Ruilong Lu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Ruilong Lu has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Jiawei Liu
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
5 shared publications - Cheng Liu
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
4 shared publications Jingtao Han
3 shared publications- Xiaoyan Ma
Guangzhou Sino Precision Steel Tube Industry Research Institute Co., Ltd., Guangzhou 511300, China
3 shared publications Cheng Liu
2 shared publications- Congfa Zhang
Beijing Institute of Spacecraft System Engineering, Beijing 100094, China
2 shared publications
Latest Publications
- Open Access
Research on Cold Roll Forming Process of Strips for Truss Rods for Space Construction
In this paper, a new technology for on-orbit cold forming of space truss rods is proposed. For the cold roll forming process of asymmetric cross sections of thin strips, the effects of roll gap and roll spacing on the forming of asymmetric cross sections of strips were investigated using ABAQUS simulation + experiments. The study shows the following. When forming a strip with a specific asymmetric cross section, the stresses are mainly concentrated in corners 2/4/6, with the largest strain value in corner 2. With increasing forming passes, when the roll gap is 0.3 mm, the maximum equivalent strain values are 0.09, 0.24, 0.64 sequentially. Roll gaps of 0.4 mm and 0.5 mm equivalent strain change amplitude are relatively similar, and their maximum equivalent strain values are approximately 0.07,0.15, 0.44. From the analysis of the stress–strain history of the characteristic nodes in corners 2/4/6, it can be seen that the stress and strain changes in the deformation process mainly occur at the moment of interaction between the upper and lower rollers, where the stress type of node 55786 shows two tensile types and one compressive type, the stress type of nodes 48594 and 15928 shows two compressive and one tensile type, and the strain of the three nodes is in accordance with the characteristics of plane strain. When the roll gap is about 0.4 mm, the forming of the strip is relatively good. With increased roll spacing, the strip in the longitudinal stress peak through the rollers shows a small incremental trend, but the peak stresses are 380 Mpa or so. When the roll spacing is 120 mm, the longitudinal strain fluctuation of the strip is the most serious, followed by the roll spacing at 100 mm, and the minimum at 140 mm. Combined with the fluctuation in strip edges under different roll spacings, manufacturing cost and volume and other factors, a roll spacing of 100 mm is more reasonable. It is experimentally verified that when the roll gap is 0.4 mm and the roll spacing is 100 mm, the strip is successfully prepared in accordance with the cross-section requirements. When the rolling gap is 0.3 mm, due to stress–strain concentration, the strip is prone to edge waves in forming. The top of corner 2 of the flange triangular region is susceptible to intermittent tear defects, and the crack extension mechanism is mainly based on the cleavage fracture + ductile fracture.
Open AccessResearch on Cold Roll Forming Process of Strips for Truss Rods for Space Construction
In this paper, a new technology for on-orbit cold forming of space truss rods is proposed. For the cold roll forming process of asymmetric cross sections of thin strips, the effects of roll gap and roll spacing on the forming of asymmetric cross sections of strips were investigated using ABAQUS simulation + experiments. The study shows the following. When forming a strip with a specific asymmetric cross section, the stresses are mainly concentrated in corners 2/4/6, with the largest strain value in corner 2. With increasing forming passes, when the roll gap is 0.3 mm, the maximum equivalent strain values are 0.09, 0.24, 0.64 sequentially. Roll gaps of 0.4 mm and 0.5 mm equivalent strain change amplitude are relatively similar, and their maximum equivalent strain values are approximately 0.07,0.15, 0.44. From the analysis of the stress–strain history of the characteristic nodes in corners 2/4/6, it can be seen that the stress and strain changes in the deformation process mainly occur at the moment of interaction between the upper and lower rollers, where the stress type of node 55786 shows two tensile types and one compressive type, the stress type of nodes 48594 and 15928 shows two compressive and one tensile type, and the strain of the three nodes is in accordance with the characteristics of plane strain. When the roll gap is about 0.4 mm, the forming of the strip is relatively good. With increased roll spacing, the strip in the longitudinal stress peak through the rollers shows a small incremental trend, but the peak stresses are 380 Mpa or so. When the roll spacing is 120 mm, the longitudinal strain fluctuation of the strip is the most serious, followed by the roll spacing at 100 mm, and the minimum at 140 mm. Combined with the fluctuation in strip edges under different roll spacings, manufacturing cost and volume and other factors, a roll spacing of 100 mm is more reasonable. It is experimentally verified that when the roll gap is 0.4 mm and the roll spacing is 100 mm, the strip is successfully prepared in accordance with the cross-section requirements. When the rolling gap is 0.3 mm, due to stress–strain concentration, the strip is prone to edge waves in forming. The top of corner 2 of the flange triangular region is susceptible to intermittent tear defects, and the crack extension mechanism is mainly based on the cleavage fracture + ductile fracture.
