Antônio Alves de Carvalho Jr.
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Antônio Alves de Carvalho Jr. has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- José Milton Elias de Matos
Department of Chemistry, Chemistry Postgraduate Program, Federal University of Piauí, Teresina, Piauí 64049-550, Brazil
2 shared publications - Kelson de Sousa Leite
Ceramic Materials Laboratory, Federal Institute of Education, Science, and Technology of Piauí—IFPI, Av. Pedro Freitas, 1020-São Pedro, Teresina 64019-368, PI, Brazil
2 shared publications - Paulo Ronaldo Sousa Teixeira
Ceramic Materials Laboratory, Federal Institute of Education, Science, and Technology of Piauí—IFPI, Av. Pedro Freitas, 1020-São Pedro, Teresina 64019-368, PI, Brazil
1 shared publication
Latest Publications
- Open Access
- 29 May 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (11) , 8743
Cashew Nut Shell Liquid as an Anticorrosive Agent in Ceramic Materials
One of the significant challenges of the ceramics industry is to increase the corrosion resistance of ceramic materials, and the study of this corrosion requires a detailed investigation using several characterization methods, such as the knowledge of technological properties including the absorption, apparent porosity, and mechanical resistance of these ceramic materials. This corrosion resistance can be further improved by using a protective coating on the surface of ceramic materials, such as cashew nut shell liquid (CNSL), which has been used as a green, environmentally friendly corrosion inhibitor. This work investigated the inhibitory action of CNSL on the corrosion of ceramic materials. Clay from the Brazilian Northeast was used in a simulated seawater environment at room temperature for the immersion corrosion test. Sets of prismatic specimens bathed in CNSL were immersed in a corrosive solution and compared with other samples without CNSL immersed in a corrosive environment. At the end of 70 days in corrosive solution, the ceramic specimens without CNSL showed signs of wear on the surface, associated with an average mass loss of 20 mg and an average corrosive rate of 0.017 mm/year. On the other hand, the bodies bathed in CNSL showed no mass loss, reinforcing the potential of CNSL as a protective agent against corrosion.
- 29 May 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (11) , 8743
Open AccessCashew Nut Shell Liquid as an Anticorrosive Agent in Ceramic Materials
One of the significant challenges of the ceramics industry is to increase the corrosion resistance of ceramic materials, and the study of this corrosion requires a detailed investigation using several characterization methods, such as the knowledge of technological properties including the absorption, apparent porosity, and mechanical resistance of these ceramic materials. This corrosion resistance can be further improved by using a protective coating on the surface of ceramic materials, such as cashew nut shell liquid (CNSL), which has been used as a green, environmentally friendly corrosion inhibitor. This work investigated the inhibitory action of CNSL on the corrosion of ceramic materials. Clay from the Brazilian Northeast was used in a simulated seawater environment at room temperature for the immersion corrosion test. Sets of prismatic specimens bathed in CNSL were immersed in a corrosive solution and compared with other samples without CNSL immersed in a corrosive environment. At the end of 70 days in corrosive solution, the ceramic specimens without CNSL showed signs of wear on the surface, associated with an average mass loss of 20 mg and an average corrosive rate of 0.017 mm/year. On the other hand, the bodies bathed in CNSL showed no mass loss, reinforcing the potential of CNSL as a protective agent against corrosion.
- Open Access
Viability of Morisca Powder Tailings for Ceramic Applications
In Juazeiro de Piauí and Castelo do Piauí, two cities in northeast Brazil, mined morisca rock is widely used in civil construction for external coating applications. Aiming at a sustainable practice for its extraction, which includes the economical use of the tailings from its mining, this work presents a solution for the use of discarded materials from processing morisca from Piauí. In this context, an analysis of the results of using morisca as a substitute for clay materials for applications in red ceramics are presented. For the analyses, XRF, XRD, microgranulometry, limits of consistency, TG, DTG, and a set of technological tests inherent to ceramic materials were used. It was concluded that morisca powder is viable as a clay substitute for red ceramic applications.
Open AccessViability of Morisca Powder Tailings for Ceramic Applications
In Juazeiro de Piauí and Castelo do Piauí, two cities in northeast Brazil, mined morisca rock is widely used in civil construction for external coating applications. Aiming at a sustainable practice for its extraction, which includes the economical use of the tailings from its mining, this work presents a solution for the use of discarded materials from processing morisca from Piauí. In this context, an analysis of the results of using morisca as a substitute for clay materials for applications in red ceramics are presented. For the analyses, XRF, XRD, microgranulometry, limits of consistency, TG, DTG, and a set of technological tests inherent to ceramic materials were used. It was concluded that morisca powder is viable as a clay substitute for red ceramic applications.