I. I. Baranov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
I. I. Baranov has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Andrey V. Koltygin
Casting Department, National University of Science and Technology “MISiS”, Leninskiy pr. 4, 119049 Moscow, Russia
4 shared publications - Viacheslav E. Bazhenov
University of Science and Technology MISIS
4 shared publications - Anastasia Lyskovich
Casting Department, National University of Science and Technology “MISiS”, Leninskiy pr. 4, 119049 Moscow, Russia
3 shared publications - V. D. Belov
National University of Science and Technology “MISIS
3 shared publications - Andrey A. Stepashkin
Center of Composite Materials, National University of Science and Technology “MISiS”, Leninskiy Pr. 4, 119049 Moscow, Russia
2 shared publications - Mikhail V. Gorshenkov
Department of Physical Materials Science, National University of Science and Technology MISiS, 119049 Moscow, Russia
2 shared publications
Latest Publications
- Open Access
The Effect of Sc and Zr Additions on the Structure, Mechanical, and Corrosion Properties of a High Thermal Conductive Al–3%Zn–3%Ca Alloy
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3 wt% Zn–3 wt% Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to center of dendritic cell. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 h was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 water solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
Open AccessThe Effect of Sc and Zr Additions on the Structure, Mechanical, and Corrosion Properties of a High Thermal Conductive Al–3%Zn–3%Ca Alloy
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3 wt% Zn–3 wt% Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to center of dendritic cell. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 h was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 water solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
- Open Access
- 10 December 2025
- Published by MDPI AG in Preprints.org
The Effect of Sc and Zr Additions on the Structure, Mechanical, and Corrosion Properties of a High Thermal Conductive Al–3%Zn–3%Ca Alloy
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3wt%Zn–3wt%Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to dendritic cores. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 hours was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
- 10 December 2025
- Published by MDPI AG in Preprints.org
Open AccessThe Effect of Sc and Zr Additions on the Structure, Mechanical, and Corrosion Properties of a High Thermal Conductive Al–3%Zn–3%Ca Alloy
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3wt%Zn–3wt%Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to dendritic cores. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 hours was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
- 27 June 2025
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 2,p. 66-75
Structure and properties of C92900 antifriction bronze produced by upward continuous casting
Antifriction tin bronzes are used in the aerospace industry to manufacture components that operate in friction assemblies at elevated temperatures. This is due to the alloy’s favorable combination of antifriction, mechanical, and corrosion properties. In particular, tin bronze C92900 (alloy Cu–10Sn–3Ni–2Pb (wt. %)) is widely used in such applications. It is employed in the production of braking system components and plunger pump parts. Currently, these parts are manufactured by machining ingots produced through casting with directional solidification. However, this method has a low material utilization rate, typically between 5 % and 15 %. The most promising method for producing C92900 ingots is upward continuous casting technology, which allows the ingot dimensions to closely match those of the finished part. This significantly reduces machining effort and increases metal utilization to 95 %. This study presents the results of process development for the upward continuous casting technology of 15 mm diameter C92900 ingots. The structure and properties of the castings were also investigated. It was shown that as the casting speed increased from 90 to 360 mm/min, the volume fraction of the γ-Cu3Sn intermetallic phase increased, while the amount of tin-based solid solution remained nearly unchanged. At the same time, the phase distribution became more refined. The macrostructure consisted of columnar and equiaxed grains. As the casting speed increased, the columnar grains became more tilted relative to the direction of heat removal. The hardness increased from 127 ± 2.73 to 136 ± 4.25 HB, and the tensile strength and elongation slightly increased up to 250 mm/min, then decreased at 360 mm/min, which was associated with the macrostructure approaching a transcrystalline form. The study also examined shrinkage cavities and segregation defects in ingots cast at 150 mm/min and analyzed their causes. Finally, the paper provides recommendations for optimal casting parameters for 15 mm diameter ingots produced by upward continuous casting technology
- 27 June 2025
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 2,p. 66-75
Structure and properties of C92900 antifriction bronze produced by upward continuous casting