- Open Access
Study of the Mechanical Properties and Microstructure of Spiral Tubes and Actuators for Controlled Extension Fabricated with Beryllium Bronze Strips
QBe2.0 strips were used to fabricate spiral tubes and actuators for controlled extension (STACERs) through the winding and stabilization method, which is a novel technique for obtaining STACERs. The raw strips and the STACERs were investigated using tensile tests and SEM for the mechanical properties and fractography observation, employing specialized test equipment for service performance, and via XRD, EBSD, and TEM were used to test the residual stress and microstructure evolution. The tensile strength/elongation for raw strips was 485.8 MPa/60%, while for STACERs, tensile strength increased by 834.67 MPa to 646 MPa, and the elongation rate decreased by 12% to 19.3%. The fractography showed that the fracture mode was ductile. The service performance tests indicated that STACERs obtained under 320 °C had a higher driving force, good pointing accuracy, and high bending stiffness, while the residual stress of raw strips was τxy = −6 MPa; for STACERs obtained between 290 °C and 350 °C, τxy decreased from −5 MPa to −74 MPa, then increased from −74 MPa to 21 MPa, and the optimum fabricating parameter was 320 °C + 2 h. The EBSD results showed that LABs and HABs for raw strips and STACERs at 320 °C + 2 h accounted for 3–97% and 24.5–75.5%, the grain sizes were 7.07 μm and 3.67 μm, and the twin fraction decreased from 57.3% to 31.8%, respectively. The KAM and Schmid factor maps indicated that the STACER was prone to recovering and recrystallizing. Coupled with the EBSD results, the TEM results indicated that the strengthening mechanism for raw strips is twinning strengthening, while that for STACER is grain-refining strengthening with a precipitation of the γ″ phase. It is a meaningful novelty that the relationship between the macro properties and microstructure has been elucidated.
Open AccessStudy of the Mechanical Properties and Microstructure of Spiral Tubes and Actuators for Controlled Extension Fabricated with Beryllium Bronze Strips
QBe2.0 strips were used to fabricate spiral tubes and actuators for controlled extension (STACERs) through the winding and stabilization method, which is a novel technique for obtaining STACERs. The raw strips and the STACERs were investigated using tensile tests and SEM for the mechanical properties and fractography observation, employing specialized test equipment for service performance, and via XRD, EBSD, and TEM were used to test the residual stress and microstructure evolution. The tensile strength/elongation for raw strips was 485.8 MPa/60%, while for STACERs, tensile strength increased by 834.67 MPa to 646 MPa, and the elongation rate decreased by 12% to 19.3%. The fractography showed that the fracture mode was ductile. The service performance tests indicated that STACERs obtained under 320 °C had a higher driving force, good pointing accuracy, and high bending stiffness, while the residual stress of raw strips was τxy = −6 MPa; for STACERs obtained between 290 °C and 350 °C, τxy decreased from −5 MPa to −74 MPa, then increased from −74 MPa to 21 MPa, and the optimum fabricating parameter was 320 °C + 2 h. The EBSD results showed that LABs and HABs for raw strips and STACERs at 320 °C + 2 h accounted for 3–97% and 24.5–75.5%, the grain sizes were 7.07 μm and 3.67 μm, and the twin fraction decreased from 57.3% to 31.8%, respectively. The KAM and Schmid factor maps indicated that the STACER was prone to recovering and recrystallizing. Coupled with the EBSD results, the TEM results indicated that the strengthening mechanism for raw strips is twinning strengthening, while that for STACER is grain-refining strengthening with a precipitation of the γ″ phase. It is a meaningful novelty that the relationship between the macro properties and microstructure has been elucidated.
