Lubomir D. Dimitrov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Lubomir D. Dimitrov has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Boris Shivachev
Institute of Mineralogy and Crystallography “Acad. Ivan Kostov”, Bulgarian Academy of Sciences, 1113 Sofia, Bulgaria
1 shared publication - Daniela Karashanova
Institute of Optical Materials and Technologies, Bulgarian Academy of Sciences, 1113 Sofia, Bulgaria
1 shared publication - Georgi Tyuliev
Institute of Catalysis, Bulgarian Academy of Sciences, 1113 Sofia, Bulgaria
1 shared publication - Konstantin Hadjiivanov
Institute of General and Inorganic Chemistry, Bulgarian Academy of Sciences, Sofia 1113, Bulgaria
1 shared publication - Květa Jirátová
Institute of Chemical Process Fundamentals, Czech Academy of Sciences, Rozvojová 135, 165 02 Prague, Czech Republic
1 shared publication - Luděk Kaluža
Institute of Chemical Process Fundamentals of the Academy of Sciences of the Czech Republic, Prague 6, Czech Republic
1 shared publication
Latest Publications
- Open Access
- 8 August 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (16) , 2278
Effect of Water on CO2 Adsorption on CaNaY Zeolite: Formation of Ca2+(H2O)(CO2), Ca2+(H2O)(CO2)2 and Ca2+(H2O)2(CO2) Complexes
Efficient CO2 capture materials must possess a high adsorption capacity, suitable CO2 adsorption enthalpy and resistance to water vapor. We have recently reported that Ca2+ cations exchanged in FAU zeolite can attach up to three CO2 molecules. Here we report the effect of water on the adsorption of CO2. Formation of Ca2+(H2O)(CO2), Ca2+(H2O)(CO2)2 and Ca2+(H2O)2(CO2) mixed ligand complexes were established. The Ca2+(H2O)(CO2) species are readily formed even at ambient temperature and are characterized by ν(12CO2) and ν(13CO2) infrared bands at 2358 and 2293 cm−1, respectively. The Ca2+(H2O)(CO2)2 species are produced at low temperature and are identified by a ν(13CO2) band at 2291 cm−1. In the presence of large amounts of water, Ca2+(H2O)2(CO2) complexes were also evidenced by ν(12CO2) and ν(13CO2) bands at 2348 and 2283 cm−1, respectively. The results demonstrate that, although it has a negative effect on CO2 adsorption uptake, water in moderate amounts does not block CO2 adsorption sites.
- 8 August 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (16) , 2278
Open AccessEffect of Water on CO2 Adsorption on CaNaY Zeolite: Formation of Ca2+(H2O)(CO2), Ca2+(H2O)(CO2)2 and Ca2+(H2O)2(CO2) Complexes
Efficient CO2 capture materials must possess a high adsorption capacity, suitable CO2 adsorption enthalpy and resistance to water vapor. We have recently reported that Ca2+ cations exchanged in FAU zeolite can attach up to three CO2 molecules. Here we report the effect of water on the adsorption of CO2. Formation of Ca2+(H2O)(CO2), Ca2+(H2O)(CO2)2 and Ca2+(H2O)2(CO2) mixed ligand complexes were established. The Ca2+(H2O)(CO2) species are readily formed even at ambient temperature and are characterized by ν(12CO2) and ν(13CO2) infrared bands at 2358 and 2293 cm−1, respectively. The Ca2+(H2O)(CO2)2 species are produced at low temperature and are identified by a ν(13CO2) band at 2291 cm−1. In the presence of large amounts of water, Ca2+(H2O)2(CO2) complexes were also evidenced by ν(12CO2) and ν(13CO2) bands at 2348 and 2283 cm−1, respectively. The results demonstrate that, although it has a negative effect on CO2 adsorption uptake, water in moderate amounts does not block CO2 adsorption sites.
- Open Access
Nanocrystalline Sulfided NiMoW Catalyst Supported on Mesoporous Aluminas for the Hydrodesulfurization of 4,6-Dimethyldibenzothiophene
Tri-metallic NiMoW catalysts prepared by impregnating mesoporous aluminas (pore sizes of ~9 nm and surface areas of ~225 m2/g) obtained by sol-gel (NiMoW/Al) and hydrothermal (NiMoW/AlHYDT) processes were investigated in the hydrodesulfurization (HDS) of thiophene and 4,6-dimethyldibenzothiophene (4,6-DMDBT) at H2 pressures of 1 MPa and 5.0 MPa, respectively. The supports and catalysts were characterized by N2 physisorption, X-ray diffraction (XRD), scanning electron microscopy (SEM), ultraviolet-visible diffuse reflectance spectroscopy (UV-Vis DRS), temperature-programmed reduction (TPR), X-ray photoelectron spectroscopy (XPS), and high-resolution transmission electron microscopy (HRTEM). The NiMoW/AlHYDT catalyst, which was the most active in both test HDS reactions, was characterized by a pore size of 7.5 nm, whereas the pore size of the catalyst on sol-gel alumina (NiMoW/Al) was only 4.8 nm. Moreover, the NiMoW/AlHYDT catalyst exhibited reduction peaks shifted to a lower temperature during TPR, indicating weaker metal support interactions, a higher degree of Mo (79%) and W (48%) sulfidation, and an optimal layer slab length distribution of Mo(W)S2 nanocrystals preferentially between 2–4 nm with an average layer stacking of 1.7 compared to the NiMoW/Al counterpart.
Open AccessNanocrystalline Sulfided NiMoW Catalyst Supported on Mesoporous Aluminas for the Hydrodesulfurization of 4,6-Dimethyldibenzothiophene
Tri-metallic NiMoW catalysts prepared by impregnating mesoporous aluminas (pore sizes of ~9 nm and surface areas of ~225 m2/g) obtained by sol-gel (NiMoW/Al) and hydrothermal (NiMoW/AlHYDT) processes were investigated in the hydrodesulfurization (HDS) of thiophene and 4,6-dimethyldibenzothiophene (4,6-DMDBT) at H2 pressures of 1 MPa and 5.0 MPa, respectively. The supports and catalysts were characterized by N2 physisorption, X-ray diffraction (XRD), scanning electron microscopy (SEM), ultraviolet-visible diffuse reflectance spectroscopy (UV-Vis DRS), temperature-programmed reduction (TPR), X-ray photoelectron spectroscopy (XPS), and high-resolution transmission electron microscopy (HRTEM). The NiMoW/AlHYDT catalyst, which was the most active in both test HDS reactions, was characterized by a pore size of 7.5 nm, whereas the pore size of the catalyst on sol-gel alumina (NiMoW/Al) was only 4.8 nm. Moreover, the NiMoW/AlHYDT catalyst exhibited reduction peaks shifted to a lower temperature during TPR, indicating weaker metal support interactions, a higher degree of Mo (79%) and W (48%) sulfidation, and an optimal layer slab length distribution of Mo(W)S2 nanocrystals preferentially between 2–4 nm with an average layer stacking of 1.7 compared to the NiMoW/Al counterpart.