Antifriction tin bronzes are used in the aerospace industry to manufacture components that operate in friction assemblies at elevated temperatures. This is due to the alloy’s favorable combination of antifriction, mechanical, and corrosion properties. In particular, tin bronze C92900 (alloy Cu–10Sn–3Ni–2Pb (wt. %)) is widely used in such applications. It is employed in the production of braking system components and plunger pump parts. Currently, these parts are manufactured by machining ingots produced through casting with directional solidification. However, this method has a low material utilization rate, typically between 5 % and 15 %. The most promising method for producing C92900 ingots is upward continuous casting technology, which allows the ingot dimensions to closely match those of the finished part. This significantly reduces machining effort and increases metal utilization to 95 %. This study presents the results of process development for the upward continuous casting technology of 15 mm diameter C92900 ingots. The structure and properties of the castings were also investigated. It was shown that as the casting speed increased from 90 to 360 mm/min, the volume fraction of the γ-Cu3Sn intermetallic phase increased, while the amount of tin-based solid solution remained nearly unchanged. At the same time, the phase distribution became more refined. The macrostructure consisted of columnar and equiaxed grains. As the casting speed increased, the columnar grains became more tilted relative to the direction of heat removal. The hardness increased from 127 ± 2.73 to 136 ± 4.25 HB, and the tensile strength and elongation slightly increased up to 250 mm/min, then decreased at 360 mm/min, which was associated with the macrostructure approaching a transcrystalline form. The study also examined shrinkage cavities and segregation defects in ingots cast at 150 mm/min and analyzed their causes. Finally, the paper provides recommendations for optimal casting parameters for 15 mm diameter ingots produced by upward continuous casting technology
- Open Access
- 20 October 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 29 (5) , 34-46
Microstructure and properties of the GEWZ522K casting magnesium alloy based on the Mg–Gd–Nd–Y–Zn–Zr system
The article discusses the solidification and phase composition of the (wt.%) Mg–4.8Gd–2.1Nd–1.6Y–0.4Zn–0.6Zr (GEWZ522K) casting alloy. It is demonstrated that in the as-cast state, the alloy structure comprises primary zirconium particles, dendrites of the magnesium solid solution (αMg), and eutectic intermetallic phases located between dendritic branches. Following solution heat treatment at t = 530±5 °C, the alloy transitions into a single-phase state and can be significantly strengthened through artificial aging after quenching. It is recommended to apply alloy aging at t = 250 °C for 8–10 h or at t = 200 °C for 15–18 h. This approach leads to the maximum strengthening of the alloy, with the best mechanical properties achieved for the alloy aged at t = 250 °C. Regardless of the aging method used, the ultimate tensile strength (UTS) of the samples surpasses 300 MPa, which significantly exceeds that of commercial casting alloys according to GOST 2856-79. The measured corrosion rate for the GEWZ522K alloy is 7.5±0.4 mm/year, that slightly higher than that for the less alloyed commercial alloy ML10 (approximately 2.5 mm/year) tested under similar conditions. Furthermore, the alloy was subjected to tests for ignition resistance when in contact with air. It was observed that with continuous airflow over the specimen’s surface, ignition centers appear at t = 625 °C due to the breakdown of the oxide film, causing the alloy to nearly completely melt. Therefore, the GEWZ522K alloy can be employed as a high-strength casting alloy. However, during the operation of cast parts, particular attention must be paid to safeguarding the surface of these parts against corrosion.
- 20 October 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 29 (5) , 34-46
Open AccessMicrostructure and properties of the GEWZ522K casting magnesium alloy based on the Mg–Gd–Nd–Y–Zn–Zr system
The article discusses the solidification and phase composition of the (wt.%) Mg–4.8Gd–2.1Nd–1.6Y–0.4Zn–0.6Zr (GEWZ522K) casting alloy. It is demonstrated that in the as-cast state, the alloy structure comprises primary zirconium particles, dendrites of the magnesium solid solution (αMg), and eutectic intermetallic phases located between dendritic branches. Following solution heat treatment at t = 530±5 °C, the alloy transitions into a single-phase state and can be significantly strengthened through artificial aging after quenching. It is recommended to apply alloy aging at t = 250 °C for 8–10 h or at t = 200 °C for 15–18 h. This approach leads to the maximum strengthening of the alloy, with the best mechanical properties achieved for the alloy aged at t = 250 °C. Regardless of the aging method used, the ultimate tensile strength (UTS) of the samples surpasses 300 MPa, which significantly exceeds that of commercial casting alloys according to GOST 2856-79. The measured corrosion rate for the GEWZ522K alloy is 7.5±0.4 mm/year, that slightly higher than that for the less alloyed commercial alloy ML10 (approximately 2.5 mm/year) tested under similar conditions. Furthermore, the alloy was subjected to tests for ignition resistance when in contact with air. It was observed that with continuous airflow over the specimen’s surface, ignition centers appear at t = 625 °C due to the breakdown of the oxide film, causing the alloy to nearly completely melt. Therefore, the GEWZ522K alloy can be employed as a high-strength casting alloy. However, during the operation of cast parts, particular attention must be paid to safeguarding the surface of these parts against corrosion.
