of 1.2 ×10 25 m −3 . The result provides a viable solution to the 980 nm pumping scheme in a quest to achieve cost-effective and low-noise L-band EDFAs.
- 12 February 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in Journal of Lightwave Technology
- Vol. 42 (10) , 3835-3843
Improving Extended L-Band Fiber Amplifiers Using Er3+: Y3+ Co-Doped Silicate With Optimized Alumino-Phospho-Silicate Glass Matrix
Fiber amplifiers operating in the L-band can benefit from further extending their gain bandwidth and improving overall operation costs. This work addresses both aspects through an optimization of the host matrix using phosphorus/aluminum (P/Al) as glass modifier and secondly through the use of yttrium as an alternative co-dopant to ytterbium. Fiber samples were fabricated using the modified chemical vapor deposition (MCVD) and solution doping technique. Using a maximum amount of phosphorus consistent with a flat refractive index profile, we find the optimum alumino-phospho-silicate glass matrix. The achieved amplifier exhibits a large gain amplification ranging from 15 to 25 dB, with its peak gain occurring at 1610 nm when pumped with a total power of 1.4 W at 978 nm. The maximum noise figure was 6.3 dB, while the gain ripple within the wavelength range of 1575 to 1626 nm was 76%. Moreover, we have obtained a low level of pair-induced quenching (3+ concentration of 1.2 ×10 25 m −3 . The result provides a viable solution to the 980 nm pumping scheme in a quest to achieve cost-effective and low-noise L-band EDFAs.
- 1 January 2024
- Published by Optica Publishing Group
- p. SoW3F.6
Larger Cladding Diameter for Improved Power Conversion Efficiency in Cladding-Pumped Super L-Band Amplifiers
We compare pump power requirements of two fibers having respective cladding diameters of 125 μm and 200 μm in cladding-pumped amplifiers. The Er3+:Yb3+ co-doped alumino-phospho-silicate fibers were optimized for super L-band operation.
- 1 January 2024
- Published by Optica Publishing Group
- p. SoW3F.6
Larger Cladding Diameter for Improved Power Conversion Efficiency in Cladding-Pumped Super L-Band Amplifiers
We compare pump power requirements of two fibers having respective cladding diameters of 125 μm and 200 μm in cladding-pumped amplifiers. The Er3+:Yb3+ co-doped alumino-phospho-silicate fibers were optimized for super L-band operation.
- 13 February 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in Journal of Lightwave Technology
- Vol. 41 (14) , 4806-4814
Baria-Silica Erbium-Doped Fibers for Extended L-Band Amplification
We present baria-silica erbium-doped fibers (Ba-EDF) for extending the bandwidth of L-band EDFAs beyond 1620 nm. Using a combination of modified chemical vapor deposition (MCVD) process and solution-doping technique, we demonstrate low loss (3+ concentration of 8×10 24 m -3 . We show that the optical properties and EDFA performance are positively affected by increasing the BaO content. Namely, when we increase the BaO concentration from 1.3 to 3 mol%, we observe a reduction of pair-induced quenching that correlates with a bi-exponential luminescence decay with a dominant 15.5 ms lifetime component. Furthermore, the slight modifications of absorption/ emission coefficients point to a red-shift of the signal excited state absorption and consequently, to a moderate extension of the L-band gain to longer wavelengths (1622 nm).
- 13 February 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in Journal of Lightwave Technology
- Vol. 41 (14) , 4806-4814
Baria-Silica Erbium-Doped Fibers for Extended L-Band Amplification
We present baria-silica erbium-doped fibers (Ba-EDF) for extending the bandwidth of L-band EDFAs beyond 1620 nm. Using a combination of modified chemical vapor deposition (MCVD) process and solution-doping technique, we demonstrate low loss (3+ concentration of 8×10 24 m -3 . We show that the optical properties and EDFA performance are positively affected by increasing the BaO content. Namely, when we increase the BaO concentration from 1.3 to 3 mol%, we observe a reduction of pair-induced quenching that correlates with a bi-exponential luminescence decay with a dominant 15.5 ms lifetime component. Furthermore, the slight modifications of absorption/ emission coefficients point to a red-shift of the signal excited state absorption and consequently, to a moderate extension of the L-band gain to longer wavelengths (1622 nm).
- 1 January 2023
- Published by Optica Publishing Group
- p. SF2H.5
Analysis of Non-Saturable Absorption for Optimization of L-Band EDF Performance
Non-saturable absorption is revisited to characterize L-band EDFs, co-doped with either Yttrium or Ytterbium as de-clustering agents. Measurements in the C-band allow to evaluate erbium pair content that correlates with measured and simulated amplifier performance.
- 1 January 2023
- Published by Optica Publishing Group
- p. SF2H.5
Analysis of Non-Saturable Absorption for Optimization of L-Band EDF Performance
Non-saturable absorption is revisited to characterize L-band EDFs, co-doped with either Yttrium or Ytterbium as de-clustering agents. Measurements in the C-band allow to evaluate erbium pair content that correlates with measured and simulated amplifier performance.
- 1 January 2022
- Published by Optica Publishing Group
- Vol. 213, SF3P.7
Fabrication and Characterization of Baria-Silicate Erbium-Doped Fiber Amplifiers
We present a baria-silicate erbium-doped fiber, fabricated using solution-doping technique, with 3 mol% BaO concentration. The fiber displays a low background loss (<10 dB/km at 1200 nm) and is used in an extended L-band amplifier.
- 1 January 2022
- Published by Optica Publishing Group
- Vol. 213, SF3P.7
Fabrication and Characterization of Baria-Silicate Erbium-Doped Fiber Amplifiers
We present a baria-silicate erbium-doped fiber, fabricated using solution-doping technique, with 3 mol% BaO concentration. The fiber displays a low background loss (<10 dB/km at 1200 nm) and is used in an extended L-band amplifier.