- Open Access
Numerical Study of Ti6Al4V Alloy Tube Heated by Super-Frequency Induction Heating
Ti6Al4V alloys have a narrow processing window, which complicates temperature control, especially during large-scale production. Therefore, a numerical simulation and experimental study on the ultrasonic induction heating process of a Ti6Al4V titanium alloy tube were conducted to obtain stable heating. The electromagnetic and thermal fields in the process of ultrasonic frequency induction heating were calculated. The effects of the current frequency and current value on the thermal and current fields were numerically analyzed. The increase in current frequency enhances the skin and edge effects, but heat permeability was achieved in the super audio frequency range, and the temperature difference between the interior and exterior of the tube was less than 1%. An increase in the applied current value and current frequency caused an increase in the tube’s temperature, but the influence of current was more prominent. Therefore, the influence of stepwise feeding, reciprocating motion, and stepwise feeding superimposed motion on the heating temperature field of the tube blank was evaluated. The coil reciprocating with the roll can maintain the temperature of the tube within the target temperature range during the deformation stage. The simulation results were validated experimentally, which demonstrated good agreement between the results. The numerical simulation method can be used to monitor the temperature distribution of Ti6Al4V alloy tubes during the super-frequency induction heating process. This is an economical and effective tool for predicting the induction heating process of Ti6Al4V alloy tubes. Moreover, online induction heating in the form of reciprocating motion is a feasible strategy for processing Ti6Al4V alloy tubes.
Open AccessNumerical Study of Ti6Al4V Alloy Tube Heated by Super-Frequency Induction Heating
Ti6Al4V alloys have a narrow processing window, which complicates temperature control, especially during large-scale production. Therefore, a numerical simulation and experimental study on the ultrasonic induction heating process of a Ti6Al4V titanium alloy tube were conducted to obtain stable heating. The electromagnetic and thermal fields in the process of ultrasonic frequency induction heating were calculated. The effects of the current frequency and current value on the thermal and current fields were numerically analyzed. The increase in current frequency enhances the skin and edge effects, but heat permeability was achieved in the super audio frequency range, and the temperature difference between the interior and exterior of the tube was less than 1%. An increase in the applied current value and current frequency caused an increase in the tube’s temperature, but the influence of current was more prominent. Therefore, the influence of stepwise feeding, reciprocating motion, and stepwise feeding superimposed motion on the heating temperature field of the tube blank was evaluated. The coil reciprocating with the roll can maintain the temperature of the tube within the target temperature range during the deformation stage. The simulation results were validated experimentally, which demonstrated good agreement between the results. The numerical simulation method can be used to monitor the temperature distribution of Ti6Al4V alloy tubes during the super-frequency induction heating process. This is an economical and effective tool for predicting the induction heating process of Ti6Al4V alloy tubes. Moreover, online induction heating in the form of reciprocating motion is a feasible strategy for processing Ti6Al4V alloy tubes.
- Open Access
Investigation of the Mechanical Properties and Microstructure of the Co40NiCrMo Alloy Used for STACERs and Prepared by the CSPB Process and the Winding and Stabilization Method
The Co40NiCrMo alloy, used for STACERs fabricated by the CSPB (compositing stretch and press bending) process (cold forming) and the winding and stabilization (winding and heat treatment) method, was investigated with regard to its tensile property, residual stress, and microstructure. The Co40NiCrMo STACER prepared by the winding and stabilization method was strengthened with lower ductility (tensile strength/elongation: 1562 MPa/5%) compared to that prepared by CSPB (tensile strength/elongation: 1469 MPa/20.4%). The residual stress of the STACER prepared by winding and stabilization (τxy = −137 MPa) showed consistency with that obtained through CSPB (τxy = −131 MPa). Combined with the driving force and pointing accuracy performances, the optimum heat treatment parameters for the winding and stabilization method were determined as 520 °C + 4 h. The HABs in the winding and stabilization STACER (98.3%, of which 69.1% were Σ3 boundaries) were much higher than those in the CSPB STACER (34.6%, of which 19.2% were Σ3 boundaries), while deformation twins and h.c.p ε-platelet networks were present in the CSPB STACER, and many more annealing twins appeared in the winding and stabilization STACER. It was concluded that the strengthening mechanism in the CSPB STACER is the combined action of deformation twins and h.c.p ε-platelet networks, while for the winding and stabilization STACER, annealing twins play the dominant role.