- Open Access
- 18 February 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 1 (1) , 39-55
Investigation of castability, mechanical, corrosion properties and flammability of ML-OPB and EWZ43 magnesium alloys
Magnesium alloys are usually considered as structural materials when the weight reduction is important - in aircraft and space industry for example. In recent years, there has been an increase in the use of new generation ignition-proof high-strength magnesium alloys in the design of aircraft parts. The properties of new ignition-proof casting magnesium alloys ML-OPB (Mg–6.7Y–2.6Zn–0.5Zr–0.35Ce– 0.35Yb; wt.%) and EWZ43 (Mg–3.8Y–4.4Nd–0.6Zr–0.6Zn; wt.%) were investigated and compared with properties of commercial magnesium alloys. The microstructure of investigated alloys in the as-cast condition comprises of a magnesium solid solution and a significant amount of eutectic. Heat treatment according to the T6 mode results in change in the eutectic phase’s morphology and also to their partial dissolution in the magnesium matrix. Long-term high-temperature holding, simulating operating conditions (500 h at 300 °C), leads to the formation of precipitates along the grain boundaries in both alloys, significantly reducing the mechanical properties. During the oxidation of the samples, it was established that the main components that involved into the oxide film and provides the protective properties of the alloys is Y, Nd and Yb. The investigated alloys have a high strength, which is not lower than that of the ML10 alloy. At the same time, the advantage of the ML-OPB alloy is a high elongation at fracture, while the EWZ43 alloy is characterized by high strength. The corrosion rate of the investigated alloys exceeds the corrosion rate of known commercial ML10 and AZ91 alloys, which implies the need for additional protection against corrosion of investigated alloys. At the same time, the castability of ML-OPB and EWZ43 alloys is no lower than that of most commercial magnesium alloys. An oxide film with high Y content and high protective properties is formed when the alloys interact with the sand mold bonded with furan resin. The ignition temperature of the investigated alloys is 100–150 °C higher than that of the ML10 alloy. The flammability test of alloys in the flame of a gas burner, made on cone samples and typical aircraft castings «bracket», showed that ML-OPB and EWZ43 alloys are almost non-flammable under the conditions of experiment.
- 18 February 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 1 (1) , 39-55
Open AccessInvestigation of castability, mechanical, corrosion properties and flammability of ML-OPB and EWZ43 magnesium alloys
Magnesium alloys are usually considered as structural materials when the weight reduction is important - in aircraft and space industry for example. In recent years, there has been an increase in the use of new generation ignition-proof high-strength magnesium alloys in the design of aircraft parts. The properties of new ignition-proof casting magnesium alloys ML-OPB (Mg–6.7Y–2.6Zn–0.5Zr–0.35Ce– 0.35Yb; wt.%) and EWZ43 (Mg–3.8Y–4.4Nd–0.6Zr–0.6Zn; wt.%) were investigated and compared with properties of commercial magnesium alloys. The microstructure of investigated alloys in the as-cast condition comprises of a magnesium solid solution and a significant amount of eutectic. Heat treatment according to the T6 mode results in change in the eutectic phase’s morphology and also to their partial dissolution in the magnesium matrix. Long-term high-temperature holding, simulating operating conditions (500 h at 300 °C), leads to the formation of precipitates along the grain boundaries in both alloys, significantly reducing the mechanical properties. During the oxidation of the samples, it was established that the main components that involved into the oxide film and provides the protective properties of the alloys is Y, Nd and Yb. The investigated alloys have a high strength, which is not lower than that of the ML10 alloy. At the same time, the advantage of the ML-OPB alloy is a high elongation at fracture, while the EWZ43 alloy is characterized by high strength. The corrosion rate of the investigated alloys exceeds the corrosion rate of known commercial ML10 and AZ91 alloys, which implies the need for additional protection against corrosion of investigated alloys. At the same time, the castability of ML-OPB and EWZ43 alloys is no lower than that of most commercial magnesium alloys. An oxide film with high Y content and high protective properties is formed when the alloys interact with the sand mold bonded with furan resin. The ignition temperature of the investigated alloys is 100–150 °C higher than that of the ML10 alloy. The flammability test of alloys in the flame of a gas burner, made on cone samples and typical aircraft castings «bracket», showed that ML-OPB and EWZ43 alloys are almost non-flammable under the conditions of experiment.