Open AccessInvestigation of the Mechanical Properties and Microstructure of the Co40NiCrMo Alloy Used for STACERs and Prepared by the CSPB Process and the Winding and Stabilization Method
The Co40NiCrMo alloy, used for STACERs fabricated by the CSPB (compositing stretch and press bending) process (cold forming) and the winding and stabilization (winding and heat treatment) method, was investigated with regard to its tensile property, residual stress, and microstructure. The Co40NiCrMo STACER prepared by the winding and stabilization method was strengthened with lower ductility (tensile strength/elongation: 1562 MPa/5%) compared to that prepared by CSPB (tensile strength/elongation: 1469 MPa/20.4%). The residual stress of the STACER prepared by winding and stabilization (τxy = −137 MPa) showed consistency with that obtained through CSPB (τxy = −131 MPa). Combined with the driving force and pointing accuracy performances, the optimum heat treatment parameters for the winding and stabilization method were determined as 520 °C + 4 h. The HABs in the winding and stabilization STACER (98.3%, of which 69.1% were Σ3 boundaries) were much higher than those in the CSPB STACER (34.6%, of which 19.2% were Σ3 boundaries), while deformation twins and h.c.p ε-platelet networks were present in the CSPB STACER, and many more annealing twins appeared in the winding and stabilization STACER. It was concluded that the strengthening mechanism in the CSPB STACER is the combined action of deformation twins and h.c.p ε-platelet networks, while for the winding and stabilization STACER, annealing twins play the dominant role.
- Open Access
- 1 April 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (4) , 046516
Effect of abrasive water pressure on the surface layer characteristics of duplex stainless steel 2205
The martensitic stainless steel shot with a high number of cycles was applied to the abrasive water jet (AWJ) to study the effect of jet pressures on the surface layer characteristics of 2205 duplex stainless steel. The Almen strips (type A) quantitatively evaluate the AWJ intensity at jet pressures of 50 MPa, 60 MPa, and 70 MPa. The surface layer characteristics were comprehensively studied using scanning electron microscopy, laser scanning confocal microscopy, x-ray diffraction, electron backscatter diffraction techniques, and microhardness tester. It was found that with the increase of the jet pressure from 50 MPa to 60 MPa and 70 MPa, the AWJ intensity increased by 5.0% and 22% and the surface roughness for Ra increased by 16% and 37%. Residual compressive stresses existed in both phases to a depth of more than 200 μm. The austenite hardening rate is higher than that of ferrite, and the maximum residual compressive stress in austenite of the surface layer of the AWJ specimen occurred at the subsurface. The maximum residual compressive stress in ferrite occurred at the surface (50 MPa, 60 MPa) and subsurface (70 MPa). The hetero-deformation induced stresses formed during the plastic deformation of the heterostructured material made the austenitic residual compressive stresses in the surface layer slightly higher than those in ferrite. The surface grain refinement depth exceeded 150 μm, and the degree of austenite grain refinement was higher than that of ferrite. The fraction of deformation-induced martensite and the depth of phase transformation increased with the increase of jet pressure. These changes caused the surface hardening of the specimen, and the jet pressure had a significant effect on the depth of the hardened layer and the microhardness at depth greater than 50 μm.
- 1 April 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (4) , 046516
Open AccessEffect of abrasive water pressure on the surface layer characteristics of duplex stainless steel 2205
The martensitic stainless steel shot with a high number of cycles was applied to the abrasive water jet (AWJ) to study the effect of jet pressures on the surface layer characteristics of 2205 duplex stainless steel. The Almen strips (type A) quantitatively evaluate the AWJ intensity at jet pressures of 50 MPa, 60 MPa, and 70 MPa. The surface layer characteristics were comprehensively studied using scanning electron microscopy, laser scanning confocal microscopy, x-ray diffraction, electron backscatter diffraction techniques, and microhardness tester. It was found that with the increase of the jet pressure from 50 MPa to 60 MPa and 70 MPa, the AWJ intensity increased by 5.0% and 22% and the surface roughness for Ra increased by 16% and 37%. Residual compressive stresses existed in both phases to a depth of more than 200 μm. The austenite hardening rate is higher than that of ferrite, and the maximum residual compressive stress in austenite of the surface layer of the AWJ specimen occurred at the subsurface. The maximum residual compressive stress in ferrite occurred at the surface (50 MPa, 60 MPa) and subsurface (70 MPa). The hetero-deformation induced stresses formed during the plastic deformation of the heterostructured material made the austenitic residual compressive stresses in the surface layer slightly higher than those in ferrite. The surface grain refinement depth exceeded 150 μm, and the degree of austenite grain refinement was higher than that of ferrite. The fraction of deformation-induced martensite and the depth of phase transformation increased with the increase of jet pressure. These changes caused the surface hardening of the specimen, and the jet pressure had a significant effect on the depth of the hardened layer and the microhardness at depth greater than 50 μm.
- 22 March 2023
- Published by Elsevier in Materials Today Communications
- Vol. 35
Surface layer characterization of 2205 duplex stainless steel subjected to abrasive water jet descaling
- 22 March 2023
- Published by Elsevier in Materials Today Communications
- Vol. 35